Information on the most widely used ASTM standards within the materials testing industry
ASTM D1621 Compressive Properties Tester for Rigid Cellular Plastics | UnitedTest
UnitedTest manufactures ASTM D1621 compression test machines for rigid cellular plastics and expanded foam. Our equipment captures full load-deflection curves to test compressive strength, modulus and deformation for foam insulation, structural foam and cellular plastic materials.
ASTM D1621 Standard Test Method for Compressive Properties of Rigid Cellular Plastics
ASTM D1621 covers the determination of compressive properties of rigid cellular materials and expanded rigid plastic foams, widely used in insulation, construction and composite core applications. The standard requires conditioned foam specimens to be compressed between two flat parallel platens at a controlled constant speed, while the system records a complete load–deflection curve. From this curve, engineers can calculate compressive strength, proportional-limit stress, compressive modulus and deformation performance. This test supports material formulation development, incoming quality inspection, product specification verification and third-party material qualification for rigid foam panels and cellular plastic components.
Test Principle
This method characterizes the compressive behavior of rigid cellular plastics by applying a controlled, uniformly increasing compressive load to a prepared specimen at a constant crosshead velocity, while continuously recording load and corresponding deformation data to generate a full load-deflection (stress-strain) curve.
Core definitional principles:
Compressive strength: If a clear yield point (the first point where strain increases without an increase in stress) occurs before 10% deformation, compressive strength is the stress at that yield point. If no yield point appears, compressive strength is defined as the stress at exactly 10% specimen deformation.
Nominal compressive stress: Calculated as the applied compressive load divided by the original minimum cross-sectional area of the specimen.
Compressive modulus of elasticity: The ratio of stress to corresponding strain within the proportional (linear elastic) region of the material, derived from the steepest straight-line portion of the load-deflection curve.
A system compliance correction procedure is specified to remove measurement error caused by deflection of the test machine frame, drive system, load cell and fixturing.

Specific Test Methods
ASTM D1621 is essentially one primary compression method with two allowable ways to obtain displacement and several optional outputs. Compress a conditioned specimen between flat platens at a constant crosshead rate, recording load versus platen displacement until yield or approximately 13% compression.
Test Equipment required for ASTM D1621 Rigid Cellular Plastics Compression Testing
| Universal testing machine | Must have a stationary member/base and a movable crosshead with a drive system capable of uniform, controlled velocity. In practice this is a calibrated universal testing machine (UTM) with compression platens. Load-measurement system: Must record compressive load with an accuracy of ±1% of the measured value or better; verified according to ASTM E4. |
| Compression Platens | Two flat, rigid plates with dimensions larger than the specimen loading surface, to ensure uniform load distribution across the specimen face. One platen is recommended to incorporate a spherical seating mechanism to compensate for non-parallelism between specimen end faces or machine platens. |
| Displacement measurement systems | Direct platen displacement method: Uses a deflectometer/extensometer that directly measures the distance between upper and lower compression platens. Transducers must be verified per ASTM E83 and meet Class C or better classification. Crosshead drive displacement method: Uses position output from the crosshead drive system. This method is only valid if drive system compliance causes less than 1% displacement error, or if a formal compliance correction is applied to reduce error below 1%. A step-by-step compliance calibration procedure is defined to measure system deflection under load and correct raw displacement data. |
| Dimension Measurement Tools | Micrometer dial gauge, vernier caliper, or steel rule capable of measuring specimen dimensions to ±1% of the measured value. For specimens ≤25.4 mm in thickness, a dial-type gauge with a minimum 6.45 cm² foot area and 0.17±0.03 kPa contact pressure is required to avoid compressing the cellular material during measurement. |
Test Specimen Information:
Cross-section shape: Square or circular.
Cross-sectional area: Minimum 25.8 cm² (4 in²), maximum 232 cm² (36 in²).
Height/Thickness: Minimum 25.4 mm (1 in); maximum height must not exceed the specimen width or diameter.
Geometric requirements: Loaded end faces must be parallel to each other and perpendicular to the specimen sides. All surfaces must be free of large visible flaws or defects.
Anisotropic materials: The direction of compressive loading relative to the suspected anisotropy axis must be specified in the report.
