Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D885 Test details for Tire Cords Fabrics and Industrial Filament Yarns

ASTM D885 Test details for Tire Cords Fabrics and Industrial Filament Yarns

Share:

ASTM D885 Tire Cord Tester | Industrial Filament Yarn Testing Machine | UnitedTest

UnitedTest manufactures ASTM D885 compliant testing machines for tire cords, tire cord fabrics and organic industrial filament yarns. Perform tensile strength, elongation, shrinkage and physical property tests for nylon, polyester and rayon tire reinforcement materials, supporting tire factory QC, material qualification and rubber reinforcement component evaluation for hoses, conveyor belts and other rubber products.


ASTM D885 establishes a complete set of standardized test procedures for industrial filament yarns, twisted tire cords, and woven tire cord fabrics produced from manufactured organic-base fibers, including nylon, polyester, rayon and related high-performance industrial yarns. Widely adopted in the tire and rubber industry, this standard covers key mechanical property tests such as breaking force, elongation at break, tenacity, modulus and thermal shrinkage of tire reinforcement materials. Test data guides raw material incoming inspection, new product development, batch quality control and third-party material qualification for pneumatic tire manufacturers. Beyond tire applications, ASTM D885 test methods are also suitable for reinforcing cords used in rubber hoses, conveyor belts, flexible rubber linings and other engineered rubber goods, helping manufacturers verify consistency, stability and long-term mechanical performance of textile reinforcements. UnitedTest’s ASTM D885 testing system delivers stable, repeatable test results to meet laboratory accreditation and customer specification requirements.


Specific Test Methods Included:

1, Tensile Properties of Yarns and Cords
Princile

A specimen is clamped at a defined gauge length and stretched at a controlled rate until rupture.

Continuous force-elongation data is used to calculate strength, elongation, modulus, and energy absorption.

Test Equipment

Constant-Rate-of-Extension (CRE) type is preferred; CRL (constant-rate-of-loading) and CRT (constant-rate-of-transverse) types are permitted but have known bias relative to CRE. All machines must comply with ASTM D76

Clamps: Cam or pneumatic clamps with snubbing surfaces (≥12.5 mm diameter) to prevent jaw breaks and slippage..

Test parameter
  • Breaking force of conditioned yarns/cords

  • Breaking tenacity (breaking force normalized by linear density, for cross-material comparison)

  • Elongation at break

  • Force-at-Specified-Elongation (FASE): measured at fiber-specific elongation setpoints

    • Greige: 6% (rayon), 14% (nylon), 10% (polyester)

    • Adhesive-dipped: 3% (rayon), 5% (nylon), 5% (polyester)

  • Modulus: initial tangent modulus and chord modulus (over a defined tenacity interval)

  • Work-to-break, specific work-to-break, and breaking toughness (energy absorption properties)

  • Oven-dried rayon-specific tensile tests (breaking force, elongation, FASE)

  • Moisture regain correction for rayon tensile propertie

2. Other Yarn and Cord Properties
Parameter

- Twist level in yarns and cords (direct-counting method)

- Cord thickness (gauge)

- Extractable matter content

- Dip (adhesive) solids pickup: quantifies RFL (resorcinol-formaldehyde-latex) adhesive content, with fiber-specific solvent protocols:

  - Nylon: 90% formic acid dissolution

  - Polyester: KOH reflux or trichloroacetic acid-dichloromethane dissolution

  - Rayon: 71% sulfuric acid dissolution

- Cord-to-elastomer adhesion (referenced to ASTM D4393 and D4776)

Equipment
  • Linear density: skein reel and analytical balance (per ASTM D1907)

  • Twist tester: direct-counting type (per ASTM D1423)

  • Thickness gauge: 10 mm presser foot, 25 kPa applied pressure (per ASTM D1777)

  • Forced-air convection ovens (105 ± 3 °C for drying; 177 ± 2 °C for thermal testing)

