Home >> Application >> By Standard >> ISO >> ISO 1 ~ 4999 >> ISO 3384-1 Compression Stress Relaxation Test for Rubber

ISO 3384-1 Compression Stress Relaxation Test for Rubber

Share:

ISO 3384-1 Compression Stress Relaxation Tester | UnitedTest

UnitedTest manufactures ISO 3384-1 compression stress relaxation testing machines for vulcanized and thermoplastic rubber. Our equipment measures force decay under fixed compressive deformation at constant temperature, supporting continuous and discontinuous measurement in gas or liquid environments for sealing, gasket and elastomer material validation.


ISO 3384-1 specifies standardized laboratory procedures to measure the reduction in counterforce exerted by vulcanized or thermoplastic rubber specimens held under constant compressive deformation at a defined test temperature, valid for both gaseous and liquid test environments. It covers two practical test methods: continuous measurement and discontinuous measurement, suitable for cylindrical and ring-shaped rubber samples. This test is critical to evaluate long-term sealing performance of elastomer gaskets, O-rings, seals and damping components, helping engineers predict sealing failure, select proper rubber formulations and conduct incoming quality inspection, product development and batch compliance verification. UnitedTest reliable ISO 3384-1 stress relaxation test system delivers stable, repeatable test data for rubber and elastomer manufacturers worldwide.


Test Principle: 

When a constant compressive strain is applied to vulcanized rubber or thermoplastic elastomers, the force required to maintain that fixed deformation decreases over time; this time-dependent viscoelastic behavior is defined as compression stress relaxation. The inverse phenomenon — progressive increase in deformation under constant applied stress — is known as creep.

Stress relaxation arises from two simultaneous, overlapping mechanisms:

  • Physical relaxation: Dominates at ambient/low temperatures and short test durations, caused by reversible molecular rearrangement and polymer chain mobility.

  • Chemical relaxation: Dominates at elevated temperatures and long test durations, driven by irreversible chemical degradation such as polymer chain scission, oxidation, and crosslink breakdown.

Two test methods (Method A and Method B) are defined, producing non-equivalent results that cannot be directly compared. Initial stress level and the prior mechanical history of the specimen also influence test results, especially for filled rubber compounds.


Specific Test Methods

There are two independent classification axes: Method A/B (where compression and measurement happen) and continuous/discontinuous (how force is read).

Method A

Compression and all counterforce measurements at the test temperature

Specimen is placed in the preheated device, compressed at test temperature, and F₀, Fₜ are measured ho

Method B

Compression and all counterforce measurements at standard laboratory temperature; specimen is stored at the test temperature between readings

Jig is removed from the oven/bath, equilibrated 2 h at laboratory temperature, measured, then returned

Continuous measurement

Force monitored for the whole test duration; deformation held within ±0.01 mm

Load-cell rig in oven; correction allowed for load-cell spring effect, mechanically or mathematically

Discontinuous measurement

Compression-testing machine measures the force needed to produce a slight extra compression at prescribed intervals

Extra compression ≤1 N (balance-type machines) or ≤0.05 mm (stress/strain-type machines), without overshoot; repeatable to ±0.01 mm


Key Parameters and Stipulations

  • Compressive strain: Standard value of 25 % ± 2 %. If 25 % strain is not achievable, 15 % ± 2 % or lower values (in 5 % steps) may be used.

  • Compression ramp time: Full target compression applied within 30–120 seconds.

  • Initial force measurement: Recorded exactly 30 min ± 1 min after compression is completed.

  • Default test duration: Minimum 168 hours (1 week) ± 2 hours. Preferred intermediate measurement points: 3 h, 6 h, 24 h, and 72 h. Longer durations may use a logarithmic time scale.

  • Test temperature: Selected from standard temperatures defined in ISO 23529; maintained constant throughout exposure.

  • Test medium: Air, other gases (e.g., nitrogen), or immersion liquids selected per ISO 1817.

  • Method B equilibration: 2-hour thermal stabilization at standard laboratory temperature before each measurement (not counted in test duration).


Test Specimen Information:

Cylindrical test pieces: 13.0 mm ± 0.5 mm diameter, 6.3 mm ± 0.3 mm thickness.

Ring test pieces (preferred for liquid testing):

  • Standard square-cross-section ring: 2.0 mm ± 0.2 mm axial thickness, 15.0 mm ± 0.2 mm inner diameter, 2.0 mm ± 0.2 mm radial width.