Sample quantity: A minimum of 5 specimens shall be tested per sample. Specimens that fail at obvious pre-existing flaws shall be discarded and retested, unless the effect of such flaws is the subject of study.
Test Parameters & Stipulations
Test speed: Crosshead displacement rate equals 10% of the specimen thickness per minute, with an absolute tolerance of ±0.25 mm (±0.01 in.) per minute.
The test is stopped at whichever occurs first:
A compressive yield point is observed on the load-deflection curve;
The specimen is compressed to approximately 13% of its original thickness (3% beyond the 10% deformation reference point).
Test Procedures for ASTM D1621 Rigid Cellular Plastics Compression Testing
Dimension Measurement
Specimen Alignment & Placement
Center the specimen between the compression platens so that the specimen centerline aligns with the platen centerline, ensuring uniform load distribution over the entire loading surface.
Position the upper platen close to but not touching the specimen. Attach the deflectometer or compression extensometer if direct displacement measurement is used.
Test Execution
Start the crosshead moving in the compression direction at the specified constant speed.
Continuously record compression platen displacement and corresponding load values to generate a complete load-deflection curve.
Test Conclusion
Halt the test when the yield point is reached or when approximately 13% deformation is achieved.
Caculation: Establish the zero-deformation (zero-strain) origin by extrapolating the steepest linear portion of the load-deflection curve back to the zero-load axis. All deformation and strain calculations are measured from this point.
Mark the 10% deformation position along the zero-load line and draw a vertical line to intersect the load-deflection curve.
If a yield point occurs before this intersection, use the load at the yield point for strength calculation.
If no yield point exists, use the load at the 10% deformation intersection.
Compressive strength = selected load value ÷ initial horizontal cross-sectional area of the specimen.
Compressive modulus of elasticity is calculated from the linear elastic region using: Ec= (W*H)/(A*D)
where Ec = compressive modulus of elasticity, W = load at a point on the linear portion, H = initial specimen height, A = initial cross-sectional area, D = corresponding deformation at that load.
Calculate the arithmetic mean and estimated standard deviation for all valid specimen results.
Industry Application Fields
This test is the primary compressive performance benchmark for rigid cellular plastics across multiple industries:
Building & construction: Rigid thermal insulation foams (EPS, XPS, polyurethane, phenolic foam) used in walls, roofs, floor systems and cold-storage construction
Packaging: High-performance protective foam materials for load-bearing and shock-absorbing applications
Aerospace & marine: Core materials for sandwich composite panels used in structural components
Automotive: Structural foam parts, interior components and thermal/acoustic insulation
Refrigeration & logistics: Insulation materials for cold chain equipment and transport containers
Related Standard:
| ISO 844 | Rigid cellular plastics – Determination of compression properties. |
| ASTM C273 | Standard Test Method for Shear Properties of Sandwich Core Materials – the most widely used North American equivalent for foam core shear testing. |
| ISO 1209-1 | Rigid cellular plastics – Determination of flexural properties. |
| ISO 1209‑2 | Rigid cellular plastics - Determination of flexural properties - Part 2: Determination of flexural strength and apparent flexural modulus of elasticity |
| ASTM D5379 | V-notched beam shear test method for composite materials, used for alternative shear characterization. |
| ISO 1922 | Rigid cellular plastics - Determination of shear properties |
| ISO 1926 | Rigid cellular plastics — Determination of tensile properties |
| GB/T 10007 | Rigid cellular plastics. Determination of shear strength. |
| EN 12090 | Thermal insulating products for building applications. Determination of shear behaviour |
| ASTM C393 | Standard Test Method for Core Shear Properties of Sandwich Constructions by Beam Flexure |
| ASTM C365 | Flatwise Compressive Properties of Sandwich Cores; determines core compressive strength and modulus for sandwich-panel design, including foam and honeycomb cores. |
| ISO 7616 | Compressive-creep methods for rigid cellular plastics; relevant when long-term deformation under sustained load matters. |
| ISO 1856 | Flexible cellular polymeric materials / flexible foam compression-set or compression testing; not substitutes for rigid-foam D1621. |
| ASTM D1621 | Standard Test Method for Compressive Properties of Rigid Cellular Plastics |
| GB/T 8813 | Chinese national standard Rigid cellular plastics—Determination of compression properties, identical to ISO 844:2014 (IDT) |
| EN 826 | Thermal insulating products for building applications — Determination of compression behaviour; product/application-oriented rather than a general rigid-foam material method. |
Keywords: ASTM D1621 compression tester,rigid cellular plastics compression test,expanded foam compressive strength tester,plastic foam compression machine,foam insulation compressive modulus test,load deflection curve testing,rigid foam test equipment,cellular plastic lab tester,polyurethane foam compression test,polyiso foam compressive property test,construction foam quality testing,universal compression tester for foam,UnitedTest foam testing machine,ASTM D1621 test rig,rigid cellular material mechanical test
Related products and device
Related Standard
ASTM D905 Standard Test Method for Strength Properties of Adhesive Bonds in Shear by Compression Loading
ASTM D905 evaluates comparative shear strength of adhesive bonds, mainly wood-to-wood, using a compressed block/shear specimen. It comparative shear performance of laboratory‑prepared wood‑to‑wood adhesive joints under compressive force; it is intended for adhesive screening, R&D and process monitoring rather than direct design‑strength calculation for finished structural products.
