Home >> Application >> By Standard >> ISO >> ISO 20000 + >> ISO 22622 Total Ankle Wear Testing — Gait-Cycle Wear Simulation for Ankle Implants

ISO 22622 Total Ankle Wear Testing — Gait-Cycle Wear Simulation for Ankle Implants

Share:

ISO 22622 Total Ankle Prosthesis Wear Testing Machine | UnitedTest

UnitedTest manufactures ISO 22622 compliant wear testers for total ankle replacement prostheses with load or displacement control. Follow defined loading, motion and environmental parameters; wear measurement by ISO 14243-2 gravimetric method.


ISO 22622 Implants for surgery defines loading profiles, relative angular movement, speed, test duration, specimen setup and environmental conditions for wear testing of total ankle-joint prostheses (TAR). The standard supports both load-controlled and displacement-controlled test machines and only provides test input parameters. Wear quantification must follow ISO 14243‑2 gravimetric testing procedure. UnitedTest supplies dedicated ankle prosthesis wear simulators for orthopaedic implant R&D, biomedical labs and medical device regulatory validation.


Test Principle: 

The prosthesis is installed in an inverted mounting orientation (reusing knee‑simulator hardware). The tester simultaneously applies cyclic rotational motions (talar plantar‑dorsiflexion, tibial internal‑external rotation/torque) and cyclic contact forces (axial force, anterior‑posterior (AP) force / displacement) to mimic normal human walking gait. Load magnitudes are scaled to a reference body weight of 720 N.

Articulating contact surfaces are fully immersed in temperature‑controlled lubricant simulating human synovial fluid. Identical soak‑control specimens run under pure axial loading without kinematic motions, to correct gravimetric mass change caused by polymer fluid absorption (creep effect) rather than material wear.

Two operation modes:

  1. Load‑control mode: inputs = axial force, AP force, talar plantar/dorsiflexion rotation, tibial rotational torque.

  2. Displacement‑control mode: inputs = axial force, AP displacement, talar plantar/dorsiflexion rotation, tibial internal‑external rotation angle.

ISO 22622 Total Ankle Wear Testing — Gait-Cycle Wear Simulation for Ankle Implants


Test Specimen Information

  • Test specimens: complete total ankle prosthesis assemblies including tibial component, talar component and bearing insert. Select the size and design configuration representing the worst‑case wear scenario; technical justification shall be documented in test report. Components shall use clinical‑equivalent backing/fixation (bone‑cement or machined replica). Sterilize specimens with the same clinical sterilization process, sterilize all group specimens together to reduce variability.

  • Soak‑control specimen: identical prosthesis assembly, used to quantify creep and fluid‑induced mass change.

  • Sample quantity: minimum 3 test specimens + 1 loaded soak‑control specimen per prosthesis model.

  • Lubricant (fluid test medium): diluted calf serum with protein concentration 20 g/L ±2 g/L, filtered by 2 μm filter. May add antimicrobial agent; stored frozen before use.


Test Equipment required for the ISO 22622 Total Ankle Wear Testing — Gait-Cycle Wear Simulation for Ankle Implants

Wear‑simulator testing machine

runs at test frequency 1.0 Hz ±0.1 Hz. It can generate cyclic forces, torques, rotations and translations with strict phase and amplitude tolerances 

(±3 % on cycle‑time phasing; ±5 % on force/motion magnitude).

Measurement systems: AP displacement resolution ≥ ±0.1 mm; tibial rotation angle resolution ≥ ±0.1°.

Independent control station for soak‑control specimens (applies only axial load, no cyclic kinematics).

recommend UnitedTest Multifunctional Hip Joint Wear Test System

Corrosion‑resistant specimen mounting & enclosed fluid chamberprevents third‑body particle contamination from environment or machine hardware. Mounting fixtures replicate anatomical fixation conditions of real implants.
Multi‑axis alignment systemestablishes and reproduces the prosthesis reference position after repeated specimen removal for wear measurement.
Restraint systems

AP displacement restraint and tibial rotation restraint with position‑dependent spring stiffness characteristics defined in standard

Lubrication & temperature control unitmaintains test lubricant at 37 °C ±2 °C.