  • Conditioning chambers (per ASTM D1776)

  • Length-measuring fixtures for shrinkage and growth test

3. Tire Cord Fabric Properties
Parameter

- Fabric width

- Mass per unit area

- Warp end count and filling pick count

- Fabric bending stiffness

Equipment

CRE tensile machine with 20 N load cell

25-mm span 3-point bending fixture or custom holder/depressor assembly


Test Parameters

CRE crosshead rate120 % of nominal gauge length per minute; 100 % alternate; aramid yarns use ASTM D7269
CRL loading rateRayon 25 ± 3 (mN/tex)/s [18 ± 2 (gf/den)/min]; nylon/polyester 50 ± 7 (mN/tex)/s [35 ± 5 (gf/den)/min]
CRT traverse rate120 % of gauge length per minute; 100 % alternate
Gauge length250 ± 1 mm [10 ± 0.05 in.], alternate 500 ± 2 mm [20 ± 0.10 in.]
Pretension5 ± 1 mN/tex [0.05 ± 0.01 gf/den], or slack start
Load‑cell rangeEstimated breaking force within 10–90 % of full scale
Jaw‑break rejectionDiscard specimens breaking in jaws or within 10 mm [3/8 in.] of jaw nip
Air velocity across specimen<250 mm/s [50 ft/min] avoids significant interlaboratory bias from the Gough–Joule effect
High‑strength cord clampingLarger snubbing surfaces or powdered rosin on cord portions held between snubbing surfaces may be used
Zero‑twist multifilament yarnInsert a small twist for tensile testing; historically up to 120 t/m [3.0 tpi]
Oven drying105 ± 3 °C [221 ± 6 °F]; 20–50 air changes/hour; constant mass = ≤0.1 % loss per 15 min in‑oven or 30 min out‑of‑oven weighing
Oven‑dried rayonDry 2–6 h; test within 10 ± 1 s of removal from oven; ambient exposure 10 ± 1 s
FASE elongations, Table 3Rayon 6 % greige / 3 % adhesive‑processed; Nylon 14 % / 5 %; Polyester 10 % / 5 %
Initial modulusTangent to initial straight‑line portion; force at 10 % elongation; report to nearest 10 mN/tex [0.1 gf/den]
Chord modulus limits, Table 4Rayon 30–60 mN/tex [0.3–0.6 gf/den]; Nylon 20–40 [0.2–0.4]; Polyester 30–60 [0.3–0.6]; M_c = 100(T_b − T_a)/(E_b − E_a)
TwistTen specimens; 5 ± 1 mN/tex; ASTM D1423
ThicknessFive specimens of four cords; 10 mm presser foot; ~25 kPa; ~5 N tension; lower foot over ~5 s; stabilize ~5 s; read 0.01 mm [0.0005 in.]
Dip pickup ovens105 ± 3 °C and 150 ± 3 °C [302 ± 6 °F]
Dip pickup resultAverage DPU to nearest 0.1 %
Stiffness20 N load cell; 25 mm opening; 50 mm specimen reduced to ten warp ends; crosshead 25 mm/min [1 in./min]; chart 125 mm/min [5 in./min]; bending force 10–90 % full scale; record to 1 mN [0.1 gf]
Elevated temperature177 ± 2 °C [350 ± 3 °F]
Wet contraction water24 ± 2 °C [75 ± 2 °F]
Growth load100 ± 1 mN/tex [1.0 ± 0.01 gf/den] total force after 5 ± 1 mN/tex pretension


Related standard: 

ISO 3341Textile glass - Yarns - Determination of breaking force and breaking elongation;
ASTM D7269Standard Test Methods for Tensile Testing of Aramid Yarns
AS 2001.2.7METHODS OF TEST FOR TEXTILES - PHYSICAL TESTS - DETERMINATION OF BREAKING FORCE AND EXTENSION OF YARNS
ASTM D885Standard Test Methods for Tensile Properties of Tire Cords and Tire Cords Fabrics;
ISO 3342Textile glass - Mats - Determination of tensile breaking force
ASTM D2256Standard Test Method for Tensile Properties of Yarns by the Single-Strand Method
ISO 2062Textiles; yarns from packages; determination of single-end breaking force and elongation at break


