Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D2143 Cyclic Pressure Test for Reinforced Thermosetting Plastic Pipe

ASTM D2143 Cyclic Pressure Test for Reinforced Thermosetting Plastic Pipe

Share:

ASTM D2143 Cyclic Pressure Strength Tester for Reinforced Thermosetting Plastic Pipe | UnitedTest

UnitedTest manufactures ASTM D2143 cyclic hydraulic pressure test machines for reinforced thermosetting plastic pipe. It collects stress versus cycles-to-failure data used for ASTM D2992 regression analysis to calculate HDB and long-term pressure ratings.


ASTM D2143 is the standard test method for evaluating cyclic pressure strength of reinforced thermosetting plastic pipe under repeated internal hydraulic pressure loading. It records the number of pressure cycles until pipe failure at defined stress levels. Instead of a simple pass-fail inspection for individual pipes, this test generates critical stress-versus-cycles-to-failure data for ASTM D2992 Procedure A regression modelling, which is applied to establish the Hydrostatic Design Basis (HDB) and long-term pressure rating for GRP pipe products. UnitedTest supplies reliable ASTM D2143 cyclic pressure test systems for fiberglass pipe qualification, pipeline material certification and long-life performance assessment.


Test Principle:

The principle is a stress–life (S–N) fatigue regression:

  1. Pipe specimens are filled with test liquid, sealed with free‑end closures, and connected to a cyclic pressurizing system.

  2. Internal pressure is pulsed on/off at ≥ 25 cycles per minute, at several different pressure (stress) levels.

  3. Each specimen is run until the test fluid penetrates the pipe wall — this is "failure," detected electrically.

  4. The number of cycles to failure is recorded at each level.

  5. Hoop stress is calculated from pressure and dimensions, then log(stress) vs. log(cycles to failure) is regressed per ASTM D2992 to establish the long‑term cyclic strength (LTHS) extrapolated to the design life (nominally 50 years / 150 × 10⁶ cycles) .

Key insight: for fiberglass pipe, cyclic loading is the governing service condition (pumps start/stop, surge, batch operations), and the cyclic regression line is usually the lower (more conservative) of the two D2992 procedures.

ASTM D2143 Cyclic Pressure Test for Reinforced Thermosetting Plastic Pipe


Test Specimen Information:

Specimen length:

Pipe nominal size ≤6 in (150 mm): free test length between end closures ≥5 × outer diameter, minimum absolute length 12 in (300 mm). 

Pipe nominal size >6 in (150 mm): free test length ≥3 × outer diameter, minimum absolute length 30 in (760 mm).

Dimension measurement: Outer diameter and wall thickness are measured according to ASTM D3567 practice.

ASTM D1598 test for long-term hydrostatic pressure of plastic pipe


Test Equipment required for the ASTM D2143 Cyclic Pressure Test for Reinforced Thermosetting Plastic Pipe

Pipe Hydrostatic Pressure Test System

Pressurizing system: Oil reservoir, oil pump, four‑way solenoid valve, electric cycler/pulsator, pressure‑relief valves, accumulators (fluid separators). 

It generates alternating cyclic hydraulic pressure on test specimens.

Pressure gauges: Minimum 1 % full‑scale precision, with max‑indicating hand and surge‑protection device. Readings shall fall within the middle 60 % of gauge scale range.

Cycle counter & electrical‑resistance‑type failure detector: Automatically records cycle numbers and halts counting once pipe wall leakage is detected.

Test fluid: 2 % sodium‑chloride aqueous salt solution or municipal tap water. Needle valves and check‑valves are also fitted in fluid loop.

Enclosures

Specimen fittings: End‑closure assemblies for free‑end mounting without inducing end‑region premature failure.

Specimen supports: Supports must not constrain pipe circumferential or axial deformation.

Temperature‑controlled bath & circulating pump

Thermostatically controlled hot‑water bath to circulate test fluid and stabilize specimen temperature within ±5 °F (±3 °C). 

