Home >> Application >> By Standard >> ASTM >> ASTM A-C >> ASTM C273 Sandwich Core Materials Shear Test

ASTM C273 Sandwich Core Materials Shear Test

Share:

ASTM C273 Sandwich Core Shear Tester | UnitedTest

UnitedTest supplies ASTM C273 sandwich core shear testing machines to measure in-plane shear strength and shear modulus of balsa, foam and honeycomb sandwich core materials for composite panel R&D and quality control.

ASTM C273 defines procedures to determine the shear properties of sandwich core materials, including in-plane shear strength and shear modulus corresponding to through-thickness shear strain. It applies to cores with continuous bonding surfaces (e.g., balsa wood, polymer foams) and discontinuous bonding surfaces (e.g., honeycomb cores). Tests may be conducted on bare cores bonded directly to loading plates, or on complete sandwich panels with facings. Widely adopted in aerospace, marine, wind energy, transportation and lightweight composite industries, this standard supports material selection, structural design validation, batch quality inspection and performance comparison of sandwich composite structures. UnitedTest manufactures reliable ASTM C273 sandwich core shear test equipment to deliver stable, repeatable shear test results for your sandwich core and finished panel evaluation.


Test Principle

The test subjects a sandwich core or panel to monotonically increasing shear force parallel to the facing plane. Load is transmitted to the specimen via rigid steel loading plates bonded to the specimen surfaces; opposing tensile or compressive displacement of the plates induces shear deformation in the core.

Key principles:

  • All shear properties (stress, strength, modulus) are calculated using the nominal shear area of the core.

  • The configuration does not produce perfect pure shear, but the mandated specimen length-to-thickness ratio minimizes secondary bending stresses.

  • Only core material shear failure is a valid failure mode. Adhesive or cohesive failures at core-to-facesheet, facesheet-to-load-plate, or core-to-load-plate interfaces are considered invalid and disqualify the test data.


Test Methods:

ConfigurationFixtureCritical detail
Tension loadingPinned or bolted plate-to-universal-joint fixtures; overall load train must be suspended, self-aligningEliminates eccentricity; preferred for general use
Compression loadingPlates taper to a knife-edge and seat in V-notch loading blocks rigidly attached to the machineBlocks aligned flat and parallel within ±0.02 mm [±0.001 in.]
With facingsSteel plates bonded to the facingsc = d − (t₁ + t₂); facesheet deformation assumed negligible for modulus.
Without facingsCore bonded directly to platesFor some honeycomb cores, two plies of adhesive are required to form deeper fillets in the cell walls and force a core failure.


Test Equipment required for ASTM C273 Sandwich Core Materials Shear Test

Universal testing machine    

Complies with ASTM E4 for force verification.

Equipped with one stationary head and one movable head with controllable constant velocity.

Force measurement accuracy within ±1% of the indicated value.

Deflection measurement device with a minimum precision of ±1%.

Test Fixtures

Two loading configurations are permitted:

  • Tension loading: Pinned or bolted load-plate-to-universal-joint fixtures with a suspended, self-aligning load train.

  • Compression loading: Loading plates tapered to knife edges that seat into rigid V-notch loading blocks, aligned flat and parallel within ±0.02 mm (±0.001 in).

ASTM C273 Sandwich Core Materials Shear Test

Dimensional Measurement Tools

Micrometers and calipers with an accuracy of ±0.025 mm (±0.001 in), capable of 1% measurement precision relative to sample dimensions.

Ball-anvil micrometers are recommended for thickness measurement of irregular facing surfaces; flat-anvil tools are used for smooth surfaces and for length/width measurements.


Test Specimen Information:

A minimum of 5 specimens per test condition is required. For statistically rigorous results, sampling follows Practice ASTM E122 for sample size calculation.

- Thickness: equal to the full thickness of the sandwich structure.

- Width: minimum 50 mm (2.0 in).

- Length: minimum 12 times the core thickness.


Test Parameters & Stipulations

Loading Mode: 

  • Both tensile and compressive loading are allowed.

  • Tensile loading induces higher through-thickness tensile stress concentrations at core ends, which may produce lower measured shear strength values. Compression-mode results show better agreement with data from ASTM C393 short-beam bending tests.

Test Speed

  • Speed is adjusted so that specimen failure occurs within 3 to 6 minutes.

  • The recommended standard crosshead displacement rate is 0.50 mm/min (0.020 in/min).

Data Acquisition

  • Recommended sampling rate: 5–10 data points per second, with a minimum of 300 data points per test.

  • Force vs. crosshead displacement and force vs. gauge displacement are recorded continuously.


Test Procedures for ASTM C273 Sandwich Core Materials Shear Test

  1. Pre-test planning: Define sampling method, specimen geometry, conditioning requirements, target properties, and test environment parameters.

