Home >> Application >> By Standard >> Others >> EN 1842 Compression Moulding Shrinkage Test of plastics compounds

EN 1842 Compression Moulding Shrinkage Test of plastics compounds

Share:

EN 1842 SMC BMC Compression Moulding Shrinkage Tester | UnitedTest

UnitedTest manufactures EN 1842 compliant testing equipment for thermoset moulding compounds. Measure compression moulding shrinkage of SMC and BMC specimens with no post-shrinkage after curing for composite material labs.


EN 1842 Plastics establishes a standardized laboratory test procedure to evaluate compression moulding shrinkage of thermoset moulding compound specimens. This standard applies exclusively to materials without post‑shrinkage after moulding, mainly polyester sheet moulding compound (SMC) and bulk moulding compound (BMC). UnitedTest provides precision test systems for SMC BMC producers, composite moulding workshops and third‑party polymer testing laboratories.


Test Principle

The principle is a direct dimensional comparison:

  • The reference length L₀ = the length of the mould cavity (or the distance between engraved gauge marks in the cavity), measured at standard atmosphere with the mould cold.

  • The specimen length L₁ = the corresponding length of the moulded part, measured at the same standard atmosphere after cooling and conditioning.

Moulding shrinkage = the difference in dimensions between a moulding and the mould cavity in which it was moulded, both the mould and the moulding being at normal temperature when measured (definition adopted from ISO 2577).

Because the mould is measured cold and the part is measured cold, the result is the net processing shrinkage — the sum of the chemical (cure) shrinkage of the polyester resin plus the thermal contraction from mould temperature down to ambient — excluding any post‑shrinkage (which is assumed negligible for SMC/BMC).

Result: MS (%) = (L₀ − L₁) / L₀ × 100

  • Positive value → shrinkage

  • Negative value → expansion (possible with highly filled / low‑profile systems)


Test Specimen Requirements

  • Specimens are compression‑moulded plaques produced with the mould‑press system described above.

  • Specimen thickness range: 3.5 mm ~ 5.5 mm.

  • Three replicate specimens shall be manufactured for one test series.

  • For SMC specimens, record production flow direction and unidirectional‑reinforcement orientation for directional shrinkage evaluation.


EN 1842 Compression Moulding Shrinkage Test of plastics compounds Required Test Equipment

Recomend UnitedTest Hot blast Oven with filme size change measuring tools:  

Compression mould and press

Mould cavity area ≥ 200 cm², punch‑die assembly capable of applying stable positive compression pressure. 

Cavity may be rectangular, square, circular, with optional engraved gauge marks and/or draft angles, complying with  ISO 12114 or EN 12576

Dimensional‑measuring instrumentResolution accurate to 0.01 mm, for measuring both mould cavity and test‑specimen dimensions
Non‑metallic cooling rack

Supports specimens vertically, minimum 20 mm clearance between samples; protective plates are recommended for outer specimens to guarantee symmetric cooling


Key test parameter: 

Mould temperature140°C1%
SMC mould coverage≥ 90 %
Moulding pressure±5%
Pressing curing time40 seconds per mm specimen thickness (or longer for full cure completion)
Mould closing time≤ 15 seconds after material charging into mould
Post‑mould conditioningMinimum 16 h storage under standard atmosphere (ISO 291); shorter duration is permitted if proven equivalent results can be achieved


Complete Test Procedures of EN 1842 Compression Moulding Shrinkage Test of plastics compounds

  1. Under standard atmosphere, measure mould‑cavity reference length L_0 (or engraved‑mark spacing) accurate to 0.01 mm and record value for shrinkage calculation.

  2. Prepare conditioned SMC/BMC charge (pre‑form BMC), load material into mould cavity and close mould within 15 seconds. Compression‑mould three specimens under specified temperature, pressure and curing‑time parameters. Mark SMC specimens for material flow/reinforcement direction information.

  3. Eject finished specimens from mould, place on non‑metallic cooling rack for cooling to room temperature. Condition specimens in standard atmosphere for minimum 16 h (or validated shorter period).

