Home >> Application >> By Standard >> Others >> EN 1447 long-term internal pressure test for GRP, GRE and fiberglass pipes

EN 1447 long-term internal pressure test for GRP, GRE and fiberglass pipes

Share:

EN 1447 GRP Pipe Long-Term Internal Pressure Resistance Tester | UnitedTest

UnitedTest manufactures EN 1447 compliant testing machines for glass-reinforced thermosetting plastics (GRP) pipes. This test measures time-to-failure under sustained internal hydrostatic pressure at controlled temperature, with external exposure in air or water, supporting GRP pipe qualification, pipeline design validation and long-term performance assessment.


EN 1447 defines a laboratory test procedure to evaluate the long-term resistance of glass-reinforced thermosetting plastics (GRP) pipes against continuous internal hydrostatic pressure at a defined temperature. Test specimens can be conditioned with either air or water as the surrounding external environment. It is a long-duration stress rupture test focused on ageing and sustained load performance, different from short-term burst pressure testing. The standard notes that extra evaluation rules are required if the pipe operates under alternative internal or external media. UnitedTest’s EN 1447 test equipment delivers stable pressure control, precise temperature regulation and reliable failure monitoring, ideal for GRP pipe manufacturers, third-party laboratories and pipeline engineering teams to complete product certification, batch quality inspection and service life prediction.


EN 1447 Hydrostatic Pressure Testing Machine for pipe sample:
ISO 9080 Long Term Hydrostatic Pressure Test for Thermoplastic Pipe testing
Advanced Hydrostatic Pressure Testing Service/Equipment


Test Principle

The core principle of the EN 1447 test is to subject a section of GRP pipe to a constant internal hydrostatic pressure at a controlled temperature, creating a defined state of stress in the pipe wall. The stress state depends on the selected end-loading condition:

  • With hydrostatic end thrust carried by the pipe wall

  • Without hydrostatic end thrust

The specimen is held under constant pressure until failure occurs. Lower test pressures (and thus lower wall stresses) typically produce longer times-to-failure.

A series of tests at different pressure levels is usually conducted, and the resulting pressure-time-to-failure data is analyzed to predict long-term performance. The regression analysis procedure itself is outside the scope of EN 1447 and is governed by ISO 10928.

Test Specimen Information

  • Quantity: The number of test pieces is specified by the referring product or system standard.

  • Free length (L): The usable length between end seals, as defined by the referring standard.

  • End preparation: Pipe ends must be cut smooth and perpendicular to the pipe axis.


Test Equipment required for the EN 1447 long-term internal pressure test for GRP, GRE and fiberglass pipes

Pipe Hydrostatic Pressure Test System

Complies with ISO 1167‑1 and ISO 1167‑2, to apply constant internal hydrostatic pressure to pipe samples;

Applies pressure without air entrapment; maintains pressure within specified limits for the full test duration. 

Automatic pressure regulation is recommended.

Pressure measuring device: Accuracy within ±1.0% of the applied test pressure


Enclosures

Minimize self-weight deformation without constraining the pipe circumferentially or longitudinally;

Three configurations: Type 1 (with end thrust), Type 2 (without end thrust, external seals), Type 3 (without end thrust, internal seals).

Temperature‑controlled bath & circulating pump

For water-external tests; maintains uniform temperature (may require circulation)

Optional

Electrical resistance meter: Detects weeping failure; measures resistance changes ≤3 MΩ between conductive test liquid and an external conductive layer

Strain measuring devices: Measure longitudinal and circumferential strain with accuracy within ±2%


Test Parameters:

Pressure ramp to desired levelwithin 5 min
Pressure conditionmaintained constant until failure
Time-to-failure recording±2 % of the duration of the test in hours or 24 h, whichever is smaller
Allowed interruption< 100 h; duration deducted from running time and noted in report
Conditioning24 h at test temperature unless otherwise specified
Dimensional measurement±1.0 %
Pressure measurement±1.0 % of test pressure
Strain measurement±2 %
Pressure-drop failure threshold> 2 %/h when no automatic regulation
Electrical-resistance failure threshold≤ 3 MΩ
End-fixture influence zone3.3 √(DN·e) mm


General Test Procedures of EN 1447 long-term internal pressure test for GRP, GRE and fiberglass pipes

  1. Condition the test specimen at the specified test temperature for 24 hours (unless otherwise required).

  2. Attach strain gauges if strain measurement is required.

  3. Install end-sealing devices and fill the assembly completely with test liquid, avoiding trapped air.

  4. Connect the assembly to the pressurizing system. For water-external tests, fully submerge the specimen in the temperature-controlled water bath.

