Information on the most widely used ASTM standards within the materials testing industry
ISO 8493 Metallic Tube Drift Expanding Test Machine | UnitedTest
UnitedTest manufactures ISO 8493 compliant drift-expanding testers for circular metallic tubes. Evaluate plastic deformation performance during drift expansion for steel and aluminium alloy tubes within specified OD and wall thickness limits.
ISO 8493 Metallic materials defines the drift-expanding test method to assess the plastic deformation capacity of circular cross-section metallic tubes under cone expansion. The default scope covers tubes with outer diameter D ≤ 150 mm, while light metals like aluminium alloys are limited to D ≤ 100 mm, and wall thickness a ≤ 10 mm. Corresponding product standards may apply tighter dimensional limits. UnitedTest supplies precision drift expanding test rigs for metal pipe mills, alloy tubing factories and third-party material inspection labs.
Test Principle:
A conical mandrel (drift) is forced into the end of a tube test piece cut from the tube. Expansion continues until the maximum outside diameter of the expanded portion reaches the value specified in the relevant product standard (see figure 1 of the standard).
In simple physical terms: the test puts the tube wall under a combination of circumferential (hoop) tensile stress and through-thickness bending at the tube end. It simulates — in a controlled, quantifiable way — the kind of deformation a tube end experiences during flaring, expanding, or end-forming operations in fabrication.
Test Specimen Information:
Length L depends on the mandrel cone angle:
| Mandrel angle β | Required test piece length L |
|---|---|
| β ≤ 30° | L ≈ 2 D |
| β > 30° (i.e. 45°, 60°) | L ≈ 1.5 D |
A shorter test piece is permitted provided the remaining cylindrical (un-expanded) part after expansion is at least 0.5 D.
End faces: both ends must lie in a plane perpendicular to the tube axis.
Edge preparation: the edge of the end to be expanded may be rounded by filing or chamfered by other methods. Note: non-rounded / non-chamfered edges are permissible if the test result meets the requirements.
ISO 8493 Metal Tube Drift Expanding Test required Testing Equipment:
| Test Machine | Variable-speed press or universal testing machine — must be capable of controlled, shock-free penetration at a defined rate. |
| Conical mandrel (drift) |
|
Key Parameters and Stipulations
| Tube OD range | ≤ 150 mm (≤ 100 mm light metals) |
| Wall thickness | ≤ 10 mm |
| Mandrel angle β | 30°, 45°, 60° (preferred); per product standard |
| Specimen length L | 2 D (β ≤ 30°) or 1.5 D (β > 30°) |
| Minimum remaining cylindrical length | ≥ 0.5 D after expansion |
| Penetration rate (dispute) | ≤ 50 mm/min |
| Acceptance criterion | No visible crack without magnification (edge micro-cracks acceptable) |
| Measured output | Dᵤ, or % expansion relative to D |
Load must be applied smoothly without shock impact. Mandrel axis must be co‑axial with tube specimen axis. Mandrel rotation relative to the tube is forbidden.
Dispute rule: mandrel penetration rate shall not exceed 50 mm/min.
Key Test Procedures:
Prepare tube specimen according to dimension and edge‑preparation rules. For welded tubes, treat weld flash as required.
Set‑up specimen and align conical mandrel co‑axially with tube axis; apply lubrication to mandrel if needed.
Operate press / universal tester to drive the conical mandrel steadily into tube end without shock, until the target expanded dimension (D_u or percentage expansion) specified in product standard is achieved.
Control penetration speed; in case of technical dispute, limit speed ≤ 50 mm/min. Mandrel must stay non‑rotating relative to the test piece.
Remove the expanded specimen, inspect for surface cracks with unaided eyes, and judge pass or failure per acceptance rules.
Compile test report if required by specification.
Industry Application Fields:
The drift-expanding test is a technological (workmanship / formability) test, not a design-property test. It is written into the delivery conditions of tube product standards and is used for:
Pressure-purpose tubing — boiler tubes, heat-exchanger tubes, superheater tubes (e.g. EN 10216 series references EN ISO 8493:2004, expanding with a 60° conical tool to a specified % OD increase) ; seamless and welded steel tubes for pressure service.
Shipbuilding / classification societies — drift-expanding is a mandatory technological test for tubes with OD up to 150 mm and wall thickness up to ~9–10 mm, alongside flattening, flanging, ring-expanding and ring-tensile tests .
Condenser, heat-exchanger and boiler fabrication — because the tube end is literally expanded into a tube sheet in service; the test simulates tube-to-tubesheet expansion.
Automotive, hydraulic/pneumatic lines, HVAC and plumbing — wherever tube ends are flared, expanded or end-formed for joining and sealing.
Welded tube manufacturing — as a screen for weld quality (the weld line is the most likely crack-initiation site during expansion).
