Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D2990 Plastic Creep & Creep-Rupture Test

ASTM D2990 Plastic Creep & Creep-Rupture Test

Share:

ASTM D2990 Plastic Creep and Creep-Rupture Tester | UnitedTest

UnitedTest manufactures ASTM D2990 creep test machines for tensile, compressive and flexural creep & creep-rupture testing of plastics. Our equipment captures long-term time-dependent deformation and failure time under constant static load and controlled temperature, supporting material comparison, long-life part design and quality validation for polymer and composite plastic components.


ASTM D2990 defines standardized laboratory procedures to measure time-dependent deformation (creep) and time-to-failure (creep-rupture) of plastic materials under constant static load and controlled environmental conditions. It covers three primary loading modes: tensile, compressive, and flexural creep, with three-point or optional four-point bending configurations for flexural testing. The generated creep data helps engineers calculate creep modulus, forecast long-term dimensional shift, compare polymer grades, validate material selection and support structural design for plastic parts that carry sustained static loads in service. UnitedTest’s ASTM D2990 compliant creep test system delivers stable load control, precise displacement monitoring and programmable environmental conditioning to meet the standard’s test requirements for R&D, incoming material inspection and third-party laboratory testing.


- Covers three loading modes: tension, compression, and flexure.

- Default flexural method uses three-point loading aligned with Test Method D790; four-point loading per D6272 is permitted as an alternative.

- Tension is the preferred mode for creep-rupture testing, as some ductile plastics do not exhibit rupture in flexural or compressive loading.

ASTM D2990 Plastic Creep


Test Principle: 

The test methods are based on the viscoelastic nature of plastics, whose mechanical response depends on time, temperature, and stress level.

  • Creep: The progressive deformation of a material held under constant static load and constant temperature. Total creep strain includes both instantaneous elastic strain and time-dependent inelastic strain (the two cannot be practically separated for plastics, so "strain" refers to their sum).

  • Creep-rupture: A continuation of the creep test until specimen failure, generating a "creep-rupture envelope" (stress-at-rupture plotted against time-to-rupture) that defines the material’s long-term load-bearing limit.

  • Creep stages: A typical creep curve includes three phases:

    1. Primary creep (decreasing creep rate)

    2. Secondary creep (steady-state, constant creep rate)

    3. Tertiary creep (accelerating deformation leading to fracture)

  • Creep modulus: Calculated as the ratio of initial applied stress to total creep strain at a given time.

  • Data is conventionally plotted on logarithmic scales for analysis and extrapolation.



Specific Test Methods

Tensile Creep and Creep-Rupture

A constant axial tensile load is applied to the specimen. The test measures the increase in gauge length (extension) as a function of time. 

For creep-rupture, the test continues until specimen breakage, and time-to-rupture is recorded. This is the preferred mode for rupture testing.

Compressive Creep and Creep-Rupture

A constant compressive load is applied, and the decrease in gauge length is measured over time. 

Two specimen configurations are specified:

  • Unconfined specimens: For materials with moderate slenderness.

  • Slender specimens: Tested with a guide tube fixture to prevent buckling during long-term loading.

Flexural Creep

Constant transverse load is applied to a beam specimen, and mid-span deflection is measured over time.

Default: Three-point bending (per D790), with load applied at the center of the support span.

Optional: Four-point bending (per D6272), with two load points creating a constant-moment region. 

Note: Flexural creep-rupture is not reliable for all ductile plastics, as some will not fracture in this mode.


Test Specimen Information:

Test ModeSpecimen Type / Dimensions
TensileType I or Type II per ASTM D638; D1822 specimens permitted for creep-rupture
Unconfined CompressiveRight cylinder or prism; preferred 12.7×12.7 mm square or 12.7 mm diameter; slenderness ratio 11–15
Slender Compressive (guide tube)Square bar: 4.850 ± 0.025 mm per side, 51 mm length; ends perpendicular to sides
FlexuralRectangular bar per D790; preferred sizes: 63.5×12.7×3.18 mm or 127×12.7×6.4 mm

Replication: 

  • Creep: Minimum 2 specimens per stress level if ≥4 stress levels are used; minimum 3 if <4 levels.

  • Creep-rupture: Minimum 2 specimens per stress level (scatter of 0.5–1 decade in time-to-rupture is typical, so more replicates may be needed).


ASTM D2990 Plastic Creep & Creep-Rupture Test required Testing Equipment: 

Creep Test Machine

Must maintain applied load within ±1% of the target value throughout the test.

