Home >> Application >> By Standard >> ASTM >> ASTM E-F >> ASTM F2009 Axial Disassembly Force Testing for Modular Prosthesis Tapers

ASTM F2009 Axial Disassembly Force Testing for Modular Prosthesis Tapers

Share:

ASTM F2009 Taper Connection Axial Disassembly Force Tester | UnitedTest

UnitedTest manufactures ASTM F2009 testing machines to measure axial tensile disassembly force of self-locking modular taper connections for hip and shoulder prostheses under controlled 2 kN preload, supporting orthopedic implant validation, product qualification and preclinical mechanical evaluation.


ASTM F2009-25 is a comparative laboratory test method that measures the axial tensile force required to pull apart a self-locking modular taper (cone/bore) connection of a hip or shoulder prosthesis after that connection has been assembled under a tightly controlled 2 kN axial preload. This test assesses the locking stability of taper junctions, helping implant engineers verify connection security, prevent unintended separation, and meet orthopedic medical device regulatory requirements. It applies to modular femoral heads, humeral components and other taper-type prosthetic junctions for total and partial joint replacement systems.


Test principle:

The test measures the axial locking strength of self-locking taper connections in modular orthopedic prostheses. After controlled assembly of the male taper (cone/trunnion) and female taper (bore/head), a controlled axial tensile force is applied to pull the components apart. The maximum force required to fully disassemble the taper junction is recorded as the primary outcome.

This method provides a simplified, repeatable model for comparing locking performance across different implant designs and material combinations, rather than replicating the full complexity of in vivo or surgical loading conditions.


Test Specimen info: 

  • Specimen type: May be finished implant components or simplified test specimens; taper geometry, material, and surface finish must match the specifications of final production implants, preferably manufactured with the same equipment.

  • Support structure: Material surrounding the female taper bore must be similar in size and shape to the finished implant.

  • Group consistency: Modular heads of identical material, outer diameter, height, and eccentricity must be used across all test groups, unless deviation is justified.

  • Sample size: A minimum of 5 taper assemblies per test group, with random component pairing unless otherwise documented.


Test Equipment for ASTM F2009 Axial Disassembly Force Testing for Modular Prosthesis Tapers

Universal testing machine

Must conform to ASTM E4, capable of delivering both compressive (assembly) and tensile (disassembly) forces at either constant displacement rate or constant loading rate; 

with continuous force and displacement monitoring.

Assembly fixtures

Preferred: Flat plate force applicator paired with a planar thrust roller bearing (X-Y bearing) to allow off-axis translation and ensure axial alignment. 

Lubrication may be used between plate and head if no bearing is installed.

Alternative: Cone-type assembly fixture (consistent with ISO 7206-10), but flat plate is recommended for lower data variability.

Disassembly fixtures

Metal cage fixture that provides even contact around the inferior edge of the modular head.

Universal joints installed on both the cage side and trunnion side to minimize misalignment and off-axis loading.

Alignment requirements

The central axis of force application must be aligned within ±1° inclination of the male taper axis and within ±0.3 mm offset of the modular head center.


Test parameters

Assembly peak static force2.0 ± 0.1 kN (2 kN nominal), along long axis of bore
Assembly, displacement control0.04 ± 0.01 mm/s
Assembly, force control (alternative)0.5 ± 0.1 kN/s
Disassembly, displacement control0.04 ± 0.02 mm/s
Disassembly, force control (alternative)20 ± 5 N/s
Alignment inclination≤ ±1° to male cone axis
Lateral offset≤ ±0.3 mm from head center
Test terminationForce drops below 100 N or 1 mm displacement at the taper junction
Minimum sample size5 taper assemblies; random pairing unless otherwise reported
Cleaning1 % detergent ultrasonic 15 min; distilled-water ultrasonic 5 min; air dry at room temperature
Informative drop-weight assembly907 g dropped 254 mm ≈ 2.26 J potential energy


Test Procedures of ASTM F2009 Axial Disassembly Force Testing for Modular Prosthesis Tapers

Step 1: Specimen Preparation

Clean all taper components following the standard cleaning protocol (Appendix X1): tap water rinse, ultrasonic cleaning in 1% detergent solution, distilled water rinses, and air drying at room temperature to remove surface contaminants. Document all specimen geometric and material properties.