  4. Measure specimen length L_1 in standard atmosphere to 0.01 mm precision, follow measurement rules for draft‑angle or engraved‑mark conditions, take one reading for each replicate specimen.

  5. Compute moulding‑shrinkage percentage MS for each specimen and calculate average value of three replicates.

  6. Compile full test report including standard reference, compound designation, mould specification, specimen thickness, full moulding‑process parameters, individual and average shrinkage values, SMC measurement direction notes and test‑execution date.


Industrial Application Fields

  • Mould / tool design: the shrinkage value is the compensation factor used to scale up the mould cavity so the finished part lands inside tolerance.

  • Material qualification & specification: confirms whether a given SMC/BMC grade is capable of holding dimensional accuracy for a given part.

  • Supplier / incoming QC and batch release: verifies batch‑to‑batch consistency of shrinkage ("uniformity of manufacture").

  • Typical end‑use sectors: automotive (body panels, structural parts, headlamp reflectors, under‑bonnet parts), electrical & electronics (switchgear housings, insulators, meter boxes), sanitary/appliance and construction components moulded from polyester SMC/BMC.

  • Users: compound suppliers, moulders, tool designers, OEM dimensional engineers, and independent test laboratories. 


Related Standard: 

ASTM D2732

Standard Test Method for Unrestrained Linear Thermal Shrinkage of Plastic Film and Sheeting.

ASTM D1042

Standard Test Method for Linear Dimensional Changes of Plastics Caused by Exposure to Heat and Moisture

ISO 2505Thermoplastics pipes — Longitudinal reversion — Test method and parameters (replace the ISO 2506). 
ISO 11501

Plastics Film and sheeting Determination of dimensional change on heating.

ASTM D2732 enforces fully unrestrained free shrink; ISO 11501 allows optional restrained test modes. 

Test data from the two standards lack direct comparability, as clearly noted in the D2732 standard text.

GB/T 12027Plastics--Film and sheeting--Determination of dimensional change on heating
GB/T 39818Plastics — Thermosetting moulding materials — Determination of shrinkage, ISO 2577:2007
EN 1842Plastics — Thermosetting moulding compounds (SMC/BMC) — Determination of compression moulding shrinkage
ASTM D1204Standard Test Method for Linear Dimensional Changes of Nonrigid Thermoplastic Sheeting or Film at Elevated Temperature
ISO 14616Plastics - Heat shrinkable films of polyethylene, ethylene copolymers and their mixtures - Determination of shrinkage stress and contraction stress
GB/T 34848Determination of shrinkage character for heat-shrinkable films.
ISO 2577Plastics‑Thermosetting moulding materials‑Determination of shrinkage
ISO 10724-1Injection moulding of thermosetting PMCs: general principles & multipurpose specimens
ISO 10724-2Injection moulding of thermosetting PMCs: small plates (specifies the D2 mould)
ISO 294-4

Injection moulding of thermoplastics — Part 4: Determination of moulding shrinkage.

It measures S_M, post-moulding shrinkage S_P and total shrinkage S_T on the same 60 × 60 × 2 mm D2 plate and explicitly states "For the determination of shrinkage of thermosets, see ISO 2577".


Keywords: EN 1842 tester, SMC compression moulding shrinkage test machine, BMC mould shrinkage tester, thermoset moulding compound shrinkage testing equipment, polyester composite mould shrinkage rig, sheet moulding compound dimensional test, bulk moulding compound compression mould test, thermoset composite dimensional stability tester, SMC BMC material quality inspection machine, composite moulding shrinkage verification fixture, thermoset polymer physical property tester, moulded composite specimen dimensional test system

Related products and device

EN 1842 Hot Oven air heating plastics compounds thermal shrinkage tester

Suitable to measure various kinds of plastic pipe or plastic materials size change after heating, or used to heat the test sample. It can be used as a heating oven as well.

