Information on the most widely used ASTM standards within the materials testing industry
EN 13770 Textile Abrasion Resistance Tester for Knitted Footwear Garments | UnitedTest
UnitedTest supplies EN 13770 abrasion testing machines for knitted footwear garments including socks, ankle socks and heavy tights. This standard defines two independent test methods to evaluate textile abrasion performance, with separate reporting requirements.
EN 13770 Textiles‑Determination of the abrasion resistance of knitted footwear garments. EN 13770 defines two test methods for the abrasion resistance of knitted footwear garments — e.g. ankle socks, socks, heavy tights — applicable irrespective of size, composition and construction. The two methods are independent. The method must be chosen before starting the test and recorded in the test report, because results from the two methods cannot be compared with each other.
Two Specific EN 13770 Test Methods, Principles, Equipment, Specimen Information, Key Parameters and Test Stipulations
| Method 1: Martindale Abrasion Machine Method | |
Test Principle | Circular hosiery specimens taken from high‑wear sock zones are stretched over a flattened rubber surface. Specimens undergo cyclic Lissajous‑pattern planar abrasion motion against standard reference abradant under defined pressure. Abrasion performance is quantified as cycle counts until test endpoint: either hole formation (thread rupture) or fabric thinning of one yarn component in plated constructions (e.g. nylon‑cotton plated knit). |
| Test Equipment | Martindale abrasion‑testing machine complying with EN ISO 12947‑1. - Modified special specimen holder assembly: guide spindle, holder body, needle ring, holder nut, rubber sphere with 20 mm flat test surface - Spring‑loaded tightening‑block spanner (to maintain rubber flatness during clamping) - Standard Martindale abradant and woven wool felt substrate - 2.5 kg pressing weight (120 ± 10 mm diameter) for mounting abradant material |
| Test Specimen |
|
| Main Test Parameters |
|
| Test Procedure | 1. Mount specimen into modified holder assembly: fix specimen via needle ring, fit rubber sphere, assemble holder body‑nut with spring‑loaded spanner to keep fabric flat and properly stretched. 2. Mount new abradant and wool felt onto Martindale tables, compress with 2.5 kg weight then secure clamping ring. 3. Install assembled specimen holders onto machine, apply 12 kPa load pieces. 4. Set counter, zero totalising counter, start machine. 5. Stop at pre‑set inspection intervals to check for abrasion endpoint, remove pills if present. 6. Record rub cycles reaching thinning or hole failure. 7. Complete test report including method reference, sample ID, sampling area, endpoint type, individual cycle values, range/mean (if needed), and any deviations from standard requirements. |
| Method 2: Abrasion on Leg Forms | |
Test Principle | Full knitted hosiery garments are fitted onto volumetric leg forms, stretched to replicate real‑wear tension status. A dedicated abrasion tester delivers reciprocating linear rubbing motion against target test zones. Abrasion resistance is measured as cycle counts until endpoint: hole breakthrough or single‑component yarn thinning, same endpoint definition as Method 1. |
| Test Equipment |
Interchangeable curved abradant shoes (10 mm width matching leg‑form curvature). Optional additional load weights for slipper.
Leg forms can be mounted vertically (test sole, toe‑heel reinforcement) or horizontally (test heel‑back, leg section).
|
| Test Specimen |
Extra test locations (leg, heel‑leg seam, toe) can be added by mutual agreement.
|
| Main Test Parameters |
|
| Test Procedure |
|
Industry Application Fields
Hosiery and sock manufacturers (in-line QC, batch release, supplier comparison) and private-label/brand buyers setting durability specifications.
Product development: evaluating fibre blends (cotton, wool, bamboo, recycled polyester), yarn counts, plated constructions (nylon/cotton, nylon/wool), toe/heel reinforcement, terry/loop density, and finishes.
Performance segments: sports, outdoor, workwear and safety footwear socks, military, medical/compression and diabetic hosiery, children's socks (high abrasion zones).
Retailer/e-tender specifications and third-party labs (SGS, Intertek, TÜV, SATRA-type labs) as sole-source or comparative durability evidence; claim substantiation ("longer lasting", "reinforced heel") and complaint/arbitration between supplier and buyer.
