Information on the most widely used ASTM standards within the materials testing industry
ISO 2577 Moulding Shrinkage Tester for Thermosetting Moulding Plastics | UnitedTest
UnitedTest manufactures ISO 2577 compliant test equipment for measuring moulding shrinkage and post-shrinkage of thermosetting moulding material specimens for plastic formulation and mould process validation.
ISO 2577 specifies laboratory test procedures to evaluate moulding shrinkage and post-shrinkage characteristics of thermosetting moulding plastic specimens. It supports material screening, mould design optimisation and production consistency checks for thermoset moulding compounds. UnitedTest supplies precision ISO 2577 shrinkage measurement systems for plastics R&D, incoming material inspection and moulding process quality control.
Definition:
| Moulding shrinkage (MS) | Difference in dimensions between a moulding and the mould cavity in which it was moulded, both measured at normal temperature |
| Post-shrinkage (PS) | Shrinkage of a plastic product after moulding, during post-treatment, storage or use |
Test Principle
The principle is a direct dimensional comparison:
The mould cavity (or the distance between engraved gauge marks in the mould) is measured at 23 °C → gives L₀.
The specimen is moulded, cooled, conditioned, and measured at the same temperature → gives L₁.
The percentage difference between cavity and specimen is the moulding shrinkage:
MS = (L₀ − L₁) / L₀ × 100 (%)
The specimen is then heat-treated in an oven (accelerated ageing) and re-measured → gives L₂.
PS₄₈ₕ or PS₁₆₈ₕ = (L₁ − L₂) / L₁ × 100 (%)
Note: the PS fraction bar is missing in the PDF text you supplied; the correct expression, as printed in the official ISO text, is (L₁ − L₂)/L₁ × 100.
Because both measurements are made at the same temperature, the result is a true, thermally-compensated shrinkage and not an artefact of thermal expansion. For injection-moulded plates, L₀ and L₁ (and L₂) are each the average of two readings taken 20 mm from the corners, in the same direction, allowing shrinkage to be reported parallel and perpendicular to the flow direction (orientation/anisotropy effect).
Test Specimen Requirements
Two specimen formats correspond to different moulding technologies:
Compression‑moulded specimen: rectangular bar, 120 mm ×15 mm ×10 mm.
Injection‑moulded specimen: flat square plate, 60 mm ×60 mm ×2 mm.
Minimum quantity: at least two specimens per sample; for fibrous thermosetting materials made by injection moulding, at least four specimens shall be tested.
ISO 2577 Moulding Shrinkage Test for Thermosetting Plastics Required Test Equipment
Recomend UnitedTest Hot blast Oven with filme size change measuring tools:
| Mechanical Convection Oven | required only for post‑shrinkage thermal ageing treatment; supports stable controlled heating temperature. Specimen supports are needed inside oven to avoid specimen deformation during heating. |
| Length‑measuring instrument | capable of measuring dimensions to accuracy of 0.02 mm, for mould cavity and specimen dimension measurement. |
| Mould and pressing/injection equipment | For compression moulding: positive or semi‑positive mould with single‑cavity or multi‑cavity structure. For injection moulding: Type D2 ISO mould specified in ISO 10724‑2, producing 60 mm × 60 mm × 2 mm square plates. Engraved reference marks can be added on mould inner walls for precise length reading. |
Key test parameter:
| Measuring resolution | Nearest 0.02 mm |
| Moulding conditions (compression) | As specified in ISO 295 or the material specification (pressure, temperature, time, etc.) |
| Moulding conditions (injection) | As specified in ISO 10724-2:1998, Clause 5 and ISO 10724-1 |
| Cooling after demoulding | On a low-thermal-conductivity surface, under an appropriate load to avoid warping |
| Plate measurement position | 20 mm from the corners, two readings in the same direction, averaged |
| Post-shrinkage temperature — UF materials | 80 °C ± 2 °C |
| Post-shrinkage temperature — all other thermosets | 110 °C ± 3 °C |
| Post-shrinkage duration | 48 h ± 1 h (rapid) or 168 h ± 2 h (normal) |
| Cooling after heat treatment | ≥ 3 h at 23 °C ± 2 °C, 45–55 % RH, then re-measure |
Complete Test Procedures of ISO 2577 Moulding Shrinkage Test for Thermosetting Plastics
Post‑demould cooling & conditioning: Place hot specimens on low‑thermal‑conductivity substrate with proper load to prevent warping. Condition under standard atmosphere for 1–72 h before measurement.