Step 2: Taper Assembly

Mount the male and female taper components in the assembly fixture on the testing machine. Apply axial compressive force at the specified constant rate until the 2.0 ± 0.1 kN peak assembly force is reached. The same assembly fixture type must be used for all tests in a comparative study.

Step 3: Taper Disassembly

Transfer the assembled taper pair to the disassembly cage fixture with universal joints on both ends. Apply axial tensile load at the specified rate while continuously recording force and displacement data. Ensure no artificial hoop stress or bending moment is introduced to the junction.

Step 4: Test Termination & Data Reporting

Stop the test when taper dissociation is confirmed. Record the maximum disassembly force for each specimen, and calculate the average, range, and standard deviation for the test group. The final report must include force-displacement curves, fixture descriptions, cleaning method details, and specimen characterization data.

ASTM F2009 Axial Disassembly Force Testing for Modular Prosthesis Tapers


Industrial‑Field Application

Orthopaedic implant / arthroplasty industry — design verification and comparative evaluation of modular hip (femoral head on stem trunnion) and modular shoulder (humeral head, eccentric heads, glenospheres) prostheses.

Materials & manufacturing — comparing metal and ceramic heads (CoCr, Ti alloys, alumina/ZTA ceramics) on metal tapers, taper angles, surface finishes, coatings, tolerances, and the effect of manufacturing equipment/change-of-process; supplier qualification and lot-to-lot consistency.

Regulatory & premarket — test evidence for FDA 510(k)/PMA declarations of conformity (F2009-25 is fully recognized) and for design-control / risk-management files; third-party testing laboratories routinely offer F2009 alongside ISO 7206-10 .

Durability & failure analysis — post-fatigue disassembly of potted stems, repeated-assembly degradation, and investigation of trunnionosis / head dissociation retrieval cases 


Related Standard: 

ASTM F1800

Standard practice for cyclic fatigue testing of metal tibial tray components of total knee joint replacements

ASTM F1875Long-term fretting corrosion of hip head-bore/cone taper junctions under cyclic loading in a corrosive environment.
ISO 7206-10

Determination of resistance to static load of modular femoral heads (used for the burst test)

ASTM F3210Fatigue testing for knee femoral components
ASTM F2777endurance test for polyethylene tibial inserts.
ASTM F2009axial disassembly (pull-off) force of taper connections of modular prostheses
ISO 7206-13torque/head-fixation (torsion) test of the head–stem taper 
ISO 11491impact resistance of ceramic femoral heads
ISO 7206-4 / ISO 7206-6

endurance of stemmed femoral components and of the neck region; ASTM F2580 for modular proximally fixed stems; 

ASTM F2068 is the US analogue of ISO 7206-4 

ASTM F1820 Disassembly forces of modular acetabular shell/liner: axial push-out, offset pull-out/lever-out, torque-out (2,000 N assembly)
ASTM F2580Fatigue of modular connections in proximally fixed femoral hip stems
ASTM F2345

Standard Test Methods for Determination of Cyclic Fatigue Strength of Ceramic Modular Femoral Heads

ASTM F1264Standard specification and test methods for intramedullary fixation devices
ASTM F2582Dynamic impingement between femoral and acetabular hip components


Keywords: ASTM F2009,axial disassembly force tester,modular prosthesis taper connection test,hip prosthesis taper test,shoulder implant taper disassembly test,orthopedic implant mechanical testing,taper junction stability test,prosthetic taper pull-out force test,medical implant validation equipment,arthroplasty component testing,orthopedic preclinical test machine,modular taper connection tester,implant assembly force test,UnitedTest orthopedic tester,medical device mechanical test equipment

Related products and device

ASTM F2345 intramedullary fixation device tester

Electronic Fatigue Testing Machine designed for long-term cyclic load testing of metals, composites, and structural components, offering precise electronic control, repeatable results, and compliance with industrial standards.

ASTM F2009-25 Axial Disassembly Force Testing Machine

Spinal Implant Constructs nail screw static and fatigue testing machine used to check the fatigue failure of medical nail, Loads are typically applied in a constant-amplitude, load-controlled sinusoidal waveform that runs more than 5 million times.

Modular Taper Pull-Off Tester for ASTM F2009-25 Hip and Shoulder Prostheses

Hydraulic fatigue dynamic testing machine mainly used at a variety of material and components, parts for both dynamic and static mechanical property testing, include tension, compression, low cycling test, match with high-low temperature chamber can execute the temperature test.