Test Application — Industry Fields

Pneumatic tire manufacturingQualification of nylon, polyester and rayon yarns, twisted cords and cord fabrics for carcass, belt and other tire reinforcement structures
Other rubber goodsReinforcing cords/fabrics for conveyor belts, V‑belts, hoses, air springs and other elastomer products
Fiber and yarn producersIncoming raw‑material QC, linear density, moisture regain, twist and tensile property verification
Cord twisting, dipping/RFL treating and weavingProcess control for twist, dip solids pickup, fabric mass, width, count and stiffness
Tire and rubber product engineeringBreaking force, tenacity, elongation, FASE, modulus and toughness data for reinforced‑rubber design calculations
Adhesion and durability evaluationH‑test/strap‑peel adhesion between textile cord and rubber compound


Keywords: ASTM D885 tester, tire cord testing machine, industrial filament yarn tester, tire cord fabric tensile tester, nylon tire cord test, polyester tire cord tester, rayon tire cord testing, tire reinforcement material test, rubber reinforcement cord tensile test, yarn breaking force tester, yarn elongation tester, thermal shrinkage test for tire cord, pneumatic tire material QC, conveyor belt cord test, rubber hose reinforcement yarn test, industrial textile tensile equipment, UnitedTest tire cord tester, ASTM D885 textile testing machine

Related products and device

ASTM D885 Tire Cords Fabric Tensile Universal Testing machine

WDW Series Computer Control Electronic Universal Testing Machine made by UNITEDTEST range from 100N to 600KN load capacity with various models like single columns, table type, door frame type etc., is used to perform tension, compression, flexure/bending, shearing, peeling etc., test for metal and nonmetal specimens.

ASTM D885 yarn snbbing and capstan tensile test fixture

Snubbing and Capstan grips are all engineered to perform high strength tensile tests where the test samples are long compared to their cross-sectional area, such as wire, rope and strapping.

ASTM D885 yarn, thread, string Bollard tensile test grips

Plastic tube, wire bollard tensile test grips are used on a Universal Testing Machine to perform tensile tests on filament material such as string, thread, wire and yarn. The specimen is wrapped around a bollard or post and then secured with a vise grip mechanism.

Related Standard

ISO 3341 Tensile Test of Textile Glass Yarn –

ISO 3341 Textile glass — Yarns — Determination of breaking force and breaking elongation

ISO 3341 specifies a method for the determination of the tensile breaking force and elongation at break of glass yarns taken from packages.

The method is applicable to various types of glass yarn (single, folded, cabled, strands, structures without twist, rovings, etc.). It is basically intended for single, folded and cabled glass yarns having a diameter of less than 2 mm, or a linear density lower than 2000 tex, taken from packages.  This test is applicable to various types of glass yarn (single, folded, cabled, strands, structures without twist, rovings, etc.). It is basically intended for single, folded and cabled glass yarns having a diameter of less than 2 mm, or a linear density lower than 2000 tex, taken from packages. 

ISO 2062 Textile tensile test: Breaking Force and Elongation of Yarns –

ISO 2062 specifies the method for determining the breaking force and elongation at break of textile yarns (single, piled, or cabled) under a constant rate of extension (CRE). It is a fundamental tensile test for yarn quality control.  

The test operates on the principle of applying a constant rate of elongation to a single yarn specimen until it breaks:

A single yarn is securely clamped between two grips at a fixed gauge length.

The lower grip moves downward at a constant speed, stretching the yarn at a rate of 100% per minute of the gauge length.

The machine continuously records the force (load) applied and the corresponding elongation.