Must apply load rapidly, smoothly, and reproducibly (1–5 seconds).

Lever-type systems must be designed to maintain constant load as the specimen deforms.

Multi-station equipment must include shock isolation (nets or cushions) to prevent vibration transfer when a specimen fails.

Loading Fixtures

Tensile: Grips with swivel or universal joints at both ends to minimize eccentric loading; grips must allow specimen centering before loading and prevent slippage during loading.

Compressive: Parallel flat anvils (one self-aligning) for uniform load distribution; a guide tube assembly (3.2 mm Schedule 40 stainless steel pipe, ~150 mm long, 6.860 ± 0.025 mm inner diameter) for slender specimens to prevent buckling.

Flexural: A rigid test rack with support span equal to 16 (+4, −2) times specimen thickness; support noses and loading stirrup with 3.2 mm radius to avoid indentation and stress concentration.

Deformation MeasurementAcceptable methods: direct-contact extensometers, dial gauges, cathetometers, or resistance strain gauges (if perfect adhesion is achieved).


Key Test Parameters:

Standard comparison temperatures: 23, 50, 70, 90, 120, and 155°C. 

Creep-rupture: Minimum 7 stress levels per temperature, targeted to produce rupture at approximately 1, 10, 30, 100, 300, 1000, and 3000 hours.

  • Creep:

    • Linear viscoelastic materials: Minimum 3 stress levels per temperature.

    • Stress-dependent materials: Minimum 5 stress levels per temperature.

    • Stress increments: Nearest 3.5 MPa (above 7 MPa) or nearest 0.7 MPa (below 7 MPa).

    • No stress level causing failure in less than 1000 hours may be used for creep testing.

    1% strain at 1000 h: Determined by interpolation from a 1000-hour isochronous stress-strain curve.

Measurement Schedule

Deformation, temperature, humidity, and control specimen data are recorded at: 1, 6, 12, 30 minutes; 1, 2, 5, 20, 50, 100, 200, 500, 700, 1000 hours. For tests longer than 1000 hours, measurements are taken at least monthly.


Test procedure of ASTM D2990 Plastic Creep & Creep-Rupture Test

  1. Mount the conditioned and dimensionally measured specimen in the test fixture; install control specimens if required.

  2. Attach the deformation measurement device and record the initial (zero-load) reference value.

  3. Apply the full test load rapidly and smoothly (1–5 seconds maximum); start timing at load onset.

  4. If testing in a liquid or chemical environment, apply the agent to the gauge length immediately after loading; replenish volatile agents periodically.

  5. Record deformation and environmental parameters according to the specified time schedule.

  6. At the end of the test interval (if no rupture occurs), remove the load rapidly and smoothly.

  7. (Optional) Measure strain recovery after load removal using the same time schedule.

  8. Calculate stress, strain, creep modulus, and perform least-squares regression on log-stress vs. log-time-to-rupture data.


Industries Application:

ASTM D2990 is used across industries where plastic components operate under sustained static load over long service lives:

  • Automotive: Structural interior/exterior parts, load-bearing brackets, and housings.

  • Aerospace: Lightweight plastic components exposed to elevated temperatures and constant loads.

  • Electrical/Electronics: Insulating components, connector housings, and support structures.

  • Construction and Infrastructure: Plastic piping, panels, fasteners, and structural profiles.

  • Chemical Processing: Pumps, valves, and piping components exposed to fluids under load.

  • Durable goods manufacturing: Material selection, quality control, and specification compliance.


Related Test Standard

ASTM D638Test Method for Tensile Properties of Plastics (tensile specimen geometry)
ASTM D695Test Method for Compressive Properties of Rigid Plastics (compressive specimen basis)
ASTM D790Test Methods for Flexural Properties (three-point bending method)
ISO 899-1  Tensile creep and creep-rupture
ISO 899-2Flexural creep Test
ASTM D1780Practice for conducting creep tests of metal‑to‑metal adhesives, typically dead‑weight/lever tensile‑shear creep, temperature/time based.
ASTM D2990Standard Test Methods for Tensile, Compressive, and Flexural Creep and Creep-Rupture of Plastics


The directly comparable international family — ASTM D2990 VS ISO 899


ASTM D2990ISO 899-1ISO 899-2
ModeTensile + compressive + flexural (3-pt & 4-pt) in one documentTensile creep (and creep to rupture)Flexural creep by three-point loading only
SpecimenD638 Type I/II; D695; D790 barISO 527-1A/1B dumb-bells, moulded or machined10 × 4 × 80 mm bar from the multipurpose specimen
Strain measurement

