Information on the most widely used ASTM standards within the materials testing industry
EN 16094 Micro-Scratch Resistance Tester for Laminate Floor Coverings | UnitedTest
UnitedTest manufactures EN 16094 micro-scratch resistance testing machines for laminate flooring. This standard covers three test procedures A, B for micro-scratch resistance and C for polishing resistance, ideal for mat surface laminate floor materials.
EN 16094 specifies three test procedures: Procedure A and B for micro-scratch resistance evaluation, and Procedure C for polishing resistance testing of laminate floor coverings. Procedure C is designed for mat surfaces with a 60° reflectometer value R′ ≤ 7, supporting reliable surface scratch performance assessment of laminate flooring products.
EN 16094 Micro-Scratch & Polishing Resistance Test for Laminate Floor Coverings
Test Principle | The test specimen is secured on a horizontal test table. Circular abrasive scrub material is mounted in a holder and presses onto the sample under a defined vertical load. The table and holder execute perpendicular translational motions following a Lissajous‑figure trajectory; the holder can freely rotate around its vertical axis. After a preset number of rubs, surface damage is quantified by gloss‑meter measurement and/or visual inspection to assess micro‑scratch or polishing‑induced surface changes. One cycle equals one full Lissajous figure consisting of 16 rubs (two outer drives 16 revolutions, inner drive 15 revolutions). |
| Test Equipment | Martindale abrasion‑testing machine complying with EN ISO 12947‑1.
|
| Test Specimen |
|
Main Test Parameters
| Parameter | Procedure A | Procedure B | Procedure C |
|---|---|---|---|
| Scrub‑material grade | Very‑fine | Medium‑fine | Ultra‑fine |
| Holder assembly | Version 2 (6 N) | Version 1 (4 N) | Version 2 (6 N) |
| Rotational speed | 48 rev/min | 48 rev/min | 48 rev/min |
| Rub count | 80 rubs (5 Lissajous cycles) | 160 rubs (10 Lissajous cycles) | 320 rubs (20 Lissajous cycles) |
| Evaluation method | Gloss‑change calculation | Visual grading (Annex B) | Gloss‑change calculation (mat‑surface polishing effect) |
Martindale with position C on both axes (large Lissajous) · 48 rev/min · (23 ± 2) °C / (50 ± 5) % RH ≥ 1 week conditioning · fresh scrub disc per specimen, discarded after use · specimen cleaned before and after · 20° geometry mandatory above 70 gloss units · 24 h storage + diffuse light + 0,3 m viewing distance for visual rating · rounding up to the next integral number · every new abrasive batch calibrated on the reference HPL · deviations must be reported.
Industry Application Fields
Laminate flooring manufacturers — R&D and QC of the wear layer (corundum-loaded melamine overlay, resin formulation, press cycle, lacquer, embossing-in-register, matte/gloss control).
Third-party test houses and certification bodies — batch release, benchmarking, certification, claim substantiation.
Product declaration and marketing — MSR-A/MSR-B classes are used alongside the abrasion class (AC) and use class (EN ISO 10874) in technical data sheets, DoP/CE documentation under EN 14041, tenders and procurement specs.
Adjacent sectors — laboratories routinely extend the same Martindale/Lissajous method to engineered wood flooring, LVT/SPC/resilient surfaces and (via sibling standards) furniture and HPL/CPL surfaces.
Related Standard:
| ISO 12947-1 | Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 1: Martindale abrasion testing apparatus |
| ISO 12947-2 | Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 2: Determination of specimen breakdown |
| ISO 12947-3 | Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 3: Determination of mass loss |
| ISO 12945‑2 | pilling & fuzzing on the modified Martindale apparatus — same machine family, different end point |
| ISO 5470-1 | Rubber- or plastics-coated fabrics - Determination of abrasion resistance - Part 1: Taber abrader |
| ISO 5470-2 | Rubber- or plastics-coated fabrics. Determination of abrasion resistance. Martindale abrader |
| ASTM D4966 | Standard Test Method for Abrasion Resistance of Textile Fabrics (Martindale Abrasion Tester Method). |
| ASTM D4970 | Standard Test Method for Pilling Resistance and Other Related Surface Changes of Textile Fabrics: Martindale Tester |
| GB/T 21196.1 | Textiles-Determination of the abrasion resistance of fabrics by the Martindale method-Part 1:Martindale abrasion testing apparatus |
| JIS L 1096, M&S P19 | other commonly referenced abrasion/pilling methods |
| GBT 4802.2 | Textiles - Determination of fabric propensity to surface fuzzing and to pilling - Part 2: Modified Martindale method |
| EN 13770 | Textiles - Determination of the abrasion resistance of knitted footwear garments |
| EN 16094 | Laminate floor coverings. Test method for the determination of micro-scratch resistance |
Why the test matters for the material
It measures appearance retention, not wear-through. The classic abrasion class (AC, EN 13329) tells you when the decorative layer is worn away. Micro-scratching happens long before that: sand and grit under footwear, dragged furniture and cleaning produce a dense network of fine scratches that scatter light — the floor looks dull, hazy or "whitened" while still being structurally intact. EN 16094 quantifies exactly that failure mode.