  2. Initial dimensional measurement: After final machining (before conditioning), measure specimen length, width, and overall thickness to the required precision.

  3. Bonding: Bond the specimen to the steel loading plates in compliance with fixture geometric requirements.

  4. Post-bonding measurement: Re-measure length and width if re-machining is performed after bonding.

  5. Conditioning: Condition specimens as required, and store them in the controlled environment until testing.

  6. Post-conditioning measurement: Re-measure specimen dimensions after conditioning and immediately before testing.

  7. Fixture installation: Mount the specimen-loading plate assembly into the test machine fixture.

  8. Displacement gauge installation: Mount the deflection gauge to measure relative displacement between the two loading plates, with the measurement point centered along the core length.

  9. Loading: Apply tensile or compressive force at the specified rate until complete specimen rupture.

  10. Data recording: Continuously record force and displacement data. Document yield force (if applicable), maximum force, failure force, displacement at failure, and failure mode/location.

  11. Data validation: Reject data from specimens with interface failures or failures originating from obvious flaws (unless the flaw is an intentional study variable), and perform retests as needed.


Industry Application Fields

Typical sectors:

  • Aerospace & defence — honeycomb/Nomex and aluminium honeycomb floors, interiors, radomes, control surfaces; the standard is explicitly approved for U.S. DoD agencies. Honeycomb sandwich structures are widespread in structural engineering because the core reacts transverse shear while the facesheets react in-plane and bending loads.

  • Wind energy — PET/PVC/balsa core qualification for blade shells and webs; PET structural foam is explicitly cited for wind blades, rail, ships and building curtain walls.

  • Marine — PVC/PET/balsa-cored hulls, decks and bulkheads.

  • Rail, road transport & automotive — lightweight sandwich panels and interior structures.

  • Building & construction — insulated metal/FRP-faced sandwich panels, foam-core boards.

  • Materials R&D, certification bodies, third-party labs — foam formulation comparison, density/orientation studies, adhesive and process optimisation, moisture/temperature effect studies


Related Standard: 

ISO 844Rigid cellular plastics – Determination of compression properties.
ASTM C273Standard Test Method for Shear Properties of Sandwich Core Materials – the most widely used North American equivalent for foam core shear testing.
ASTM C297Rigid cellular plastics – Determination of flexural properties.
ASTM C365Flatwise compressive strength/modulus of core
ASTM C364Edgewise compressive strength of sandwich panel
ASTM D5379

V-notched beam shear test method for composite materials, used for alternative shear characterization.

ISO 1922Rigid cellular plastics - Determination of shear properties
ISO 1926
Rigid cellular plastics — Determination of tensile properties 
GB/T 10007Rigid cellular plastics.Determination of shear strength.
EN 12090Thermal insulating products for building applications. Determination of shear behaviour
ASTM C393

Standard Test Method for Core Shear Properties of Sandwich Constructions by Beam Flexure

ASTM D1621Standard Test Method for Compressive Properties of Rigid Cellular Plastics
ASTM D7249Facing strength/stiffness by long-beam 4-point flexure
ASTM D905Standard Test Method for Strength Properties of Adhesive Bonds in Shear by Compression Loading


Keywords: ASTM C273, sandwich core shear tester, sandwich core shear test, in-plane shear strength, shear modulus, honeycomb core shear test, balsa core shear test, foam core shear tester, composite sandwich panel test, lightweight composite shear testing, aerospace composite test, wind turbine core material test, marine sandwich structure test, core material mechanical test, sandwich construction shear property test, UnitedTest shear testing machine

Related products and device

ASTM C273 Sandwich Core Materials Shear Test Universal Testing Machine

A single column tensile tester is a sophisticated material testing instrument designed for measuring mechanical properties of various materials under tension, compression, bending, shear, and other loading conditions. As the name suggests, it features a single vertical column supporting a moving crosshead that applies force to test specimens.

ASTM C273 balsa core shear test, foam core shear tester, composite sandwich panel test

UnitedTest manufactures and exports compressive shear test fixtures, ISO 6238 wood adhesive shear jigs, ASTM D905 block shear fixtures, ASTM D4501 rigid‑substrate shear tools, and compatible universal testing machines. Buy ISO 6238 and ASTM D905 compressive shear test fixtures from UnitedTest.

Shear methods tensile test fixture

Vice Tensile test fixture for plastics is based on the test standatd ASTM D638, determination of the tensile properties of unreinforced and reinforced plastics in the form of standard dumbbell-shaped test specimens when tested under defined conditions of pretreatment, temperature, speed.

