Information on the most widely used ASTM standards within the materials testing industry
ISO 1922 Rigid Cellular Plastics Shear Property Tester | UnitedTest
UnitedTest manufactures ISO 1922 shear testing machines for rigid cellular plastics. Our equipment accurately measures shear strength, shear modulus and fracture shear strain for foam insulation, structural foam and rigid cellular plastic materials for quality control and material qualification.
ISO 1922 defines a standardized laboratory procedure to measure shear strength of rigid cellular plastics, and additionally provides calculation methods for shear modulus and shear strain at fracture. This standard is widely adopted for rigid foam materials used in construction insulation, packaging, composite core panels and structural components. Shear performance data helps engineers evaluate material deformation, bonding reliability and structural safety under lateral shear load, supporting product formulation development, batch inspection, third-party lab testing and compliance verification. UnitedTest’s ISO 1922 shear test machine delivers stable, repeatable test results to meet your rigid cellular plastic material testing requirements.
Test Principle
The test applies controlled shear stress to a geometrically defined foam specimen using rigid metal supports bonded directly to the specimen surfaces. By moving one set of supports relative to the fixed set along the longitudinal axis of the specimen assembly, uniform shear deformation is induced across the foam core. There are two core configurations and two test procedures:
Single-shear configuration: one foam layer between two plates, creating one shear plane.
Double-shear configuration: two foam layers between three plates, creating two parallel shear planes.
Procedure A: for shear strength only.
Procedure B: for shear strength, modulus and strain, using high-precision displacement measurement.
Specific Test Methods
Single shear test: One foam specimen is bonded between two rigid loading plates. One plate is fixed to the test machine frame, the other to the movable crosshead. Shear acts across a single plane within the foam.

Double shear test: Two foam specimens are bonded between three rigid plates. The two outer plates are fixed, and the central plate is pulled in tension. This creates two identical shear planes and balances the loading, reducing bending effects.
| Feature | Procedure A | Procedure B |
|---|---|---|
| Primary purpose | Shear strength measurement only | Shear strength, shear modulus and shear strain |
| Displacement measurement | Test machine crosshead displacement | Extensometer or equivalent precision device |
| Displacement accuracy | ±5 % or ±0.1 mm (whichever is more accurate) | ≥ ±1 % |
| Recommended use | Routine quality control for strength | Full material characterization and design data |
Test Equipment required for ISO 1922 Shear Properties Test for Rigid Cellular Plastics
| Universal testing machine | Capable of constant crosshead speed of (1 ± 0.5) mm/min, with speed variation ≤10 % during the test. Conforms to Class 1 of ISO 7500-1, with force measurement error ≤1 %. Equipped with grips, adaptors and universal joints to ensure axial alignment and eliminate bending moments. |
| Rigid specimen supports | Flat rectangular plates (typically mild steel), 330 mm long, 50 mm wide and (16 ± 1) mm thick. 2 plates for single shear, 3 plates for double shear. Load-spreading plates (50 × 50 × 5 mm) are integrated into the grip assembly. Adaptor thickness matches specimen thickness to maintain alignment. |
| Displacement measurement systems | Machine-integrated displacement sensor for Procedure A. Extensometer (or equivalent) mounted between the rigid supports for Procedure B, centered along the specimen length. |
| Adhesive system | Shear strength and modulus must be significantly higher than the foam being tested, to ensure failure occurs within the cellular material, not at the bond interface. Must be chemically compatible with the test material. Epoxy-based adhesive is recommended for most materials. |
Test Specimen Information:
Single shear specimen
- Dimensions: length = 250 mm; width = 50mm; thickness = (25 ± 0.5) mm.
- Square cut with 90° corners.
- Moulding skins are removed; surfaces are machined without altering the original cellular structure.
Double shear specimen
- Dimensions: length = 250 mm; width = 50mm; thickness = as-produced original product thickness.
- Moulded skins, facings and coatings are retained.
Specimen quantity: A minimum of 5 valid specimens per test direction.
Test Parameters & Stipulations
Test speed: Constant crosshead speed of (1 ± 0.5) mm/min, parallel to the longitudinal axis of the specimen assembly.
Preload and zeroing:
For Procedure B, displacement is zeroed when a tensile preload of 5 N is reached.
It is recommended to zero the force reading after mounting the assembly to correct for the weight of the supports and fixture.
Test Procedures for ISO 1922 Shear Properties Test for Rigid Cellular Plastics
Cut and machine specimens to the specified dimensions, removing or retaining skins as required by the configuration.