Key Test Parameters: 

Test frequency1.0 Hz ±0.1 Hz
Fluid temperature37 °C ±2 °C
LubricantCalf serum 20 g/L ±2 g/L protein
Gait cycle waveformsAxial force, AP force/displacement, talar plantar‑dorsiflexion angle, tibial torque / tibial rotation angle (graph curves in Figure 6‑11; discrete numerical data in Annex A (load‑control), Annex B (displacement‑control))
Restraint stiffnessPosition‑dependent linear spring restraints for AP translation and tibial rotation
Termination cycle target5 × 10⁶ gait cycles (may extend upon request)
Intermediate measurement pointsAt minimum: 5 × 10⁵ cycles, 1 × 10⁶ cycles, then every 1 × 10⁶ cycles
Lubricant refreshFull replacement at least every 5 × 10⁵ cycles; daily replenish evaporated liquid with deionized water
TolerancePhase ±3 % cycle time; force / motion amplitude ±5 % of maximum value


Detailed Test Procedures of ISO 22622 Total Ankle Wear Testing — Gait-Cycle Wear Simulation for Ankle Implants

  1. Perform initial dimension / mass measurement for wear baseline, clean specimens following ISO 14243‑2 requirements.

  2. Mount tibial component; align axial‑force axis parallel to tibial axis within ±1°. Configure degrees‑of‑freedom according to standard mounting rules.

  3. Mount talar component and set reference position.

  4. Install soak‑control specimen on dedicated control station.

  5. Fill enclosure with serum lubricant to fully submerge articulating surfaces; stabilize temperature at 37 °C±2 °C.

  6. Start simulator at 1.0 Hz, apply the gait cycle waveforms (either Annex A load‑control set or Annex B displacement‑control set). Only axial load is applied to soak‑control specimen.

  7. Maintain lubricant, replenish evaporation daily, fully replace lubricant every 5 × 10⁵ cycles.

  8. Pause test at predefined cycle intervals, remove, clean and measure gravimetric mass loss for test and control specimens. Re‑align and reinstall specimens to resume cyclic testing.

  9. Repeat cycles‑measurement‑reinstallation loop until test termination criterion is triggered.

  10. Calculate gravimetric wear rate (subtract creep‑mass change from total mass loss). Take photographic documentation of worn articular surfaces.


Industrial‑Field Application

ISO 22622 belongs to orthopaedic surgical implant standards (ICS 11.040.40). It applies to the orthopaedic medical‑device industry:

  • In‑vitro pre‑clinical wear performance evaluation for total ankle‑joint replacement prostheses before clinical trials or market approval.

  • Supports regulatory submission (recognized standard by FDA and notified bodies for medical‑device conformity assessment).

  • Used for material comparison, new‑prosthesis design verification, batch‑level performance validation of ankle implants (metal‑on‑polyethylene bearing pairs mostly).


Related Standard: 

ISO 14243‑1

Wear of total knee-joint prostheses. 

Loading and displacement parameters for wear-testing machines with load control and corresponding environmental conditions for test

ISO 14243‑2Part 2: Methods of measurement — how wear is measured (gravimetric, mass loss, creep/fluid‑uptake correction). Mandatory companion.
ISO 14243‑3

Part 3: displacement‑control version (AP translation and tibial rotation are prescribed inputs). Same axial force and flexion profiles; polarity of AP displacement and rotation was reversed between the 2004 and 2014 editions. 

Choose force control when kinematics/friction/design effects matter; displacement control when isolating a single variable such as material .

ISO 14243‑4

Part 4: Wear of the patella-femoral joint - 

Loading and displacement parameters for wear-testing machines and corresponding environmental conditions for test

ISO 14243‑5Part 5: Durability performance of the patellofemoral joint
ISO 14242‑1/‑2/‑3Equivalent family for hip joint prostheses (loading/displacement parameters, measurement) 
ASTM F3141Guide for Total Knee Replacement Loading Profiles — force‑control waveforms for activities of daily living beyond walking (stairs, squat, turning) .