ASTM D906 Standard Test Method for Strength Properties of Adhesives in Plywood Type Construction in Shear by Tension Loading
ASTM D906 specifies a tensile-loading method for determining the comparative shear strength of wood-to-wood adhesives in plywood-type (three-ply cross-laminated) construction. It measures comparative shear strength of wood-to-wood adhesives exclusively for cross-laminated plywood-style three-ply veneer assemblies. Not designed for finished consumer wood products or parallel single-grain laminated joints.
ISO 6237 Adhesives – Wood-to-wood adhesive bonds – Determination of shear strength by tensile loading.
ISO 6237 specifies a laboratory method for determining the shear strength of wood-to-wood adhesive bonds using a standard specimen loaded in tension under strictly defined conditions of preparation, conditioning, and testing. It is intended only for adhesives used in bonding wood to wood in either parallel-laminated or cross-laminated construction, and is not intended for testing manufactured/finished products.
ISO 27528 defined to measure the maximum axial pull-out force required to extract screws from wood composite panels, covering two core test modes: face screw withdrawal and edge screw withdrawal. It serves as a global unified test method for evaluating the screw holding capacity of fibreboard, particleboard, OSB, plywood and other engineered wood panels with thickness ≥ 15 mm.
ASTM D1761 test methods provide a basic procedure for evaluating the withdrawal and lateral resistance of fasteners installed in wood and wood-based materials. The tests also provide a basis for determining comparable performance of different types and sizes of fasteners installed in wood and wood-based materials. Quantify the mechanical connection performance of nails, staples, screws, bolts, lag screws and timber connectors embedded in solid wood, plywood, OSB, fiberboard and other wood-based composites. Spikes are classified as nails within this standard.
ASTM D1037 - Standard Test Methods for Evaluating Properties of Wood-Base Fiber and Particle Panel Materials
ASTM D1037 test methods cover the determination of the properties of wood-base fiber and particle panel materials that are produced as mat-formed panels such a particleboard, medium density fiberboard, hardboard, and oriented strand board.
ASTM D1037 test methods cover small-specimen tests for wood-base fiber and particle panel materials that are made to provide: Data for comparing the mechanical and physical properties of various materials,
Data for determining the influence on the basic properties of such factors as raw material and processing variables, post-treatments of panels, and environmental influences, and
Data for manufacturing control, product research and development, and specification acceptance.
ASTM D897 prescribed a method for determining the comparative tensile properties of adhesive bonds in a standard specimen when tested under specific conditions. Its primary purpose was to measure the tensile strength of an adhesive bond between two rigid substrates (metal to metal).
ASTM D1002 is the most widely used standard test for measuring the apparent shear strength of metal‑to‑metal adhesive single‑lap joints under tension loading. It provides comparative data for adhesive selection, process control, and quality assurance in structural bonding applications. It is the most common test for evaluating adhesive shear performance.
ISO 1922 Rigid cellular plastics – Determination of shear properties
ISO 1922 defines a standardized procedure to measure shear strength of rigid cellular plastics, and additionally provides methods to calculate shear modulus and shear strain at fracture.