Dimensional stability tester

Professional film heat shrink tester is precision lab equipment engineered to evaluate thermal shrinkage characteristics and thermal dimensional stability of diverse raw materials, including plastic films. compliant with international testing standards ASTM D2732 and ISO 11501.

Heat Shrinkage Tester

Integrated Film Thermal Shrinkage Performance Tester, simultaneously captures real-time test data including temperature, thermal shrinkage force, residual shrinkage force and shrinkage displacement, Conform with ISO 14616, DIN 53369, ASTM D2732 as a shrink force tester or comprehensive shrink tester

Related Standard

ISO 2577 Moulding Shrinkage Test for Thermosetting Plastics –

ISO 2577 Plastics‑Thermosetting moulding materials‑Determination of shrinkage

ISO 2577 defines laboratory methods to measure moulding shrinkage and post‑shrinkage of thermosetting moulding material test specimens.


ISO 11501 Heat dimensional change of plastic films sheeting –

ISO 11501 Plastics — Film and sheeting — Determination of dimensional change on heating

ISO 11501 specifies a uniform laboratory test method to quantify thermal dimensional variation of plastic films and thin sheets (max thickness 1 mm), covering both machine (longitudinal) and transverse directions, for all plastics whether heat-shrinkable or non-shrink grade. 

ASTM D2732 Thermal Shrinkage Testing for Plastic Films Sheeting –

ASTM D2732 standardized laboratory method to measure the degree of unrestrained (free) linear thermal shrinkage of plastic films and sheets ≤ 0.76 mm (0.030 in.) thick at a specified temperature. Quantifies irreversible rapid linear dimensional reduction when plastic film is exposed to high temperature under zero or minimal external restraint. 

ISO 13636 Non-oriented PET Films sheeting test requirement (APET) –

ISO 13636 specifies requirements anf test methods for non-oriented PET (APET) sheets — made from virgin, recycled, or combined PET, thickness < 2.0 mm. It explicitly excludes foamed sheets and shrinkable films (those are covered elsewhere, e.g. biaxially oriented PET in ISO 15988). The mandatory performance tests including Tensile stress at yield, Heat shrinkage, Oxygen transmission rate (OTR), haze value, Intrinsic viscosity (IV).

ISO 15988 Biaxial stretch PET films test methods details –

ISO 15988 specifies requirements for biaxially oriented transparent PET (BOPET) films, mainly used for packaging, either alone or as a laminated layer with other films. The main test stipualted in this standard include tensile strength and strain, Dimensional change on heating, Oxygen transmission coefficient, Water vapour transmission coefficient, Haze, Wetting tension, thickness etc., 

ISO 15987 Biaxially oriented nylon films tensile expansion testing methods –

ISO 15987 specifies classification, mandatory visual, dimensional, mechanical, barrier, optical, surface energy, and food contact safety requirements for transparent BOPA film, supplied in roll form, either used standalone or laminated with PE, CPP, PET, aluminium foil for multi-layer packaging structures. The test stipulated in ISO 15987 mainly include, tensile strength & tensile strain at break, Oxygen transmission coefficient, Dimensional change on heating, Haze, Wetting tension etc., 

ISO 17555 BOPP films biaxial stretch testing methods –

ISO 17555 applies to packaging-grade BOPP films containing ≥95% polypropylene resin; usable as single-layer film or laminates paired with other plastic substrates. The test stipulated in ISO 17555 mainly include, tensile strength & strain at break, Dimensional change on heating (thermal shrinkage), Coefficient of water vapour transmission, Haze, Wetting tension etc., 

ISO 2505 Thermoplastic Pipes Longitudinal Reversion Test (PF Heat Reversion Test) –

ISO 2505 Thermoplastics pipes — Longitudinal reversion — Test method and parameters.

ISO 2505 specifies a method for determining the longitudinal reversion (i.e., length change after heating) of thermoplastics pipes. Two heating media are allowed: Heated liquid bath, Air oven. 

In 2023 adds materials: PE 100-RC, PB-H, PB-R, PE-RT, PP-RCT, PE-UHMW.