ASTM F2003 / 

ISO 5834‑3

Accelerated aging of UHMWPE (often applied before simulator testing).
ISO 22622Implants for surgery — Wear of total ankle-joint prostheses — Loading and displacement parameters for wear-testing machines with load or displacement control and corresponding environmental conditions
ISO 7207‑1Metal intramedullary nailing systems part 1 to 3
ASTM F1264Standard specification and test methods for intramedullary fixation devices


Keywords: ISO 22622 tester, total ankle prosthesis wear test machine, TAR ankle joint wear simulator, ankle arthroplasty implant wear tester, load controlled ankle prosthetic wear rig, displacement controlled ankle wear testing equipment, ISO 14243-2 gravimetric wear test system, orthopaedic ankle implant durability tester, surgical ankle replacement cyclic wear fixture, biomedical implant joint wear test machine, ankle prosthesis lab performance validation equipment, orthopedic implant wear simulation tester

Related products and device

ISO 22622 Total Ankle prostheses Multifunctional Wear Test System

Multifunctional Joint Wear Test System is design and produced fully according the ISO 14243-1, has the function of abrasion test of positive shoulder joint and reverse shoulder joint and knee joint restraint test function, which is very comprehensive, and has strong customization and scalability.

Dual axis Torsion & Bend Fatigue Testing machine

Electronic Dynamic Universal Testing Machine/ Cyclic Testing Equipment widely used at material and components, parts dynamic mechanical property test, include tension, compression, low cycling test, match with high-low temperature chamber can execute the temperature test.

intramedullary fixation device tester

Electronic Fatigue Testing Machine designed for long-term cyclic load testing of metals, composites, and structural components, offering precise electronic control, repeatable results, and compliance with industrial standards.

orthopaedic implant quality control system

Spinal Implant Constructs nail screw static and fatigue testing machine used to check the fatigue failure of medical nail, Loads are typically applied in a constant-amplitude, load-controlled sinusoidal waveform that runs more than 5 million times.

Static bending universal testing machine

UnitedTest universal testing machine with various test fixture, like peel, flexure, puncture, tear, pneumatic grip, belt tension etc., can be used to almost all materials include but not limited to steel rod, rubber, steel wire, plastic, seat belt, textile, wood, panel etc., mechanical performance inspection.

4 points bending fixture

The four point bending flexural test provides values for the modulus of elasticity in bending, flexural stress ,flexural strain and the flexural stress-strain response of the material. This test is very similar to the three point bending flexural test.

3 points bending grip

3 points bending grip used to measure the flexural modulus or flexural strength of a plastic material, conform with stanard ASTM D790, ISO 178.

intramedullary fixation devices torsion tester

Torsion tester is mainly used to execute torsion test for various kinds materials, manual loading, high accuracy torsion transducer to measure torque, photoelectric encoder to measure torsion angle, digital display test result. Easy to operate and with budgetary price, most suitable for research institute and colleague, factory laboratory etc. to check the torsion character of different materials.

Related Standard

ASTM F1717 Spinal Implant Constructs Test –

ASTM F1717 Standard Test Methods for Spinal Implant Constructs in a Vertebrectomy Modelis a fundamental standard for evaluating the static and fatigue mechanical performance of spinal implant assemblies. Unlike ISO 12189, which focuses on a single device(an interbody cage), ASTM F1717 tests the entire posterior spinal construct—typically rods, screws, and cross-connectors—stabilizing a segment where a vertebral body has been removed (a "vertebrectomy" or "corpectomy" model). It simulates worst-case spinal instability to assess the implant's ability to maintain alignment and support loads.