Warp inspection & screening: Reject specimens with warp exceeding 1 % of specimen length.
Moulding shrinkage measurement: Measure specimen dimension at 23 °C. For bars: measure along main axis. For square plates: take two readings 20 mm away from corners in one direction; measure two orthogonal directions for orientation effect assessment.
Post‑shrinkage procedure (optional): Put pre‑measured specimens into pre‑heated oven, keep specimens separated and supported to avoid distortion. Apply specified temperature and duration. After heating finishes, cool specimens ≥3 h in standard atmosphere, then repeat dimension measurement with same measuring method.
Calculation: Compute percentage moulding shrinkage (MS) and post‑shrinkage
Industrial Application Fields
ISO 2577 data is used wherever thermosets must hold a dimension:
Mould/tool design and compensation — the toolmaker needs the initial shrinkage to cut the cavity oversize so the finished part lands in tolerance.
Production control & batch uniformity — comparing MS/PS lot-to-lot proves the compound is being made consistently.
Dimensional-accuracy qualification — post-shrinkage tells you whether a grade is suitable for tight-tolerance parts that will see heat in service.
Material data sheets & single-point data — ISO 2577 is the source method cited by ISO 10350-1 for comparable single-point shrinkage data of moulding materials, i.e. it feeds supplier datasheets and CAD/CAE databases.
Typical end markets: electrical/electronic components (switches, sockets, breaker housings, coil formers), automotive under-hood and electrical parts, appliance handles and knobs, sanitary/heat-resistant ware, phenolic and amino moulding compounds, BMC/SMC part.
Related Standard:
| ASTM D2732 | Standard Test Method for Unrestrained Linear Thermal Shrinkage of Plastic Film and Sheeting. |
| ASTM D1042 | Standard Test Method for Linear Dimensional Changes of Plastics Caused by Exposure to Heat and Moisture |
| ISO 2505 | Thermoplastics pipes — Longitudinal reversion — Test method and parameters (replace the ISO 2506). |
| ISO 11501 | Plastics Film and sheeting Determination of dimensional change on heating. ASTM D2732 enforces fully unrestrained free shrink; ISO 11501 allows optional restrained test modes. Test data from the two standards lack direct comparability, as clearly noted in the D2732 standard text. |
| GB/T 12027 | Plastics--Film and sheeting--Determination of dimensional change on heating |
| GB/T 39818 | Plastics — Thermosetting moulding materials — Determination of shrinkage, ISO 2577:2007 |
| EN 1842 | Plastics — Thermosetting moulding compounds (SMC/BMC) — Determination of compression moulding shrinkage |
| ASTM D1204 | Standard Test Method for Linear Dimensional Changes of Nonrigid Thermoplastic Sheeting or Film at Elevated Temperature |
| ISO 14616 | Plastics - Heat shrinkable films of polyethylene, ethylene copolymers and their mixtures - Determination of shrinkage stress and contraction stress |
| GB/T 34848 | Determination of shrinkage character for heat-shrinkable films. |
| ISO 2577 | Plastics‑Thermosetting moulding materials‑Determination of shrinkage |
| ISO 10724-1 | Injection moulding of thermosetting PMCs: general principles & multipurpose specimens |
| ISO 10724-2 | Injection moulding of thermosetting PMCs: small plates (specifies the D2 mould) |
| ISO 294-4 | Injection moulding of thermoplastics — Part 4: Determination of moulding shrinkage. It measures S_M, post-moulding shrinkage S_P and total shrinkage S_T on the same 60 × 60 × 2 mm D2 plate and explicitly states "For the determination of shrinkage of thermosets, see ISO 2577". |
Keywords: ISO 2577 shrinkage tester, thermosetting moulding material shrinkage test machine, plastic moulding shrinkage tester, thermoset post shrinkage test equipment, mould shrinkage measurement instrument, thermosetting compound dimensional change tester, plastic moulding process test rig, thermoset material lab testing machine, mould shrinkage verification tester, UnitedTest ISO 2577 testing machine, thermosetting resin shrinkage analyser, ISO 2577 test, ISO 2577 moulding shrinkage, thermoset shrinkage test, moulding shrinkage tester, post-shrinkage test ISO 2577, thermosetting moulding materials shrinkage determination, ISO 2577 testing equipment, moulding shrinkage test machine supplier, how to measure moulding shrinkage of thermoset plastics, ISO 2577 vs ISO 294-4 difference, ISO 2577 test specimen size 120x15x10, post shrinkage oven 110 °C 168 h, GB/T 39818 vs ISO 2577, compression moulding shrinkage measurement equipment, D2 mould 60x60x2 shrinkage test, ISO 2577 shrinkage test equipment manufacturer, thermoset moulding shrinkage testing machine price, buy mould shrinkage test apparatus, plastics shrinkage testing lab setup
Related products and device
Related Standard
EN 1842 Plastics — Thermoset moulding compounds (SMC-BMC) — Determination of compression moulding shrinkage
EN 1842 specifies a laboratory method for determining the moulding shrinkage of compression‑moulded test specimens made from thermoset moulding compounds. It applies only to materials that show no post‑shrinkage after moulding — i.e. typical polyester SMC (sheet moulding compound) and BMC (bulk moulding compound).