  5. Increase internal pressure to the target level within 5 minutes.

  6. Maintain constant pressure until failure occurs, and record the elapsed time-to-failure.

  7. Resume testing after short interruptions (<100 hours) if applicable, and document all interruptions.

ISO 9080 Long Term Hydrostatic Pressure Test for Thermoplastic Pipe testing


Failure Modes & Detection:

EN 1447 defines three failure modes:

  1. Bursting: Catastrophic rupture of the pipe wall with immediate liquid loss and pressure drop. Detected visually or by pressure loss.

  2. Leaking: Continuous loss of test liquid through the pipe wall. Detected visually or by a pressure drop >2% of test pressure per hour (when no automatic pressure regulation is used).

  3. Weeping: Slow permeation of liquid through the pipe wall (only detectable in air environment tests). Detected visually or by a drop in electrical resistance to ≤3 MΩ between the internal liquid and an external conductive layer.


Related Standards: 

ASTM D2143

Standard Test Method for Cyclic Pressure Strength of Reinforced, Thermosetting Plastic Pipe

ASTM D2992Practice for Obtaining Hydrostatic or Pressure Design Basis for Fiberglass (Glass-Fiber-Reinforced Thermosetting-Resin) Pipe and Fittings
ASTM D1598Time-to-failure under constant internal pressure (Procedure B)
ASTM D1599short-time hydraulic pressure (used to verify scaling of fittings/joints)
ISO 1167Thermoplastics pipes, fittings and assemblies for the conveyance of fluids - Determination of the resistance to internal pressure
AWWA C950fiberglass pressure pipe (US water-works practice)
ISO 14692 Petroleum and natural gas industries - Glass-reinforced plastics (GRP) piping
ISO 10467Product standard for GRP-UP pressure/non-pressure drainage & sewerage; invokes ISO 7509 to establish p₅₀.
ISO 7509Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes - Determination of time to failure under sustained internal pressure
ISO 10639Product standard for GRP-UP pressure water supply; invokes ISO 7509.
ISO 10928

(Plastics piping systems — Glass-reinforced thermosetting plastics (GRP) pipes and fittings — Methods for regression analysis and their use): The primary normative reference.

EN 1447 generates raw test data, which is processed according to ISO 10928 to establish long-term pressure rating curves

ISO 24690

Determines long-term pressure endurance by residual failure strength after ageing rather than holding to failure; it deliberately shares EN 1447 features:

Type 1/2/3 end seals, ≤5 min pressurisation, <100 h interruption rule, ±1 % pressure / ±2 % strain / ±1 % dimensional accuracy, the 3.3√(DN·e) valid-failure-zone logic, three failure modes, and ISO 10928 regression.

ISO 25780Jacking GRP pipe standard; invokes ISO 7509.
EN 1447Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes - Determination of long-term resistance to internal pressure
ISO 9080Plastics piping and ducting systems - Determination of the long-term hydrostatic strength of thermoplastics materials in pipe form by extrapolation
ASTM D2837Obtains HDB/PDB for thermoplastic plastic pipe (similar statistical logic but for non‑reinforced thermoplastics, not fiberglass thermoset composites)


Industry fields of application

ISO 7509 applies to glass-reinforced thermosetting plastics (GRP) pipes — typically filament-wound or centrifugally cast pipes made with unsaturated polyester (UP), vinyl ester (VE), or epoxy resins reinforced with glass fiber. These pipes are used in:

  • Municipal water supply and drainage / sewerage (pressure and non-pressure).

  • Irrigation and agricultural water transmission.

  • Petroleum, natural gas, and offshore/onshore process piping (referenced by ISO 14692 series).

  • Industrial corrosive-fluid piping (chemical plants, desalination, power plant cooling water).

  • Jacking / trenchless installation projects (e.g., ISO 25780).

Product standards that invoke ISO 7509 include ISO 10467 (GRP-UP pressure/non-pressure drainage and sewerage), ISO 10639 (GRP-UP pressure water supply), and ISO 25780 (jacking pipes). These standards use ISO 7509 data to derive the p₅₀ — the projected failure pressure at 50 years — which in turn sets the allowable long-term working pressure.