  • Alternative O-ring specimen: ISO 3601-1 size 14 × 2.65-G-N (14 mm inner diameter, 2.65 mm cross-section diameter).

  • Non-standard seals, gaskets, and custom O-ring sizes may be used for application-specific testing.


ISO 3384-1 Compression Stress Relaxation Test for Rubber required Testing Equipment: 

Compression Device

Consists of two parallel, flat, highly polished plates made of chromium-plated steel, stainless steel, or other corrosion-resistant material.

Plate surface finish: Ra ≤ 0.4 μm.

Plate rigidity: maximum bending ≤ 0.01 mm under full test load.

Parallelism tolerance: ±0.01 mm for discontinuous jigs, ±0.1 mm for continuous rigs when assembled without a specimen.

Plates must be large enough to fully contain the compressed specimen and allow free lateral expansion.

For ring specimens, plates have central holes (≥2 mm diameter) for pressure equalization and fluid circulation.

Capable of applying specified compression at controlled speed, maintaining constant deformation throughout the test, and withstanding oven temperatures.

Counterforce Measuring Device

Force measurement accuracy: ±1 % of the measured value across the test range.

For continuous systems: maintains specimen deformation within ±0.01 mm for the test duration.

For discontinuous systems: applies minimal additional compression with no overshoot, and repeats compression position within ±0.01 mm.

Test Environment System

Gaseous media: Air oven conforming to ISO 188 (Method A recommended). A nitrogen atmosphere may be used to isolate thermal aging effects from oxidative aging.

Liquid media: Immersion bath or closed vessel (for volatile/toxic fluids) with free liquid circulation through plate holes; temperature controlled via an integrated heater/circulation system or by placing the bath inside a compliant air oven.


Key Test Procedures of ISO 3384-1 Compression Stress Relaxation Test for Rubber

Pre-Test Preparation: Apply a thin layer of inert lubricant (e.g., silicone fluid, fluorosilicone fluid, molybdenum disulfide) for gaseous testing; use the test liquid as lubricant for immersion testing.

Method A Procedure:

1. Preheat the compression device and test environment to the target test temperature.

2. Place the specimen in the preheated compression device and allow full thermal equilibrium.

3. Compress the specimen to the target strain within 30–120 seconds, then lock the deformation.

4. Record the initial counterforce F0 exactly 30 min ± 1 min after compression is completed, at the test temperature.

5. Measure counterforce Ft continuously or at predefined time intervals, all at the test temperature.

6. Optional: After the final high-temperature measurement, cool the specimen to standard laboratory temperature and measure residual counterforce to assess recovery behavior.

Method B Procedure

1. Preheat the test environment chamber to the target test temperature.

2. Compress the specimen to the target strain at standard laboratory temperature within 30–120 seconds, then lock the deformation.

3. Record the initial counterforce F0 exactly 30 min ± 1 min after compression, at standard laboratory temperature.

4. Immediately transfer the compressed specimen assembly to the temperature-controlled test environment.

5. At each scheduled measurement interval:

   - Remove the assembly from the test environment.

   - Condition at standard laboratory temperature for 2 hours to reach thermal equilibrium.

   - Measure counterforce Ft.

   - Return the assembly immediately to the test environment.


Industries application:

The test is essentially a sealing-force retention / durability test. Typical products evaluated: O-rings, static and dynamic seals, gaskets, weatherstrips, engine-bay gaskets, HVAC sealing systems, hydraulic and pneumatic seals, and rubber mounts/vibration-control components.

Typical sectors: automotive (engine, transmission, fuel, coolant and battery-box seals), aerospace, rail, oil & gas / petrochemical (oil- and chemical-resistant gaskets, valve seals), industrial machinery, medical devices, chemical processing, electrical equipment, construction/building seals and consumer products.

Typical uses: material development and compound screening, supplier qualification and QC, validation of sealing performance in hot air, nitrogen, oils, fuels or service fluids (rings are preferred for liquid immersion), and generation of time–temperature data for service-life estimation. 

ISO 7743 rubber compression test for stress and strain with parallel platens


Related Test Standard

ASTM D695Standard Test Method for Compressive Properties of Rigid Plastics
GB/T 1685.1Chinese national counterpart, modified adoption of ISO 3384-1:2024, published 2026-07-02, effective 2027-02-01, replacing GB/T 1685-2008. 
ASTM D3410Shear‑loading compression test for polymer‑matrix composites with unsupported gauge section, suited for high‑strength continuous‑fiber composite laminates (not pure end‑loading as D695).
ASTM D575

Standard Test Methods for Rubber Properties in Compression.