It is the main consumer-perceived defect and warranty driver. Most complaints about laminate floors are visual, not structural. A measurable ΔR′ (A), a documented scratch pattern (B) and polishing resistance (C) let a manufacturer set, defend and validate warranty claims.
It captures both loss and gain of gloss. On a glossy surface scratching lowers gloss; on a mat surface the ultra-fine action can polish it and create shiny traffic-path patches. Procedure C was added in 2021 specifically because A and B could not describe that effect.
It makes product differentiation objective. Corundum content and distribution in the overlay, resin cure, press parameters, lacquer chemistry and embossing-in-register all change the MSR class. Without EN 16094, claims like "scratch resistant" are unmeasurable marketing.
It improves lab-to-lab reproducibility. Abrasive fleece varies from batch to batch; the 2021 edition's reference HPL calibration (with acceptance windows of 5–20 %, MSR-B3/B4 and 15–30 %) is what makes results comparable between laboratories and over time.
It feeds compliance and specification. Results support DoP/CE documentation, eco-label and sustainability schemes, retailer/specifier requirements and tender specifications.
Keywords: EN 16094 tester, laminate floor scratch test, micro scratch resistance tester, polishing resistance test, laminate flooring surface test, 60 degree reflectometer test, floor covering scratch tester, laminate wear testing machine, mat surface scratch test, flooring material surface durability test, laminate floor quality inspection equipment, scratch resistance test instrument, UnitedTest flooring tester
Related products and device
Related Standard
ISO 12947-1 Textiles — Determination of the abrasion resistance of fabrics by the Martindale method — Part 1: Martindale abrasion testing apparatus
ISO 12947-1 defines mandatory construction, dimensional, performance and auxiliary‑material requirements for Martindale abrasion testers, which are used to carry out the practical test procedures laid down in ISO 12947‑2,‑3,‑4. It is the specification for the machine and the consumables — the "hardware norm". The actual abrasion procedures live in Parts 2, 3 and 4, and Part 1 is written to guarantee that a Martindale result obtained in one lab is physically comparable to one obtained in another.
ISO 5470-1: Rubber- or plastics-coated fabrics -- Determination of abrasion resistance -- Part 1: Taber abrader.
ISO 5470-1 specifies a method for determining the abrasion resistance of rubber- or plastics-coated fabrics using the Taber abrader apparatus. This test simulates wear under controlled conditions to evaluate a material's durability.
ISO 12947-3 Textiles — Determination of the abrasion resistance of fabrics by the Martindale method — Part 3: Determination of mass loss
ISO 12947-3 applies to all textile fabrics including nonwovens, and is used to determine the mass loss of specimens after controlled abrasion. It is explicitly not intended for fabrics where the specifier states the end performance is a deliberately low abrasion wear life.
ISO 13937-2 Textiles – Tear properties of fabrics – Part 2: Determination of tear force of trouser‑shaped test specimens (Single tear method).
ISO 13937-2 is method for determining the tear force required to propagate an already-started single tear, using a rectangular specimen slit into two "trouser legs". Mainly for woven fabrics; may also apply to fabrics made by other techniques (e.g. some nonwovens). Not applicable to knitted fabrics, woven elastic fabrics, highly anisotropic fabrics, or loose fabrics where the tear tends to transfer from one direction to another. Only CRE (constant-rate-of-extension) machines are permitted.
ASTM D5035 : Standard Test Method for Breaking Force and Elongation of Textile Fabrics (Strip Method)
ASTM D5035 is the standard test method for determining breaking force (tensile strength) and elongation at break of textile fabrics using the strip method. It defines two core procedures--raveled strip (for woven fabrics) and cut strip (for nonwovens, coated/felted fabrics)--and supports both dry and wet testing.
ISO 12945-2 Textiles — Determination of fabric propensity to surface pilling, fuzzing or matting — Part 2: Modified Martindale method
ISO 12945-2 specifies a method for determining the resistance to pilling, fuzzing and matting of textile fabrics using a modified Martindale machine. It ranks fabrics in the same order of surface-change propensity as is likely to occur in end-use wear.