Fluid circulates during pressure‑off periods of each cycle.


Test Parameters:

Cycling rate≥ 25 ± 2 cycles/min; must be re‑adjusted to this rate whenever specimens are added/removed
Pressure levelsSeveral levels, chosen to spread failure points across ≥3–5 logarithmic decades of cycles
Test fluid2 % NaCl solution or municipal water
Test temperature control±5 °F (±3 °C) at inlet and outlet
Conditioning time1 h at temperature before starting
Pressure gauge≥1 % FS accuracy; operating in mid‑60 % of scale; surge‑protected
AirAll air must be eliminated from the entire system
Valid failure location> 1 diameter from end closure (else discard)
Hoop stress formulaS = P(D − t) / 2t (S = hoop stress; P = internal pressure; D = average OD; t = minimum wall thickness)
QC shortcutOnce the regression is established, one agreed pressure point may be used for routine quality control


General Test Procedures of ASTM D2143 Cyclic Pressure Test for Reinforced Thermosetting Plastic Pipe

  1. Mount pipe specimens with end closures into test setup and fully purge air from the whole hydraulic circuit.

  2. Close specimen‑line valves; run oil pump and adjust pressure regulator to set target cyclic pressure level.

  3. Open bypass needle valves; start circulation pump to circulate temperature‑controlled salt‑water through specimens for thermal conditioning.

  4. Adjust bypass needle valves to maintain target test temperature; connect and reset failure‑detector and cycle‑counter devices, start main pressurizing pump.

  5. Adjust system to achieve cyclic rate of 25 ± 2 cycles/minute. Keep this cycle rate when changing specimen quantity on‑line.

  6. When any specimen fails, record the failure‑cycle count and document failure mode (wall fracture / localized leaking / weeping).

  7. Perform statistical regression analysis of hoop‑stress versus cycles‑to‑failure according to ASTM D2992 practice.


Failure definitions  — this is the heart of the method

Failure

Transmission of test fluid through the pipe wall in any manner — wall fracture, localized leaking, or weeping — at a distance greater than one diameter from the end closure.

 Specimens failing within one diameter of an end closure must be discarded (end effects are not valid data).

Wall fractureA break in the wall causing immediate loss of fluid and continued loss at essentially zero pressure.
Localized leakingOne or more small fractures permitting fluid transfer at a rate detectable by the failure detector.
WeepingGeneral transmission of fluid through the wall with no visible fracture, at a detectable rate; at higher rates it looks like moisture condensation on the specimen surface.
Failure detector

A device measuring electrical resistance between the test fluid and a conductive material wrapped around the specimen circumference;

 it flags failure when resistance drops to 10–20 MΩ, or, for municipal water, when the first drop of fluid passes through the wall.


Related Standards: 

ASTM D2143

Standard Test Method for Cyclic Pressure Strength of Reinforced, Thermosetting Plastic Pipe

ASTM D2992Practice for Obtaining Hydrostatic or Pressure Design Basis for Fiberglass (Glass-Fiber-Reinforced Thermosetting-Resin) Pipe and Fittings
ASTM D1598Time-to-failure under constant internal pressure (Procedure B)
ASTM D1599short-time hydraulic pressure (used to verify scaling of fittings/joints)
ISO 1167Thermoplastics pipes, fittings and assemblies for the conveyance of fluids - Determination of the resistance to internal pressure
AWWA C950fiberglass pressure pipe (US water-works practice)
ISO 14692 Petroleum and natural gas industries - Glass-reinforced plastics (GRP) piping
ISO 9080Plastics piping and ducting systems - Determination of the long-term hydrostatic strength of thermoplastics materials in pipe form by extrapolation
ASTM D2837Obtains HDB/PDB for thermoplastic plastic pipe (similar statistical logic but for non‑reinforced thermoplastics, not fiberglass thermoset composites)


Industry fields of application

  • Oil & gas / produced water and injection lines: fiberglass line pipe specifications use D2143 both as a short‑term QC screen (≥ 750 cycles) and as the data source for the long‑term cyclic HDB at 150 °F .