Keywords: EN 1447 tester,GRP pipe long term internal pressure test,glass reinforced thermosetting plastic pipe pressure testing,hydrostatic stress rupture test,GRP pipeline ageing test,long-term pressure resistance test rig,FRP pipe pressure failure test,thermoset composite pipe testing,GRP pipe certification test,water supply GRP pipe test,sewage GRP pipe test,hydrostatic pressure test machine,composite piping mechanical test,pipe service life evaluation,GRP pipe quality control equipment,UnitedTest pressure tester

Related products and device

EN 1447 GRP Pipe Hydrostatic Pressure Testing Machine

hydrostatic pressure testing machine is designed according to ISO 1167, ASTM D1598, ASTM D1599. Under a stipulated constant hydrostatic pressure force, keeping provision time; or inside the pipe, apply a constant and rapid hydraulic pressure to make the specimen broken in a short period time, check the max. pressure force, then calculate the ring stress.

EN 1447 GRP pipe long term pressure performance hydrostatic pressure tester constant temperature tank

Constant temperature water tank is a crucial piece of equipment for hydrostatic pressure tests, particularly for long-term and burst tests. It is designed to maintain a constant pressure and temperature during testing, which is essential for accurately assessing the strength and durability of pipe.

EN 1447 GRP Pipe End cap of pipe pressure test

Stainless Steel End Caps For Pipe Hydrostatic Pressure and Burst Testing are designed for internal hydrostatic pressure testing of pipes and fittings. It is used to seal the sample in order to generate internal pressure in the sample, with the characters: ISO 1167 Type A structure.

Related Standard

ISO 7509 GRP Pipe Sustained Internal Hydrostatic Pressure Test –

ISO 7509 Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes - Determination of time to failure under sustained internal pressure

ISO 7509 specifies a laboratory method for measuring how long a GRP pipe specimen survives under a constant internal hydrostatic pressure at a controlled temperature. It is a long-term, slow-rate stress-rupture test — not a short-term burst test.

ISO 1167 Thermoplastics pipes resistance to internal pressure test –

ISO 1167: 2006 Thermoplastics pipes, fittings and assemblies for the conveyance of fluids -- Determination of the resistance to internal pressure.

ISO 1167 test method specifies a general test method for determining the resistance to internal hydrostatic pressure at a given temperature of thermoplastics pipes, fittings and piping systems for the transport of fluids. The method accommodates water-in-water, water-in-air and water-in-liquid tests. It defines uniform hydrostatic pressure testing to evaluate short-term and long-term pressure-bearing durability of thermoplastic fluid-transport piping systems.


Hydrostatic pressure testing is a valuable method for assessing the strength and integrity of pressurized systems, ensuring that they can meet operational demands without failure. Hydrostatic pressure testing can evaluate these items by filling pipelines, tanks, or containers with water before pressure is applied to detect any potential leaks or issues. 

Hydrostatic pressure tester is critical across multiple industries, from pipeline engineering to industrial piping. It helps prevent costly failures or leaks by verifying whether the system can safely reach the specified pressure levels.

ASTM D1598 test for long-term hydrostatic pressure of plastic pipe –

ASTM D1598 Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure. It is a fundamental test method used to determine the long-term hydrostatic strength and resistance of thermoplastic pipe by applying a constant internal pressure until the pipe specimen fails (ruptures). Which is critical for establishing hydrostatic design basis and ensuring long-term pipeline reliability.

ASTM D2241 PVC SDR Pressure Rated Pipe Testing Methods –

ASTM D2241 Standard Specification for Poly(Vinyl Chloride) (PVC) Pressure-Rated Pipe (SDR Series)

ASTM D2241 governs SDR‑series PVC pressure pipes for pressurized water and chemically‑compatible pressurized liquids. The mechanical performance test include sustained pressure, burst pressure, flattening, extrusion quality and impact, plus marking rules.


ASTM D2143 Cyclic Pressure Test for Reinforced Thermosetting Plastic Pipe –

ASTM D2143 Standard Test Method for Cyclic Pressure Strength of Reinforced, Thermosetting Plastic Pipe

ASTM D2143 determines the failure characteristics of reinforced thermosetting plastic pipe under cyclic internal hydraulic pressure — i.e., how many pressure cycles a pipe survives at a given pressure/stress level. Its real purpose is not to pass/fail a single pipe, but to generate the stress‑vs‑cycles‑to‑failure data points that feed the regression analysis in ASTM D2992 Procedure A, from which the long‑term Hydrostatic Design Basis (HDB) and pressure rating of a pipe product are derived.


