Information on the most widely used ASTM standards within the materials testing industry
ISO 2285 Rubber Tension Set & Tensile Creep Tester | UnitedTest
UnitedTest manufactures ISO 2285 testing machines for vulcanized and thermoplastic rubber, measuring tension set under constant elongation, plus elongation, creep and tension set under constant tensile load for rubber materials ranging from 20 IRHD to 94 IRHD.
ISO 2285 defines standardized laboratory methods to evaluate dimensional changes of vulcanized or thermoplastic rubber specimens during and after short-term tensile loading, covering two core test conditions: constant elongation and constant tensile load. The constant elongation test assesses elastic recovery after sustained strain, which can be performed at ambient or elevated temperature, while the constant tensile load test records real-time elongation, creep deformation and residual tension set after load release. This standard applies to rubber materials with hardness between 20 IRHD and 94 IRHD, widely used for raw material incoming inspection, compound formulation development, finished rubber component quality control, and performance verification for seals, gaskets, hoses and elastic rubber parts. Our UnitedTest ISO 2285 tester delivers stable clamping, precise load control and temperature-compatible testing environment to meet the full test requirements of this international standard.
Test Principle:
Rubber is viscoelastic: part of a deformation is elastically recoverable, part is permanent (viscous/plastic). ISO 2285 isolates the permanent component after a defined strain/time/temperature history.
Tension set at constant elongation: The residual elongation remaining after sustained fixed strain, expressed as a percentage of the applied elongation. It quantifies the ability of rubber to recover its original dimensions after prolonged stretching.
Tension set at constant load: The residual elongation remaining after sustained fixed load, expressed as a percentage of the original unloaded length.
Creep: The time-dependent increase in elongation under constant load, expressed as a percentage of the initial elongation measured immediately after loading.
Fundamentally, the tests characterize the elastic recovery and viscoelastic behavior of vulcanized and thermoplastic rubbers under tensile stress.
Specific Test Methods
1. Constant-Elongation Tension Set Test
This method measures the residual elongation (tension set) of rubber after it is stretched to a fixed strain level, held for a specified time (at ambient or elevated temperature), then released and allowed to recover. For elevated-temperature tests, three cooling/strain-release protocols are specified (Method A is the preferred default):
Method A: Remove the strained specimen from the oven, immediately release strain, rest for 30 min, then measure recovered length.
Method B: Remove the strained specimen from the oven, keep it stretched for 30 min, release strain, rest for another 30 min, then measure.
Method C: Release strain while the specimen is still inside the hot oven, rest 30 min in the oven, remove and rest another 30 min, then measure.
2. Constant-Load Test
This method applies a fixed tensile stress to the specimen at standard laboratory temperature and determines three properties:
Elongation: The strain reached 30 seconds after load application.
Creep: The progressive increase in elongation over 60 minutes under constant load.
Tension set: The residual elongation measured after unloading and a 10-minute recovery period.
Test Specimen Information:
Standard sheet thickness: 2 mm ± 0.2 mm (large ring specimens: 4 mm ± 0.2 mm).
1, Specimens for constant-elongation testing
Strip specimens: 2–10 mm wide (6 mm preferred); reference length 25–50 mm (50 mm preferred).
Strips with enlarged ends: Narrow gauge section of 25–50 mm serves as the reference length.
Ring specimens:
Large ring: 4 mm thick, outer diameter 52.6 ± 0.2 mm, inner diameter 44.6 ± 0.2 mm; preferred reference length 40 mm.
Small ring: 2 mm thick, outer diameter 33.5 ± 0.2 mm, inner diameter 29.5 ± 0.2 mm; preferred reference length 25 mm.
2, Specimens for constant-load testing
Dumbbell-shaped specimens, 2 mm thick, with reference marks spaced 90 mm ± 0.5 mm apart in the central narrow section.