ISO 11501 Plastics — Film and sheeting — Determination of dimensional change on heating
ISO 11501 specifies a uniform laboratory test method to quantify thermal dimensional variation of plastic films and thin sheets (max thickness 1 mm), covering both machine (longitudinal) and transverse directions, for all plastics whether heat-shrinkable or non-shrink grade.
ASTM D2732 standardized laboratory method to measure the degree of unrestrained (free) linear thermal shrinkage of plastic films and sheets ≤ 0.76 mm (0.030 in.) thick at a specified temperature. Quantifies irreversible rapid linear dimensional reduction when plastic film is exposed to high temperature under zero or minimal external restraint.
ISO 13636 specifies requirements anf test methods for non-oriented PET (APET) sheets — made from virgin, recycled, or combined PET, thickness < 2.0 mm. It explicitly excludes foamed sheets and shrinkable films (those are covered elsewhere, e.g. biaxially oriented PET in ISO 15988). The mandatory performance tests including Tensile stress at yield, Heat shrinkage, Oxygen transmission rate (OTR), haze value, Intrinsic viscosity (IV).
ISO 15988 specifies requirements for biaxially oriented transparent PET (BOPET) films, mainly used for packaging, either alone or as a laminated layer with other films. The main test stipualted in this standard include tensile strength and strain, Dimensional change on heating, Oxygen transmission coefficient, Water vapour transmission coefficient, Haze, Wetting tension, thickness etc.,
ISO 15987 specifies classification, mandatory visual, dimensional, mechanical, barrier, optical, surface energy, and food contact safety requirements for transparent BOPA film, supplied in roll form, either used standalone or laminated with PE, CPP, PET, aluminium foil for multi-layer packaging structures. The test stipulated in ISO 15987 mainly include, tensile strength & tensile strain at break, Oxygen transmission coefficient, Dimensional change on heating, Haze, Wetting tension etc.,
ISO 17555 applies to packaging-grade BOPP films containing ≥95% polypropylene resin; usable as single-layer film or laminates paired with other plastic substrates. The test stipulated in ISO 17555 mainly include, tensile strength & strain at break, Dimensional change on heating (thermal shrinkage), Coefficient of water vapour transmission, Haze, Wetting tension etc.,
ISO 2505 Thermoplastics pipes — Longitudinal reversion — Test method and parameters.
ISO 2505 specifies a method for determining the longitudinal reversion (i.e., length change after heating) of thermoplastics pipes. Two heating media are allowed: Heated liquid bath, Air oven.
In 2023 adds materials: PE 100-RC, PB-H, PB-R, PE-RT, PP-RCT, PE-UHMW.
The longitudinal Reversion rate of pipe materials refers to the percentage change in length of thermoplastic pipe materials under specific temperatures, used to assess the thermal contraction properties of the material. The measurement method is based on the national standard ISO 2505, GB/T 6671-2001, which is mainly divided into two types: liquid bath test (Method A) and air oven test (Method B).
ASTM D1204 Standard Test Method for Linear Dimensional Changes of Nonrigid Thermoplastic Sheeting or Film at Elevated Temperature
ASTM D1204 is method to measure linear dimensional change (shrinkage or expansion) of nonrigid thermoplastic sheeting/film when exposed to a specified elevated temperature and time in air. Applies to nonrigid thermoplastic sheeting/film made by calender or extrusion processes, the heating medium is air (mechanical convection oven) — this points is the fundamental difference from ASTM D2732 (liquid bath).
