Home >> Application >> By Standard >> Others >> EN 12090 Shear Test for Thermal Insulating Products

EN 12090 Shear Test for Thermal Insulating Products

Share:

EN 12090 Shear Behaviour Tester for Building Thermal Insulation | UnitedTest

UnitedTest manufactures EN 12090 shear test machine for thermal insulating products. This standard evaluates shear strength and shear modulus of building insulation materials via tangential shear loading, supporting construction material certification, quality control and R&D.


EN 12090 specifies a reliable test method to measure the practical shear behaviour of building thermal insulation materials. The test specimen is securely bonded between rigid mounting plates, and the plates are displaced tangentially against each other at a precisely controlled test speed. Engineers capture force-displacement data throughout the test to calculate key performance indicators including shear strength and optional shear modulus. This standard is widely used for foam insulation, mineral wool, rigid cellular insulation and other construction thermal insulating products, helping labs, manufacturers and certification bodies verify structural stability under shear load, assess long-term in-service performance, and meet European construction regulatory requirements. UnitedTest supplies fully compliant EN 12090 shear behaviour testing machines with custom fixtures, stable speed control and accurate data acquisition for consistent, repeatable insulation shear testing.


Test Principle

A test specimen is bonded to rigid support plates, which transmit shear stress by applying two opposite parallel forces tangentially to the major faces of the specimen. The full force-displacement curve is recorded to derive shear strength and (if required) shear modulus.

The standard explicitly notes that this test does not measure pure shear, but it replicates the real-world tangential stresses acting on insulation in wall systems and other building assemblies more realistically than alternative methods such as bending tests. Both test configurations show some degree of thickness dependence in measured shear strength values.


Test Methods:

Two alternative test arrangements are specified:

  • Single test specimen method: One specimen is bonded between two parallel rigid plates. One plate is fixed to the test machine frame, and the other is attached to the movable crosshead to apply longitudinal shear force. This method is limited to a maximum product thickness of 50 mm.

  • Double test specimen method: Two identical specimens are arranged symmetrically. A central movable plate applies shear to both specimens simultaneously, against two outer fixed plates. This configuration balances lateral forces and reduces bending effects on the specimens.


Test Equipment required for EN 12090 Shear Test for Thermal Insulating Products

Universal testing machine    

Must deliver a constant displacement rate of (3 ± 0.5) mm/min parallel to the longitudinal axis of the test assembly.

Force measurement accuracy: maximum error of 1 % of applied force F.

Displacement measurement accuracy: maximum error of 1 % of relative displacement Y between movable and fixed supports.

Simultaneous force-displacement data recording is mandatory when shear modulus is to be determined.

A displacement transducer is recommended for high-accuracy deformation measurement, especially with thick adhesive layers. 

Blank tests using metal blocks may be performed to subtract deformation of the equipment and adhesive itself.

Specimen supports

Single specimen assembly: Two flat, rigid steel supports (330 mm long × 50 mm wide, typically 16 mm thick mild steel), connected to machine grips via adaptors and universal joints. 

The adaptor thickness must match the specimen thickness.

Double specimen assembly: Three flat, rigid support plates. The two outer plates are fixed and the central plate moves. 

Extremely high rigidity is required to maintain parallel alignment; two validated configurations are defined in the standard.

EN 12090 Shear Test for Thermal Insulating Products

Adhesive

The bonding adhesive must have a higher shear strength and higher shear modulus than the insulation material under test, to ensure failure occurs within the specimen rather than at the bond line. 


Test Specimen Information:

ArrangementLengthWidthThickness
Single250 mm (+0 / −1 mm)50 mm (−0,1 mm)Product thickness, maximum 50 mm
Double, each part200 mm (−0,5 mm)100 mm (+0 / −1 mm)Product thickness (no 50 mm cap in the test standard itself)

Quantity: At least 5 specimens, unless otherwise specified in the relevant product standard or agreed between parties.


Test Parameters & Stipulations

  • Loading rate: (3 ± 0.5) mm/min constant crosshead speed.