  • Offshore GRP piping qualification: BSEE/UK offshore GRP recommended practice qualifies joints and fittings by testing replicates to 15 × 10⁶ cycles per ASTM D2143 at rated temperature, with reporting per D2143 .

  • ISO 14692 / GB/T 29165.2 (Petroleum & natural gas — GRP piping, Part 2: Qualification and manufacture): the "limited cycle qualification test (7 000 cycles)" is run at 25 ± 2 cycles/min per ASTM D2143 .

  • Chemical process, water/wastewater, desalination, power plant cooling and FGD, marine/firewater systems — anywhere GRP pipe sees repeated pressure surges rather than constant pressure.

  • Product standards that call up D2143: ASTM D2996 (filament‑wound pipe), D2997 (centrifugally cast pipe), D2517 (reinforced epoxy gas pressure pipe), D5685 (fiberglass pressure fittings) .

  • Manufacturer R&D / formulation qualification: detecting whether a resin, glass, liner, or winding‑angle change degrades fatigue life (D2992 §12 requires re‑evaluation after material/process change).


Keywords: ASTM D2143 cyclic pressure tester, reinforced thermosetting plastic pipe cyclic hydraulic test machine, GRP pipe cyclic pressure strength tester, fiberglass pipe cycle to failure test equipment, cyclic internal pressure test rig for FRP pipe, ASTM D2992 supporting cyclic pressure test, hydrostatic design basis data generation tester, thermoset composite pipe fatigue pressure test machine, glass fiber reinforced pipe cyclic burst tester, UnitedTest ASTM D2143 testing machine, composite pipe pressure cycle fatigue test instrument

Related products and device

ASTM D2143 Pipe Cyclic Pressure Strength Testing Machine

hydrostatic pressure testing machine is designed according to ISO 1167, ASTM D1598, ASTM D1599. Under a stipulated constant hydrostatic pressure force, keeping provision time; or inside the pipe, apply a constant and rapid hydraulic pressure to make the specimen broken in a short period time, check the max. pressure force, then calculate the ring stress.

ASTM D2992 supporting cyclic pressure test, hydrostatic design basis data generation tester

Constant temperature water tank is a crucial piece of equipment for hydrostatic pressure tests, particularly for long-term and burst tests. It is designed to maintain a constant pressure and temperature during testing, which is essential for accurately assessing the strength and durability of pipe.

ASTM D2992 End cap of pipe pressure test

Stainless Steel End Caps For Pipe Hydrostatic Pressure and Burst Testing are designed for internal hydrostatic pressure testing of pipes and fittings. It is used to seal the sample in order to generate internal pressure in the sample, with the characters: ISO 1167 Type A structure.

Related Standard

ASTM D2992 Fiberglass Pipe Hydrostatic Test for Obtaining Hydrostatic or Pressure Design Basis –

ASTM D2992 Practice for Obtaining Hydrostatic or Pressure Design Basis for Fiberglass (Glass-Fiber-Reinforced Thermosetting-Resin) Pipe and Fittings

ASTM D2992 is not a "pass/fail" test — it is a statistical extrapolation practice. It defines how to take short-term pressure-rupture data on fiberglass (GRP) pipe and fittings, fit a log-log regression line, and extrapolate it to a 50-year design life in order to publish a Hydrostatic Design Basis (HDB) or Pressure Design Basis (PDB) for that specific product and manufacturing process.

ASTM D1599 Pipe short-time hydraulic burst pressure test –

ASTM D1599 is titled "Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings." It is a fundamental short-term, destructive pressure test used to determine the ultimate failure pressure (often called the "burst pressure") of thermoplastic pipe, tubing, or fittings under rapidly applied internal pressure at a specified temperature. Typically completed within 60–70 seconds, mainly for quality control and short-term design validation. 