ISO 6914Rubber — Determination of ageing characteristics by measurement of stress relaxation in tension
ISO 6056Compression stress relaxation specifically for O‑rings / rings.
ASTM D6147

Rubber Compression Stress Relaxation Test

ISO 3384-1/ ISO 3384-2

The corresponding international standard series for vulcanized rubber compression stress relaxation; 

covering both constant-temperature measurement and intermittent ambient-temperature measurement procedures.

ISO 604Plastics -- Determination of compressive properties 
ISO 7743Rubber, vulcanized or thermoplastic; determination of compression stress-strain properties
ASTM D573Test Method for Rubber – Deterioration in an Air Oven (reference for oven conditioning protocols)
JIS K 6254Japanese standard for compression and tensile stress–strain properties. It is MOD relative to ISO 7743
ISO 815-1Compression set at ambient or elevated temperatures . It measures permanent deformation after prolonged compression, not short-term stress–strain behaviour.
ISO 188Rubber, vulcanized or thermoplastic — Accelerated ageing and heat resistance tests
ISO 18899Rubber — Guide to the calibration of test equipment


Keywords: ISO 3384-1 tester,rubber compression stress relaxation tester,constant temperature stress relaxation test,vulcanized rubber stress relaxation,thermoplastic elastomer compression test,elastomer sealing performance test,gasket stress relaxation,O-ring durability test,rubber force decay test,continuous stress relaxation measurement,discontinuous stress relaxation test,rubber material quality control,elastomer long-term performance tester,UnitedTest rubber testing machine,rubber seal aging test,elastomer compression deformation test

Related products and device

ISO 3384-1 Rubber Compression Stress Relaxation Testing Machine

WDW Series Computer Control Electronic Universal Testing Machine made by UNITEDTEST range from 100N to 600KN load capacity with various models like single columns, table type, door frame type etc., is used to perform tension, compression, flexure/bending, shearing, peeling etc., test for metal and nonmetal specimens.

thermoplastic elastomer compression test,elastomer sealing performance test

Compression test fixture is used to investigate the compressive behaviour of the test specimens and for determining the compressive strength, compressive modulus and other aspects of the compressive stress/strain relationship under the conditions defined.

Related Standard

ASTM D6147 Rubber Compression Stress Relaxation Test –

ASTM D6147 Standard Test Method for Vulcanized Rubber and Thermoplastic Elastomer – Determination of Force Decay (Stress Relaxation) in Compression

ASTM D6147 specifies two methods for determining the decrease in counterforce exerted by a test specimen of vulcanized rubber or thermoplastic elastomer (TPE) that has been compressed to a constant deformation under specified conditions of time and temperature. The method was developed on the basis of testing both in air and in liquids.  


ASTM D695 Plastic & composites Compressive Testing –

ASTM D695: Standard Test Method for Compressive Properties of Rigid Plastics

ASTM D695 test covers the determination of the mechanical properties of unreinforced and reinforced rigid plastics, including high-modulus composites, when loaded in compression at relatively low uniform rates of straining or loading. Test specimens of standard shape are employed. This procedure is applicable for a composite modulus up to and including 41,370 MPa (6,000,000 psi). It is technically equivalent to ISO 604 Plastics‑Determination of Compressive Properties. This test applies end‑loading compression on standard‑geometry specimens under controlled environmental and displacement‑rate conditions, delivering compressive strength, yield strength, offset yield strength, compressive elastic modulus, and compressive deformation data.


ASTM D2412 Plastic Pipe Deflection Testing by Compression Loading Test –

ASTM D2412: Standard Test Method for Determination of External Loading Characteristics of Plastic Pipe by Parallel-Plate Loading

ASTM D2412 test method covers the determination of load-deflection characteristics of plastic pipe under parallel-plate loading. It covers thermoplastic resin pipe, reinforced thermosetting resin pipe (RTRP), and reinforced polymer mortar pipe (RPMP). Pipes tested under ASTM D2412 must be smaller than the envelope of the two compression platens by at least a half an inch. Square or circular platens can be used, with most customers choosing a square platen. Care must be taken to account for the mid-section of the pipe which will expand slightly as the pipe is compressed.

The characteristics determined by ASTM D2412 test method are pipe stiffness, stiffness factor, and load at specific deflections.