Direct on specimen preferred;

 grip separation permitted with correction factors; 

anvil displacement OK for compression

Extensometer on gauge length required for engineering-design data; 

grip separation only for research/QC

Die movement corrected for rig self-deformation, or optical/video
Compressive creepCoveredNoNo


Keywords: ASTM D2990 creep tester,plastic creep rupture test machine,tensile compressive flexural creep test,polymer long term deformation test,plastic creep modulus measurement,creep rupture test equipment,thermoplastic creep testing,static load creep test,plastic material mechanical characterization,long term polymer performance test,creep displacement monitoring,plastic component durability test,UnitedTest creep tester,plastic lab testing instrument,polymer material qualification test

Related products and device

ASTM D2990 Plastic creeping testing machine

High Temperature Creep and Relaxation Testing Machine is designed as low cost solutions for long-term creep and stress relaxation testing applications of metallic and alloy materials under high temperature in accordance with ASTM, BS, EN, ISO and other similar international testing standards.

ASTM D2990 thermoplastic creep testing, static load creep test machine

WDW Series Computer Control Electronic Universal Testing Machine made by UNITEDTEST range from 100N to 600KN load capacity with various models like single columns, table type, door frame type etc., is used to perform tension, compression, flexure/bending, shearing, peeling etc., test for metal and nonmetal specimens.

creep displacement monitoring, plastic component durability test

Compression test fixture is used to investigate the compressive behaviour of the test specimens and for determining the compressive strength, compressive modulus and other aspects of the compressive stress/strain relationship under the conditions defined.

Related Standard

ASTM D638 Tensile Testing for Plastics –

ASTM D638 determining the tensile properties of unreinforced and reinforced plastics using dumbbell-shaped (dogbone) specimens tested under closely controlled conditions of conditioning, temperature, humidity, and crosshead speed. For measuring the tensile mechanical properties of unreinforced and reinforced plastics, including thermoplastics, thermosets, molded plastics, and plastic composites.

ASTM D695 Plastic & composites Compressive Testing –

ASTM D695: Standard Test Method for Compressive Properties of Rigid Plastics

ASTM D695 test covers the determination of the mechanical properties of unreinforced and reinforced rigid plastics, including high-modulus composites, when loaded in compression at relatively low uniform rates of straining or loading. Test specimens of standard shape are employed. This procedure is applicable for a composite modulus up to and including 41,370 MPa (6,000,000 psi). It is technically equivalent to ISO 604 Plastics‑Determination of Compressive Properties. This test applies end‑loading compression on standard‑geometry specimens under controlled environmental and displacement‑rate conditions, delivering compressive strength, yield strength, offset yield strength, compressive elastic modulus, and compressive deformation data.


ASTM D790 Bending Test Flexural Properties of Unreinforced and Reinforced Plastics –

ASTM D790: Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials

ASTM D790 determines flexural (bending) properties for unreinforced plastics, reinforced plastics, high‑modulus composites and electrical insulating materials via three‑point bending on simply‑supported rectangular beam specimens. It applies to rigid and semi‑rigid materials. Flexural strength cannot be calculated if the specimen neither yields nor fractures on its outer surface before reaching 5 % maximum outer‑fiber strain.

ASTM D2412 Plastic Pipe Deflection Testing by Compression Loading Test –

ASTM D2412: Standard Test Method for Determination of External Loading Characteristics of Plastic Pipe by Parallel-Plate Loading

ASTM D2412 test method covers the determination of load-deflection characteristics of plastic pipe under parallel-plate loading. It covers thermoplastic resin pipe, reinforced thermosetting resin pipe (RTRP), and reinforced polymer mortar pipe (RPMP). Pipes tested under ASTM D2412 must be smaller than the envelope of the two compression platens by at least a half an inch. Square or circular platens can be used, with most customers choosing a square platen. Care must be taken to account for the mid-section of the pipe which will expand slightly as the pipe is compressed.

The characteristics determined by ASTM D2412 test method are pipe stiffness, stiffness factor, and load at specific deflections.

ASTM D3410 Shear Loading compression Test for Polymer Matrix Composite Materials with Unsupported Gage Section –

ASTM D3410 Shear Loading compression Test Method for Compressive Properties of Polymer Matrix Composite Materials with Unsupported Gage Section. 