ASTM F2009 Flat Plate Assembly Fixture and Planar Thrust Bearing

Electronic Dynamic Universal Testing Machine/ Cyclic Testing Equipment widely used at material and components, parts dynamic mechanical property test, include tension, compression, low cycling test, match with high-low temperature chamber can execute the temperature test.

ASTM F2009 Disassembly Cage and Universal Joint Alignment

UnitedTest universal testing machine with various test fixture, like peel, flexure, puncture, tear, pneumatic grip, belt tension etc., can be used to almost all materials include but not limited to steel rod, rubber, steel wire, plastic, seat belt, textile, wood, panel etc., mechanical performance inspection.

UnitedTest UTM Configuration for ASTM F2009 Testing

The four point bending flexural test provides values for the modulus of elasticity in bending, flexural stress ,flexural strain and the flexural stress-strain response of the material. This test is very similar to the three point bending flexural test.

ASTM F2009,axial disassembly force tester

3 points bending grip used to measure the flexural modulus or flexural strength of a plastic material, conform with stanard ASTM D790, ISO 178.

modular prosthesis taper connection test

Torsion tester is mainly used to execute torsion test for various kinds materials, manual loading, high accuracy torsion transducer to measure torque, photoelectric encoder to measure torsion angle, digital display test result. Easy to operate and with budgetary price, most suitable for research institute and colleague, factory laboratory etc. to check the torsion character of different materials.

Related Standard

ISO 7206-10 Femoral Head Static Compression and Tensile test –

ISO 7206-10: Implants for surgery --Partial and total hip joint prostheses -- Part 10: Determination of resistance to static load of modular femoral heads. 


It specifies a method for determining the static load resistance of the connection between a modular femoral head and a tapered cone of a femoral stem (the "head/cone junction") in hip joint prostheses. Include static compression (fracture) and tensile (disassembly) tests to quantify the load capacity of modular femoral heads with conical taper (Morse taper) connections. 


ASTM F1717 Spinal Implant Constructs Test –

ASTM F1717 Standard Test Methods for Spinal Implant Constructs in a Vertebrectomy Modelis a fundamental standard for evaluating the static and fatigue mechanical performance of spinal implant assemblies. Unlike ISO 12189, which focuses on a single device(an interbody cage), ASTM F1717 tests the entire posterior spinal construct—typically rods, screws, and cross-connectors—stabilizing a segment where a vertebral body has been removed (a "vertebrectomy" or "corpectomy" model). It simulates worst-case spinal instability to assess the implant's ability to maintain alignment and support loads.

ASTM F382 Metallic Bone Plates fatigue bending test –

ASTM F382 Standard Specification and Test Method for Metallic Bone Plates

ASTM F382 unified terminology, geometric classification, material requirements, marking & packaging rules, and mechanical test protocols for metallic bone plates used in surgical skeletal internal‑fixation. It define two mandatory test methods:  Single‑Cycle Bend Test and Bending Fatigue Test. Both adopt four‑point bending configuration. It is of great significance for ensuring the safety and reliability of metallic bone plates, which are widely used to align and fix bone segments in orthopedic reconstructive surgeries. 

ASTM F1798 Spinal Implant Subassembly Static and Fatigue Testing System –

ASTM F1798 Standard Test Method for Evaluating the Static and Fatigue Properties of Interconnection Mechanisms and Subassemblies Used in Spinal Arthrodesis Implants.

ASTM F1798 provides standardized methods for mechanically testing the interconnections within spinal implant systems. It is for evaluating the uniaxial static/fatigue strength and loosening resistance of interconnection mechanisms in spinal arthrodesis implant subassemblies, providing a standardized way to characterize mechanical performance of connections like rod-clamp, screw-rod, and hook-rod assemblies. It is critical for design validation, regulatory compliance, and clinical safety in the spinal implant industry.

ASTM F2706 Fatigue Static Test of Spinal implant constructs –

ASTM F2706 is a critical biomechanical evaluation tool in the medical device industry, specifically for spinal implants. ASTM F2706 establishes standardized mechanical test methods to evaluate the static (strength) and fatigue (long-term durability) performance of spinal implant assemblies intended for use in the occipito-cervical (OC) and cervico-thoracic (CT) regions (from the skull to the upper back). It simulates a worst-case scenario: a complete vertebrectomy (removal of a vertebra), creating a highly unstable spine segment that the implant must stabilize.