ASTM D4966 Standard Test Method for Abrasion Resistance of Textile Fabrics (Martindale Abrasion Tester Method)
ASTM D4966 determination of the abrasion resistance of textile fabrics using the Martindale abrasion tester; generally applicable to knit, woven and nonwoven fabrics — material thickness may limit suitability because of specimen-holder capacity. It applies to woven, knit and non‑woven textiles, though excessive fabric thickness may restrict testing due to specimen‑holder physical limits.
ASTM D4970 Standard Test Method for Pilling Resistance and Other Related Surface Changes of Textile Fabrics: Martindale Tester.
ASTM D4970 is the Martindale (Lissajous‑motion) fabric‑on‑fabric pilling test used to predict how badly a fabric will pill, fuzz or otherwise change its surface appearance in wear, reported on an arbitrary 5‑to‑1 rating scale (5 = no pilling, 1 = very severe pilling).
ISO 12947-2 Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 2: Determination of specimen breakdown
ISO 12947-2 measuring how many abrasion cycles — or "rubs" — a fabric withstands before itreaches a defined end point. A circular specimen is mounted in a holder under a defined loadand rubbed against a standard woven wool abradant in a translational movement tracing a Lissajous figure, while the holder rotates freely about its own axis. The abrasion resistance isreported as the number of rubs at the last inspection interval before specimen breakdownoccurs.
Because the end point is defined inside the standard — two broken threads for woven fabrics,one for knitted fabrics, a fully worn-off area for pile and flocked fabrics, a hole of at least 2.5mm for nonwovens — results are objective and comparable between laboratories. That is whythe Martindale figure is the durability number most often written into upholstery and contracttextile specifications.
ISO 17704 Footwear — Test methods for uppers, linings and insocks — Abrasion resistance
ISO 17704 is method for determining the resistance of uppers, linings and insocks — irrespective of material — to wet and dry abrasion, in order to assess suitability for the end use. Note the standard deliberately gives no pass/fail criteria; it produces a description and rating of damage at prescribed rub counts.
EN 13770 Textiles‑Determination of the abrasion resistance of knitted footwear garments
EN 13770 define two test methods for the abrasion resistance of knitted footwear garments — e.g. ankle socks, socks, heavy tights — applicable irrespective of size, composition and construction. the two methods are independent. The method must be chosen before starting the test and recorded in the test report, because results from the two methods cannot be compared with each other.
FAQs for EN 16094:2021 Micro‑scratch Resistance Test
A. EN 16094:2021 is the European standard titled "Laminate floor coverings — Test method for the determination of micro-scratch resistance".
The standard specifies two procedures for micro-scratch resistance (A and B) and one procedure for resistance to polishing (C), and it applies to all types of laminate floor coverings. Procedure C is specifically intended for mat surfaces.
Compared with the 2012 edition, the 2021 version added two things:
Procedure C — evaluation of the polishing effect on mat laminate surfaces;
A reference black high-gloss HPL plate — used to calibrate/verify every new batch of scrub material.
Q2. Why is the EN 16094 test important?
A. Because it measures the failure mode that customers actually complain about. A laminate floor rarely "wears through" in service — it goes dull, hazy or shiny-patched first. Sand and grit under shoes, dragged furniture and routine cleaning create a dense network of very fine scratches that scatter light long before the décor layer is damaged. EN 16094 quantifies exactly that:
Appearance retention, not wear-through. The classic abrasion class (AC rating per EN 13329) tells you when the décor layer is worn away. EN 16094 tells you how the surface looks after realistic micro-abrasion — a much earlier and more sensitive indicator.
It captures both loss and gain of gloss. Scratching lowers gloss on a glossy floor; on a mat floor, ultra-fine abrasion can polish the surface and create glossy traffic-path patches. Only Procedure C describes that effect — which is why it was added in 2021.
Warranty and claim defence. A measured ΔR′ (Procedure A), a documented scratch pattern (Procedure B) and a polishing value (Procedure C) turn "scratch resistant" from marketing language into defensible data.
R&D feedback for the material. Corundum content and distribution in the overlay, melamine resin cure, press cycle, lacquer chemistry and embossing-in-register all shift the MSR class. The test lets formulators rank formulations objectively.
Compliance and specification. Results feed technical data sheets, DoP/CE documentation under EN 14041, retailer and specifier requirements, eco-label schemes and tender documents.
Comparability between labs. The 2021 reference-HPL calibration procedure is what makes results repeatable over time and comparable between laboratories.
Q3. How many specimens and how are they conditioned?
A.
6 specimens of 150 mm × 150 mm for the micro-scratch tests, plus 3 more for the polishing test — 9 pieces in total.