Clean specimen surfaces and bond them to the rigid supports using a qualified adhesive; allow full cure (curing time may count toward the conditioning period).
Condition the bonded assemblies in the selected standard atmosphere.
Mount the assembly into the test machine grips using adaptors and universal joints to ensure alignment.
Set the crosshead speed to 1 mm/min.
For Procedure B: attach the extensometer centered along the specimen length, and zero displacement at 5 N preload.
Apply load at constant speed, continuously recording force and displacement.
Continue testing until specimen fracture or until load drops by 10 % after the peak load.
Repeat for all specimens; discard and replace any specimen that fails at the adhesive interface.
Calculate shear strength, and if applicable, shear modulus and shear strain.
Industry Application Fields
Building and construction / thermal insulation: XPS, EPS, PUR/PIR rigid foam boards used in external wall insulation (ETICS), inverted/green/plaza roofs, floor slabs, cold-store decks, underfloor heating, road/rail subgrade and bridge-deck insulation. Shear behaviour is a declared characteristic for product certification/Declaration of Performance under product standards such as EN 13164 (XPS), and is used in factory production control and ISO/IEC 17025-accredited third-party verification .
Sandwich structures and composites: foam-core qualification for structural insulated panels, aircraft interiors, military/relocatable shelters, marine hulls and decks, automotive lightweight panels, wind-turbine blades, rail interiors, sports equipment and industrial enclosures/containers .
Packaging, refrigeration/cold chain and buoyancy/flotation devices .
R&D and QA/QC: optimising density, cell orientation, facings and processing; generating shear-modulus inputs for finite-element models of layered assemblies; in-house statistical process control, incoming-material acceptance and product development .
Indicative values: commercial XPS longitudinal shear strength is roughly 0.15–0.5 MPa, increasing with density and strongly direction-dependent
Related Stadard:
| ISO 844 | Rigid cellular plastics – Determination of compression properties. |
| ASTM C273 | Standard Test Method for Shear Properties of Sandwich Core Materials – the most widely used North American equivalent for foam core shear testing. |
| ISO 1209-1 | Rigid cellular plastics – Determination of flexural properties. |
| ISO 1209‑2 | Rigid cellular plastics - Determination of flexural properties - Part 2: Determination of flexural strength and apparent flexural modulus of elasticity |
| ASTM D5379 | V-notched beam shear test method for composite materials, used for alternative shear characterization. |
| ISO 1922 | Rigid cellular plastics - Determination of shear properties |
| ISO 1926 | Rigid cellular plastics — Determination of tensile properties |
| GB/T 10007 | Rigid cellular plastics.Determination of shear strength. |
| EN 12090 | Thermal insulating products for building applications. Determination of shear behaviour |
| ASTM C393 | Standard Test Method for Core Shear Properties of Sandwich Constructions by Beam Flexure |
| ASTM D1621 | Standard Test Method for Compressive Properties of Rigid Cellular Plastics |
| ASTM E1730 | Adhesives - Wood-to-wood adhesive bonds - Determination of shear strength by compressive loading |
| ASTM D905 | Standard Test Method for Strength Properties of Adhesive Bonds in Shear by Compression Loading |
Keywords: ISO 1922 shear tester, rigid cellular plastics shear test, foam shear strength tester, shear modulus test machine, shear strain at fracture test, rigid foam testing equipment, cellular plastic mechanical test, insulation foam shear property test, structural foam shear tester, plastic foam quality control, composite core material shear test, laboratory shear test rig, foam material characterization, rigid cellular plastic specimen testing, UnitedTest shear testing machine
Related products and device
Related Standard
ASTM D905 Standard Test Method for Strength Properties of Adhesive Bonds in Shear by Compression Loading
ASTM D905 evaluates comparative shear strength of adhesive bonds, mainly wood-to-wood, using a compressed block/shear specimen. It comparative shear performance of laboratory‑prepared wood‑to‑wood adhesive joints under compressive force; it is intended for adhesive screening, R&D and process monitoring rather than direct design‑strength calculation for finished structural products.
ASTM D906 Standard Test Method for Strength Properties of Adhesives in Plywood Type Construction in Shear by Tension Loading
ASTM D906 specifies a tensile-loading method for determining the comparative shear strength of wood-to-wood adhesives in plywood-type (three-ply cross-laminated) construction. It measures comparative shear strength of wood-to-wood adhesives exclusively for cross-laminated plywood-style three-ply veneer assemblies. Not designed for finished consumer wood products or parallel single-grain laminated joints.