ASTM F382 Metallic Bone Plates fatigue bending test –

ASTM F382 Standard Specification and Test Method for Metallic Bone Plates

ASTM F382 unified terminology, geometric classification, material requirements, marking & packaging rules, and mechanical test protocols for metallic bone plates used in surgical skeletal internal‑fixation. It define two mandatory test methods:  Single‑Cycle Bend Test and Bending Fatigue Test. Both adopt four‑point bending configuration. It is of great significance for ensuring the safety and reliability of metallic bone plates, which are widely used to align and fix bone segments in orthopedic reconstructive surgeries. 

ASTM F1798 Spinal Implant Subassembly Static and Fatigue Testing System –

ASTM F1798 Standard Test Method for Evaluating the Static and Fatigue Properties of Interconnection Mechanisms and Subassemblies Used in Spinal Arthrodesis Implants.

ASTM F1798 provides standardized methods for mechanically testing the interconnections within spinal implant systems. It is for evaluating the uniaxial static/fatigue strength and loosening resistance of interconnection mechanisms in spinal arthrodesis implant subassemblies, providing a standardized way to characterize mechanical performance of connections like rod-clamp, screw-rod, and hook-rod assemblies. It is critical for design validation, regulatory compliance, and clinical safety in the spinal implant industry.

ASTM F2706 Fatigue Static Test of Spinal implant constructs –

ASTM F2706 is a critical biomechanical evaluation tool in the medical device industry, specifically for spinal implants. ASTM F2706 establishes standardized mechanical test methods to evaluate the static (strength) and fatigue (long-term durability) performance of spinal implant assemblies intended for use in the occipito-cervical (OC) and cervico-thoracic (CT) regions (from the skull to the upper back). It simulates a worst-case scenario: a complete vertebrectomy (removal of a vertebra), creating a highly unstable spine segment that the implant must stabilize.

ASTM F2706 establishes standardized mechanical test methods to evaluate the static (strength) and fatigue (long-term durability) performance test, defines in‑vitro mechanical test protocols for posterior occipital‑cervical (OC) and occipital‑cervical‑thoracic (OCT) spinal fixation assemblies under a vertebrectomy worst‑case model, aiming for relative mechanical comparison of implant designs, rather than defining pass‑fail performance thresholds. 


ASTM F1264 Intramedullary Fixation Device Torsion & Bend Fatigue Test –

ASTM F1264 Standard Specification and Test Methods for Intramedullary Fixation Devices

ASTM F1264 is a standard specification used to describe the design and mechanical function of intramedullary fixation devices (IMFDs). It establishes terminology, classification, material, marking‑labeling requirements and four mandatory‑annex mechanical test methods for intramedullary nails/rods used in skeletal fracture fixation. It does not define mandatory clinical performance thresholds; tests deliver comparative mechanical data rather than absolute clinical pass‑fail criteria.

it also includes four standard testing methods: 

1, static four point bending test method (Annex A1), 

2, static torsion test method (Annex A2), 

3, bending fatigue test method (Annex A3), 

4, bending fatigue test method for IMFD locking screws (Annex A4). 


The UTDS series Dynamic/Fatigue Testing machine used for bone needle,  bending intramedullary nail fatigue test is mainly used for biomechanical performance testing of various materials, including artificial blood vessels, soft tissues, bones, bone plates, and vertebrae Interfusion device, knee joint, spine Dynamic and static mechanical tests on materials such as column fixators, metal coatings, hip joints, and intramedullary nails, including tension, compression, bending, and torsion.

ISO 14243-1 Wear Simulate Test for knee-joint prostheses - Loading and displacement –

ISO 14243-1 Implants for surgery. Wear of total knee-joint prostheses. Loading and displacement parameters for wear-testing machines with load control and corresponding environmental conditions for test

ISO 14243-1 specifies test conditions for load‑controlled knee wear simulators, covering loading, displacement parameters and corresponding environmental test conditions for total knee arthroplasty (TKA) prostheses wear evaluation.

ISO 22622 — Total Ankle Replacement Wear Test: Frequently Asked Questions

Q1. What is ISO 22622 in one sentence?

