Information on the most widely used ASTM standards within the materials testing industry
ISO 5470-2 Martindale Abrasion Tester for Rubber & Plastics Coated Fabrics | UnitedTest
UnitedTest manufactures ISO 5470-2 Martindale abrader to test dry and wet abrasion resistance of rubber or plastics-coated fabrics for quality control, formulation comparison and compliance verification.
ISO 5470-2 sets out the laboratory test method for abrasion resistance assessment of rubber- or plastics-coated fabrics with a Martindale abrader. The standard supports both dry-abrasion and wet-abrasion test conditions, widely adopted for product development, coating formulation comparison, batch quality control, type approval and contractual specification compliance. UnitedTest provides reliable ISO 5470-2 compliant Martindale abrasion testing machines for coated fabric manufacturers and testing laboratories.
Core Test purpose / principle
Two distinct test methods share the same core physical principle. Relative cyclic planar Lissajous‑figure motion is generated between the test specimen and abradant, delivering multi‑directional rubbing action.
Method 1: Specimens are clamped in holders; abradant sits on the horizontal machine table. Constant pressure is applied onto the specimen against stationary abradant. A wet‑abrasion variant is available by saturating the abradant assembly.
Method 2: The positions are reversed: test specimens are mounted onto the machine table, while abradant material is secured inside the moving specimen holders.
Tests can end either after a preset number of abrasion revolutions (then damage is graded), or stop when specimens reach a predefined abrasion damage level (then record the cycle count). Each full Lissajous abrasion cycle corresponds to 16 elliptical revolutions of the specimen holder.

Lissajous figure
Test Equipment required of ISO 5470-2 Martindale Abrasion Test for Rubber or Plastics-Coated Fabrics
| Martindale abrasion‑testing machine | as specified in ISO 12947-1 — including specimen holders, spindles, loading weights, abrading tables, clamping rings.
|
| Auxiliary consumables |
|
Test Specimen Information:
Method 1 (specimens in holders)
At least 4 specimens, cut sample, large enough to be held firmly, taken from non-adjacent areas within the usable width of the roll (usable width per ISO 2286-1).
Double-coated fabrics: if both faces are tested, take another set of at least 4.
Irregular embossing or print (patches): sample so that every part of the pattern is tested — this may require more than 4 specimens.
If the result is expressed as mass loss, weigh each specimen first.
Method 2 (specimens on the table)
At least 4 specimens of 125 mm × 125 mm, again from non-adjacent areas; same rules for patterned material and for mass-loss determination.
Test Parameters & Stipulations
| Contact pressure | (12 ± 0.2) kPa |
| Tester speed | (48 ± 4) rev/min |
| Effective rubbing area | 60 mm × 60 mm Lissajous trace |
| Exposed specimen test area (Method 1) | (645 ± 5) mm² |
| One complete abrasion cycle | 16 revolutions |
| Dry‑test conditioning time | ≥16 h (ISO 2231 atmosphere) |
| Specimen‑backing foam (thin fabrics) | 30±2 kg/m³ PU foam |
| Wool felt specification | 750±50 g/m²; 2.5±0.5 mm |
Test Procedures for ISO 5470-2 Martindale Abrasion Test for Rubber or Plastics-Coated Fabrics
Method 1.
Remove the clamping ring, insert the specimen centrally with the surface to be abraded facing outwards, press the face against a hard surface while fitting/screwing the back plate to avoid wrinkling; repeat for all specimens.
Add PU foam backing for materials < 500 g/m² (unless pronounced rear lamination).
Check the mounted specimen is not baggy, creased or distorted.
Place dry or wet felt on the abrading table (matching the test condition).
Place the matching dry or wet abradant over the felt, test face up — a fresh piece per test; replace it every 50 000 cycles beyond 51 200 revolutions.
Put the weightpiece on the abradant, clamp wrinkle-free, then remove the weightpiece.
Repeat for all stations; fit the filled holders onto the abradant.
Apply the 12 ± 0.2 kPa vertical load to each holder and start the machine.
At the revolutions listed in Table 2, remove and inspect each specimen with the × 6 magnifier under bright indirect light, preferably comparing with an unabraded reference; rate per Table 3 and stop as required.