ISO 6237 Adhesives – Wood-to-wood adhesive bonds – Determination of shear strength by tensile loading.
ISO 6237 specifies a laboratory method for determining the shear strength of wood-to-wood adhesive bonds using a standard specimen loaded in tension under strictly defined conditions of preparation, conditioning, and testing. It is intended only for adhesives used in bonding wood to wood in either parallel-laminated or cross-laminated construction, and is not intended for testing manufactured/finished products.
ISO 27528 defined to measure the maximum axial pull-out force required to extract screws from wood composite panels, covering two core test modes: face screw withdrawal and edge screw withdrawal. It serves as a global unified test method for evaluating the screw holding capacity of fibreboard, particleboard, OSB, plywood and other engineered wood panels with thickness ≥ 15 mm.
ASTM D1761 test methods provide a basic procedure for evaluating the withdrawal and lateral resistance of fasteners installed in wood and wood-based materials. The tests also provide a basis for determining comparable performance of different types and sizes of fasteners installed in wood and wood-based materials. Quantify the mechanical connection performance of nails, staples, screws, bolts, lag screws and timber connectors embedded in solid wood, plywood, OSB, fiberboard and other wood-based composites. Spikes are classified as nails within this standard.
ASTM D1037 - Standard Test Methods for Evaluating Properties of Wood-Base Fiber and Particle Panel Materials
ASTM D1037 test methods cover the determination of the properties of wood-base fiber and particle panel materials that are produced as mat-formed panels such a particleboard, medium density fiberboard, hardboard, and oriented strand board.
ASTM D1037 test methods cover small-specimen tests for wood-base fiber and particle panel materials that are made to provide: Data for comparing the mechanical and physical properties of various materials,
Data for determining the influence on the basic properties of such factors as raw material and processing variables, post-treatments of panels, and environmental influences, and
Data for manufacturing control, product research and development, and specification acceptance.
ASTM D897 prescribed a method for determining the comparative tensile properties of adhesive bonds in a standard specimen when tested under specific conditions. Its primary purpose was to measure the tensile strength of an adhesive bond between two rigid substrates (metal to metal).
ASTM D1002 is the most widely used standard test for measuring the apparent shear strength of metal‑to‑metal adhesive single‑lap joints under tension loading. It provides comparative data for adhesive selection, process control, and quality assurance in structural bonding applications. It is the most common test for evaluating adhesive shear performance.
Frequently Asked Questions (FAQs) about ISO 1922 Shear Properties Test for Rigid Cellular Plastics
Q1: What is ISO 1922?
A: ISO 1922 is an international standard published by ISO/TC 61/SC 10, titled Rigid cellular plastics – Determination of shear properties. The current 2018 fifth edition specifies a standardized laboratory method to measure the shear strength, shear modulus and shear strain of rigid cellular plastic materials.
Q2. Why is the ISO 1922 shear test important for the material?
A: Because in a sandwich panel the foam core's main structural job is to transfer shear between the two face sheets. Under bending, one skin is in compression and the other in tension; if core shear strength or stiffness is too low the panel can fail by core cracking, shear buckling, delamination or sudden stiffness collapse even while the skins are intact. The test therefore:
gives designers allowable shear stress and shear modulus for stiffness/FEA models;
captures anisotropy (extruded foams such as XPS have direction-dependent values);
supports factory production control, product declaration/certification and incoming-material acceptance;
complements compression testing — compression loads the board perpendicular to its faces, ISO 1922 loads it parallel to the faces, and the two values are not interchangeable.
Q3. Which materials and industries use it?
A: Rigid cellular plastics: XPS, EPS, PUR/PIR, PVC and PET foam cores, insulation boards and sandwich-panel cores. Typical fields: building insulation (ETICS, inverted/green roofs, floors, cold stores), structural insulated panels, aerospace interiors, marine decks, automotive lightweight panels, wind-blade cores, rail interiors, packaging, refrigeration and third-party/ISO 17025 labs.
Q4. Procedure A vs Procedure B — what is the difference?
| Procedure A | Procedure B | |
|---|---|---|
| Output | Shear strength only | Strength + modulus + strain |
| Displacement | Machine system, ±5 % or ±0.1 mm (whichever is more accurate) | Extensometer/similar between rigid supports, ≥ ±1 % precision |
| Recording | Force + movable-plate displacement | Simultaneous force–displacement required |
| Zeroing | — | Set extension to zero at 5 N tensile preload; extensometer centred along specimen length |
| Standard's note | "not recommended for measuring modulus" | Recommended method for modulus, strain "(and strength as well)" |
Q5. How many specimens, and what about anisotropy?