ASTM D3410 measuring in‑plane compressive properties for high‑modulus‑fiber‑reinforced polymer‑matrix composites using pure shear‑loading via wedge grips, with an unsupported gage section on the test coupon. Test method determines the in-plane compressive properties of polymer matrix composite materials reinforced by high-modulus fibers. It is applicable to composites made from unidirectional tape, wet-tow placement, textile (for example, fabric), short fibers, or similar product forms. Some product forms may require deviations from the test method.

ISO 899-2 Plastic three-point flexural creep test –

ISO 899-2 Plastics — Determination of creep behaviour — Part 2: Flexural creep by three-point loading

ISO 899-2 specifies how to measure the time-dependent bending deformation of a freely supported plastic beam under a constant mid-span load, under controlled pre-treatment, temperature and humidity. Apply for rigid and semi-rigid, non-reinforced, filled and fibre-reinforced plastics; specimens moulded directly or machined from sheets or moulded articles.

ISO 899-1 Tensile Creep Testing for Plastics –

ISO 899-1 Plastics — Determination of creep behaviour — Part 1: Tensile creep

ISO 899-1 determines tensile creep of plastics in the form of standard test specimens under specified conditions of pretreatment, temperature and humidity. It applies to rigid and semi-rigid, non-reinforced, filled and fibre-reinforced plastics, using dumb-bell-shaped specimens that are either directly moulded or machined from sheets or moulded articles.


Frequently Asked Questions: ASTM D2990 Plastic Creep & Creep-Rupture Test

Q1: What is ASTM D2990?

A: ASTM D2990-17 is the standard test method for measuring tensile, compressive, and flexural creep and creep-rupture properties of plastics under controlled environmental conditions, it defines procedures for evaluating time-dependent deformation and failure of plastic materials under constant static load.


Q2: Why is ASTM D2990 testing important?

A: Plastics are viscoelastic materials — their mechanical behavior changes over time under sustained load, unlike metals. Short-term tests (such as ASTM D638 for tensile strength) only capture instantaneous properties. ASTM D2990 provides critical long-term performance data that engineers need to:

  • Design plastic parts that will not deform excessively or fail during their service life

  • Establish safe operating stress limits for given temperatures and lifetimes

  • Compare materials quantitatively for long-load applications

  • Comply with industry specifications and regulatory requirements


Q3: What types of loading does ASTM D2990 cover?

A: The standard covers three loading modes:

  • Tensile creep and creep-rupture — axial pulling load (preferred for rupture testing)

  • Compressive creep and creep-rupture — axial compressive load (with optional guide tube for slender specimens)

  • Flexural creep — three-point bending by default; four-point bending per ASTM D6272 is permitted as an alternative


Q4: What is the difference between creep and creep-rupture testing?

A:

  • Creep testing measures progressive deformation (strain) over time under a constant load that does not cause failure during the test period. It generates creep modulus and isochronous stress-strain data.

  • Creep-rupture testing continues until the specimen breaks, measuring time-to-failure at each stress level. It produces a creep-rupture envelope that defines the material's long-term load-bearing limit.


Q5: What materials can be tested according to ASTM D2990?

A: ASTM D2990 applies to all rigid and semi-rigid plastic materials, including thermoplastics, thermosets, reinforced plastics, composites, and electrical insulating materials. It is widely used for materials such as ABS, SAN, PBT, nylon, PTFE, epoxy, polycarbonate, and glass-reinforced polymers.


Q6: How long does an ASTM D2990 test take?

A: Test duration depends on the purpose:

  • Standard creep characterization: typically 1,000 hours (~42 days)

  • Creep-rupture testing: up to 3,000 hours (~125 days) across multiple stress levels

  • Long-term design validation: 6 months or longer, especially at elevated temperatures

  • Accelerated methods using time-temperature superposition (WLF principle) can extrapolate shorter test data to predict multi-year performance.


Q7: What specimens are used for ASTM D2990 testing?

A: Specimen geometry depends on the test mode:

  • Tension: Type I or Type II specimens per ASTM D638

  • Unconfined compression: 12.7 × 12.7 mm square or 12.7 mm diameter cylinders, slenderness ratio 11–15

  • Slender compression: 4.85 mm square bars, 51 mm long (used with guide tube)

  • Flexure: Rectangular bars per ASTM D790 (e.g., 63.5 × 12.7 × 3.18 mm or 127 × 12.7 × 6.4 mm)


Q8: What is the difference between ASTM D2990 and ISO 899?