ASTM D2992 Fiberglass Pipe Hydrostatic Test for Obtaining Hydrostatic or Pressure Design Basis –

ASTM D2992 Practice for Obtaining Hydrostatic or Pressure Design Basis for Fiberglass (Glass-Fiber-Reinforced Thermosetting-Resin) Pipe and Fittings

ASTM D2992 is not a "pass/fail" test — it is a statistical extrapolation practice. It defines how to take short-term pressure-rupture data on fiberglass (GRP) pipe and fittings, fit a log-log regression line, and extrapolate it to a 50-year design life in order to publish a Hydrostatic Design Basis (HDB) or Pressure Design Basis (PDB) for that specific product and manufacturing process.

EN 1796 GRP-UP Pipe Mechanical & Pressure Test Methods –

EN 1796 Plastics piping systems for water supply with or without pressure — Glass‑reinforced thermosetting plastics (GRP) based on unsaturated polyester resin (UP)

EN 1796 is the European product/system standard for plastics piping systems for water supply with or without pressure, made from glass-reinforced thermosetting plastics (GRP) based on unsaturated polyester (UP) resin. It covers pipes, fittings (bends, branches, reducers, saddles, flanged adaptors) and joints, classifies them by DN / PN / SN, and sets the type-test (TT) and batch-release (quality-control) test scheme that a manufacturer, a certification body or a third-party laboratory must run to prove a 50-year design life for buried (and, with care, non-buried) water pipelines.

It defines material composition (E‑glass/C‑glass/R‑glass reinforcement, UP resin, elastomer gaskets), wall‑layer construction (inner liner, structural layer, outer protective layer), dimensional tolerances, marking rules, mechanical performance, long‑term creep, hydrostatic pressure resistance and full joint performance requirements. 


ISO 13254 Plastic pipe and joints watertightness test by internal hydrostatic pressure –

ISO 13254 specifies a hydrostatic pressure test method for evaluating the watertightness of two categories of non-pressure thermoplastics components: (1) multi-piece fabricated products (e.g., custom-molded fittings) and (2) joints in thermoplastics piping systems.The test validates sealing performance under simulated service conditions for drainage, sewerage, and stormwater systems.

The standard aims to ensure consistent assessment of leak resistance, critical for applications like drainage, irrigation, and underground conduits where fluid ingress could compromise system integrity.

ISO 4437-1 Tensile, Hydrostatic pressure test for Plastics PE piping systems for the supply of gaseous fuels –

ISO 4437-1:2024 Plastics piping systems for the supply of gaseous fuels — Polyethylene (PE) Part 1: General

ISO 4437-1:2014 specifies the general properties of polyethylene (PE) compounds for the manufacture of pipes and fittings intended to be used for the supply of gaseous fuels. It also specifies the test parameters for the test methods referred to in this International Standard.   

ASTM D1598, D1599 Plastic Pipe Constant or short time pressure testing methods –

ASTM D1598: Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure.

ASTM D1598 test method covers the determination of the time-to-failure of both thermoplastic and reinforced thermosetting/resin pipe under constant internal pressure.This test method provides a method of characterizing plastics in the form of pipe under the conditions prescribed.


ASTM D1599: Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings.

ASTM D1599 test method establishes the short-time hydraulic failure pressure of thermoplastic or reinforced thermosetting resin pipe, tubing, or fittings. Data obtained by this test method are of use only in predicting the behavior of pipe, tubing, and fittings under conditions of temperature, time, method of loading, and hoop stress similar to those used in the actual test. They are generally not indicative of the long-term strength of thermoplastic or reinforced thermosetting resin pipe, tubing, and fittings


ASTM D1599 Pipe short-time hydraulic burst pressure test –

ASTM D1599 is titled "Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings." It is a fundamental short-term, destructive pressure test used to determine the ultimate failure pressure (often called the "burst pressure") of thermoplastic pipe, tubing, or fittings under rapidly applied internal pressure at a specified temperature. Typically completed within 60–70 seconds, mainly for quality control and short-term design validation. 

Frequently Asked Questions (FAQs) - EN 1447 long-term internal pressure test for GRP pipe

Q1. What is the EN 1447 test?