A: A set of five specimens. If anisotropy is suspected, prepare sets with major axes parallel to and normal to the suspected anisotropy directions. Reject any specimen that fails at the adhesive interface before the foam fails, and test replacements until ≥ 5 significant results remain. Report direction relative to anisotropy.
Q6. Can an ordinary UTM run ISO 1922, or do I need a special fixture?
A: The UTM is the base platform, but compression platens alone are not enough. You need the dedicated bonded rigid-plate assembly (330×50×16 mm supports, adaptors, universal joints, parallel alignment) plus the correct displacement measurement. Before buying, check:
a low-force load cell with enough resolution for foam (often well below 5 kN for 250×50 mm specimens);
stable 1 mm/min closed-loop speed control;
rigid, parallel supports and self-aligning joints to avoid eccentric bending;
two synchronised channels (force + displacement) and software that outputs the Clause 10 formulas and Clause 12 report fields;
extensometer / environmental-chamber expandability for Procedure B and conditioning;
calibration traceability, spare fixtures, software upgrades and response time — not just the bare machine price.
Q7: Why is adhesive selection so critical for this test?
A: The adhesive bonding the foam to the rigid supports must have significantly higher shear strength and modulus than the test material. This ensures ultimate failure occurs within the cellular foam itself, not at the bond line. Adhesive interface failure invalidates the test result. Annex A of the standard recommends epoxy-based adhesives for most rigid foam materials.
Q8: How does ISO 1922 compare to ASTM C273?
A: Both standards measure shear properties of sandwich core materials, but they differ in specimen geometry, loading fixture design and dimensional tolerances. ISO 1922 specifies 250 mm long specimens with dedicated single/double bonded-plate fixtures, while ASTM C273 uses a different specimen size and loading arrangement. They are not interchangeable for formal product certification.
Q9: Why choose ISO 1922 Shear Test Machine | Rigid Cellular Plastics Tester from UnitedTest?
A: Looking for an ISO 1922 test machine for rigid cellular plastics? UnitedTest manufactures universal testing machines and bonded-plate shear fixtures configured for ISO 1922:2018 — Rigid cellular plastics: Determination of shear properties. A compliant setup calls for an ISO 7500-1 Class 1 load frame, a constant (1 ± 0.5) mm/min crosshead speed, 330 × 50 × 16 mm rigid supports with universal-joint adaptors, and — when shear modulus and fracture strain are required — a ±1 % extensometer recording force and displacement together. UnitedTest systems are built around the parameters the standard actually uses: 250 × 50 mm single or double specimens, τ_M = F_m/A, G = hθ/A and γ = Δs/h, repeatable plate alignment, and report-ready data for shear strength, shear modulus and shear strain. Whether you test XPS, EPS, PUR/PIR, PVC or PET foam cores, insulation boards or sandwich panels, ask UnitedTest for a complete ISO 1922 shear test package: UTM, single/double shear fixture, adhesives guidance, installation and operator training. Contact UnitedTest today for a fixture drawing and quotation matched to your product thickness.
UnitedTest is a professional manufacturer of material testing systems dedicated to delivering high-precision, standard-compliant test equipment for the cellular plastics and composite industries. Our ISO 1922 shear testing machines are fully engineered to meet the requirements of ISO 1922:2018 Rigid cellular plastics – Determination of shear properties, providing reliable, repeatable test results for quality control, R&D and material certification.
Each system features a rigid load frame conforming to ISO 7500-1 Class 1 accuracy, with precise constant speed control at 1 mm/min as specified by the standard. We supply complete fixture kits for both single shear and double shear configurations, including high-rigidity steel specimen supports, universal joint alignment assemblies and optional high-precision extensometers to support both Procedure A (shear strength only) and Procedure B (full shear strength, modulus and strain characterization).
Suitable for testing rigid PU foam, PVC foam, PET foam, PMI foam, polystyrene foam and other rigid cellular materials, UnitedTest ISO 1922 testers are widely used by foam manufacturers, sandwich composite producers, aerospace & marine component suppliers, construction insulation companies and third-party testing laboratories. We also provide custom fixture solutions, specimen preparation guidance and full after-sales calibration services to help users achieve consistent test data in full compliance with international standards.
Require More Customized Solutions?