A: Both standards address plastic creep testing but differ in technical content, and results cannot be directly compared. Key differences:

  • ASTM D2990 covers tension, compression, and flexure; ISO 899-1 covers tension and ISO 899-2 covers flexure only — ISO 899 does not include compressive creep.

  • Specimen dimensions, conditioning protocols, and calculation methods differ.

  • ASTM D2990 permits both three-point and four-point flexural loading; ISO 899-2 specifies three-point bending.


Q9: How many stress levels are required for creep-rupture testing?

A: At each test temperature, a minimum of seven stress levels are required, selected to produce rupture at approximately 1, 10, 30, 100, 300, 1,000, and 3,000 hours. At least two specimens per stress level are required, though more are often needed due to typical data scatter of 0.5 to 1 full decade in time-to-rupture.


Q10: Can ASTM D2990 test results be extrapolated to longer service lives?

A: Yes. Logarithmic plots of stress vs. time-to-rupture and creep modulus vs. time are typically linear, allowing extrapolation beyond actual test duration. The time-temperature superposition principle (WLF method) can also be used to construct master curves covering decades of time. However, extrapolation should be done cautiously, especially for materials subject to thermal aging or chemical degradation.


Q11: What is the difference between three-point and four-point flexural creep?

A:

  • Three-point bending (default): Single load at mid-span; maximum stress occurs at the center point. Simpler setup, widely used.

  • Four-point bending (optional): Two load points create a constant-moment region with uniform maximum stress over a larger area. Preferred for reinforced materials as it better distributes stress and reduces sensitivity to local defects.


Q12. Can UnitedTest customize a D2990 / ISO 899 system?

A: UnitedTest (Beijing United Test Co., Ltd.) manufactures material testing machines for metal and non-metal materials and offers customized creep and stress-rupture systems engineered to ASTM/ISO requirements, so a D2990 configuration is typically scoped project-by-project: loading mode, station count, force range, temperature range, deformation measurement and DAQ.


Q13. Why choose ASTM D2990 Creep and Creep-Rupture Testing Systems by UnitedTest?

A: UnitedTest manufactures high-precision ASTM D2990 compliant tensile, compressive, and flexural creep test systems for plastics. Reliable long-term creep and creep-rupture testing equipment with environmental control.


UnitedTest designs and manufactures precision ASTM D2990 compliant creep testing machines for measuring the tensile, compressive, and flexural creep and creep-rupture properties of plastics and polymer composites. Our test systems deliver accurate, repeatable long-term performance data that material engineers and quality laboratories depend on for product design, material qualification, and regulatory compliance.


Engineered for ASTM D2990 Compliance

Every UnitedTest creep test frame is built to meet the strict requirements of ASTM D2990-17 Standard Test Methods for Tensile, Compressive, and Flexural Creep and Creep-Rupture of Plastics. Key compliance features include:

  • Load accuracy within ±1% across the full test range, maintained continuously over thousands of hours of testing

  • Deformation measurement resolution meeting the ±1% accuracy requirement, with non-contact and contact extensometer options

  • Multi-station dead-weight loading frames with lever-arm systems designed to maintain constant load as specimens deform

  • Integrated environmental chambers with precise temperature control (±2°C) and humidity regulation (±5% RH)

  • Vibration-isolated machine frames to prevent shock transfer between test stations during specimen rupture

  • Three-point and four-point flexural creep fixtures compatible with ASTM D790 and ASTM D6272 specimen geometries

  • Compressive creep fixtures with self-aligning anvils and optional guide tube assemblies for slender specimens


Complete Testing Solutions for Every Application

Whether you need a single-station research-grade system or a multi-station production testing line, UnitedTest delivers turnkey solutions configured for:

  • Tensile creep and creep-rupture testing using ASTM D638 Type I/II specimens

  • Compressive creep testing for both unconfined and slender specimen configurations

  • Flexural creep testing with interchangeable 3-point and 4-point bending fixtures

  • Elevated and sub-ambient temperature testing from -70°C to 310°C

  • Chemical environment testing with sealed specimen chambers

  • Automated data acquisition with continuous strain logging and real-time creep modulus calculation

< Previous: ASTM D2924 External Pressure Resistance Test of Fiberglass Pipe

> Next: ASTM D2992 Fiberglass Pipe Hydrostatic Test for Obtaining Hydrostatic or Pressure Design Basis

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.