ISO 2285 Tension & Elongation Test for Rubber & TPE Required Testing Equipment:
| Creep Test Machine | Applies load smoothly without transient overload, and maintains the test load within ±1% of the target value. |
| For constant-elongation measurements | Straining device: Equipped with one fixed and one movable holder. It uses self-tightening clamps for strip specimens, jaws for enlarged-end strips, and flat pulleys (≈5 mm wide, 10 mm diameter) for ring specimens. It must be low-mass for oven use and may be configured as a multi-unit system. Oven: Conforming to ISO 188 requirements, used for tests conducted above standard laboratory temperature. Length-measuring device: With a resolution of 0.1 mm. For ring specimens, a graduated cone (for inner diameter measurement) or rigid straightening channels are required. |
| For constant-load measurements | Straining device: Consists of specimen clamps and dead weights (or equivalent loading mechanism). Thickness/width gauge: Compliant with ISO 23529 Method A; width measurement resolution of 0.05 mm for die-cut specimens. Length-measuring device: With a resolution of 0.1 mm.
|
Key Test Parameters:
1, Constant-elongation test parameters
| Strain levels | 15%, 20%, 25%, 50%, 75%, 100%, 200%, 300% (each with defined tolerance) |
| Recommended strain | 100% for vulcanized rubber; 20% for thermoplastic rubbers (below yield point) |
| Test duration | 24 h, 72 h, or 168 h (tolerance: −2 / 0 h), starting 30 min after strain application |
| Test temperature | Selected per ISO 23529; 70 °C ± 1 °C recommended |
| Recovery time | 30 min (0 / +3 min) at standard laboratory temperature |
2, Constant-load test parameters
| Applied stress | 2.5 MPa ± 0.1 MPa (based on original cross-section); 1.0 MPa allowed if 2.5 MPa is excessive |
| Elongation measurement timing | 30 s ± 2 s after loading |
| Creep measurement timing | 60 min ± 1 min after loading |
| Tension set recovery time | 10 min ± 1 min after unloading |
Test procedure of ISO 2285 Tension & Elongation Test for Rubber & TPE
1. Constant-elongation test procedure
Measure the unstrained reference length L1 of each specimen at standard temperature, then mount it in the straining device.
Stretch the specimen to the target strain. After 10–20 minutes, measure the strained reference length L2 and verify the strain accuracy. Discard and replace the specimen if the strain is out of tolerance.
Ambient-temperature test: Hold the strain for the specified period, release the load, rest the specimen on a flat non-sticky surface for 30min, then measure the recovered length L5.
Elevated-temperature test: After 20–30 minutes of pre-stretching, place the device in the oven for the full test duration. At the end of the period, apply one of the three cooling/release methods (A/B/C) and measure the recovered length.
2. Constant-load test procedure
Measure the initial reference length L1, thickness, and width of the specimen at standard temperature.
Clamp the specimen and apply the constant load without shock.
Elongation: Measure the reference length L2 at 30 s ± 2 s after loading.
Creep: Measure the reference length L3 at 60 min ± 1 min after loading.
Tension set: Unload the specimen, rest it on a flat surface for 10 min ± 1 min, then measure the recovered reference length L4.
Industries Application:
Rubber compounders and vulcanized-rubber / TPE manufacturers, chemical engineers, and any organisation responsible for rubber testing and quality — the standard is explicitly positioned for these users, to understand compound quality and improve durability and strength.
Cure-state verification and batch QC of thin-walled products — the constant-load method's primary intended use per the ISO note.
Sealing technology: O-rings, gaskets and seals are routinely tested in tension set as a supplement to compression set; the tensile set result correlates approximately with compression set and is sensitive to crosslink state after thermal load.
Civil-engineering / construction seals: for example, GB/T 23662-2022 (rubber seals for concrete pavement expansion joints) cites ISO 2285:2019.
Heat-ageing / elevated-temperature material evaluation, using ISO 188 ovens, and incoming-material or production-release testing in independent laboratories and certification bodies.