Durability/eco-design and circular-economy programmes, where extended service life is a measurable sustainability KPI.
Related Standard:
| ISO 12947-1 | Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 1: Martindale abrasion testing apparatus |
| ISO 12947-2 | Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 2: Determination of specimen breakdown |
| ISO 12947-3 | Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 3: Determination of mass loss |
| ISO 12945‑2 | pilling & fuzzing on the modified Martindale apparatus — same machine family, different end point |
| ISO 5470-1 | Rubber- or plastics-coated fabrics - Determination of abrasion resistance - Part 1: Taber abrader |
| ISO 5470-2 | Rubber- or plastics-coated fabrics. Determination of abrasion resistance. Martindale abrader |
| ASTM D4966 | Standard Test Method for Abrasion Resistance of Textile Fabrics (Martindale Abrasion Tester Method). |
| ASTM D4970 | Standard Test Method for Pilling Resistance and Other Related Surface Changes of Textile Fabrics: Martindale Tester |
| GB/T 21196.1 | Textiles-Determination of the abrasion resistance of fabrics by the Martindale method-Part 1:Martindale abrasion testing apparatus |
| JIS L 1096, M&S P19 | other commonly referenced abrasion/pilling methods |
| GBT 4802.2 | Textiles - Determination of fabric propensity to surface fuzzing and to pilling - Part 2: Modified Martindale method |
| EN 13770 | Textiles - Determination of the abrasion resistance of knitted footwear garments |
| EN 16094 | Laminate floor coverings. Test method for the determination of micro-scratch resistance |
Keywords: EN 13770 abrasion tester, knitted footwear garment abrasion test, sock abrasion resistance tester, ankle sock abrasion testing, heavy tights textile abrasion machine, textile abrasion test equipment, knitted fabric abrasion measurement, footwear textile durability test, UnitedTest textile abrasion tester, textile wear resistance test machine
Related products and device
Related Standard
ISO 12947-1 Textiles — Determination of the abrasion resistance of fabrics by the Martindale method — Part 1: Martindale abrasion testing apparatus
ISO 12947-1 defines mandatory construction, dimensional, performance and auxiliary‑material requirements for Martindale abrasion testers, which are used to carry out the practical test procedures laid down in ISO 12947‑2,‑3,‑4. It is the specification for the machine and the consumables — the "hardware norm". The actual abrasion procedures live in Parts 2, 3 and 4, and Part 1 is written to guarantee that a Martindale result obtained in one lab is physically comparable to one obtained in another.
ISO 5470-1: Rubber- or plastics-coated fabrics -- Determination of abrasion resistance -- Part 1: Taber abrader.
ISO 5470-1 specifies a method for determining the abrasion resistance of rubber- or plastics-coated fabrics using the Taber abrader apparatus. This test simulates wear under controlled conditions to evaluate a material's durability.
ISO 12947-3 Textiles — Determination of the abrasion resistance of fabrics by the Martindale method — Part 3: Determination of mass loss
ISO 12947-3 applies to all textile fabrics including nonwovens, and is used to determine the mass loss of specimens after controlled abrasion. It is explicitly not intended for fabrics where the specifier states the end performance is a deliberately low abrasion wear life.
ISO 13937-2 Textiles – Tear properties of fabrics – Part 2: Determination of tear force of trouser‑shaped test specimens (Single tear method).
ISO 13937-2 is method for determining the tear force required to propagate an already-started single tear, using a rectangular specimen slit into two "trouser legs". Mainly for woven fabrics; may also apply to fabrics made by other techniques (e.g. some nonwovens). Not applicable to knitted fabrics, woven elastic fabrics, highly anisotropic fabrics, or loose fabrics where the tear tends to transfer from one direction to another. Only CRE (constant-rate-of-extension) machines are permitted.
ASTM D5035 : Standard Test Method for Breaking Force and Elongation of Textile Fabrics (Strip Method)
ASTM D5035 is the standard test method for determining breaking force (tensile strength) and elongation at break of textile fabrics using the strip method. It defines two core procedures--raveled strip (for woven fabrics) and cut strip (for nonwovens, coated/felted fabrics)--and supports both dry and wet testing.