  • Alignment tolerance: The distance between the two major planes of the test assembly must not vary by more than 1 %.

  • Result rules: Results are reported as mean values to two significant figures. Results cannot be extrapolated to other thicknesses; product-to-product comparisons are only valid for specimens of similar thickness tested by the same method.


Test Procedures for EN 12090 Shear Test for Thermal Insulating Products

  1. Measure the three dimensions of the specimen in accordance with EN 12085.

  2. Bond the specimen to the rigid supports with a suitable adhesive.

  3. Check that the distance between the two major planes of the test assembly does not vary by more than 1 %.

  4. Mount the assembly in the test machine.

  5. Apply force to the movable support plate to produce vertical movement at (3 ± 0,5) mm/min.

  6. Record the force–displacement curve (F, y).

  7. Continue to rupture / maximum force.

  8. Discard any specimen that fails in the adhesive layer between specimen and rigid supports, and repeat with a new specimen.


Industry Application Fields

Materials: mineral wool (MW), expanded polystyrene (EPS), extruded polystyrene (XPS), rigid polyurethane/polyisocyanurate (PUR/PIR), phenolic foam (PF), cellular glass (CG), wood wool/wood fibre (WW/WF), expanded perlite, expanded cork (ICB), and other factory-made or in-situ thermal insulating products .

Product / application areas:

  • Building envelopes: external thermal insulation composite systems (ETICS / EIFS), cavity walls, bonded and mechanically fixed insulation systems.

  • Perimeter insulation: basement walls and insulation under loadbearing foundation slabs, where vertical/horizontal forces create shear in the insulation layer .

  • Multi-layer / sandwich boards: quality control of adhesive bonds between layers; core shear data for panel design .

  • Building equipment & industrial installations: EN 14307 (XPS), EN 14309 (EPS), and BS ISO 18097 reference EN 12090 .

Who uses it:

  • Insulation manufacturers — product development, formulation comparison, factory production control (FPC), performance declarations.

  • Accredited / notified test laboratories and certification bodies — compliance testing, CE marking, technical approvals .

  • Specifiers, structural/building engineers and consultants — selecting products for wall assemblies where tangential stresses, sliding, layering and adhesive joints are critical.

  • Regulators and standards committees — harmonised comparative data.


Related Standard: 

ISO 844Rigid cellular plastics – Determination of compression properties.
ASTM C273Standard Test Method for Shear Properties of Sandwich Core Materials – the most widely used North American equivalent for foam core shear testing.
ASTM C297Rigid cellular plastics – Determination of flexural properties.
ASTM C365Flatwise compressive strength/modulus of core
ASTM C364Edgewise compressive strength of sandwich panel
EN 1605

deformation under compressive load & temperature

ISO 1922Rigid cellular plastics - Determination of shear properties
ISO 1926
Rigid cellular plastics — Determination of tensile properties 
EN 12089Thermal insulating products for building applications - Determination of bending behaviour
EN 12090Thermal insulating products for building applications. Determination of shear behaviour
ASTM C393

Standard Test Method for Core Shear Properties of Sandwich Constructions by Beam Flexure

ASTM D1621Standard Test Method for Compressive Properties of Rigid Cellular Plastics
ASTM D7249Facing strength/stiffness by long-beam 4-point flexure
ASTM D905Standard Test Method for Strength Properties of Adhesive Bonds in Shear by Compression Loading
EN 826Thermal insulating products for building applications. Determination of compression


Keywords: EN 12090 shear tester, thermal insulation shear behaviour test, building insulation shear strength, shear modulus test, rigid foam insulation shear test, mineral wool shear testing machine, construction thermal insulation test equipment, insulation material mechanical test, EN 12090 test fixture, building material lab testing, thermal insulating product certification, shear force displacement test, insulation QC test rig, European construction material test, cellular plastic shear tester

Related products and device

EN 12090 Thermal Insulating Products Shear Test Universal Testing Machine

A single column tensile tester is a sophisticated material testing instrument designed for measuring mechanical properties of various materials under tension, compression, bending, shear, and other loading conditions. As the name suggests, it features a single vertical column supporting a moving crosshead that applies force to test specimens.

