Home >> Products >> Plastic Pipe Industry Testing >> Pipe Hydrostatic Pressure Test >> Hydrostatic pressure constant temperature tank​
Hydrostatic pressure constant temperature tank​

Hydrostatic pressure constant temperature tank​

HDPE pipe hydrostatic pressure long-term, burst test constant temperature tank​

HDPE pipe hydrostatic pressure long-term, burst test constant water tank. The constant temperature water tank is a crucial piece of equipment for hydrostatic pressure tests, particularly for long-term and burst tests. It is designed to maintain a constant pressure and temperature during testing, which is essential for accurately assessing the strength and durability of pipes under sustained conditions.

Feature of water tank:
1, Constant-temperature tank is composed of 304# stainless steel interior and aluminum alloy/steel plate outer plate, no corrosion,
2, Imported circulation pump, high accuracy heater and temperature holding system;
3, Rigid and thick heat insulation polyurethane foam, and temperature proof layer to ensure the temperature and energy keeping performance, avoid energy loss.
4, For big tank, the cover of tank equipped with automatic lifting device, more reliable and convenient;

General introduction

The constant temperature water tank is a crucial piece of equipment for hydrostatic pressure tests, particularly for long-term and burst tests. It is designed to maintain a constant pressure and temperature during testing, which is essential for accurately assessing the strength and durability of pipes under sustained conditions.

Feature of water tank:
1, Constant-temperature tank is composed of 304# stainless steel interior and aluminum alloy/steel plate outer plate, no corrosion,
2, Imported circulation pump, high accuracy heater and temperature holding system;
3, Rigid and thick heat insulation polyurethane foam, and temperature proof layer to ensure the temperature and energy keeping performance, avoid energy loss.
4, For big tank, the cover of tank equipped with automatic lifting device, more reliable and convenient;


图片.png

Key Features

  • Temperature range
  • Material
  • Cooling function

15℃~ 95℃ (Add cooling device optional)

1, Constant-temperature tank is composed of 304# stainless steel interior and aluminum alloy/steel plate outer plate, no corrosion,
2, Imported circulation pump, high accuracy heater and temperature holding system;
3, Rigid and thick heat insulation polyurethane foam, and temperature proof layer to ensure the temperature and energy keeping performance, avoid energy loss.
4, For big tank, the cover of tank equipped with automatic lifting device, more reliable and convenient;

Main technical specification

Working station1 to 20 working stations
Burst testAll stations can execute the burst test
Hydrostatic pressure testAll stations can execute the long-term hydrostatic pressure test
Max. pressure0 ~ 10Mpa (100 bar) / 0 ~ 20Mpa (200   bar)
Constant pressure accuracy-1%, +2%
Pressure resolution0.001Mpa
Time count range1~9999h 59min 59s
Time display accuracy1s
Constant temperatureAmbient temperature to 95℃
15℃ to Ambient temp. with cooling unit
Temp. indication accuracy±0.5℃
Power supply380V AC 50HZ, 3 phase
Pipe sample diameter range10-2000mm   (Customized)
Standard End capφ16, φ20,   φ25, φ32, φ40, φ50, φ63, φ75, φ110, φ125, φ140, φ160, φ180, φ200, φ225,   φ250,φ280, φ315, φ355, φ400, φ450, φ500, φ560, φ630, φ710, φ800, φ900, φ1000,   φ1100, φ1200, φ1300…
Customized end capφ1/2",φ3/4",φ1" ….   φ20" etc., inch sizeor any other size according requirement.


Main accessories

Constant temperature tank (stainless steel interior)


include the heater, circulation pump, pneumatic lifting rod etc.,
1 set

Standard

ISO 7509 GRP Pipe Sustained Internal Hydrostatic Pressure Test –

ISO 7509 Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes - Determination of time to failure under sustained internal pressure

ISO 7509 specifies a laboratory method for measuring how long a GRP pipe specimen survives under a constant internal hydrostatic pressure at a controlled temperature. It is a long-term, slow-rate stress-rupture test — not a short-term burst test.