The longitudinal Reversion rate of pipe materials refers to the percentage change in length of thermoplastic pipe materials under specific temperatures, used to assess the thermal contraction properties of the material. The measurement method is based on the national standard ISO 2505, GB/T 6671-2001, which is mainly divided into two types: liquid bath test (Method A) and air oven test (Method B). 




ASTM D1204 Plastic Films Dimensional stability testing at high temperature –

ASTM D1204 Standard Test Method for Linear Dimensional Changes of Nonrigid Thermoplastic Sheeting or Film at Elevated Temperature

ASTM D1204 is method to measure linear dimensional change (shrinkage or expansion) of nonrigid thermoplastic sheeting/film when exposed to a specified elevated temperature and time in air. Applies to nonrigid thermoplastic sheeting/film made by calender or extrusion processes, the heating medium is air (mechanical convection oven) — this points is the fundamental difference from ASTM D2732 (liquid bath). 

FAQs for EN 1842 Compression Moulding Shrinkage Test (SMC / BMC)

Q1. What is EN 1842?

EN 1842:1997 is a European Standard (CEN/TC 249, Plastics; ICS 83.080.10) titled Plastics — Thermoset moulding compounds (SMC-BMC) — Determination of compression moulding shrinkage. It defines a laboratory method for measuring how much a compression-moulded thermoset part shrinks relative to the mould cavity it was made in. 


Q2. What exactly does "compression moulding shrinkage" mean here?

It is the difference in dimensions between a moulding and the mould cavity in which it was moulded, with both the mould and the moulding at normal (standard-atmosphere) temperature when measured. Because both are measured cold, the result is net processing shrinkage — chemical cure shrinkage plus thermal contraction from 140 °C down to ambient — and it excludes post-shrinkage.


Q3. Which materials does EN 1842 cover — and which does it exclude?

It applies only to thermoset moulding compounds that exhibit no post-shrinkage after moulding, i.e. typical polyester SMC (sheet moulding compound) and BMC (bulk moulding compound). It is not intended for materials that continue to shrink in service, and it is not an injection-moulding or thermoplastic method.


Q4. Why is the EN 1842 test important?

Because shrinkage is the number that decides whether a moulded SMC/BMC part fits. Specifically:

  • Tool design — the cavity must be cut oversize by the measured shrinkage; a 0.1 % error = 1 mm of mismatch on a 1 m part.

  • Material qualification — it shows whether a grade can hold the dimensional tolerance a part demands.

  • Batch release / incoming QC — fixed moulding conditions make shrinkage a reproducible fingerprint for production control and uniformity of manufacture.

  • Formulation — it validates low-profile/low-shrink additive packages; a small negative value (expansion) is often the target for Class-A surfaces.


Q5. What are the test specimen requirements?

Compression-moulded plaques, 3 specimens per test, thickness 3.5 mm to 5.5 mm. Material must be sampled after maturation and within shelf-life, kept bagged against volatile loss and moisture uptake, and conditioned to equilibrium under standard atmosphere before moulding. On SMC, the machine/production direction and any unidirectional reinforcement direction must be marked.


Q6. How is the result calculated?

MS (%) = (L₀ − L₁) / L₀ × 100, where L₀ is the cold mould reference length (cavity length or gauge-mark distance) and L₁ is the corresponding length of the conditioned specimen. One measurement per specimen; report individual values plus the average. Positive = shrinkage; negative = expansion.


Q7. Why must the measurement direction be reported for SMC?

SMC shrinkage is anisotropic — fibre orientation and the SMC machine direction make shrinkage direction-dependent. Measuring in only one direction hides a variable that drives warp, mismatch and assembly problems. That is why clause 9 requires the direction relative to the SMC machine direction and/or the unidirectional reinforcement.


Q8. How does EN 1842 differ from ISO 2577?