EN 12090 rigid foam insulation shear test

UnitedTest manufactures and exports compressive shear test fixtures, ISO 6238 wood adhesive shear jigs, ASTM D905 block shear fixtures, ASTM D4501 rigid‑substrate shear tools, and compatible universal testing machines. Buy ISO 6238 and ASTM D905 compressive shear test fixtures from UnitedTest.

EN 12090 test fixture, building material lab testing

Vice Tensile test fixture for plastics is based on the test standatd ASTM D638, determination of the tensile properties of unreinforced and reinforced plastics in the form of standard dumbbell-shaped test specimens when tested under defined conditions of pretreatment, temperature, speed.

Related Standard

ASTM C273 Sandwich Core Materials Shear Test –

ASTM C273 Standard Test Method for Shear Properties of Sandwich Core Materials

ASTM C273 defines procedures to determine the shear properties of sandwich core materials, including in-plane shear strength and shear modulus corresponding to through-thickness shear strain. It applies to cores with continuous bonding surfaces (e.g., balsa wood, polymer foams) and discontinuous bonding surfaces (e.g., honeycomb cores). Tests may be conducted on bare cores bonded directly to loading plates, or on complete sandwich panels with facings.

ISO 1922 Shear Properties Test for Rigid Cellular Plastics –

ISO 1922 Rigid cellular plastics – Determination of shear properties

ISO 1922 defines a standardized procedure to measure shear strength of rigid cellular plastics, and additionally provides methods to calculate shear modulus and shear strain at fracture.


ASTM D1761 Test Methods for Mechanical Fasteners in Wood –

ASTM D1761 test methods provide a basic procedure for evaluating the withdrawal and lateral resistance of fasteners installed in wood and wood-based materials. The tests also provide a basis for determining comparable performance of different types and sizes of fasteners installed in wood and wood-based materials.  Quantify the mechanical connection performance of nails, staples, screws, bolts, lag screws and timber connectors embedded in solid wood, plywood, OSB, fiberboard and other wood-based composites. Spikes are classified as nails within this standard.

ASTM D1037 Test Methods for Wood-Base Fiber and Particle Panel Materials –

ASTM D1037 - Standard Test Methods for Evaluating Properties of Wood-Base Fiber and Particle Panel Materials 


ASTM D1037 test methods cover the determination of the properties of wood-base fiber and particle panel materials that are produced as mat-formed panels such a particleboard, medium density fiberboard, hardboard, and oriented strand board.


ASTM D1037 test methods cover small-specimen tests for wood-base fiber and particle panel materials that are made to provide: Data for comparing the mechanical and physical properties of various materials,

Data for determining the influence on the basic properties of such factors as raw material and processing variables, post-treatments of panels, and environmental influences, and

Data for manufacturing control, product research and development, and specification acceptance.

ASTM D897 Tensile Test of Adhesive Bonds –

ASTM D897 prescribed a method for determining the comparative tensile properties of adhesive bonds in a standard specimen when tested under specific conditions. Its primary purpose was to measure the tensile strength of an adhesive bond between two rigid substrates (metal to metal). 

ASTM D1002 Lap Shear Test of Adhesively Bonded Metal Specimens –

ASTM D1002 is the most widely used standard test for measuring the apparent shear strength of metal‑to‑metal adhesive single‑lap joints under tension loading. It provides comparative data for adhesive selection, process control, and quality assurance in structural bonding applications. It is the most common test for evaluating adhesive shear performance.

ASTM D1621 Rigid Cellular Plastics Compression Testing –

ASTM D1621 Standard Test Method for Compressive Properties of Rigid Cellular Plastics

ASTM D1621 determining the compressive properties of rigid cellular materials, expanded/rigid plastic foams, particularly expanded plastics. It compresses a conditioned foam specimen between two flat platens at a controlled speed and records a complete load–deflection curve.