ASTM D2992 Fiberglass Pipe Hydrostatic Test for Obtaining Hydrostatic or Pressure Design Basis –

ASTM D2992 Practice for Obtaining Hydrostatic or Pressure Design Basis for Fiberglass (Glass-Fiber-Reinforced Thermosetting-Resin) Pipe and Fittings

ASTM D2992 is not a "pass/fail" test — it is a statistical extrapolation practice. It defines how to take short-term pressure-rupture data on fiberglass (GRP) pipe and fittings, fit a log-log regression line, and extrapolate it to a 50-year design life in order to publish a Hydrostatic Design Basis (HDB) or Pressure Design Basis (PDB) for that specific product and manufacturing process.

ASTM D1598 test for long-term hydrostatic pressure of plastic pipe –

ASTM D1598 Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure. It is a fundamental test method used to determine the long-term hydrostatic strength and resistance of thermoplastic pipe by applying a constant internal pressure until the pipe specimen fails (ruptures). Which is critical for establishing hydrostatic design basis and ensuring long-term pipeline reliability.

ISO 9080 Long Term Hydrostatic Pressure Test for Thermoplastic Pipe –

ISO 9080 Plastics piping and ducting systems — Determination of the long-term hydrostatic strength of thermoplastics materials in pipe form by extrapolation.

ISO 9080 specifies a statistical extrapolation method (Standard Extrapolation Method, SEM) to predict long‑term hydrostatic performance of thermoplastic pipe materials, instead of conducting multi‑decade real‑time ageing tests.

ISO 1167 Thermoplastics pipes resistance to internal pressure test –

ISO 1167: 2006 Thermoplastics pipes, fittings and assemblies for the conveyance of fluids -- Determination of the resistance to internal pressure.

ISO 1167 test method specifies a general test method for determining the resistance to internal hydrostatic pressure at a given temperature of thermoplastics pipes, fittings and piping systems for the transport of fluids. The method accommodates water-in-water, water-in-air and water-in-liquid tests. It defines uniform hydrostatic pressure testing to evaluate short-term and long-term pressure-bearing durability of thermoplastic fluid-transport piping systems.


Hydrostatic pressure testing is a valuable method for assessing the strength and integrity of pressurized systems, ensuring that they can meet operational demands without failure. Hydrostatic pressure testing can evaluate these items by filling pipelines, tanks, or containers with water before pressure is applied to detect any potential leaks or issues. 

Hydrostatic pressure tester is critical across multiple industries, from pipeline engineering to industrial piping. It helps prevent costly failures or leaks by verifying whether the system can safely reach the specified pressure levels.

ASTM D1598, D1599 Plastic Pipe Constant or short time pressure testing methods –

ASTM D1598: Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure.

ASTM D1598 test method covers the determination of the time-to-failure of both thermoplastic and reinforced thermosetting/resin pipe under constant internal pressure.This test method provides a method of characterizing plastics in the form of pipe under the conditions prescribed.


ASTM D1599: Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings.

ASTM D1599 test method establishes the short-time hydraulic failure pressure of thermoplastic or reinforced thermosetting resin pipe, tubing, or fittings. Data obtained by this test method are of use only in predicting the behavior of pipe, tubing, and fittings under conditions of temperature, time, method of loading, and hoop stress similar to those used in the actual test. They are generally not indicative of the long-term strength of thermoplastic or reinforced thermosetting resin pipe, tubing, and fittings


ASTM D1599 Pipe short-time hydraulic burst pressure test –

ASTM D1599 is titled "Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings." It is a fundamental short-term, destructive pressure test used to determine the ultimate failure pressure (often called the "burst pressure") of thermoplastic pipe, tubing, or fittings under rapidly applied internal pressure at a specified temperature. Typically completed within 60–70 seconds, mainly for quality control and short-term design validation. 

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.