Downstream sectors that specify stretched or thin-walled elastomer parts (automotive, fluid power, industrial equipment, appliances) use the data indirectly through product specifications that call up ISO 2285
Related Test Standard
| ASTM D638 | Test Method for Tensile Properties of Plastics (tensile specimen geometry) |
| ASTM D1414 | Rubber O-ring test methods; contains a tension set test. Often compared with ISO/DIN ISO 2285 in sealing labs, but the procedures and results are not interchangeable. |
| ISO 2285 | Rubber, vulcanized or thermoplastic—Determination of tension set under constant elongation,and of tension set,elongation and creep under constant tensile load |
| ASTM D412 | Broad tensile test for vulcanized rubber / TPE that also derives a tensile set after a 10-minute retraction; similar to ISO 37, but not equivalent to ISO 2285. |
| GB/T 42279 | Rubber,vulcanized or thermoplastic—Determination of tension set under constant elongation,and of tension set,elongation and creep under constant |
| ISO 188 | Rubber — Accelerated ageing and heat resistance tests (specifies oven performance requirements) |
| ISO 8013 | Rubber, vulcanized — Determination of creep in compression or shear (for design-level creep evaluation) |
| ISO 899-1 | Tensile creep and creep-rupture |
| ISO 899-2 | Flexural creep Test |
| ISO 815-1 | Rubber, vulcanized or thermoplastic — Determination of compression set — Part 1 (the compression-mode equivalent of tension set testing) |
| ASTM D2990 | Standard Test Methods for Tensile, Compressive, and Flexural Creep and Creep-Rupture of Plastics |
| JIS K6273 | Japanese determination of tensile set, elongation and creep, commonly cited as the national counterpart. |
Keywords: ISO 2285 tester, rubber tension set test machine, rubber tensile creep tester, vulcanized rubber tension set, thermoplastic rubber creep test, constant elongation tension set, constant tensile load creep, IRHD rubber test, rubber elastic recovery test, rubber seal material testing, rubber gasket lab test, rubber elongation test, rubber compound quality control, rubber material deformation test, rubber tensile deformation tester, UnitedTest rubber testing equipment
Related products and device
Related Standard
ISO 899-1 Plastics — Determination of creep behaviour — Part 1: Tensile creep
ISO 899-1 determines tensile creep of plastics in the form of standard test specimens under specified conditions of pretreatment, temperature and humidity. It applies to rigid and semi-rigid, non-reinforced, filled and fibre-reinforced plastics, using dumb-bell-shaped specimens that are either directly moulded or machined from sheets or moulded articles.
ISO 899-2 Plastics — Determination of creep behaviour — Part 2: Flexural creep by three-point loading
ISO 899-2 specifies how to measure the time-dependent bending deformation of a freely supported plastic beam under a constant mid-span load, under controlled pre-treatment, temperature and humidity. Apply for rigid and semi-rigid, non-reinforced, filled and fibre-reinforced plastics; specimens moulded directly or machined from sheets or moulded articles.
ASTM D412 test methods cover procedures used to evaluate the tensile (tension) properties of vulcanized thermoset rubbers and thermoplastic elastomers. These methods are not applicable to ebonite and similar hard, low elongation materials.
ASTM D412 is the primary standard for evaluating the tensile properties of vulcanized thermoset rubbers and thermoplastic elastomers (TPEs). It provides precise procedures for determining critical mechanical characteristics that define material performance under stretching forces.
The methods appear as follows:
Test Method A—Dumbbell and Straight Section Specimens
Test Method B—Cut Ring Specimens
ASTM D2990 Standard Test Methods for Tensile, Compressive, and Flexural Creep and Creep-Rupture of Plastics
ASTM D2990 defines procedures to measure time-dependent deformation (creep) and time-to-failure (creep-rupture) of plastic materials under constant static load and controlled environmental conditions.
ISO 188 defines air‑oven (hot‑air) ageing procedures for vulcanized rubber and thermoplastic elastomers (TPEs). It specifies for conducting accelerated ageing tests and heat resistance tests on vulcanized rubber and thermoplastic elastomers, serving as a fundamental testing specification for evaluating rubber’s thermal stability and long-term service performance.
ISO 527-1 covers the test procedures for determining tensile properties of plastics and plastic composites. Tensile properties of plastics that are determined through the practices of ISO 527-1 include tensile strength, tensile modulus and other properties related to stress strain characteristics of plastic materials.
ISO 527-2 specifies the test conditions for determining the tensile properties of moulding and extrusion plastics, based upon the general principles given in ISO 527-1. The methods described in ISO 527-2 are selectively suitable for use with the following range of materials: rigid and semi-rigid thermoplastics moulding, extrusion and cast materials, including compounds filled and reinforced by, for example, short fibres, small rods, plates or granules but excluding textile fibres (see ISO 527-4 and ISO 527-5).