ASTM D1598, D1599 Plastic Pipe Constant or short time pressure testing methods –

ASTM D1598: Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure.

ASTM D1598 test method covers the determination of the time-to-failure of both thermoplastic and reinforced thermosetting/resin pipe under constant internal pressure.This test method provides a method of characterizing plastics in the form of pipe under the conditions prescribed.


ASTM D1599: Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings.

ASTM D1599 test method establishes the short-time hydraulic failure pressure of thermoplastic or reinforced thermosetting resin pipe, tubing, or fittings. Data obtained by this test method are of use only in predicting the behavior of pipe, tubing, and fittings under conditions of temperature, time, method of loading, and hoop stress similar to those used in the actual test. They are generally not indicative of the long-term strength of thermoplastic or reinforced thermosetting resin pipe, tubing, and fittings


ISO 1167 Thermoplastics pipes resistance to internal pressure test –

ISO 1167: 2006 Thermoplastics pipes, fittings and assemblies for the conveyance of fluids -- Determination of the resistance to internal pressure.

ISO 1167 test method specifies a general test method for determining the resistance to internal hydrostatic pressure at a given temperature of thermoplastics pipes, fittings and piping systems for the transport of fluids. The method accommodates water-in-water, water-in-air and water-in-liquid tests. It defines uniform hydrostatic pressure testing to evaluate short-term and long-term pressure-bearing durability of thermoplastic fluid-transport piping systems.


Hydrostatic pressure testing is a valuable method for assessing the strength and integrity of pressurized systems, ensuring that they can meet operational demands without failure. Hydrostatic pressure testing can evaluate these items by filling pipelines, tanks, or containers with water before pressure is applied to detect any potential leaks or issues. 

Hydrostatic pressure tester is critical across multiple industries, from pipeline engineering to industrial piping. It helps prevent costly failures or leaks by verifying whether the system can safely reach the specified pressure levels.

ISO 9080 Long Term Hydrostatic Pressure Test for Thermoplastic Pipe –

ISO 9080 Plastics piping and ducting systems — Determination of the long-term hydrostatic strength of thermoplastics materials in pipe form by extrapolation.

ISO 9080 specifies a statistical extrapolation method (Standard Extrapolation Method, SEM) to predict long‑term hydrostatic performance of thermoplastic pipe materials, instead of conducting multi‑decade real‑time ageing tests.

ISO 4437-1 Tensile, Hydrostatic pressure test for Plastics PE piping systems for the supply of gaseous fuels –

ISO 4437-1:2024 Plastics piping systems for the supply of gaseous fuels — Polyethylene (PE) Part 1: General

ISO 4437-1:2014 specifies the general properties of polyethylene (PE) compounds for the manufacture of pipes and fittings intended to be used for the supply of gaseous fuels. It also specifies the test parameters for the test methods referred to in this International Standard.   

ASTM D1598 test for long-term hydrostatic pressure of plastic pipe –

ASTM D1598 Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure. It is a fundamental test method used to determine the long-term hydrostatic strength and resistance of thermoplastic pipe by applying a constant internal pressure until the pipe specimen fails (ruptures). Which is critical for establishing hydrostatic design basis and ensuring long-term pipeline reliability.

FAQs for ASTM D2143 Cyclic Pressure Strength Test

Q1. What is ASTM D2143?

It's the standard test method for determining the failure characteristics of reinforced thermosetting plastic pipe (fiberglass/GRP/RTRP) under cyclic internal hydraulic pressure. Specimens are pressurized in repeating on/off cycles until test fluid penetrates the wall, and cycles to failure are recorded.



Q2. Is ASTM D2143 a pass/fail test?