Related Standard

ISO 1922 Shear Properties Test for Rigid Cellular Plastics –

ISO 1922 Rigid cellular plastics – Determination of shear properties

ISO 1922 defines a standardized procedure to measure shear strength of rigid cellular plastics, and additionally provides methods to calculate shear modulus and shear strain at fracture.


ISO 6237 Tensile Shear Test for Wood-to-Wood Adhesive Bonds –

ISO 6237 Adhesives – Wood-to-wood adhesive bonds – Determination of shear strength by tensile loading.

ISO 6237 specifies a laboratory method for determining the shear strength of wood-to-wood adhesive bonds using a standard specimen loaded in tension under strictly defined conditions of preparation, conditioning, and testing. It is intended only for adhesives used in bonding wood to wood in either parallel-laminated or cross-laminated construction, and is not intended for testing manufactured/finished products.

ISO 27528 screw withdrawal resistance test of wood-based panels –

ISO 27528 defined to measure the maximum axial pull-out force required to extract screws from wood composite panels, covering two core test modes: face screw withdrawal and edge screw withdrawal. It serves as a global unified test method for evaluating the screw holding capacity of fibreboard, particleboard, OSB, plywood and other engineered wood panels with thickness ≥ 15 mm.

ASTM D1761 Test Methods for Mechanical Fasteners in Wood –

ASTM D1761 test methods provide a basic procedure for evaluating the withdrawal and lateral resistance of fasteners installed in wood and wood-based materials. The tests also provide a basis for determining comparable performance of different types and sizes of fasteners installed in wood and wood-based materials.  Quantify the mechanical connection performance of nails, staples, screws, bolts, lag screws and timber connectors embedded in solid wood, plywood, OSB, fiberboard and other wood-based composites. Spikes are classified as nails within this standard.

ASTM D1037 Test Methods for Wood-Base Fiber and Particle Panel Materials –

ASTM D1037 - Standard Test Methods for Evaluating Properties of Wood-Base Fiber and Particle Panel Materials 


ASTM D1037 test methods cover the determination of the properties of wood-base fiber and particle panel materials that are produced as mat-formed panels such a particleboard, medium density fiberboard, hardboard, and oriented strand board.


ASTM D1037 test methods cover small-specimen tests for wood-base fiber and particle panel materials that are made to provide: Data for comparing the mechanical and physical properties of various materials,

Data for determining the influence on the basic properties of such factors as raw material and processing variables, post-treatments of panels, and environmental influences, and

Data for manufacturing control, product research and development, and specification acceptance.

ASTM D897 Tensile Test of Adhesive Bonds –

ASTM D897 prescribed a method for determining the comparative tensile properties of adhesive bonds in a standard specimen when tested under specific conditions. Its primary purpose was to measure the tensile strength of an adhesive bond between two rigid substrates (metal to metal). 

ASTM D1002 Lap Shear Test of Adhesively Bonded Metal Specimens –

ASTM D1002 is the most widely used standard test for measuring the apparent shear strength of metal‑to‑metal adhesive single‑lap joints under tension loading. It provides comparative data for adhesive selection, process control, and quality assurance in structural bonding applications. It is the most common test for evaluating adhesive shear performance.

ASTM D1621 Rigid Cellular Plastics Compression Testing –

ASTM D1621 Standard Test Method for Compressive Properties of Rigid Cellular Plastics

ASTM D1621 determining the compressive properties of rigid cellular materials, expanded/rigid plastic foams, particularly expanded plastics. It compresses a conditioned foam specimen between two flat platens at a controlled speed and records a complete load–deflection curve.

Frequently Asked Questions (FAQs) About ASTM C273 Sandwich Core Materials Shear Test

Q1. What is ASTM C273?

ASTM C273/C273M-20 is the standard plate-shear test method for determining the shear strength and shear modulus of sandwich construction core materials. A core or sandwich specimen is bonded between two rigid steel loading plates, and the plates are displaced in opposite directions so the core is sheared parallel to the plane of the facings. It covers continuous-bonding-surface cores (balsa wood, foams) and discontinuous ones (honeycomb). 


Q2. Why is the ASTM C273 test important?

Because the core carries almost all of the transverse shear in a loaded sandwich panel, its shear strength and shear modulus are fundamental design inputs, not optional data. Thin, stiff facings take bending and in-plane loads; the lightweight core keeps them apart and transfers shear between them. If the core shears, the panel loses load transfer — regardless of how strong the facings are. C273 is the most direct way to generate those two numbers for material specifications, panel design, R&D, quality assurance and FEA models.


Q3. Why must the force line pass through diagonally opposite corners?

That geometry minimises the eccentric bending and peel components that would otherwise be introduced by off-axis loading. It is the defining design rule of the C273 fixture: plate length, core length-to-thickness ratio and loading offset x must be set together so the resultant force acts along the diagonal. A correct line of action may also be obtained by adjusting the core length-to-thickness ratio, provided dimensional requirements are met.