ASTM D638 determining the tensile properties of unreinforced and reinforced plastics using dumbbell-shaped (dogbone) specimens tested under closely controlled conditions of conditioning, temperature, humidity, and crosshead speed. For measuring the tensile mechanical properties of unreinforced and reinforced plastics, including thermoplastics, thermosets, molded plastics, and plastic composites.
ASTM D790: Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials
ASTM D790 determines flexural (bending) properties for unreinforced plastics, reinforced plastics, high‑modulus composites and electrical insulating materials via three‑point bending on simply‑supported rectangular beam specimens. It applies to rigid and semi‑rigid materials. Flexural strength cannot be calculated if the specimen neither yields nor fractures on its outer surface before reaching 5 % maximum outer‑fiber strain.
ASTM D2412: Standard Test Method for Determination of External Loading Characteristics of Plastic Pipe by Parallel-Plate Loading
ASTM D2412 test method covers the determination of load-deflection characteristics of plastic pipe under parallel-plate loading. It covers thermoplastic resin pipe, reinforced thermosetting resin pipe (RTRP), and reinforced polymer mortar pipe (RPMP). Pipes tested under ASTM D2412 must be smaller than the envelope of the two compression platens by at least a half an inch. Square or circular platens can be used, with most customers choosing a square platen. Care must be taken to account for the mid-section of the pipe which will expand slightly as the pipe is compressed.
The characteristics determined by ASTM D2412 test method are pipe stiffness, stiffness factor, and load at specific deflections.
ISO 8013— Rubber, vulcanized — Determination of creep in compression or shear
ISO 8013 defines standardized methods for determining the creep behavior of vulcanized rubber under continuously applied compressive or shear forces at controlled temperatures. This standard does not apply to rubber under intermittent deformation.
Frequently Asked Questions (FAQs) about ISO 2285 Tension & Elongation Test
Q1. What is ISO 2285:2019?
A. ISO 2285:2019, 8th edition, is the international test method for determining dimensional changes in vulcanized or thermoplastic rubber during and after relatively short periods of tensile loading, under either constant elongation or constant tensile load. It is published by ISO/TC 45/SC 2 and applies to rubber in the hardness range 20 IRHD to 94 IRHD.
Q2. What does the ISO 2285 test actually measure?
A. It measures:
Tension set under constant elongation;
Tension set, elongation and creep under constant load.
In plain terms: it tells you how much a rubber sample fails to return to its original length after being stretched or loaded for a defined time.
Q3. Which materials does ISO 2285 cover?
A. Vulcanized rubber and thermoplastic rubber / thermoplastic elastomer (TPE), in the hardness range 20–94 IRHD. The standard is intended for relatively short-term tensile loading, not long-term creep design data.
Q4. What is “tension set” in simple terms?
A. Tension set is the permanent elongation left after unloading, expressed as a percentage. Under constant elongation it is expressed relative to the imposed elongation; under constant load it is expressed relative to the original unloaded length.
Q5. What is “creep” in ISO 2285, and can I use it for product design?
A. Creep is the increase in elongation under constant load during a specified time, expressed as a percentage of the elongation at the beginning of that time. No — ISO 2285 explicitly states that its creep measurement is not intended for product design or for evaluating low-creep materials. For those purposes ISO 8013 applies, and ISO 2285 results and ISO 8013 results do not agree.
Q6. Why is the ISO 2285 tension set test important for rubber materials?
A. Because it measures elastic recovery, not just strength. A compound can pass a tensile-strength test yet still take a permanent set after being stretched. ISO 2285 quantifies that irreversible deformation under a controlled strain/load/time/temperature history, making it useful for compound development, cure verification and batch release.
Q7. Why does it matter for seals, O-rings and thin-walled rubber parts?
A. Many elastomer components are assembled or used in a stretched condition. High tension set means the part does not return to its designed geometry, which can reduce interference, sealing force or fit. ISO 2285 is widely used alongside compression-set testing for O-rings and sealing compounds, and its constant-load method is specifically noted for quality control of thin-walled products.
Q8. What strain levels are allowed, and which should I choose?
A. Allowed strains are 15 % ± 1,5 %, 20 % ± 2 %, 25 % ± 2,5 %, 50 % ± 5 %, 75 % ± 7,5 %, 100 % ± 10 %, 200 % ± 10 %, 300 % ± 10 %.
100 % is preferred for vulcanized rubber, but do not exceed one third of elongation at break at the test temperature.