ISO 12945-2 Textiles — Determination of fabric propensity to surface pilling, fuzzing or matting — Part 2: Modified Martindale method
ISO 12945-2 specifies a method for determining the resistance to pilling, fuzzing and matting of textile fabrics using a modified Martindale machine. It ranks fabrics in the same order of surface-change propensity as is likely to occur in end-use wear.
ASTM D4966 Standard Test Method for Abrasion Resistance of Textile Fabrics (Martindale Abrasion Tester Method)
ASTM D4966 determination of the abrasion resistance of textile fabrics using the Martindale abrasion tester; generally applicable to knit, woven and nonwoven fabrics — material thickness may limit suitability because of specimen-holder capacity. It applies to woven, knit and non‑woven textiles, though excessive fabric thickness may restrict testing due to specimen‑holder physical limits.
ASTM D4970 Standard Test Method for Pilling Resistance and Other Related Surface Changes of Textile Fabrics: Martindale Tester.
ASTM D4970 is the Martindale (Lissajous‑motion) fabric‑on‑fabric pilling test used to predict how badly a fabric will pill, fuzz or otherwise change its surface appearance in wear, reported on an arbitrary 5‑to‑1 rating scale (5 = no pilling, 1 = very severe pilling).
ISO 12947-2 Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 2: Determination of specimen breakdown
ISO 12947-2 measuring how many abrasion cycles — or "rubs" — a fabric withstands before itreaches a defined end point. A circular specimen is mounted in a holder under a defined loadand rubbed against a standard woven wool abradant in a translational movement tracing a Lissajous figure, while the holder rotates freely about its own axis. The abrasion resistance isreported as the number of rubs at the last inspection interval before specimen breakdownoccurs.
Because the end point is defined inside the standard — two broken threads for woven fabrics,one for knitted fabrics, a fully worn-off area for pile and flocked fabrics, a hole of at least 2.5mm for nonwovens — results are objective and comparable between laboratories. That is whythe Martindale figure is the durability number most often written into upholstery and contracttextile specifications.
ISO 17704 Footwear — Test methods for uppers, linings and insocks — Abrasion resistance
ISO 17704 is method for determining the resistance of uppers, linings and insocks — irrespective of material — to wet and dry abrasion, in order to assess suitability for the end use. Note the standard deliberately gives no pass/fail criteria; it produces a description and rating of damage at prescribed rub counts.
FAQs for EN 13770 Test (Knitted Footwear Abrasion Resistance)
A European standard that specifies two laboratory test methods for measuring the abrasion (wear) resistance of knitted footwear garments — for example ankle socks, socks and heavy tights. The result is always expressed as the number of rubs (Method 1) or cycles (Method 2) needed to reach a defined endpoint.
Any knitted footwear garment: ankle socks, crew socks, dress socks, sports socks, heavy tights, and knitted shoe-liners. The standard explicitly applies irrespective of size, fibre composition and knit structure, so it covers cotton, wool, bamboo, polyester, nylon, blends, plated constructions, terry/cushioned soles and reinforced toe/heel designs alike.
Because a sock is not a flat fabric. It is elastic, tubular and worn stretched over a three-dimensional foot inside a shoe, flexing under load. The two methods reproduce that condition at different levels:
Method 1 (Martindale) — a flat-ish, stretched circular specimen on a modified holder; efficient and inexpensive, good for routine quality control.
Method 2 (leg forms) — the whole garment stretched on a volumetric leg form, "as in wear"; the more realistic, whole-product approach, preferred for R&D, claim substantiation and dispute arbitration.
No. The Introduction of EN 13770 states that the method must be chosen before the test starts and recorded in the report, because results of the different methods cannot be compared with each other. Never mix or convert rub counts and cycle counts.
A hole, which usually develops when one thread/loop breaks, causing an opening to appear. In knits you typically see hole formation rather than the "two broken threads" endpoint used for woven fabrics.