EN 826 Thermal insulating products for building applications — Determination of compression behaviour
EN 826 specifies the equipment and procedures used to determine the compression behaviour of test specimens. It is applicable to thermal insulating products and can be used:to determine the compressive stress to be applied in compressive creep tests;for applications where insulation products are exposed only to short-term loads;for quality control; to obtain reference values from which design values can be calculated using safety factors.
ASTM C273 Standard Test Method for Shear Properties of Sandwich Core Materials
ASTM C273 defines procedures to determine the shear properties of sandwich core materials, including in-plane shear strength and shear modulus corresponding to through-thickness shear strain. It applies to cores with continuous bonding surfaces (e.g., balsa wood, polymer foams) and discontinuous bonding surfaces (e.g., honeycomb cores). Tests may be conducted on bare cores bonded directly to loading plates, or on complete sandwich panels with facings.
Frequently Asked Questions (FAQs) about ASTM D1621 Rigid Cellular Plastics Compression Testing
Q1. What is ASTM D1621?
ASTM D1621-16 (2023) is the standard test method for determining the compressive properties of rigid cellular materials, particularly expanded plastics. It compresses a conditioned foam specimen between two flat platens at a controlled speed and records a complete load–deflection curve.
Q2. Which materials are tested with ASTM D1621?
Rigid cellular plastics — typically PU/PUR, PIR, EPS, XPS, phenolic, PMI and PET foams. It is used for insulation boards, structural foam cores and rigid protective packaging. It is not a flexible-foam method.
Q3. What properties does the test report?
Compressive strength (at yield or at 10% deformation), deformation/strain at maximum load, and — when requested — the apparent compressive modulus. The full curve also allows stress at any load, such as at the proportional limit.
Q4. Why is the ASTM D1621 test important?
Because it converts a foam's behaviour under static compressive load into reproducible numbers for load-bearing capacity and stiffness. Those numbers drive R&D, quality control, specification acceptance/rejection, supplier comparison and third-party certification.
Q5. Why is it important for foams specifically, rather than solid plastics?
Foams deform by cell-wall bending, collapse and densification rather than bulk yielding. Their results are unusually sensitive to density, cell orientation, specimen thickness, face parallelism and machine compliance. D1621 fixes all of these variables so two laboratories can compare the same material meaningfully.
Q6. Why is "10% deformation" used as compressive strength?
Many rigid foams never show a clear yield point — they keep carrying load as cells collapse. The stress at 10% compressive strain gives a consistent, arbitrary-but-comparable reference value. If a yield point occurs before 10%, the yield stress is used instead.
Q7. Why does the test continue to about 13% compression?
To make sure the 10% evaluation point is fully captured with a margin for curve analysis. The test stops at yield or approximately 13% compression of original thickness, whichever occurs first. If a different deformation is specified, compress about 3% beyond it and substitute that value in the calculations.
Q8. What is "Point O" / zero-deformation correction?
The initial curve is often curved because of platen seating and surface irregularity. D1621 requires extending the steepest straight portion of the lower curve back to the zero-load line. That intersection is Point O, and every deformation is measured from it — not from first contact.
Q9. What is the ASTM D1621 test speed?
10% of the specimen thickness per minute, ±0.25 mm/min (±0.01 in./min). For a 25.4 mm (1 in.) specimen that is ≈2.54 mm/min, often rounded to 2.5 mm/min. Thicker specimens are tested proportionally faster.
Q10. Is ASTM D1621 the same as ISO 844?
Note 1 of D1621 states the two are technically equivalent. However, ISO 844 has since been revised — the current edition is ISO 844:2026, which defines Procedure A (platen displacement, nominal properties) and Procedure B (extensometer, conventional properties) . Always name the exact edition in a contract; "similar" does not mean results are automatically interchangeable .
Q11. How does D1621 differ from ASTM D695, ASTM C365 and EN 826?
D695 covers solid rigid plastics; C365 covers flatwise compression of sandwich cores; EN 826 covers building thermal-insulating products. D1621 is the general rigid cellular plastics material method. GB/T 8813-2020 is the Chinese ISO 844-based equivalent. One UTM can support several of these, but the fixture, specimen and calculation method must be changed.