Q4. Should I use tension loading or compression loading?

Both are permitted. Tension loading uses pinned or bolted plate-to-universal-joint fixtures with a suspended, self-aligning load train and is the more common general setup. Compression loading uses plates tapering to a knife-edge seated in V-notch blocks aligned flat and parallel within ±0.02 mm [±0.001 in.] . For some cores tension mode gives a lower strength, while compression-mode results agree better with short-beam ASTM C393 — so always report the mode and keep it consistent within a test program.


Q5. Which materials can be tested?

Balsa wood, rigid polymer foams (PET, PVC, PUR/PIR, EPS/XPS, phenolic), aluminium and aramid/Nomex honeycomb, and other cores with either continuous or discontinuous bonding surfaces. Testing may be done on bare core bonded directly to the plates or on a full sandwich with its facings bonded to the plates.


Q6: What is the difference between tension and compression loading in ASTM C273?

Both loading modes are permitted, but they produce slightly different results:

  • Compression loading generates lower through-thickness tensile stress concentrations at core ends, and results generally agree well with ASTM C393 beam flexure test data.

  • Tension loading produces higher through-thickness tensile stress concentrations, which may cause lower measured shear strength values for some core materials. The choice depends on the intended service loading condition of the final component.


Q7: What is the standard test speed for ASTM C273?

The test speed is set so that specimen failure occurs within 3 to 6 minutes. The recommended standard crosshead displacement rate is 0.50 mm/min (0.020 in/min). If the material strength is unknown, preliminary trials are run to determine the appropriate speed.


Q8: How does ASTM C273 compare to ASTM C393?

Both standards measure core shear properties, but by different methods:

  • ASTM C273: Direct plate shear test — applies shear load directly via bonded loading plates; provides more accurate shear modulus data.

  • ASTM C393: Beam flexure test — derives shear properties from bending a sandwich beam; simpler fixturing but combines shear and bending effects. ASTM C273 compression-mode results typically correlate well with ASTM C393 data.


Q9: Why choose UnitedTest ASTM C273 Test Systems — Precision Shear Testing for Sandwich Core Materials? 

UnitedTest is a leading manufacturer of high-performance universal testing machines and specialized test fixtures engineered to meet the exact requirements of ASTM C273/C273M standard test method for shear properties of sandwich core materials.


Our ASTM C273 test systems deliver accurate, repeatable core shear strength and shear modulus measurements for honeycomb cores, foam cores, balsa wood, and all sandwich composite core materials used in aerospace, marine, wind energy, automotive, and construction applications.

Why Choose UnitedTest for Your ASTM C273 Testing Needs?

Full Compliance with ASTM C273 Standard

Every UnitedTest C273 testing machine is designed and calibrated to meet all requirements of ASTM C273-20 and ASTM E4 force verification standards. Our precision load cells, high-resolution displacement sensors, and rigid test frames ensure ±1% force accuracy and ±1% deflection precision — exceeding the minimum requirements of the standard.

Complete Fixture Solutions for Tension and Compression Modes

UnitedTest offers both tensile and compressive ASTM C273 test fixture configurations:

  • Tension fixtures: Pinned and bolted load-plate-to-universal-joint designs with self-aligning load trains

  • Compression fixtures: Knife-edge loading plates with precision V-notch support blocks aligned to ±0.02 mm parallelism

  • All loading plates are engineered with bending stiffness exceeding 2.67 MN·mm²/mm per mm of core thickness, ensuring rigid load introduction without plate deflection errors.


Integrated Software for Automated Data Analysis

Our proprietary TestMaster software automatically calculates all key parameters defined in ASTM C273:

  • Ultimate core shear strength

  • 2% offset shear strength

  • Core shear modulus (with user-selectable linear range)

  • Shear stress-strain curves

  • Statistical analysis (mean, standard deviation, coefficient of variation)

  • Standardized three-character failure mode coding

Environmental Testing Capabilities

For advanced material characterization, UnitedTest systems integrate seamlessly with environmental chambers for elevated temperature, low temperature, and humidity-controlled testing — enabling full-conditioning shear testing per ASTM D5229/D5229M requirements.

Trusted by Composite Laboratories Worldwide

From aerospace material qualification labs to sandwich panel manufacturers and R&D centers, UnitedTest ASTM C273 testing machines deliver the reliability, accuracy, and compliance that quality teams depend on. Every system comes with factory calibration certificates, installation support, and comprehensive training.

< Previous: ASTM C203 Flexural Testing for Block-Type Thermal Insulation

> Next: ASTM C297 Flatwise Tensile Strength Test of Sandwich Constructions

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.