Third-party inspection, certification, incoming QC and failure/arbitration testing — the "in case of dispute" clauses exist precisely for this.
Typical users: tube mills and their test laboratories, classification societies and certification bodies, EPC contractors and purchasers, and product-standard committees.

Related standard:
| EN 10232 | Metallic Materials - Tube (in Full Section) - Bend Test |
| IS 2328 | (India standard) — corresponds to ISO 8492 |
| ASTM B968 | flattening of copper and copper-alloy pipe and tube. |
| ISO 7438 | General bend test for flat metal strip/sheet specimens. |
| TCVN 5891 | Metallic materials. Tube (in full section).Bend test |
| ISO 8491 | Tube (in full section) bend test, bend rather than flatten |
| ISO 8492 | Metallic materials. Tube. Flattening test |
| ISO 8493 | Metallic materials - Tube - Drift-expanding test |
GOST 8695 | Metal pipes. Flattening testing method |
| EN 10233 | Metallic materials. Tube. Flattening test |
| EN 10234 | Metallic materials; Tube; Drift expanding test |
| DIN 50136 | German Flattening test |
Why This Test Matters for a Material
Evaluate end‑formability: It directly quantifies the tube’s capacity for plastic radial expansion at tube ends. Many tube products require end flaring / expanding during fabrication or assembly. Poor drift‑expanding performance will lead to cracking during component manufacturing.
Quality screening for welded tubes: For welded tubes, the test exposes potential brittleness or defects at weld seams, verifying weld ductility and weld‑zone integrity.
Acceptance inspection: Acts as a production quality‑control check to verify incoming tube material conforms to product‑specification ductility requirements.
Predict in‑service risk: Tubes that fail this test are more prone to crack initiation when subjected to end‑expanding processing or local overload, which may cause component leakage or structural failure in service.
Material comparison: Provides standardized, repeatable test data to compare ductility among different tube heats, batches, manufacturing processes or grades of tubular material.
Keywords: ISO 8493 tester, metallic tube drift expanding test machine, metal pipe cone expansion tester, steel tube drift expansion test rig, aluminium alloy tube expansion test equipment, circular tube plastic deformation tester, tubular product drift expanding quality test, seamless tube expansion test fixture, light metal tubing expansion performance tester, boiler tube drift expanding verification machine, pressure vessel tube mechanical test system, metal tube ductility expansion testing machine
Related products and device
Related Standard
ISO 8491 define a unified bend test method for evaluating the plastic bending ductility of circular full-section metallic tubes, exclusively for tubes with outer diameter D ≤ 65 mm (product standards may narrow this diameter range further).
Main Industry fields: boilers & pressure vessels, oil & gas pipelines, automotive (exhaust/chassis tubing), heat exchangers, structural steel tubing, power generation (including nuclear).
ISO 8492 Metallic materials — Tube — Flattening test
ISO 8492 is a method for determining the ability of metallic tubes of circular cross-section to undergo plastic deformation by flattening; it may also be used to reveal defects in the tubes. ISO 8492 defines how to flatten; how far to flatten (distance H), where the weld goes, and what counts as failure are delegated to the relevant product standard or purchase order.
EN 10234 Metallic materials. Tube. Drift expanding test
EN 10234 defines a procedure for determining the ability of metallic tubes of circular cross-section to undergo plastic deformation by drift (cone) expansion — i.e. how far a tube end can be expanded radially before it cracks. Applicable for outside diameter ≤ 150 mm (≤ 100 mm for light metals such as aluminium) and wall thickness ≤ 10 mm; the applicable D or T range may be narrowed further by the relevant product standard.
EN 10232 is the European version of ISO 8491,defines a unified cold bend test for intact circular full-section metallic tubes, designed to quantify plastic bending ductility for tubes with outer diameter D ≤ 65 mm.
ASTM A500 covers carbon steel tubing in round, square, rectangular, or special shapes, primarily used for welded, riveted, or bolted construction in bridges, buildings, and general structural applications. It specifies four mandatory test categories, tension test, flattening test, Chemical Composition Analysis and Dimensional & Visual Inspection. For us, will focus on the mechanical test.
ASTM D2105 Standard Test Method for Longitudinal Tensile Properties of "Fiberglass" (Glass‑Fiber‑Reinforced Thermosetting‑Resin) Pipe and Tube
ASTM D2105 determine the comparative longitudinal tensile properties of a fiberglass pipe specimen by pulling it in axial tension to failure under defined conditioning, temperature, and machine‑crosshead‑speed conditions.