Return specimens to the same holder/table, restart, repeat at each inspection point; re-wet at the points marked in Table 2 (≤ 30 g water rubbed in, weightpiece for 10 s).
Method 2.
Apply double-sided tape to the back of each 125 mm × 125 mm specimen and fix it, crease-free, to the abradant table.
Place a piece of abradant fabric in each specimen holder, large enough to clamp firmly.
Back the abradant with a same-size piece of PU foam; clamp the assembly without bagginess/creases.
Then follow Method 1 steps 8.1.10–8.1.14 (loading, running, inspection, rating, re-wetting).
Assessment. Rate each specimen with Table 3; if mass loss is required, condition and weigh before testing and re-condition for the same time and re-weigh after the set number of cycles.
Industry Application Fields
| Object | Two methods for determining the resistance of a material to wet and dry abrasion |
| Applicable to | The coated surface(s) of rubber- or plastics-coated fabrics |
| Not applicable to | The uncoated face of a coated fabric — that falls under the ISO 12947 series (uncoated textiles) |
Typical industry fields / end uses: coated fabrics are used wherever the polymer layer (PVC, PU, rubber, TPU…) carries the appearance and the barrier function. The test is therefore written into specifications for:
Automotive and transport interiors (seat covers, door panels, headliners, bus/train/rail seating)
Contract and domestic furniture upholstery, office seating
Protective and work clothing, foul-weather gear, gloves
Technical textiles: tarpaulins, truck covers, tents, awnings, membranes, inflatables, conveyor covers
Footwear and leather substitutes, luggage, bags, belts
Marine (boat seating/covers), healthcare (mattress covers, examination couches), sports and leisure goods
It is used for quality control, product development and coating-formulation comparison, type approval, and contractual specification compliance

Related Standard:
| ISO 12947-1 | Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 1: Martindale abrasion testing apparatus |
| ISO 12947-2 | Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 2: Determination of specimen breakdown |
| ISO 12947-3 | Textiles - Determination of the abrasion resistance of fabrics by the Martindale method - Part 3: Determination of mass loss |
| ISO 12945‑2 | pilling & fuzzing on the modified Martindale apparatus — same machine family, different end point |
| ISO 5470-1 | Rubber- or plastics-coated fabrics - Determination of abrasion resistance - Part 1: Taber abrader |
| ISO 5470-2 | Rubber- or plastics-coated fabrics. Determination of abrasion resistance. Martindale abrader |
| ASTM D4966 | Standard Test Method for Abrasion Resistance of Textile Fabrics (Martindale Abrasion Tester Method). |
| ASTM D4970 | Standard Test Method for Pilling Resistance and Other Related Surface Changes of Textile Fabrics: Martindale Tester |
| GB/T 21196.3 | Textiles-Determination of the abrasion resistance of fabrics by the Martindale method-Part 3:Determination of mass loss |
| JIS L 1096, M&S P19 | other commonly referenced abrasion/pilling methods |
| GBT 4802.2 | Textiles - Determination of fabric propensity to surface fuzzing and to pilling - Part 2: Modified Martindale method |
Keywords: ISO 5470-2,Martindale abrader,coated fabric abrasion tester,rubber coated fabric test,plastic coated fabric abrasion resistance,dry abrasion test,wet abrasion test,Martindale abrasion tester,textile coating test,coated textile quality control,lab abrasion testing equipment, UnitedTest abrasion machine, Martindale abrasion tester, Martindale abrasion testing machine, ISO 5470-2 tester, Martindale abrader manufacturer, coated fabric abrasion tester, Martindale wear tester supplier, Martindale abrasion tester manufacturer / supplier
Related products and device
Related Standard
ISO 12947-1 Textiles — Determination of the abrasion resistance of fabrics by the Martindale method — Part 1: Martindale abrasion testing apparatus
ISO 12947-1 defines mandatory construction, dimensional, performance and auxiliary‑material requirements for Martindale abrasion testers, which are used to carry out the practical test procedures laid down in ISO 12947‑2,‑3,‑4. It is the specification for the machine and the consumables — the "hardware norm". The actual abrasion procedures live in Parts 2, 3 and 4, and Part 1 is written to guarantee that a Martindale result obtained in one lab is physically comparable to one obtained in another.