When the garment is knitted with a filament yarn plated together with a spun staple yarn (e.g. nylon/cotton or nylon/wool), the spun component can wear away first, leaving a thin base of the filament yarn. That "thinned" area is a legitimate endpoint, even though no hole has appeared. This is unique to hosiery and is why EN 13770 defines two endpoints.
Whichever your specification requires — hole, thinning, or both. If both are determined, the report must state clearly which rub/cycle count belongs to which endpoint.
Yes — the machine itself is the standard EN ISO 12947-1 Martindale. But you must add the modified sock abrasion holder assembly (needle ring + 20 mm rubber sphere + holder nut/body) and the spring-loaded tightening block spanner, and you must apply the 12 kPa loading piece. A standard flat abrasion head will not reproduce the stretched state the method requires.
The garment must be tested on the leg form of the same size as the garment. For multi-size ("one size fits all") socks, testing may be repeated on several leg-form sizes. The size actually used must be reported.
Yes. With the leg form vertical you test the sole and the toe/heel reinforcement; with the leg form horizontal you test the back of the heel and the leg.
Yes. In Method 1, pills must be removed with sharp, curved-blade scissors during inspection, because pills obscure the surface and distort the assessment.
Method 1: reference to Method 1 of EN 13770; sample reference; sampling area (sole/heel); endpoint (thinning and/or hole); individual rub counts per endpoint; range/mean if required; any deviation that could have affected results.
Method 2 adds: sample reference including size designation, any additional load used, and the leg-form size used.
Because flat abrasion testing cannot replicate real sock wear. A sock is engineered to contour to a foot and is abraded while stretched and flexing inside a shoe. Flat testing ignores that stretch, curvature and tension pattern, so it can rank two yarns differently from real life. EN 13770 was written specifically to reproduce the worn geometry and the stretch state.
Heel and toe are the failure hot-spots — holes there are the number-one consumer complaint and return reason for socks; both methods target exactly those known wear areas.
It captures the failure mode flat tests miss — "thinning" of plated nylon/cotton knits, where the spun yarn abrades away and only the filament skeleton remains.
It quantifies design levers — fibre type and blend, yarn count, plating, loop length and density, reinforcement yarns, terry cushioning, plating and finishing treatments can all be ranked objectively with a number.
It supports specifications, trade and dispute resolution — a single EU-harmonised method with mandatory report items removes ambiguity between supplier, brand and third-party laboratory.
It underpins durability and sustainability claims — extended service life is now a measurable KPI in eco-design and circular-economy programmes.
Not directly. As with all laboratory abrasion tests, the result is a comparative ranking under controlled conditions, not a calendar life prediction. It becomes meaningful when correlated with wear trials or historical field data. ASTM D4966 carries the same caution for flat fabrics.
Conditioning — always 20 ± 2 °C / 65 ± 4 % RH (EN 20139), specimens relaxed and tension-free.
Mounting tension/stretch — over-stretching the knit during cutting and mounting is the classic error; use the spring-loaded block (35 N) and the correct leg-form size.
Abradant condition and replacement — respect the 50 000-rub (Method 1) and 500-cycle (Method 2) replacement rules; change soiled felt.
Operator judgement of the endpoint — use short inspection intervals near the endpoint, brush/de-pill the surface, and if possible use the same trained assessor or photographic reference standards.
Number of specimens — use the full sampling plan (≥4 discs per sock, or 12 tests in Method 2) and report mean and range.
EN 13770 uses the Martindale machine and motion of ISO 12947-1 but replaces the specimen holder with a special sock assembly. ISO 12947-2/-3/-4 (specimen breakdown, mass loss, appearance change) and ASTM D4966 are the general flat-fabric Martindale routes; GB/T 21196.1–.4 is the Chinese equivalent of the ISO 12947 series. None of them reproduces the stretch state of a worn sock, so none replaces EN 13770 for hosiery.
No. Pilling is covered by EN ISO 12945-1/-2 and ASTM D4970, which use the same Martindale platform but a different test head and a completely different endpoint. EN 13770 only instructs you to cut off pills so they do not interfere with the abrasion assessment.