The test ends when the yarn breaks. The maximum force recorded is the breaking force, and the stretch at that point is the elongation at break (expressed as a percentage).

ISO 3790 Netting Yarn Elongation Test –

ISO 3790 — Fishing nets — Determination of elongation of netting yarns

ISO 3790 specifies a laboratory method for determining the elongation of netting yarns taken either from packages (cones, bobbins, spools) or from netting, in their final physical state — i.e., the yarn is tested as supplied/as used, without altering its structure. Tests may be run in dry or wet state, but the standard explicitly says wet-state tests are "particularly appropriate in indicating the behaviour of the yarn in use".

ISO 3342 Tensile Test of Textile Glass Fiber Mats –

ISO 3342 Textile glass - Mats - Determination of tensile breaking force

ISO 3342 specifies a standardized method for measuring the tensile breaking force of textile glass mats. It is primarily intended for chopped-strand mats but is also applicable to certain types of continuous-strand mats, usually those for pultrusion processes.

ASTM D2256 Thread and Yarn Tensile Testing of Single-Strand String –

ASTM D2256 is the standard test method for tensile properties of yarns by the single-strand method. It is the predominant standard used in North America and is technically very similar to ISO 2062. It quantifies breaking force, elongation at break, and derived properties (tenacity, modulus, toughness) under diverse conditions, serving as a benchmark for quality control, product development, and material specification. 

Frequently Asked Questions (FAQs) – ASTM D885 Test details for Tire Cords Fabrics and Industrial Filament Yarns

Q1: What is ASTM D885/D885M?

A: ASTM D885/D885M is a consensus standard published by ASTM International that defines standardized test methods for evaluating tire cords, tire cord fabrics, and industrial filament yarns made from manufactured organic-base fibers (primarily nylon, polyester, and rayon). The 2025 edition covers tensile performance, physical dimensions, chemical coating content, and fabric mechanical properties for reinforcement materials used in pneumatic tires and other rubber goods.


Q2. Which materials does it cover?

Industrial filament yarns wholly made from manufactured organic‑base fibers, twisted cords made from them, woven tire cord fabrics, and other structures made specifically for pneumatic tires. The methods are explicitly relevant to nylon, polyester and rayon yarns, cords and fabrics. Section 1.1.1 also allows application to the same structures when used to reinforce other rubber goods.


Q3. Why is ASTM D885 testing important for the material? (Core answer)

Because the cord is the load‑bearing skeleton of a pneumatic tire. Section 14.2 states that the force‑bearing ability of a reinforced rubber product is related to the strength of the yarn or cord used as reinforcement, so breaking force is used directly in engineering calculations. Beyond that:

  • Breaking tenacity normalizes force by linear density, allowing fair comparison of different cord sizes and fiber types.

  • Elongation affects finished‑product uniformity and dimensional stability in service.

  • FASE and modulus describe how the cord responds to processing and to varying loads; FASE monitors changes during twisting, dipping, weaving and incorporation into rubber.

  • Work‑to‑break and breaking toughness quantify mechanical energy absorption, relevant to impact and fatigue resistance.

  • Moisture regain, linear density, twist, dip pickup and adhesion control whether the cord and the rubber compound actually behave as one composite. RFL dip exists to improve adhesion; dip solids pickup is a process‑control variable, and H‑test/strap‑peel adhesion reflects bond quality.

  • Without standardized conditioning, gauge length, speed, clamps and reporting, the "same" cord can produce different numbers in different labs. D885 creates a common measurement language for fiber producers, corders, dippers, weavers, tire makers and rubber‑goods manufacturers.


Q4. What tensile testing machine does D885 require?

A single‑strand tensile machine conforming to ASTM D76, of CRE, CRL or CRT type — with CRE (constant‑rate‑of‑extension) preferred. It needs an autographic recorder (rectilinear coordinates preferred) or electronic calculation/display, plus cam or pneumatic clamps with fixed snubbing surfaces integral with one clamping face. Snubbing surfaces may be circular with diameter not less than 12.5 mm [½ in.] or semi‑involute. Automated specimen‑loading CRE testers are permitted.