ASTM F2706 establishes standardized mechanical test methods to evaluate the static (strength) and fatigue (long-term durability) performance test, defines in‑vitro mechanical test protocols for posterior occipital‑cervical (OC) and occipital‑cervical‑thoracic (OCT) spinal fixation assemblies under a vertebrectomy worst‑case model, aiming for relative mechanical comparison of implant designs, rather than defining pass‑fail performance thresholds. 


ASTM F1264 Intramedullary Fixation Device Torsion & Bend Fatigue Test –

ASTM F1264 Standard Specification and Test Methods for Intramedullary Fixation Devices

ASTM F1264 is a standard specification used to describe the design and mechanical function of intramedullary fixation devices (IMFDs). It establishes terminology, classification, material, marking‑labeling requirements and four mandatory‑annex mechanical test methods for intramedullary nails/rods used in skeletal fracture fixation. It does not define mandatory clinical performance thresholds; tests deliver comparative mechanical data rather than absolute clinical pass‑fail criteria.

it also includes four standard testing methods: 

1, static four point bending test method (Annex A1), 

2, static torsion test method (Annex A2), 

3, bending fatigue test method (Annex A3), 

4, bending fatigue test method for IMFD locking screws (Annex A4). 


The UTDS series Dynamic/Fatigue Testing machine used for bone needle,  bending intramedullary nail fatigue test is mainly used for biomechanical performance testing of various materials, including artificial blood vessels, soft tissues, bones, bone plates, and vertebrae Interfusion device, knee joint, spine Dynamic and static mechanical tests on materials such as column fixators, metal coatings, hip joints, and intramedullary nails, including tension, compression, bending, and torsion.

ISO 7206-4, ISO 7206-6: Fatigue testing of femoral stem and femoral neck of hip prostheses –

ISO 7206‑4 and ISO 7206‑6 are key international standards defining fatigue endurance tests for stemmed femoral components of partial and total hip joint prostheses. ISO 7206‑4 evaluates the femoral stem under simulated proximal loosening; ISO 7206‑6 evaluates the femoral neck under well‑fixed, normal in‑vivo loading. 

ISO 7206-8 Hip Joint Replacement Torsion Testing, endurance properties of stemmed femoral components –

ISO 7206-8: Implants for surgery -- Partial and total hip joint prostheses -- Part 8: Endurance performance of stemmed femoral components with application of torsion. 


ISO 7206-8 standard as a series of test methods capable of effectively evaluating the endurance performance of stemmed femoral components designed for total and partial hip joint prosthesis. The standard allows experts to subject test specimens to loading conditions that mirror those seen in real conditions when patients use their hip joint prosthesis. The standard’s objective is to determine if hip implants perform as expected, ensuring their functionality and safety will be reliable for the patients who depend on them.


​ASTM F2009 Axial Disassembly Force Testing: Frequently Asked Questions (FAQs)

Q1: What is ASTM F2009?

A: ASTM F2009 is the standard test method for determining the axial disassembly force of taper connections in modular orthopedic prostheses. It provides a standardized laboratory procedure to measure how much axial tensile force is required to pull apart self-locking taper junctions, such as those used in hip and shoulder implant systems.


Q2: Why is the ASTM F2009 test important?

A: The test is critical because taper junction dissociation is a known failure mode in modular orthopedic implants. Unintended in vivo disassembly can cause severe pain, implant dysfunction, and revision surgery. ASTM F2009 provides a quantitative, repeatable method to evaluate locking strength, enabling manufacturers to optimize designs, select appropriate materials, and ensure implant safety before clinical use.


Q3: Which industries and applications use ASTM F2009?

A: The test is primarily used in the orthopedic medical device industry. It applies to modular total/partial hip prostheses (femoral head-to-stem connections) and modular shoulder prostheses (humeral head-to-base connections). It is used for design verification, material selection, quality control, regulatory submissions, and third-party laboratory testing.


Q4: What assembly force is specified in ASTM F2009?

A: The standard specifies a peak static assembly force of 2.0 ± 0.1 kN applied along the taper axis. This can be delivered either at a constant displacement rate of 0.04 ± 0.01 mm/s or at a constant loading rate of 0.5 ± 0.1 kN/s.