ISO 5470-1: Rubber- or plastics-coated fabrics -- Determination of abrasion resistance -- Part 1: Taber abrader.
ISO 5470-1 specifies a method for determining the abrasion resistance of rubber- or plastics-coated fabrics using the Taber abrader apparatus. This test simulates wear under controlled conditions to evaluate a material's durability.
ISO 13937-2 Textiles – Tear properties of fabrics – Part 2: Determination of tear force of trouser‑shaped test specimens (Single tear method).
ISO 13937-2 is method for determining the tear force required to propagate an already-started single tear, using a rectangular specimen slit into two "trouser legs". Mainly for woven fabrics; may also apply to fabrics made by other techniques (e.g. some nonwovens). Not applicable to knitted fabrics, woven elastic fabrics, highly anisotropic fabrics, or loose fabrics where the tear tends to transfer from one direction to another. Only CRE (constant-rate-of-extension) machines are permitted.
ASTM D5035 : Standard Test Method for Breaking Force and Elongation of Textile Fabrics (Strip Method)
ASTM D5035 is the standard test method for determining breaking force (tensile strength) and elongation at break of textile fabrics using the strip method. It defines two core procedures--raveled strip (for woven fabrics) and cut strip (for nonwovens, coated/felted fabrics)--and supports both dry and wet testing.
ISO 12945-2 Textiles — Determination of fabric propensity to surface pilling, fuzzing or matting — Part 2: Modified Martindale method
ISO 12945-2 specifies a method for determining the resistance to pilling, fuzzing and matting of textile fabrics using a modified Martindale machine. It ranks fabrics in the same order of surface-change propensity as is likely to occur in end-use wear.
ASTM D4966 Standard Test Method for Abrasion Resistance of Textile Fabrics (Martindale Abrasion Tester Method)
ASTM D4966 determination of the abrasion resistance of textile fabrics using the Martindale abrasion tester; generally applicable to knit, woven and nonwoven fabrics — material thickness may limit suitability because of specimen-holder capacity. It applies to woven, knit and non‑woven textiles, though excessive fabric thickness may restrict testing due to specimen‑holder physical limits.
ASTM D4970 Standard Test Method for Pilling Resistance and Other Related Surface Changes of Textile Fabrics: Martindale Tester.
ASTM D4970 is the Martindale (Lissajous‑motion) fabric‑on‑fabric pilling test used to predict how badly a fabric will pill, fuzz or otherwise change its surface appearance in wear, reported on an arbitrary 5‑to‑1 rating scale (5 = no pilling, 1 = very severe pilling).
ISO 17704 Footwear — Test methods for uppers, linings and insocks — Abrasion resistance
ISO 17704 is method for determining the resistance of uppers, linings and insocks — irrespective of material — to wet and dry abrasion, in order to assess suitability for the end use. Note the standard deliberately gives no pass/fail criteria; it produces a description and rating of damage at prescribed rub counts.
Frequently Asked Questions (Q&A) for ISO 5470‑2 Martindale Abrasion Test
ISO 5470-2:2021 is an international test method that determines the abrasion resistance of the coated surface of rubber- or plastics-coated fabrics using a Martindale abrader. It specifies two methods (specimen in holder / specimen on table) and can be run dry or wet.
2. Why is this test important for coated fabrics?
On a coated fabric the polymer layer carries everything that matters: colour, gloss, embossing/print, waterproofing, cleanability, chemical and stain resistance. The coating is usually only a fraction of a millimetre thick. Once it is rubbed through, the product has functionally failed even though the base fabric is still strong. ISO 5470-2 reproduces that failure progression in the lab, so manufacturers can predict service life, qualify suppliers, compare coating formulations and defend warranty claims with reproducible numbers.
3. What is the difference between Method 1 and Method 2?
Method 1: the specimen is clamped in the circular holder and rubbed against abradant placed on the table (felt + abradant underneath). This is the routine configuration.
Method 2: the arrangement is reversed — the specimen (125 mm × 125 mm) is taped to the abradant table, and the abradant is carried in the holder. Used when the product specification calls for it or when the specimen is better supported flat.
4. What is the difference between ISO 5470-1 and ISO 5470-2?
Same series, different machines:
ISO 5470-1:2016 uses a Taber abrader (rotating turntable + two abrasive wheels).