ISO 2577 is the general thermoset shrinkage method (current edition 2007): it covers compression and injection moulding, uses 120 × 15 × 10 mm bars or ~60 × 60 × 2 mm plates, measures to 0.02 mm, discards specimens warped > 1 %, and adds post-shrinkage after oven exposure (80 °C for urea-formaldehyde, 110 °C for others; 48 h rapid / 168 h normal). EN 1842 is the SMC/BMC-specific, compression-only, higher-resolution (0.01 mm) variant that assumes no post-shrinkage. EN 1842 takes its shrinkage definition from ISO 2577:1984.


Q9. How does EN 1842 differ from EN ISO 12114 / ISO 12114?

ISO 12114 measures cure characteristics — exotherm heat, thermal expansion, cure shrinkage and net shrinkage — recorded in-mould by pressure, temperature and displacement sensors during a simulated moulding cycle (Method II; shear-edge mould ≥ 200 cm²). It produces a curve of behaviour during cure. EN 1842 measures a single final dimension after cooling. They are complementary: EN 1842 even accepts an ISO 12114-type mould.


Q10. Can UnitedTest customize the system for our material or other standards?

Yes. UnitedTest accepts OEM/ODM and custom engineering: mould cavity size and shape (rectangular / square / circular / shear-edge per EN ISO 12114 or prEN 12576), temperature range, pressure range and control mode, plus software workflows for EN 1842, ISO 2577, EN ISO 12114, ISO 295 and customer-specific internal procedures.


Q11. Can we retrofit our existing UnitedTest universal testing machine or compression testing machine?

In many cases yes — heated platen sets, EN 1842 mould tooling and control upgrades can be supplied as a package to extend an existing UnitedTest load frame. UnitedTest application engineers assess frame stiffness, platen parallelism, temperature control and control-loop requirements before recommending retrofit versus a dedicated system.


Q12. Which industries buy EN 1842 test setups?

Automotive (SMC body panels, structural and under-bonnet parts), electrical and electronics (switchgear housings, insulators, meter boxes), sanitary ware and appliances, construction products, plus SMC/BMC compound producers, independent test laboratories and university/R&D institutes.


Q13. Why choose EN 1842 Compression Moulding Shrinkage Testing Machine from UnitedTest?

UnitedTest is professional manufacturer for EN 1842:1997 compression moulding shrinkage testing machine for SMC and BMC thermoset composites. Complete lab solution for mould shrinkage measurement conforming to European standard EN 1842.


UnitedTest is a trusted global manufacturer supplying complete laboratory test systems complying with EN 1842:1997 (Plastics‑‑Thermoset moulding compounds SMC‑BMC‑‑Determination of compression moulding shrinkage).

Our EN 1842 test equipment is specially built for thermoset polyester SMC and BMC composite material laboratories, composite raw‑material factories, automotive composite component manufacturers, electrical‑parts producers, and third‑party testing institutes.


Full‑system solution includes: precision compression mould set (≥ 200 cm² cavity), hydraulic hot compression press, high‑accuracy 0.01 mm dimensional measuring unit, non‑metallic cooling rack, and test‑report software following EN 1842 reporting requirements. The system supports specimen production, conditioning, dimension reading, automatic moulding‑shrinkage MS calculation, stores individual‑specimen results and average value, and outputs test reports matching EN 1842 test‑report clauses.

Testing SMC/BMC compression‑moulding shrinkage per EN 1842 is critical input for mould‑tool development, raw‑material incoming inspection, low‑shrink SMC grade evaluation, supplier‑buyer material‑performance verification. UnitedTest’s EN 1842 shrinkage test set follows standard requirements: default 140 °C mould temperature control, 7 MPa moulding‑pressure control, configurable cure‑time setting, supports 3.5‑5.5 mm thickness plaques. Our system also reminds operators for SMC flow‑direction marking and annual mould‑wear inspection.


If you need reliable EN 1842‑compliant SMC‑BMC mould‑shrinkage laboratory setup, contact UnitedTest for equipment quotation, custom mould modification and lab‑application technical support.

< Previous: EN 10233 Tube Flattening Test Method, Specimen, Equipment and Test Machines

> Next: API Spec 10D — Bow-Spring Casing Centralizer Test

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.