Frequently Asked Questions (FAQs) about EN 12090 Shear Behaviour Test

EN 12090:2013 specifies how to determine the shear behaviour of thermal insulating products for building applications. UnitedTest supplies EN 12090 shear test machines, single- and double-specimen shear fixtures, and universal testing systems configured for this method — from the required (3 ± 0.5) mm/min constant crosshead speed and ≤ 1 % force and displacement accuracy to simultaneous force–displacement recording for shear strength (τ) and shear modulus (G). Whether you test EPS, XPS, mineral wool, PUR/PIR, phenolic foam or cellular glass in an accredited laboratory or a factory production-control line, a correctly aligned, rigid fixture is what separates a valid EN 12090 result from a discarded one.


Q1. Does EN 12090 measure pure shear?

A: No. The standard states explicitly that the test does not determine pure shear behaviour; it measures the effect of applying two opposite parallel forces tangentially to the major faces of the specimen. "Shear" is used by convention. This loading is chosen because it represents the stresses on insulation in real building applications — especially walls — more closely than bending-type shear methods.


Q2. What properties does an EN 12090 test report?

A: Two: shear strength τ (maximum force divided by the shear plane area, in kPa) and, if required, shear modulus G (shear stress divided by relative deformation in the linear region below the proportional limit, in kPa). Both are reported as the mean of individual values to two significant figures, together with all individual results.


Q3. Which materials does EN 12090 cover?

A: Thermal insulating products in general — mineral wool (MW), EPS, XPS, PUR/PIR, phenolic foam (PF), cellular glass (CG), wood wool / wood fibre, expanded cork, expanded perlite and multi-layer insulation boards. Product standards such as EN 13162–EN 13171 decide whether shear behaviour is a declared characteristic and may specify different specimen dimensions.


Q4. Why is the EN 12090 shear test important for insulation materials?

A: Because insulation in a wall is loaded tangentially, not just in compression. In an ETICS façade, the self-weight of the render and insulation system, wind action and thermal movement create shear stress in the insulation layer and at its adhesive bonds. EN 12090 reproduces that stress state, giving a declared mechanical property that engineers, specifiers and certification bodies can use instead of an estimate.


Q5. Why is shear strength critical for ETICS / external wall insulation systems?

A: It governs the ability of a bonded system to carry its own permanent weight over decades. ETICS approval guidance (ETAG 004-type requirements) includes a minimum shear strength commonly cited as ≥ 0.02 N/mm² (20 kPa); typical XPS values are around 0.20 N/mm². Shear and tensile properties also drive resistance to wind suction and to mechanical fixings. A low or highly scattered shear result signals a product that may creep, delaminate or slide in service.


Q6. Why is shear modulus needed as well as shear strength?

A: Strength gives the ultimate load capacity; modulus gives the stiffness under service load. G controls elastic deflection, layer displacement and stability of the insulation as a statically effective layer, and it is an input to structural calculations and finite-element models. EN 12090 derives G from the slope of the initial linear portion of the force–displacement curve, which is why simultaneous F and y recording is mandatory when G is requested.


Q7. Why not use a bending test such as EN 12089 or ASTM C393 instead?

A: EN 12090's scope says tangential loading on the major faces is more representative of wall stresses than bending methods. A bending test introduces combined tensile, compressive and shear stresses and depends on span and facing behaviour; the plate-shear arrangement isolates the in-plane response of the insulation itself. Bending remains useful for flexural behaviour, but it is not a substitute.


Q8. Why does specimen thickness matter so much in EN 12090?

A: Both arrangements show thickness-dependent results; the single-specimen method additionally shows more scatter at greater thicknesses. Therefore the standard forbids extrapolating results to other thicknesses and requires that products be compared only on specimens of similar thickness tested with the same arrangement. Always report the actual thickness — this is especially relevant today, because ETICS boards of 100–200 mm are common while the single-specimen method caps thickness at 50 mm.