Not primarily. Its main role is to generate stress (or pressure) vs. cycles-to-failure data points. Those points are fed into the regression analysis of ASTM D2992 Procedure A (cyclic) to establish the long-term Hydrostatic Design Basis (HDB) / Pressure Design Basis (PDB) and the 50-year (≈150 × 10⁶ cycle) strength of the pipe. It can also be used as a short-term QC screen (e.g., a minimum-cycle survival requirement agreed between purchaser and supplier).


Q3. Is there an ISO equivalent?

No — the standard states explicitly: "There is no known ISO equivalent to this standard." ISO 14692-2 / GB/T 29165.2 instead references ASTM D2143 for its cycling rate.


Q4. What does it NOT cover?

It omits creep and non-recoverable deformation, and it has no precision and bias statement (no controlled round-robin has been run — sample count, duration and specialized apparatus make one impractical).


Q5. What is "weeping" and why does it matter? 

Fluid migrating through the wall with no visible fracture, appearing as surface condensation. It matters because GRP pipe loses integrity by progressive matrix micro-cracking long before it bursts — a burst test alone would over-rate the material.



Q6. How is failure detected automatically?

A failure detector measures the electrical resistance between the test fluid and a conductive material wrapped around the specimen circumference. It signals failure when resistance drops to the 10–20 MΩ range, or — when municipal water is used — when the first drop of fluid passes through the wall. The detector automatically stops the cycle counter.


Q7. How long is a specimen?

For pipe ≤ 6 in. (150 mm): length between end closures ≥ 5 × OD, never less than 12 in. (300 mm).

For pipe > 6 in.: ≥ 3 × OD, never less than 30 in. (760 mm).

Dimensions measured per ASTM D3567; conditioning per ASTM D618.


Q8. How many specimens are needed?

D2143 itself defers to ASTM D2992. Procedure A requires a minimum of 18 failure points spread across decades: at least 3 points each in 10³–10⁴, 10⁴–10⁵, 10⁵–10⁶ and 10⁶–10⁷ cycles, plus at least 1 point beyond 15 × 10⁶ cycles.



Q9. Why is cyclic testing critical for fiberglass pipe specifically?

FRP/GRP is anisotropic and damage-tolerant in a dangerous way: repeated pressure cycling grows resin-matrix micro-cracks and glass/resin debonding, producing weeping long before rupture. Static burst or short-term tests measure ultimate strength and look impressive, but do not capture this progressive permeability failure. D2143 is the only standardized way to expose it.


Q10. Why does it matter commercially / for compliance?

The HDB/HDS printed on fiberglass pipe — and hence the allowable operating pressure and service factor — derives from the D2143 + D2992 Procedure A regression. Product standards and purchaser specs (fiberglass line pipe, offshore GRP piping, API 15LR/15HR, AWWA C950, ASTM D2996/D2997/D2517/D5685) rely on this design basis. Without D2143 data there is no defensible cyclic pressure rating.


Q11. Why is it a good manufacturing-quality sentinel?

Fatigue life is acutely sensitive to winding angle, resin content, cure state, liner integrity and fiber placement. A shift in the regression line is the standard way to detect that a resin, glass, liner or process change has degraded the product — and D2992 §12 formally requires re-evaluation after such a change.


Q12. What real service condition does it simulate?

Pump start/stop, batch transfer, water hammer, surge, slug flow and intermittent operation. A constant-pressure test (D1598) does not reproduce this damage mechanism, which is exactly why D2992 keeps Procedure A separate.


Q13. Which industries use it?

Oil & gas (produced water, injection, gathering lines), offshore GRP piping, chemical and petrochemical process piping, water/wastewater and desalination, power-plant cooling water and FGD, marine and firewater systems — anywhere GRP pipe sees repeated pressure surges.


Q14. How is it used in oil & gas GRP qualification?

Fiberglass line pipe specs use D2143 as a short-term QC screen (≥ 750 cycles) and as the data source for the long-term cyclic HDB regression at 150 °F. ISO 14692-2 / GB/T 29165.2 uses 25 ± 2 cycles/min per ASTM D2143 for its 7 000-cycle limited cyclic qualification test. Offshore GRP recommended practice qualifies joints/fittings to 15 × 10⁶ cycles per D2143 at rated temperature.