For TPEs with a yield point, only results below the yield point are valid; 20 % ± 2 % is preferred where possible.
Measure the strained length 10–20 min after reaching strain; if the calculated strain is out of tolerance, discard the piece and test a replacement.
Q9. What does a high or low tension-set result tell me?
A. A high value means more permanent deformation and poorer recovery; a low value means better elastic recovery. In a cure-study context, higher set is consistent with a lower state of cure / crosslink density — but formulation, strain level, temperature and release history also influence the number, so it should not be read as a standalone cure meter.
Q10. How does ISO 2285 reflect state of cure or crosslinking?
A. The ISO 2285 scope note says an increase in the state of cure or degree of crosslinking is usually reflected in a decrease in set, creep or elongation. That makes the test a sensitive QC signal for under-cure, compound drift or inconsistent vulcanisation.
Q11. Why can’t I just run a conventional tensile-to-break test?
A. A tensile-to-break test gives tensile strength, elongation at break and modulus. It does not hold a specimen at a fixed strain or load for hours and then measure recovery. ISO 2285 captures the time-dependent, viscoelastic permanent deformation that a fast pull-to-break test misses.
Q12. Why is tension set often paired with compression set?
A. Real components see mixed loading. Tension set and compression set are both permanent-deformation tests, just under opposite loading modes; sealing laboratories commonly run them together because the tensile-set result correlates approximately with compression-set behaviour. ISO 815-1 is listed in the ISO 2285 Bibliography as the compression-set counterpart.
Q13. What test duration and temperature are used?
A. Nominal strained periods are 24 h, 72 h or 168 h, with a tolerance of +0 / −2 h — i.e. 22–24 h, 70–72 h, 166–168 h — counted from 30 min after the strain is applied. Test temperature is selected from ISO 23529; if the product specification gives none, 70 °C ± 1 °C is recommended.
Q14. What load and timing apply to the constant-load method?
A. Apply 2,5 MPa ± 0,1 MPa based on the original cross-sectional area, without shock; 1,0 MPa may be used if 2,5 MPa is too large. Then:
30 s ± 2 s → measure L₂ for elongation;
60 min ± 1 min → measure L₃ for creep;
unload, rest on a flat non-sticky wooden surface for 10 min ± 1 min → measure L₄ for tension set.
Q15. What are Methods A, B and C, and why must they be reported?
A. They are the three cooling and strain-release options after elevated-temperature exposure — not the two test methods:
Method A (preferred): remove from oven → release immediately → recover 30 min → measure.
Method B: remove from oven but keep strained 30 min → release → recover a further 30 min → measure.
Method C: release while still in the hot oven → after 30 min remove → recover a further 30 min → measure.
Recovery is 30 min (+3 / −0 min), i.e. 30–33 min. Different release histories change the result, so the method used must be reported.
Q16. Why choose ISO 2285 Tension Set Testing Machine, Rubber Creep & Elongation Tester from UnitedTest?
A. UnitedTest manufactures ISO 2285 tension set test equipment for laboratories measuring tension set, elongation and creep in vulcanized rubber and thermoplastic elastomers. ISO 2285:2019 defines two routes: a constant-elongation test, where a strip, tab-end or ring specimen is held at a specified strain — typically 100 %, or 20 % for many TPEs — for 24 h, 72 h or 168 h at standard laboratory temperature or in an ISO 188 oven at, for example, 70 °C ± 1 °C; and a constant-load test, where a dead-weight or equivalent rig applies 2.5 MPa ± 0.1 MPa at standard laboratory temperature while elongation is read at 30 s and creep at 60 min.
Engineered for both quality control laboratories and R&D facilities, UnitedTest testing machines support all standard specimen types specified in ISO 2285 — strip specimens, enlarged-end strips, and ring specimens — with optional temperature-controlled ovens for elevated-temperature testing per ISO 188. Each system comes calibrated according to ISO 18899 guidelines and includes integrated length-measuring instrumentation with 0.1 mm resolution.
Whether you require a standalone constant-elongation straining frame, a complete constant-load creep testing station, or a multi-station automated configuration, UnitedTest provides durable, repeatable, and cost-effective rubber testing solutions trusted by manufacturers, testing laboratories, and research institutions worldwide.
Require More Customized Solutions?