The surface must be substantially flat.
If the plank width is less than 150 mm, a specimen may be assembled from two pieces with the length joint in the middle.
Conditioning must start at least one week before testing, in air at (23 ± 2) °C and (50 ± 5) % RH.
Gloss readings must be taken at least 5 mm away from any joint and parallel to the décor/structure direction or joint.
Q4. How long does one EN 16094 test take?
A. The abrasion itself is short — at 48 rev/min:
Procedure A: 80 rubs ≈ 1.7 min
Procedure B: 160 rubs ≈ 3.3 min
Procedure C: 320 rubs ≈ 6.7 min
The real time is in preparation and conditioning: ≥ 1 week conditioning before the test, plus for Procedure B a mandatory 24 h storage at (23 ± 2) °C / (50 ± 5) % RH after abrasion before the visual assessment.
Q5. How does EN 16094 differ from the abrasion class (AC1–AC5) in EN 13329?
A. They measure different things and are complementary:
EN 13329 / AC rating = resistance to wear-through of the surface layer (Taber-type rotating abrasion) plus impact, stain and swelling — it answers "how long until the décor layer is damaged?".
EN 16094 / MSR rating = resistance to fine surface scratching and gloss change (Martindale / Lissajous) — it answers "how long does the floor keep looking new?".
A high-AC floor can still have a mediocre MSR class, and vice versa. Premium laminates typically target AC4/AC5 together with MSR-A1/MSR-B1.
Q6. What are the most common sources of error?
A.
Re-using or mis-cutting the scrub disc — it must be 89 ± 1 mm, fresh for each specimen, and discarded after use.
Skipping batch calibration on the reference HPL (5.9) — the biggest cause of lab-to-lab disagreement.
Wrong Lissajous setting — both axes must be at outer position C (large figure, 60 × 60 mm); a small or distorted figure invalidates the test. Verify per Annex A (16 rubs, 31 curves, sides measured to ± 0.2 mm).
Wrong load — 4 N (413 g) for Procedure B versus 6 N (612 g) for A and C.
Measuring gloss in different places before and after — always use the positioning device and the same four points.
Using 60° on a high-gloss floor — above 70 gloss units, 20° geometry is mandatory.
Insufficient conditioning — less than one week, or out of (23 ± 2) °C / (50 ± 5) % RH.
Poor visual assessment conditions in Procedure B — illumination (1200 ± 400) lx, viewing distance (0.3 ± 0.05) m, multiple viewing angles, experienced observers (three in case of doubt), assessment only after the 24 h storage.
Q7. Why choose EN 16094 Laminate Floor Micro‑scratch Resistance Tester from UnitedTest?
UnitedTest supplies EN 16094:2021 Martindale Micro‑scratch Resistance Tester for laminate flooring. Compliant with Procedure A/B/C, Lissajous‑figure verification, laminate floor micro‑scratch & polishing‑resistance test machine for QC and certification labs.
UnitedTest manufactures professional EN 16094 Martindale scratch‑resistance testing machine, fully built to meet requirements of European standard EN 16094:2021 for laminate floor‑covering micro‑scratch resistance and polishing‑resistance performance test.
Our tester supports all three test procedures (Procedure A, Procedure B, Procedure C). It implements correct large‑size Lissajous‑figure trajectory with axes outer‑C position setting, compatible with 4 N (413 g) and 6 N (612 g) scrub‑material holders. It works together with gloss‑meter, positioning fixture, diffuse‑light assessment setup to deliver reliable gloss‑change measurement and visual scratch grading for high‑gloss, semi‑gloss and mat‑finish laminate flooring.
✅ Standard Compliance: EN 16094:2021, referenced to EN ISO 12947‑1, EN ISO 12945‑2
✅ Full‑function: Micro‑scratch test (A/B) + mat‑surface polishing‑effect test (C)
✅ Built‑in Lissajous‑figure verification function per Annex A, ensures movement trace symmetry
✅ Exact weight tolerance for version 1 & version 2 holders for consistent test load
✅ Suitable for laminate‑floor factory quality‑control, R&D new‑product development, third‑party ISO‑17025 laboratory certification and European market pre‑compliance testing.
This equipment simulates real‑world fine micro‑scratch damage and polishing‑brightening defects caused by daily foot traffic, tracked‑in grit and furniture friction. UnitedTest’s EN 16094 test machine helps flooring manufacturers obtain repeatable MSR‑A / MSR‑B classification results, evaluate matte‑surface polishing tendency, optimize wear‑layer formulation and surface texture design, reduce consumer complaint risks.
Require More Customized Solutions?