It is the international standard that defines how to drive a wear simulator — the motions, forces, speed, duration, specimen setup and fluid environment — so that a total ankle replacement (TAR) can be wear-tested reproducibly under simulated level walking.


Q2. What exactly does it specify — and what does it not specify?

Specifies (the "input" side): relative angular movement between articulating components (talar plantar/dorsiflexion and tibial internal/external rotation), the applied force or displacement patterns, test speed and duration, sample configuration, and the test environment.

Does not specify: how to measure wear (that is ISO 14243‑2), fatigue strength of metal components, fixation/bone-interface performance, coating adhesion, or any clinical pass/fail threshold.


Q3. Why was a separate ankle standard necessary, when knee and hip standards already existed?

Because the ankle is not a scaled-down knee. The ankle carries high load over a small contact area, has a single dominant axial-force peak (unlike the knee's double peak), only about ±15° of plantar/dorsiflexion, small AP translations, and significant axial rotation that is shared with the subtalar joint. Before ISO 22622, published wear studies used wildly inconsistent kinematics and loads, so reported polyethylene wear for TAR ranged from roughly 3 to 26 mm³ per million cycles for the same class of material — results were not comparable between labs.


Q4. Who is the standard intended for?

Orthopaedic implant manufacturers and R&D teams, contract biomechanics/tribology laboratories, regulatory and notified-body reviewers, academic groups studying joint-replacement wear, and testing-machine manufacturers building simulators.


Q5. Which mode should a laboratory use?

Both are permitted. Displacement control is easier to implement and gives tighter, more repeatable kinematics. Load control is argued to be more physiological because the implant's own geometry and constraint determine the resulting AP translation and axial rotation — which also influences contact stress. Published cadaveric work found that the motions produced under load control stayed within the envelopes specified by the displacement-control profiles, so the two modes produced broadly comparable kinematics. Choose based on your simulator's capability and on what your regulatory reviewer expects.


Q6. Can I use my existing knee simulator?

Yes — this is a deliberate feature of the standard. ISO 22622 is built on ISO 14243‑1 and ISO 14243‑3 and explicitly allows the same equipment used for total knee replacement wear testing. The ankle prosthesis is mounted in the inverted position: the talar component occupies the station that the femoral component would occupy in a knee test, and the tibial component stays in the tibial station. The biggest practical hazard is sign/direction inversion — the standard warns explicitly that great care must be taken not to confuse the directions of motion when implementing the curves.


Q7. What is the "reference position" and why does it matter?

It is the angular and linear alignment of the tibial component relative to the talar component that gives static equilibrium when only a positive axial force is applied along the axial force axis (equivalent to 0° plantar/dorsiflexion in vivo). All motions and forces are measured from this datum, and it must be reproducible after every weighing stop. For flat or moderately constrained tibial bearings with no distinct lowest point, the definition breaks down — the manufacturer must then define the neutral position and record it in the test report.


Q8. What are the restraint systems in load control, and why are they needed?

Because an ankle prosthesis on its own cannot resist horizontal loads — the natural joint relies on ligaments. ISO 22622 therefore requires synthetic ligament analogues:

AP restraint: 20 N/mm ± 1 within ±6 mm of the reference position; 140 N/mm ± 5 beyond +6 mm; 120 N/mm ± 5 below 0 mm.

Tibial rotation restraint: zero within ±4° of reference; then 0.60 N·m/° ± 0.01 for external rotation and 1.10 N·m/° ± 0.01 for internal rotation. The direction is inverted for a right-side implant.


Q9. How long does a test take in real time?

Five million cycles at 1 Hz is 5 000 000 seconds ≈ 1 389 hours ≈ 58 days of continuous running. Adding six weighing stops, cleaning, fluid changes and re-installation, a realistic campaign is typically around 10–14 weeks per group, plus polymer pre-soak conditioning before the start.


Q10. Where do the peak values sit in the gait cycle?

The axial force curve is asymmetric with a single dominant push-off peak: it rises to the maximum of ~2 366 N at roughly 47–48 % of the cycle, then falls to a long low plateau of about 190–210 N through swing phase (~59–95 %). Maximum dorsiflexion occurs near 49 %, and maximum plantarflexion (−15°) near 64 %.