ASTM F2663 Standard Test Method for Bead Unseating of Tubeless Passenger and Light Truck Tires
ASTM F2663 quantify the resistance of tubeless tires against bead unseating, which means the tire bead slipping off the rim flange leading to sudden air loss. It covers passenger tires, light‑truck tires, and temporary spare tires. It only defines test methodology, not mandatory performance limit values for tires.
ASTM A370 Standard Test Methods and Definitions for Mechanical Testing of Steel Products
ASTM A370 test methods cover procedures and definitions for the mechanical testing of steels, stainless steels, and related alloys. The various mechanical tests herein described are used to determine properties required in the product specifications. Variations in testing methods are to be avoided, and standard methods of testing are to be followed to obtain reproducible and comparable results. In those cases in which the testing requirements for certain products are unique or at variance with these general procedures, the product specification testing requirements shall control.
Covering tests like Tension, Bend, Hardness, Brinell, Rockwell, Portable, and Impact, each catering to distinct aspects of mechanical property assessment. Moreover, it accommodates annexes for specific product types, including Bar Products, Tubular Products, Fasteners, Round Wire Products, and more, ensuring a holistic approach to testing.
FAQs for ISO 8493 Drift‑Expanding Test (Metallic Tube Drift Expansion Test)
Q1. What is ISO 8493?
ISO 8493 is an International Standard titled "Metallic materials — Tube — Drift-expanding test" (ISO 8493:1998). It specifies a method for determining the ability of metallic tubes of circular cross-section to undergo plastic deformation in drift expansion. It was adopted unchanged in Europe as EN ISO 8493:2004, which supersedes EN 10234:1993.
Q2. What, in plain language, is a "drift-expanding test"?
A hardened conical mandrel (called a "drift") is pushed axially into the end of a short length of tube. The cone progressively forces the tube end to open up (expand) until a specified outside diameter is reached. The expanded end is then examined for cracks. It is also widely known in industry as a tube expanding test, tube drifting test, or tube flaring/expansion test.
Q3. What is the purpose of the test?
To prove that the tube has enough ductility in the circumferential (hoop) direction to survive end-expansion, flaring, or tube-to-tubesheet expansion during fabrication and service — and, as a by-product, to reveal material and manufacturing defects such as laminations, inclusions, unfused weld roots, or embrittlement from incorrect heat treatment.
Q4. Which tubes does ISO 8493 apply to?
By default:
Outside diameter D ≤ 150 mm
For light metals (e.g. aluminium alloys): D ≤ 100 mm
Wall thickness a ≤ 10 mm
The standard states that the applicable OD/wall-thickness range "may be more exactly specified in the relevant product standard" — so the product standard always has the final word.
Q5. Is ISO 8493 a material property test or a quality-control test?
It is a technological (workmanship / formability) test, not a design-property test. It gives a pass/fail verdict and an expansion capability, not a numeric strength value such as yield strength or tensile strength. It is normally written into the delivery conditions of tube product standards and used for batch acceptance.
Q6. What equipment does ISO 8493 require?
Only two things:
A variable-speed press or universal testing machine capable of smooth, shock-free, constant-rate penetration;
A conical mandrel (drift) with a polished surface of sufficient hardness.
That simplicity is a major reason the test is so widely used — no machined coupons, no extensometers, no grips.
Q7. What mandrel (cone) angles are used?
Preferred angles: 30°, 45°, and 60°. The exact angle β is normally specified by the relevant product standard. (For reference, EN 10216-5 pressure-tube practice commonly uses a 60° conical tool.)
Q8. Why must the mandrel be polished and hard?
Two reasons: (a) low friction keeps the deformation controlled and repeatable, and the standard permits lubrication for the same reason; (b) a soft or rough mandrel can gall, score, or tear the tube wall and create a false failure that is an artefact of the tool, not of the material.
Q9. Is there a groove in the mandrel?
For longitudinally welded tubes, the conical mandrel may be provided with a groove to accommodate the internal weld flash — otherwise the flash is crushed against the mandrel and can give misleading results.
Q10. Can the mandrel rotate during the test?
No. the conical mandrel shall not rotate relative to the test piece during the test. Rotation changes the stress/strain state and would make results non-comparable between laboratories.
Q11. Is lubrication allowed?
Yes — "the conical mandrel may be lubricated." Because lubrication is permitted but not mandated, labs should record whether lubrication was used, especially for arbitration testing.
Q12. How fast may the mandrel be driven in?
ISO 8493 sets the speed only for disputes: in case of dispute, the rate of penetration shall not exceed 50 mm/min. Speed matters because strain-rate sensitivity can change apparent ductility, so arbitration requires a controlled, slow rate.
Q13. Can I use a shorter specimen?
Yes — but only if the remaining cylindrical (un-expanded) portion after expansion is at least 0.5 D. This ensures the un-expanded part still constrains the deformation properly.
Q14. How must the specimen ends be prepared?