Q9. Where else is shear behaviour relevant besides façades?

A: Perimeter insulation at basement walls and under loadbearing foundation slabs (vertical/horizontal forces in the insulation layer), multi-layer boards bonded with adhesive (shear tests double as a bond-quality check), sandwich panel cores, and insulation for building equipment and industrial installations (EN 14307 / EN 14309).


Q10. What equipment is needed for an EN 12090 test?

A: A universal testing machine with a controlled constant-speed drive, a set of rigid specimen supports / shear fixtures (single or double arrangement), an adhesive stronger than the product, and a system to record force and displacement simultaneously. A displacement transducer is recommended — and often necessary — when shear modulus is required or a thick adhesive layer is used.


Q11. Can one universal testing machine run both the single and double specimen arrangements?

A: Yes — the machine is the same; the fixture set changes. The single arrangement uses two parallel rigid plates (one fixed, one moving) with 330 × 50 × 16 mm supports and adaptors whose thickness equals the specimen thickness. The double arrangement uses three parallel rigid plates, with the two outer plates fixed in parallel vertical planes and the central plate on the moving crosshead. A dual-column electromechanical UTM with interchangeable fixtures and a universal-joint load train is the standard industry configuration.


Q12. Do I need an extensometer or displacement transducer?

A: Only crosshead displacement may be enough for shear strength alone, but for shear modulus you need accurate relative displacement of the plates. EN 12090 explicitly allows (and recommends for thick adhesive layers) a displacement transducer, and permits a blank test to zero out machine and adhesive compliance. If you plan to also run ISO 1922 Procedure B or ASTM C273, specify a clip-on extensometer from the start.


Q13. What specimen sizes does EN 12090 require?

A: Single specimen: 250 mm long × 50 mm wide, thickness = original product thickness with a maximum of 50 mm. Double specimen: two parts, each 200 mm long × 100 mm wide, thickness = product thickness. Skins, facings and coatings must be retained, and dimensions measured per EN 12085. Parallelism/flatness between the two major faces must be within 0.5 % of thickness (max 0.5 mm).


Q14. How many specimens are required?

A: The number is set by the relevant product standard or European Technical Specification; if none is specified, at least five specimens must be tested. If there is no product standard at all, the number may be agreed between the parties.


Q15. How does EN 12090 differ from ISO 1922?

A: Both use single/double plate-shear arrangements and reject adhesive failures, but ISO 1922:2018 applies to rigid cellular plastics, runs at (1 ± 0.5) mm/min (vs 3 ± 0.5 mm/min), fixes the single specimen at 250 × 50 × 25 mm (vs product thickness ≤ 50 mm), conditions at 23 ± 2 °C / 50 ± 10 % RH, requires an ISO 7500-1 Class 1 machine, and defines Procedure A (strength only) and Procedure B (extensometer for modulus and strain).


Q16. How does EN 12090 differ from ASTM C273?

A: ASTM C273/C273M-20 targets sandwich core materials (foam, balsa, honeycomb) for panel design. It requires specimen length ≥ 12 × thickness, width ≥ 50 mm, ~0.5 mm/min with failure in 3–6 minutes, and — like EN 12090 — explicitly states it does not produce pure shear and accepts only core shear failures. EN 12090 is specific to building thermal insulation products, uses fixed specimen sizes, and runs at 3 ± 0.5 mm/min.


Q17. Which standards are related to EN 12090?

A: EN 12085 is the normative dimensional reference. EN 12090 belongs to the CEN/TC 88 family alongside EN 822–825, EN 826 (compression), EN 1602, EN 1603/1604, EN 1605, EN 1606 (creep), EN 1607/1608 (tensile), EN 1609, EN 12086–12089 (water vapour, water absorption, bending), EN 12091, EN 12429–12431, EN 13793 and EN 13820. It is called up by product standards EN 13162–EN 13171 and EN 14307 / EN 14309.

< Previous: None

> Next: EN 826 Compression Testing Machine for Thermal Insulation

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.