ISO 5470-2:2021 uses a Martindale abrader (Lissajous motion).
The Martindale method rubs the whole exposed area in all directions and keeps the specimen flat, avoiding known Taber drawbacks: a narrow abraded strip, local heating of the coating, and subjective end points.
5. What abradants are allowed?
Either a wool abradant fabric (to ISO 12947-1:1998, Table 1) or silicon carbide cloth, grade P 180 (fused SiC on cotton backing, warp breaking strength ≥ 961 N/50 mm, weft ≥ 392 N/50 mm). Results obtained with different abradants are NOT comparable — say so on every report. Non-standard abradants may be used by agreement but must be fully described in the test report.
At least four per surface, taken from non-adjacent areas within the usable width of the roll (ISO 2286-1). For double-coated fabrics where both faces are tested, take a second set of at least four. With irregular embossing or printed patterns, take enough specimens to cover every part of the pattern — often more than four.
Method 1: sized to fit the holder clamping system (die-cut to match the 645 mm² exposed area).
Method 2: 125 mm × 125 mm, fixed to the table with double-sided tape.
PU foam backing (3 mm) is used behind specimens lighter than 500 g/m² (may be omitted if the material has a pronounced rear lamination).
Dry: condition ≥ 16 h in the ISO 2231 standard atmosphere and test in it.
Wet: no pre-conditioning; saturate the abradant + felt (Method 1) or the mounted specimen (Method 2) with the water-jet until uniform darkening. During the run, re-wet with up to 30 g of water rubbed in with the fingertips, then place the weightpiece on top for 10 ± 1 s. Wet data exposes failures caused by perspiration, humidity and wet cleaning — a coating that passes dry can fail badly wet.
9. How does ISO 5470-2 differ from ASTM D4966 / Wyzenbeek?
ASTM D4966 is the US Martindale method for textile fabrics; ASTM D4157 (Wyzenbeek) is an oscillatory cylinder (back-and-forth) method common in US upholstery specs. ISO 5470-2 is specifically written for coated fabrics and adds the wet-abrasion variant and the coating-failure (top-coat) rating scale. Results between these methods are not interchangeable.
10. Why choose ISO 5470‑2 Martindale Abrasion Tester from UnitedTest Manufacturer?
UnitedTest is a professional manufacturer of ISO 5470‑2:2021 Martindale abrader for rubber‑ or plastics‑coated fabrics. Our Martindale abrasion testing machine fully complies with ISO 5470‑2:2021 international standard, supporting both dry abrasion and wet abrasion test, implementing both Method 1 and Method 2 for coated‑fabric abrasion‑resistance measurement.
Our ISO 5470‑2 Martindale tester is widely used in quality‑control laboratory, material R&D lab, third‑party inspection institutes for testing PVC coated fabric, PU coated textile, tarpaulin, automotive upholstery fabric, outdoor membrane materials and protective coated textiles.
✅ Strictly meets core ISO 5470‑2 parameters:
12 kPa standard contact pressure
Standard Lissajous 60 × 60 mm motion track
Running speed 48 ±4 revolutions per minute
Multi‑station options (2 /4 /6 /9 stations) for high‑throughput testing
Complete accessories kit: wool abradant, silicon‑carbide cloth, standard wool felt, PU foam backing, weight‑piece, water‑jet assembly for wet‑abrasion testing
Touch‑screen control, automatic revolution counter, programmable inspection interval reminder for wet‑test re‑wetting operation
Realizes visual damage‑rating test and mass‑loss abrasion test as per standard requirements
Many customers confuse ISO 5470‑2 Martindale tester with common ISO 12947 textile Martindale machine. UnitedTest’s ISO 5470‑2 model reserves special functions for coated‑fabric requirements: dedicated wet‑abrasion workflow, parallelism calibration structure for specimen holder and abradant table, matching clamping fixtures for Method 1 / Method 2 specimen mounting.
If you are looking for reliable ISO 5470‑2 testing equipment for rubber and plastic coated fabrics, UnitedTest provides complete instrument supply, standard‑based training, after‑sales support and customization service. Our machines help you generate valid, reportable test data for product specification verification and international trade acceptance.