Both ends must lie in a plane perpendicular to the tube axis. The edge of the end to be expanded may be rounded by filing or chamfered by other methods. Note: non-rounded/non-chamfered edges are permissible if the test result meets the requirements — good edge preparation simply reduces false edge-crack rejections.
Q15. What about welded tubes?
The internal weld flash may be removed. This, plus the optional grooved mandrel, is how the standard handles longitudinally welded tube.
Q16. What is the target end-point of the expansion?
Either of these, as specified by the relevant product standard:
the maximum outside diameter after testing, Dᵤ, or
the relative expansion expressed as a percentage of the original diameter D.
Q17. Is drift-expanding the same as flanging (ISO 8494)?
No, but they are close relatives. ISO 8494 (flanging test) shares the same size limits (OD ≤ 150 mm, wall ≤ 10 mm), the same L ≈ 1.5 D specimen, the same ≥ 0.5 D remaining-cylinder rule, the same ≤ 50 mm/min dispute rate, and the same naked-eye acceptance rule — but it goes further: it pre-forms with a conical mandrel (commonly 90°) and then forms a flat flange with a flanging tool to a specified flange diameter.
Q18. How does it differ from the flattening test (ISO 8492)?
ISO 8492 compresses a short ring between parallel platens to a specified distance H; it is applicable to much larger tubes (OD ≤ 600 mm, wall ≤ 15 % of OD). Many product standards allow drift-expanding to replace flattening for wall thickness ≤ 10 mm at the manufacturer's discretion; conversely, for large diameters, ring expanding (ISO 8495) or ring tensile (ISO 8496) replace drift expanding.
Q19. Are there non-ISO corporate equivalents?
Yes. For example Ford FLTM BA 155-01 ("Determination of tube deformability by drift expansion") uses a 60° conical drift with a minimum hardness of Rockwell C 45, driven at a constant maximum 25 mm/min, with neither sample nor drift allowed to rotate. Useful to know when supplying automotive customers.
Q20. Can one machine do ISO 8493 and the other tube tests?
Yes. Because ISO 8493, 8492, 8494 and 8495 all run on a variable-speed press or universal testing machine and differ mainly in tooling, a single suitable press with interchangeable mandrels, platens and flanging tools can cover the whole family — which is exactly how most tube-mill laboratories are equipped.
Q21. Why choose ISO 8493 Drift‑Expanding Test Machine & Test Fixtures from UnitedTest?
UnitedTest manufactures ISO 8493 drift‑expanding test machines & fixtures for metallic tubes. Comply with EN ISO 8493:2004 standard for tube end flaring / expansion ductility quality control for steel, aluminium welded & seamless tubes.
UnitedTest supplies complete ISO 8493 drift‑expanding testing solutions for metallic circular tubes, fully complying with ISO 8493:1998 and EN ISO 8493:2004 European standardANSI Webst.... Our drift‑expand fixtures can be fitted to our universal material testing machines to perform tube flaring / end expansion tests, evaluating plastic deformation capacity for seamless and longitudinally welded steel tubes, aluminium and other light‑metal tubes.
Ideal for tube manufacturing factories, automotive component plants, heat‑exchanger tube workshops, third‑party testing laboratories and R&D institutes. UnitedTest provides standard conical mandrels (30°,45°,60° preferred angles) and custom grooved mandrels for welded tubes to eliminate weld‑flash interference.
Our test system supports controlled penetration speed ≤ 50 mm/min for dispute‑condition testing, accurate displacement measurement, automatic data logging and standard‑compliant test‑report output. Verify tube‑end formability, screen weld‑zone brittleness, perform incoming material inspection and batch quality assurance to prevent cracking during tube flaring and pipe‑fitting assembly.
We offer complete packages including test jigs, hardened polished mandrel sets, specimen alignment accessories and test software templates for ISO 8493 drift‑expanding test reports. Custom fixture dimensions are available for your tube OD and wall‑thickness range.
✅ Fully compliant with ISO 8493:1998, EN ISO 8493:2004 drift‑expanding test standard
✅ Fits UnitedTest universal testing machines, variable‑speed press frame
✅ Standard mandrel angles: 30°, 45°, 60°; custom grooved mandrels for welded tubes
✅ Controlled penetration speed max 50 mm/min for dispute‑valid tests
✅ For seamless & welded steel tubes, light‑metal (aluminium) tubes
✅ For quality‑control lab, tube mill, automotive tubular parts, heat‑exchanger industry
✅ Output ISO 8493‑required test data: D_u, relative expansion percentage, test pass‑fail result
✅ Complete accessories, alignment tooling and standard‑format test‑report templates
✅ Custom fixture sizes for tube outer diameter up to 150 mm, wall thickness up to 10 mm.
Require More Customized Solutions?