FAQs for ISO 2577 Thermosetting Plastics Shrinkage Test
Q1. What is ISO 2577?
ISO 2577 is an International Standard that specifies a method for determining the moulding shrinkage and the shrinkage after heat treatment (post-shrinkage) of moulded test specimens made from thermosetting moulding materials. The current edition is ISO 2577:2007 (3rd edition, published December 2007), which cancelled and technically revised ISO 2577:1984. It is still confirmed and current.
Q2. What exactly does the standard measure?
Two distinct characteristics:
Moulding shrinkage (MS) — the dimensional difference between a moulding and the mould cavity it was made in, with both mould and moulding at normal temperature when measured.
Post-shrinkage (PS) — the shrinkage that occurs after moulding, during post-treatment, storage or use (quantified here by a defined oven heat treatment).
Q3. Which materials is ISO 2577 for?
Thermosetting moulding materials only — e.g. phenolic (PF), urea-formaldehyde (UF), melamine-formaldehyde (MF), unsaturated polyester (UP / BMC / SMC), epoxy and amino moulding compounds, including powder moulding compounds (PMCs) and fibre-filled grades.
Q4. Can ISO 2577 be used for thermoplastics?
No. Thermoplastics use ISO 294-4 (Injection moulding of thermoplastics — Part 4: Determination of moulding shrinkage) or ASTM D955. ISO 294-4 itself states: "For the determination of shrinkage of thermosets, see ISO 2577." The two families are deliberately kept apart because thermosets cure chemically and keep shrinking in service, while thermoplastics mainly shrink by cooling.
Q5. Why does moulding shrinkage matter so much for thermosets?
Because a thermoset part cannot be re-melted or reworked. The tool must be cut to the correct size the first time. Moulding shrinkage is the number a toolmaker uses to size the cavity so the cool part lands inside tolerance. A 0.3 % error on a 120 mm dimension is already 0.36 mm — enough to scrap an electrical housing, a switch block or a precision insulator.
Q6. Why does the standard measure post-shrinkage separately?
Thermosets shrink in two stages. The first is cure + thermal contraction between the hot cavity and the cooled part (MS). The second is continued shrinkage during service, driven by post-cure, loss of volatiles/moisture and relaxation of frozen-in stress (PS). A compound can mould beautifully and still drift out of tolerance after it ships. Only a post-shrinkage test reveals this before money is committed to a tool.
Q7. Why are two oven temperatures specified — 80 °C for UF and 110 °C for everything else?
Urea-formaldehyde moulding materials are thermally less stable and lose volatiles/undergo further condensation at lower temperatures, so they are aged at 80 °C ± 2 °C. All other thermosets are aged at 110 °C ± 3 °C, an accelerated but not destructive conditioning temperature that represents elevated service conditions.
Q8. Why are there two exposure times (48 h and 168 h)?
48 h ± 1 h = rapid determination — for quick comparison, production control, incoming inspection.
168 h ± 2 h = normal determination — the reference value for material data sheets and for dimensional-accuracy qualification.
Post-shrinkage depends strongly on exposure time, so the standard requires the exposure time to be recorded and to follow the material specification. Values from different exposure times are not interchangeable.
Q9. Why do plates use the average of two readings taken 20 mm from the corners?
Plate corners are prone to rounding, flash and filling defects. Measuring 20 mm in from the corners, twice in the same direction and averaged, gives a stable, repeatable value and filters out edge effects.
Q10. Why is the direction of measurement reported for plates?
Injection-moulded thermosets — especially fibre-filled ones — shrink anisotropically: fibres and molecules align with flow, so shrinkage parallel to flow differs from shrinkage across it. The standard therefore requires the direction to be stated relative to the injection direction, and allows the two orthogonal shrinkages to be measured and reported independently.
Q11. What are the most common sources of error?
Measuring the mould warm, or at a different temperature than the specimen
Not checking the mould for wear (cavity length drifts over time)
Allowing specimens to warp during cooling (no load, or a conductive/metallic cooling surface)
Using a positive multi-cavity mould, where cavity-to-cavity density variation causes inconsistent shrinkage
Comparing PS values obtained at different exposure times
Measuring at the plate corners instead of 20 mm from them
Mixing up L₀/L₁/L₂ or using L₀ instead of L₁ as the denominator for post-shrinkage
Q12. Which standards are related or equivalent to ISO 2577?