Q15. How does it relate to ASTM D2992?

D2143 is the data generator; D2992 is the analysis practice. D2992 Procedure A (cyclic) takes D2143 failure points, runs the log-log regression, applies 95 % confidence/prediction limits, assigns an HDB/PDB category and extrapolates to the design life.


Q16. How does it differ from D1598 and D1599?


D2143D1598
D1599
LoadingCyclic (pulsating)Constant internal pressureRapid ramp to burst
OutputCycles to failureTime to failureBurst pressure
DurationCycles up to 15 × 10⁷+10 000+ h60–70 s
UseCyclic design basis (D2992 Proc. A)Static design basis (D2992 Proc. B)Fast QC / lot acceptance

D1599 is a "sprint," D1598 a "marathon," and D2143 a "fatigue/repeated-load" test. They answer different questions and complement rather than replace each other.


Q17. Why choose ASTM D2143‑21 Cyclic Pressure Strength Test Machine by UnitedTest?

UnitedTest manufactures ASTM D2143‑21 cyclic pressure strength test machine for fiberglass / GRP reinforced thermosetting plastic pipe. Perform cyclic internal hydraulic fatigue test, cycles‑to‑failure measurement, automatic leakage failure detection for FRP pipe certification & quality control. Compliant with ASTM D2992, D3567, D618 standards.


UnitedTest is professional manufacturer of ASTM D2143 cyclic pressure strength testing equipment for reinforced thermosetting plastic pipe, fiberglass pipe and GRP pipe systems. Our complete cyclic internal hydraulic pressure test system strictly complies with ASTM D2143‑21 standard requirements, supporting cyclic fatigue test for FRP pipe with OD‑to‑wall‑thickness ratio ≥ 10:1UnitedTest.

The UnitedTest ASTM D2143 test system simulates real‑world fluctuating cyclic water pressure service condition, automatically counts pressure cycles until pipe failure, detects weeping, localized leakage and wall fracture via electrical‑resistance‑based failure detector, and stops test automatically once specimen failure occurs. It maintains the mandatory test cyclic rate 25 ± 2 cycles per minute, integrates thermostatically controlled temperature bath with ±5 °F (±3 °C) temperature accuracy, pressure gauges with ≥1 % full‑scale precision, accumulator fluid separator, multi‑specimen test channels and circulating fluid loop for salt‑water or municipal water test medium.


Our testing machine helps pipe factories, third‑party testing laboratories, R&D institutes and certification labs to complete:

  • Material qualification cyclic pressure fatigue testing for fiberglass‑reinforced thermosetting resin pipe

  • Acquire cycles‑to‑failure data to calculate cyclic hydrostatic design basis following ASTM D2992 practice

  • Routine production quality‑control cyclic pressure screening test for mass‑produced GRP pipe

  • Record failure modes: wall fracture, localized leaking, weeping for engineering evaluation

  • Full test‑data logging for standard‑compliant ASTM D2143 test report output


UnitedTest ASTM D2143 cyclic pressure tester supports multi‑specimen parallel testing, adjustable pressure range, temperature conditioning system, air‑purge function and surge‑protection pressure measurement. End‑closure fittings and specimen supports avoid end‑region premature failure. All critical test parameters including cycle count, pressure value, fluid temperature and failure‑trigger timestamp are saved for traceability.

We provide turn‑key lab solution including installation, operation training, calibration guidance for ASTM D2143‑21 standard test method. If you need reliable cyclic pressure test machine for reinforced thermosetting plastic pipe fatigue performance evaluation, contact UnitedTest for technical proposal and quotation.

< Previous: ASTM D2137 Rubber Brittleness Point Test of Flexible Polymers and Coated Fabrics

> Next: ASTM D2208 Leather Breaking Strength Testing by Grab Method

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you