A. EN 1447:2009+A1:2010, “Plastics piping systems — Glass-reinforced thermosetting plastics (GRP) pipes — Determination of long-term resistance to internal pressure”, is the European CEN/TC 155 method for determining the time to failure of GRP pipes held under constant internal hydrostatic pressure at a specified temperature, with air or water outside the pipe. It fixes the apparatus, specimens, procedure, failure criteria and reporting — but not the product acceptance limits.


Q2. What exactly does it measure?

A. One primary output: time to failure at each applied pressure level. Optional outputs are longitudinal and circumferential strain. A series of such points across different pressure levels builds a pressure–time-to-failure dataset used for long-term extrapolation.


Q3. Is EN 1447 a product specification or a test method?

A. A test method. The foreword states that material-dependent parameters and performance requirements are placed in the referring standard — e.g. EN 1796 (water supply), EN 14364 (drainage/sewerage) or CEN/TS 14632 (conformity assessment). EN 1447 does not say “pass/fail”; it says “here is how to generate comparable data”.


Q4. Who needs this test?

A. GRP/GRE pipe manufacturers, third-party and accredited testing laboratories, certification bodies, product designers, water utilities, quality-control teams, and R&D institutes formulating or changing resin, liner or winding processes. Typical end uses: potable and raw water transmission, pressure sewers, firewater and cooling-water mains, effluent and process-water lines, ballast water, chemical transport, seawater injection, and trenchless rehabilitation. 


Q5. What counts as failure, and how is it detected?

A. Three modes — bursting, leaking, weeping. Three detection routes: (i) pressure drop > 2 % of the set hydrostatic pressure per hour when automatic regulation is not used; (ii) visible loss of test liquid through the wall; (iii) electrical resistance between the conductive test liquid and a conductive outer layer falling to ≤ 3 MΩ.


Q6. Why is the EN 1447 test important for GRP pipes?

A. Because GRP is an anisotropic composite laminate with a viscoelastic/viscoplastic polymer matrix. Under sustained hoop stress it creeps, relaxes and loses strength with time; a pipe that easily survives a 1-minute burst test can weep or leak after a few thousand hours at a fraction of that pressure. EN 1447 is the controlled experiment that makes this time-dependent decay measurable. Its data, regressed through ISO 10928 (typically from ~10 000 h up to a 50-year prediction), become the HDB / PDB / LTHS, pressure class (PN), allowable design stress/strain, wall thickness and temperature derating. In short: it is the bridge between a laboratory sample and a 50-year design life.


Q7. Why isn't a short-term burst test or a factory hydrotest enough?

A. A factory hydrotest proves the pipe was sound that day. It applies high pressure briefly and tells you nothing about creep rupture, resin microcracking, fibre/resin debonding, water-induced interfacial degradation or slow weeping. Published GRP studies show long-term pressure capacity can fall to roughly 40–60 % of short-term strength depending on laminate and environment. Only a sustained-pressure programme reveals that decay curve.


Q8. What is “weeping”, and why does EN 1447 treat it as failure?

A. Weeping is liquid passing through the pipe wall, detectable visually or electronically, without catastrophic rupture. In GRP it usually means the resin/liner has microcracked and the fibre reinforcement is still intact — the pipe looks fine but has already lost containment. EN 1447 is unusual in defining weeping explicitly and giving a dedicated detection channel (≤ 3 MΩ resistance). Ignoring it would over-rate the pipe dangerously.


Q9. How does the test data become a pressure rating or design basis?

A. EN 1447 → raw (pressure, time-to-failure, failure mode, failure position) points → ISO 10928 regression (two methods, chosen for normal vs skewed log-transformed data) → 50-year extrapolated long-term value → design basis with safety factor (commonly design stress ≈ ½ of 50-year failure stress, safety factor ≈ 1.8–2, design strain ≈ 0.18–0.35 %) → PN/class and wall thickness in the system standard.


Q10. Does passing EN 1447 mean the pipe will last 50 years?

A. No. The 50-year figure is an extrapolated design point, not a guaranteed service life. Real life also depends on joints, installation, soil/embedment, chemical compatibility, temperature excursions, cyclic loading and UV/handling damage. EN 1447 qualifies the pipe barrel under specific controlled conditions; system-level qualification and joint testing are separate.


Q11. Does EN 1447 save money as well as improve safety?