Q5. What grips are needed for high‑tenacity tire cord?

Cam or pneumatic clamps with snubbing surfaces. As cord diameter and strength increase, larger snubbing surfaces or greater holding capacity may be required to prevent slippage or excessive jaw breaks; if slippage still occurs, applying powdered rosin to the cord portions held between the snubbing surfaces has been found useful, especially for adhesive‑treated organic cords. Bollard/capstan‑type grips are the practical industry solution for cords that slip in flat jaws.


Q6. What other instruments are needed besides the universal tester?

A twist tester (ASTM D1423), thickness gauge (ASTM D1777, 10 mm presser foot, ~25 kPa), precision balance (1 mg), weighing bottles/desiccator, dip‑pickup glassware (extraction flasks, condensers, Gooch/G4 crucibles, glass‑fiber filters), a 20 N load cell plus stiffness rack/depressor or 3‑point bending fixture, H‑test mold and vulcanizing press for adhesion, and length/force devices for the X1–X3 appendices.


Q7. What gauge length and test speed are used?

Gauge length 250 ± 1 mm [10 ± 0.05 in.], with an alternate 500 ± 2 mm [20 ± 0.10 in.]. CRE crosshead rate = 120 % of nominal gauge length per minute (100 % alternate). CRL: rayon 25 ± 3 (mN/tex)/s, nylon/polyester 50 ± 7 (mN/tex)/s. CRT: 120 % of gauge length per minute (100 % alternate).


Q8. Why is rayon treated differently?

Rayon tensile properties are strongly moisture‑dependent. If actual regain is within ±0.3 % of the specification regain, report the observed value; if outside, apply a material‑specific adjustment factor derived from the slope of "breaking force vs. regain" (Section 17) or "elongation vs. regain" (Section 20). For oven‑dried rayon, dry at 105 ± 3 °C for 2–6 h, then mount and start the tester 10 ± 1 s after the specimen leaves the oven.


Q9. Breaking force vs. breaking tenacity vs. breaking toughness — what is the difference?

Breaking force is the maximum force at rupture (N or lbf). Breaking tenacity = breaking force / linear density (mN/tex or gf/den), enabling size‑independent comparison. Work‑to‑break is the area under the force–elongation curve; breaking toughness is work‑to‑break normalized by linear density (J/g or in.·lbf/in.·den), i.e. energy absorption per unit mass. 


Q10. How is cord‑to‑rubber adhesion tested?

Section 34 directs you to ASTM D4393 (strap peel) or ASTM D4776/D4776M (H‑test). In the H‑test, a cord is embedded between two rubber blocks, vulcanized, conditioned and pulled axially from the rubber on a CRE tester; the maximum pull‑out force is the adhesion result. ASTM D4776‑25 conditioning is 24 ± 1 °C / 55 ± 2 % RH for at least 4 h and up to 4 days.  The ISO counterpart is ISO 4647 / BS ISO 4647:2021, and China's GB/T 2942‑2009 is a modified adoption of ISO 4647:1982.


Q11. Which ASTM standards does D885 reference?

Section 2 lists D76, D123, D276, D1423, D1776, D1777, D1907, D1909, D2257, D2258, D2462, D2494, D2654, D3774, D3775, D3776, D3888, D4393, D4776, D4848, D4850, D6477 and D7269. Note that D276 was withdrawn in 2021; D885 references its last approved historical version. Closest companions: D2256 (general single‑strand yarn tensile), D7269 (aramid yarns), D4776/D4393 (adhesion), D2229 (steel cord adhesion) and D6775 (webbing/tape/braid tensile).

< Previous: ASTM D882 Tensile test of Thin Plastic Sheeting

> Next: ASTM D897 Tensile Test of Adhesive Bonds

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.