Q5: What is the disassembly loading rate in ASTM F2009?

A: Disassembly may be performed in displacement control at 0.04 ± 0.02 mm/s, or in force control at 20 ± 5 N/s. Force and displacement must be recorded continuously throughout the test.


Q6: When is the test considered complete?

A: Testing terminates when dissociation is evident, defined as either the measured force dropping below 100 N or when 1 mm of displacement occurs at the taper junction.


Q7: What are the alignment requirements in ASTM F2009?

A: The force application axis must be aligned within ±1° of the male taper axis and within ±0.3 mm offset from the modular head center. Universal joints are required on both sides of the test setup to minimize misalignment and off-axis loading during disassembly.


Q8: How many specimens are required for ASTM F2009?

A: A minimum of five taper assemblies per test group must be tested. Component pairing should be random unless otherwise documented and justified in the report.


Q9: Can finished implants be used as test specimens?

A: Yes. Specimens may be finished implant components or simplified test specimens, but the taper geometry, material, and surface finish must match production specifications. Ideally, they should be manufactured using the same equipment as production parts.


Q10: How does ASTM F2009 relate to ISO 7206-10?

A: ISO 7206-10 defines a cone-type assembly fixture for taper testing, which ASTM F2009 acknowledges as an acceptable alternative. However, ASTM F2009 recommends a flat plate fixture for superior repeatability. Results from different assembly methods should not be directly compared.


Q11. Why is it important for the material or surface, not just the finished implant?

A. The result is an interface property. Changing head material, taper angle mismatch, roughness, hardness, coating, lubrication or contamination can change the pull-off force even when the same alloy is used. That is why F2009-25 requires pre-test characterization of bore/cone diameters, taper angle, roughness, circularity, straightness, concentricity, engagement length, hardness and head geometry. Random pairing, identical head geometry across groups and the same assembly fixture type are required so that measured differences can be attributed to the design or material variable being studied.


Q12. Why choose UnitedTest as Your Trusted Manufacturer of ASTM F2009 Taper Disassembly Test Machines? 

UnitedTest designs and manufactures high-precision universal testing systems fully compliant with ASTM F2009 standard requirements for axial disassembly force testing of modular prosthesis taper connections. Our test machines deliver accurate, repeatable measurement of taper locking strength for orthopedic implant manufacturers, research laboratories, and regulatory testing facilities worldwide.


Our ASTM F2009 taper connection test systems integrate high-resolution load frames, precision alignment fixtures, and intuitive test software to automate both assembly and disassembly procedures per the standard. Each system includes:

  • Universal test frame calibrated to ASTM E4 specifications, with dual capability for compression assembly and tensile disassembly testing

  • Flat-plate assembly fixture with integrated planar thrust roller bearing for optimal alignment and low data variability

  • Disassembly cage fixture with universal joints on both ends, ensuring ±1° angular alignment and ±0.3 mm offset accuracy

  • Modular head adapters compatible with standard hip and shoulder prosthesis sizes (28 mm, 32 mm, 36 mm heads, 12/14 tapers, etc.)

  • UnitedTest Pro software with pre-programmed ASTM F2009 test methods, real-time force-displacement graphing, and automated report generation

Why Choose UnitedTest for Your ASTM F2009 Testing Needs?

✅ Full ASTM F2009-25 compliance – meets all alignment, force, and speed requirements of the latest 2025 edition 

✅ Dedicated orthopedic implant testing expertise – specialized fixtures for hip prosthesis taper testing and shoulder prosthesis taper testing 

✅ Precision you can trust – high-resolution load cells and displacement sensors for accurate disassembly force measurement 

✅ Turnkey solutions – machine, fixtures, software, and installation support from a single manufacturer 

✅ Customizable configurations – adaptable for ceramic-on-metal, metal-on-metal, and other material taper combinations


UnitedTest serves medical device manufacturers, contract testing laboratories, and research institutions globally with reliable, cost-effective modular taper disassembly force testing equipment. Whether you need a standalone ASTM F2009 test system or a multi-standard orthopedic implant testing lab, UnitedTest delivers solutions built for accuracy, repeatability, and long-term performance.

< Previous: ASTM F2003 UHMWPE Accelerated Aging Oxygen Bomb Test

> Next: ASTM F2068 Fatigue test system of Femoral Prostheses Implants, Hip Implants Testing

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.