ASTM D3410 Shear Loading compression Test for Polymer Matrix Composite Materials with Unsupported Gage Section –

ASTM D3410 Shear Loading compression Test Method for Compressive Properties of Polymer Matrix Composite Materials with Unsupported Gage Section. 

ASTM D3410 measuring in‑plane compressive properties for high‑modulus‑fiber‑reinforced polymer‑matrix composites using pure shear‑loading via wedge grips, with an unsupported gage section on the test coupon. Test method determines the in-plane compressive properties of polymer matrix composite materials reinforced by high-modulus fibers. It is applicable to composites made from unidirectional tape, wet-tow placement, textile (for example, fabric), short fibers, or similar product forms. Some product forms may require deviations from the test method.

ISO 14126 In-Plane Compressive Test of Fiber-Reinforced Material –

ISO 14126 Compression test Fibre-reinforced plastic composites — Determination of compressive properties in the in-plane direction

ISO 14126 specifies how to determine in‑plane compressive properties (i.e. load applied parallel to the plane of lamination, in directions "1" and "2") of fibre‑reinforced plastic composites with thermosetting or thermoplastic matrices. Specimens are machined from a flat test plate or from finished/semi‑finished products.

ISO 604 Compressive Strength Testing of Plastics –

ISO 604 specifies a method for determining the compressive properties of plastics under defined conditions. It is used to investigate the compressive behavior of test specimens and to determine key mechanical properties such as compressive strength, compressive modulus, and other aspects of the compressive stress/strain relationship. Specimen length is adjusted to avoid buckling that would distort results. 

ASTM D575 Rubber Compression Test Method –

ASTM D575 Standard Test Methods for Rubber Properties in Compression

ASTM D575 defines two laboratory test procedures to characterize the compression‑deflection behavior of solid rubber compounds. It does not apply to hard rubber or sponge rubber materials. It contains two inverse procedures: Method A fixes the deflection and measures the force; Method B fixes the force and measures the deflection.


ISO 7743 rubber compression test for stress and strain with parallel platens –

ISO 7743 Rubber, vulcanized or thermoplastic — Determination of compression stress-strain properties

ISO 7743 defines standardized methods for measuring the compression stress-strain properties of vulcanized or thermoplastic rubber, applicable to standard laboratory test pieces, finished products, or product segments.


Frequently Asked Questions (FAQs) About ISO 3384-1 Compression Stress Relaxation Test for Rubber

Q1: What is ISO 3384-1?

A: ISO 3384-1:2024 is an international standard titled Rubber, vulcanized or thermoplastic — Determination of stress relaxation in compression — Part 1: Testing at constant temperature. Published in March 2024 as the third edition, it specifies laboratory procedures to measure the decrease in counterforce exerted by rubber specimens held under constant compressive deformation at a defined test temperature. It covers testing in both gaseous and liquid environments.


Q2: What is the difference between Method A and Method B in ISO 3384-1?

A: The two methods produce non-equivalent results and are selected based on the intended service scenario:

  • Method A (Isothermal Testing): Compression is applied and all counterforce measurements are performed at the target test temperature for the full test duration. It is preferred for fundamental research and applications where components operate continuously at elevated temperatures.

  • Method B (Ambient Measurement with Thermal Exposure): Compression and all force measurements are performed at standard laboratory temperature, while compressed specimens are stored at the test temperature between measurements. Results include material shrinkage effects from cooling, making it suitable for temperature-cycling applications.


Q3: What is the difference between continuous and discontinuous measurement procedures?

A: These refer to how force data is collected during the test:

  • Continuous procedure: An integrated load cell monitoring system tracks counterforce in real time throughout the entire test, delivering a complete relaxation curve. Deformation must be maintained within ±0.01 mm.

  • Discontinuous procedure: Force is measured at predefined time intervals using a compression testing machine, by applying a minimal additional compression (≤1 N or ≤0.05 mm) to detect the counterforce point. This is the more common approach for Method B testing.


Q4: What specimen types are specified in ISO 3384-1?

A: Two standard specimen geometries are defined, and results from different sizes/shapes are not comparable:

  1. Cylindrical disc: 13.0 mm ± 0.5 mm diameter, 6.3 mm ± 0.3 mm thickness.

  2. Ring test piece (preferred for liquid testing): Standard square-cross-section ring with 2.0 mm thickness, 15.0 mm inner diameter, and 2.0 mm radial width. An ISO 3601-1 size 14 × 2.65 O-ring may also be used as an alternative standard specimen. Custom seals, gaskets, and O-rings may be tested for application-specific evaluation.