Normative: ISO 295, ISO 10724-1, ISO 10724-2
Thermoplastic counterpart: ISO 294-4:2018 / EN ISO 294-4:2019; ASTM D955-21 (US, thermoplastics only)
Adjacent for thermosets: EN 1842:1997 (SMC/BMC compression moulding shrinkage); ISO 1268-11 (BMC/long-fibre small plates); ISO 10350-1 (comparable single-point data — cites ISO 2577)
National adoptions: GB/T 39818-2021 (China, ISO 2577:2007 MOD); UNE-ISO 2577:2014 (Spain); NEN-ISO 2577:2008 (NL); SS-ISO 2577:2011 (Sweden); IS 13360-3-5:2013 (India); JB/T 6542-1993, JB/T 3958.2-2015 (Chinese electrical thermoset sector standards)
Q13. Is ISO 2577 a "machine test"?
It is a dimensional / specimen-preparation test method, not a mechanical-strength test. The "equipment" is a mould + press or injection machine, a 0.02 mm measuring instrument, and an ageing oven. Laboratories usually buy it as a package, because MS and PS both depend on how the specimen was moulded.
Q14. Why choose ISO 2577 Thermosetting Plastics Shrinkage Test Machine from UnitedTest?
UnitedTest manufactures ISO 2577 compliant testing equipment for measuring moulding shrinkage and post‑shrinkage of thermosetting plastics, BMC, SMC, phenolic, melamine and urea‑formaldehyde moulding compounds. Complete lab solution for quality control, R&D and mould validation.
UnitedTest is a professional manufacturer of ISO 2577 shrinkage testing machines for thermosetting moulding materials. Our lab instruments support accurate measurement of moulding shrinkage and heat‑treatment post‑shrinkage for compression‑moulded bars and ISO‑D2 injection‑moulded square plates according to ISO 2577:2007 international standardISO.
Thermosetting moulding compounds (BMC, SMC, phenolic resin, melamine, urea‑formaldehyde) suffer dimensional shrinkage after moulding and long‑term thermal exposure. Accurate shrinkage data is critical for mould cavity design, incoming raw‑material inspection, batch‑to‑batch quality control and precision component material selection. Our ISO 2577 test system helps polymer laboratories, compounding factories and moulding manufacturers get repeatable, audit‑ready shrinkage percentage data.
Our ISO 2577 shrinkage test solution includes high‑precision dimension measuring equipment (0.02 mm resolution), temperature‑controlled laboratory oven for post‑shrinkage thermal ageing, specimen support fixtures and standard test‑report templates fully aligned with ISO 2577 requirements.
Key advantages of UnitedTest ISO 2577 shrinkage test equipment:
✅ Fully complies with ISO 2577:2007 test procedure, together with referenced standards ISO 295, ISO 10724‑1, ISO 10724‑2
✅ Supports both compression‑moulded bar specimens (120 × 15 × 10 mm) and injection‑moulded D2 square plates (60 × 60 × 2 mm)
✅ Precision dimension measurement up to 0.02 mm accuracy for mould cavity and specimen length
✅ Programmable high‑temperature oven for post‑shrinkage test: 80 °C for urea‑formaldehyde; 110 °C for other thermosets, with 48 h /168 h ageing cycles
✅ Standard atmosphere conditioning guidance for specimen cooling (23 °C ±2 °C, RH 45‑55 %)
✅ Built‑in calculation for moulding shrinkage MS and post‑shrinkage PS48h / PS168h; export complete ISO‑compliant test reports ✅ Suitable for QC production lab, polymer R&D, third‑party testing laboratory, material compounding and thermoset injection / compression moulding factories
Common materials tested on UnitedTest ISO 2577 shrinkage tester: ‑ Phenolic moulding compounds ‑ Melamine formaldehyde materials ‑ Urea‑formaldehyde moulding powders ‑ BMC (Bulk Moulding Compound) ‑ SMC (Sheet Moulding Compound) ‑ Fibre‑filled thermosetting moulding materials
If you are looking for reliable ISO 2577 shrinkage test equipment for thermosetting plastics, contact UnitedTest for technical datasheet, quotation and lab‑application consultation.