Q11. What is the test specimen?

The complete functional construct: tibial component + bearing + talar component (three-part, mobile-bearing designs included). If the tibial component is modular, the tray must be in place, and the articulating surface must sit on its normal immediate backing (bone cement or a machined replica of the tray's inner surface) that still allows non-destructive removal for weighing.


Q12. Why is "worst case" selection mandatory?

Because wear is highly sensitive to size, clearance, insert thickness and conformity. Clause 5.2 requires the user to choose the size combination and design detail representing the worst expected case for wear, and to provide a written justification. This is a common review question from notified bodies.


Q13. How many specimens are required?

At least three test specimens plus one loaded soak control (Clause 5.4). Multi-station simulators commonly run three wear stations plus a fourth control station.


Q14. What is the test fluid, and why calf serum?

Calf serum diluted with deionized water to a protein concentration of 20 g/L ± 2 g/L, normally filtered through a 2 µm filter, stored frozen, optionally with an antimicrobial such as sodium azide. Protein content is critical: it governs the lubrication regime and the resulting wear rate and particle morphology. Using a non-biological substitute can shift measured wear rates by a substantial margin (published estimates of roughly 15–20 %), so it should only be used if agreed in advance.


Q15. Why is a soak control specimen required?

Polymer (UHMWPE) components absorb fluid and creep under load. The load soak control is subjected to the same fluid and the same time-varying axial force but no motion, so its mass change can be subtracted from the test specimens' mass change to give true wear. Without it, fluid uptake can easily exceed the few milligrams of actual wear being measured.


Q16. Must specimens be sterilized?

Yes. Components must be sterilized exactly as for clinical use, because sterilization (especially gamma irradiation in air) changes polyethylene wear and oxidation behaviour. Test and control components within a group should be sterilized together in a single container where possible.


Q17. Why does this test matter so much for bearing materials?

Because wear debris drives failure. Polyethylene particles released from the bearing surface trigger macrophage-mediated periprosthetic osteolysis and aseptic loosening, the dominant causes of revision after total ankle arthroplasty. A validated simulator test quantifies the debris burden a material will generate over roughly five years of walking before it is ever implanted.


Q18. How strongly does the test discriminate between materials?

Very strongly. Under ISO 22622-type simulation, conventional UHMWPE liners produced about 16.7 ± 1.3 mg/MC versus about 2.0 ± 0.3 mg/MC for highly cross-linked polyethylene — an eightfold difference, with smaller and rounder particles from the cross-linked material. A 2024 study on aged bearings reported 3.77 ± 0.36 mg/MC for direct compression-moulded UHMWPE, 1.44 ± 0.22 mg/MC for gamma cross-linked vitamin-E PE, and essentially zero (−0.04 ± 0.19) mg/MC for chemically cross-linked vitamin-E PE.


Q19. Why not just use a simple pin-on-disc screening test?

Because pin-on-disc cannot reproduce the multi-directional cross-shear, the physiological contact stresses, the protein-containing serum lubrication, or the damage modes (burnishing, abrasion, pitting, scratching, delamination) that appear on retrieved ankle implants. Simulator testing under ISO 22622 produces damage patterns that match clinical retrievals.


Q20. Can the method evaluate things other than polyethylene?

Yes. It is routinely applied to compare UHMWPE variants, to evaluate hard-on-hard or coated bearings (oxidised zirconium, TiN, DLC, ceramic-coated talar components), to assess mobile-bearing backside wear, and — with agreed deviations — adverse-condition testing such as increased load, high range of motion, or roughened/third-body-damaged inserts. Accelerated ageing per ASTM F2003 is frequently applied before testing to simulate worst-case oxidation, and debris is often characterised per ASTM F1877.

< Previous: ISO 22407 Fatigue testing Axial plane bending test

> Next: ISO 23658 Bead Peel Test for Sealants Adhesion

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now