Q12. Can ASTM D1621 be used for flexible foam?
No. Flexible cellular materials are covered by methods such as ASTM D3574 / ISO 1856 (compression set) and ISO 3386. Using D1621 on a seating or mattress foam gives non-conforming results.
Q13. Can D1621 data be used for long-term design?
Not on its own. The standard explicitly says results are not significant for engineering design when the load–time scale differs widely from the test. Impact, creep (e.g. ISO 7616 / ISO 1922) and fatigue testing are required for those applications.
Q14: Why does ASTM D1621 recommend a spherical seat on one platen?
A: A spherical seating mechanism compensates for minor non-parallelism between the specimen end faces or between the upper and lower platens. This ensures that the compressive load is distributed uniformly across the entire specimen face, preventing edge stress concentrations and producing more accurate and repeatable test results.
Q15: Why UnitedTest compression testing machines are ideal for ASTM D1621?
A: UnitedTest testing machines are purpose-built to satisfy every requirement of ASTM D1621: load accuracy meets ASTM E4, displacement accuracy meets ASTM E83, speed control matches the 10% thickness/min specification, oversized platens with optional spherical seat are available, and the dedicated test software automatically performs compliance correction, plots stress-strain curves, and calculates compressive strength and modulus — delivering fully compliant, report-ready results in one workflow.
Q16: Why choose ASTM D1621 Compression Testing Machine for Rigid Cellular Plastics from UnitedTest?
UnitedTest is a leading manufacturer of high-precision universal compression testing machines engineered to meet the strict requirements of ASTM D1621 — Standard Test Method for Compressive Properties of Rigid Cellular Plastics. Our test systems deliver accurate, repeatable compressive strength and modulus measurements for expanded polystyrene (EPS), extruded polystyrene (XPS), polyurethane foam, phenolic foam and all types of rigid cellular plastics.
Each UnitedTest ASTM D1621 compression tester features:
Load measurement accuracy of ±1% or better, fully compliant with ASTM E4 calibration standards
Precision crosshead drive with 10% thickness/min speed control per ASTM D1621 specifications
Oversized compression platens with optional spherical seating for uniform load distribution
Integrated deflectometer support and advanced software for automatic compliance correction
Full data acquisition, stress-strain curve plotting and automatic compressive strength / modulus calculation
ASTM D1621 is the reference test method for measuring the compressive properties of rigid cellular plastics — including PU, PIR, EPS, XPS, phenolic, PMI and PET foams. A conditioned specimen is compressed between two flat platens at 10% of its thickness per minute while the system records a complete load–deflection curve. From that curve, laboratories report compressive strength at yield or at 10% deformation, deformation at maximum load, and the apparent compressive modulus.
UnitedTest (Beijing United Test Co., Ltd.) supplies ASTM D1621 compression testing systems built around the WDW series computer-controlled electronic universal testing machine. Configured with oversized flat compression platens, an optional spherical seating platen, a deflectometer verified to ASTM E83 Class C or better, and test software set up for zero-deformation correction, 10% strength calculation and compliance subtraction, the system addresses the ±1% load and displacement accuracy the standard demands. Force measurement meets or exceeds ASTM E4 and ISO 7500-1 requirements, giving foam producers, insulation board manufacturers, packaging laboratories and third-party test houses repeatable, audit-ready results.
The same platform also supports ISO 844, GB/T 8813, EN 826 and ASTM C365 when the fixture and test method are changed — making it a practical single investment for multi-standard rigid foam compression testing. Whether you are screening a new foam formulation, releasing a production batch of XPS insulation board, or qualifying a sandwich core, UnitedTest can match the load capacity, platen size, test space and displacement measurement to your actual specimen and expected stress.
Serving the building insulation, packaging, aerospace composite, automotive and cold-chain industries worldwide, UnitedTest testing machines provide laboratories and quality control departments with reliable, cost-effective solutions for ASTM D1621, ISO 844 and other foam material test standards.
Call to action: Tell us your foam type, specimen size, expected maximum stress and required standard — we will recommend the right ASTM D1621 test configuration.
Require More Customized Solutions?