Q5: Why is the compression stress relaxation test important for rubber materials?

A: This test is critically important because:

  • It directly predicts sealing reliability — gradual loss of compressive counterforce is the leading cause of leakage failure in gaskets, O-rings and static sealing components.

  • It enables material formulation optimization by comparing crosslink systems, antioxidant packages and filler loadings.

  • It helps distinguish between reversible physical relaxation and irreversible chemical degradation mechanisms.

  • It provides standardized quality control data for incoming material inspection and product specification compliance.

  • It supports service life assessment and component design safety margins for elastomer sealing applications.


Q6: What is the standard compression strain for ISO 3384-1 testing?

A: The standard compression strain is 25 % ± 2 %. If 25 % compression cannot be achieved for a given material or specimen, a compression of 15 % ± 2 % or lower values (in 5 % steps) may be used. The compression must be applied within 30 to 120 seconds.


Q7: What is the standard test duration for ISO 3384-1?

A: Unless otherwise specified, the minimum test duration is 168 hours (1 week) ± 2 hours. Preferred intermediate measurement points are 3 h, 6 h, 24 h, and 72 h. For longer test durations, a logarithmic time scale is recommended. The test period starts after the initial compression is completed.


Q8: Can ISO 3384-1 be used for testing in liquids such as oils?

A: Yes. The standard explicitly supports testing in liquid environments. Ring specimens are particularly suitable for liquid testing because the central holes in the compression plates allow fluid circulation and pressure equalization inside the ring. Test liquids should preferably be selected from those listed in ISO 1817.


Q9: What other standards are related or similar to ISO 3384-1?

A:

  • Normatively referenced: ISO 188 (accelerated ageing), ISO 18899 (equipment calibration guide), ISO 23529 (specimen preparation and conditioning).

  • Related ISO standards: ISO 3384-2 (temperature cycling testing), ISO 6914 (tensile stress relaxation), ISO 11346 (lifetime estimation), ISO 1817 (liquid effect testing).

  • ASTM equivalent: ASTM D6147 (Standard Test Method for Force Decay / Stress Relaxation in Compression), which follows comparable principles with a two-method structure.


Q10: What industries rely on ISO 3384-1 testing?

A: The test is essential across industries using compression-loaded elastomer sealing components:

  • Automotive: engine seals, cooling system gaskets, fuel system O-rings, under-hood rubber parts

  • Aerospace: high-temperature and fluid-resistant sealing components for engines and hydraulic systems

  • Oil & gas: pipeline flange gaskets, valve seals, downhole elastomer components

  • General industry: plumbing seals, appliance rubber parts, hydraulic system seals, industrial gasket manufacturing


Q11. Why choose ISO 3384-1 Compression Stress Relaxation Tester | Rubber Force Decay Test Machine from UnitedTest? 

UnitedTest manufactures high-precision ISO 3384-1 test machines for compression stress relaxation testing of vulcanized rubber and thermoplastic elastomers. Supports Method A & Method B, continuous & discontinuous measurement, ideal for seal and gasket quality control.


UnitedTest is a professional manufacturer of material testing equipment specialized in ISO 3384-1 compression stress relaxation test systems for vulcanized rubber and thermoplastic elastomers. Our force decay testing machines are fully compliant with ISO 3384-1:2024 (Third edition), supporting both Method A (isothermal testing at test temperature) and Method B (ambient measurement with thermal exposure), with both continuous and discontinuous measurement procedures available.

Engineered for O-ring, gasket, seal and elastomer component manufacturers, our ISO 3384-1 test equipment delivers ±1% force measurement accuracy, precision parallel platens with Ra ≤ 0.4 μm surface finish, and rigid plate construction with ≤0.01 mm deflection under load. The system supports testing in both air/gaseous environments and liquid immersion, making it suitable for R&D formulation optimization, incoming material quality control, and long-term sealing performance validation across automotive, aerospace, oil & gas, and general industrial applications.

As a trusted global rubber testing machine supplier, UnitedTest provides customizable compression stress relaxation solutions with full technical support, calibration services, and compliance with ISO 18899 calibration guidelines, ensuring reliable, repeatable test results aligned with international rubber testing standards.

< Previous: ISO 3380 Leather Shrinkage Temperature Test

> Next: ISO 3385 Soft foam impact fatigue test by constant-load pounding

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.