A. Yes, both directions. Without long-term regression, manufacturers either over-design (excess resin, glass and wall thickness) or under-design (premature weeping/leaking, warranty claims, pipeline replacement). It also provides documented evidence for CE/product certification, export approval, batch consistency, and re-qualification after a resin or process change — avoiding a full re-test programme when a formulation is tweaked. 


Q12. Can a test be paused after a power failure?

A. Yes, if the interruption is less than 100 h. Deduct the interruption from total running time and note it in the test report. Longer interruptions invalidate the run.


Q13. EN 1447 vs ISO 10928 — what is the relationship?

A. Complementary, not competing. EN 1447 = data generation; ISO 10928 = data analysis. EN 1447 states that establishing the pressure-versus-time-to-failure relationship is outside its scope. ISO 10928:2024 / EN ISO 10928:2025 is the current edition; catalogues list ISO 10928:2009 as the edition contemporary with EN 1447.


Q14. Is EN 1447 equivalent to ASTM D2992, ASTM D1598 or ISO 1167?

A. Functionally similar, legally different. The closest US chain is ASTM D1598 (constant-pressure time-to-failure for thermoplastic and reinforced thermosetting/resin pipe) + ASTM D2992 (Procedure A cyclic, Procedure B static, to obtain HDB/PDB). ISO 1167 / ISO 9080 / ASTM D2837 serve the same architecture for thermoplastics. EN 1447 + ISO 10928 ≈ ASTM D1598 + D2992, but failure criteria, weeping detection, end-seal classification and reporting differ — do not claim direct equivalence in a certificate.


Q15. What about ISO 24690:2025 — does it replace EN 1447?

A. No, it is a newer alternative. Published October 2025, it determines long-term pressure endurance from residual failure strength after ageing rather than holding to failure. It deliberately reuses much of the EN 1447 logic: Type 1/2/3 seals, ≤ 5 min pressurisation, < 100 h interruption rule, ±1 % / ±2 % / ±1 % accuracies, the valid failure-zone concept, three failure modes, and ISO 10928 regression.


Q16. Can a standard ISO 1167 hydrostatic tester be used for EN 1447?

A. The core platform (pressurising station, constant-temperature tank, independent channels, PC control, end caps) is shared, but an EN 1447 configuration additionally needs: GRP-specific end closures reproducing Type 1/2/3 stress states, an air-environment test position with 3 MΩ weeping detection, verified long-duration pressure stability, and export of pressure / time / temperature / failure mode / failure position for ISO 10928. Confirm the configuration with the supplier before ordering — do not assume an off-the-shelf ISO 1167 unit is EN 1447-ready.


Q17. How long does a test campaign take, and how many stations do I need?

A. Individual tests run until failure — from hours for high-pressure points to 10 000 h+ (~14 months) for the long-time points needed for 50-year extrapolation. Because the campaign is parallel by nature, multi-station systems (commonly 3, 5, 6, 10, 12, 20 or 40+ independently controlled channels) are the practical norm; each station should allow its own pressure, temperature and duration without cross-interference when a neighbouring specimen fails.


Q18. Why choose GRP Pipe HDB/PDB Test System to EN 1447 from UnitedTest?

A. Learn all about EN 1447 long-term internal pressure resistance testing for glass-reinforced thermosetting plastics (GRP) pipes. UnitedTest manufactures compliant DIN EN 1447 hydrostatic test machines.

UnitedTest is specialised in plastic and GRP pipe testing and supplies complete laboratory solutions for pipe manufacturers, quality-inspection laboratories, research institutes and certification facilities. The HYD series pipe hydrostatic pressure testers are built around computer-controlled, independent test stations, a constant-temperature tank and purpose-made pipe end closures; published configurations cover 10 MPa / 20 MPa, 10–2000 mm pipe diameters and expandable station counts.

For EN 1447 work, ask our engineers to configure the GRP-specific items: Type 1 / Type 2 / Type 3 end closures, air-environment test positions with weeping detection, long-duration pressure stability and automatic regulation, interruption and failure-event logging, and data export of pressure, time, temperature, failure mode and failure position relative to the valid failure zone for ISO 10928 analysis.

Configuration checklist to send with your enquiry: pipe material (GRP / GRE / UP or VE resin), DN range and wall thickness, required test pressure and temperature, external environment (air or water), end-thrust condition, required test duration / number of failure points, number of independent stations, and whether strain or electrical weeping detection is required.

< Previous: None

> Next: IEC 60068-2-75 Hammer Test for Enclosure Impact Verification

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.