Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D7405 MSCR Test by Dynamic Shear Rheometer

ASTM D7405 MSCR Test by Dynamic Shear Rheometer

Share:

ASTM D7405 MSCR Asphalt Binder Tester | Multiple Stress Creep Recovery DSR Rheometer | UnitedTest

UnitedTest manufactures ASTM D7405 compliant dynamic shear rheometer systems for MSCR testing of asphalt binders. The Multiple Stress Creep and Recovery test measures percent recovery (%R) and non-recoverable creep compliance (Jnr), assessing elastic behaviour, stress sensitivity and rutting resistance for neat and polymer-modified bitumen in Superpave pavement design and asphalt lab quality control.


ASTM D7405 defines the Multiple Stress Creep and Recovery (MSCR) test performed with a dynamic shear rheometer (DSR) to characterize asphalt binder performance at specified test temperatures. This method calculates percent recovery (%R) and non-recoverable creep compliance (Jnr), which quantify elastic response, stress dependency and susceptibility to permanent deformation or rutting. It works for both unmodified base asphalt binders and polymer-modified binders such as SBS modified bitumen, and serves widely in Superpave grading, pavement material qualification, R&D and routine quality assurance for road construction laboratories. 


UnitedTest supplies high-precision DSR and MSCR testing equipment fully aligned with ASTM D7405 for asphalt testing facilities and bitumen production plants.


Test Principle 

ASTM D7405 is a stress‑controlled creep‑and‑recovery test performed in shear:

  1. A constant shear stress is applied to the binder for 1s (creep), then removed for 9s (zero‑stress recovery).

  2. At the end of creep the total strain consists of a recoverable (delayed‑elastic) part and a permanent (non‑recoverable) part.

  3. Divided by the applied stress, the residual strain becomes the non‑recoverable creep compliance Jₙᵣ (kPa⁻¹) — a direct measure of the binder's contribution to permanent deformation (rutting). Lower Jₙᵣ = better rutting resistance.

  4. The fraction of strain given back during the 9 s rest is the percent recovery R (%) — the measure of elastic response, and the property that separates a genuinely elastomer‑modified binder from one that is merely hard.

  5. Running the same sequence at two stress levels (0.100 and 3.200 kPa) exposes stress dependence / non‑linearity, which is exactly what the conventional single‑point rutting factor G*/sin δ (measured inside the linear viscoelastic range) cannot see .


Test Specimens

  • Specimen preparation follows ASTM D7175 standard procedures for DSR asphalt binder samples.

  • Specimens can be original unaged asphalt, short‑term aged (RTFOT D2872), long‑term aged (PAV D6521), or combined RTFOT+PAV aged residues.

  • A specimen previously tested under dynamic oscillatory shear in DSR may be reused for MSCR, provided it stays unloaded for at least 1 min before starting MSCR cycles.


ASTM D7405 MSCR Test by Dynamic Shear Rheometer test equipment required:

Dynamic Shear Rheometer (DSR)

Must operate in stress‑control mode, complying with requirements in ASTM D7175.

Temperature‑control unit for precise specimen thermal conditioning.

DSR software capable of time‑stamped strain‑stress recording and mathematical extrapolation for target time‑point strain values when exact sampling misses 1.0 s and 10.0 s timestamps.

Geometry

25 mm parallel‑plate setup, test gap fixed at 1 mm. Plate radius parameter shall be set to 100 % in instrument software.


Test Parameters and stipulation:

Creep loading duration1.00 s per cycle
Zero‑stress recovery duration9.00 s per cycle; total cycle length = 10 s
Low creep stress0.100 kPa
High creep stress3.200 kPa
Cycles at 0.100 kPaTotal 20 cycles: first 10 = conditioning; cycles 11‑20 (N = 1‑10) = data acquisition
Cycles at 3.200 kPa10 cycles (N = 1‑10) for data acquisition
Total test runtime300 s, no rest interval between consecutive cycles
Test temperatureTypically the PG high‑temperature grade (without grade bumping) of the performance‑graded binder, per D6373 / AASHTO M 332; reported to 0.1 °C precision
Data‑sampling frequency≥ 0.10 s interval during creep phase; ≥ 0.45 s interval during recovery phase; explicit data points or extrapolated values required at 1.00 s and 10.00 s for each cycle


Detailed Test Procedures of ASTM D7405 MSCR Test by Dynamic Shear Rheometer

  1. Bring the specimen to thermal equilibrium at the target temperature per D7175; if previously sheared dynamically, rest unloaded ≥1 min.

  2. Run each cycle: 1.00 s creep at constant stress, 9.00 s recovery at zero stress; full torque within 0.003 s; record strain at the prescribed sampling rates, capturing 1.00 s and 10.00 s.

  3. Without rest periods, perform 20 cycles at 0.100 kPa; discard the first 10 (conditioning), keep cycles N = 1–10.

  4. Immediately continue with 10 cycles at 3.200 kPa (total 300 s).

  5. For every analysed cycle at both stresses, record ε₀, ε_c, ε_r and compute ε₁ and ε₁₀.

  6. Compute per‑cycle R and Jₙᵣ, then the ten‑cycle averages and the two percent‑difference values; apply the zero‑substitution and ε₁‑substitution rules where recovery is negative.

  7. Report all eight items with the stated rounding.


Industry / Application Fields

  • Asphalt binder specification and PG grading. MSCR is the high‑temperature grading test in AASHTO M 332 (and ASTM D8239), replacing the RTFO G*/sin δ ≥ 2.20 kPa criterion. Binders are designated PG 64S‑22, PG 64H‑22, PG 64V‑22, PG 64E‑22, tested at the climatic high temperature with a traffic letter: S ≤ 4.5, H ≤ 2.0, V ≤ 1.0, E ≤ 0.5 kPa⁻¹ for Jₙᵣ3.2, with Jₙᵣdiff ≤ 75 % in all cases . (External; limits vary slightly by edition — earlier MP19 used 4.0 for "S".)

  • Replacement for "grade bumping." Instead of artificially raising the temperature grade for slow/heavy traffic, the traffic letter carries the traffic requirement — specifying both is paying twice for one requirement .

  • Verification of polymer modification / elasticity. Percent recovery is the practical discriminator between elastomeric (SBS‑type) modification, plastomeric modification, and hard unmodified binder; AASHTO R 92 evaluates elastic response on a %R–Jₙᵣ curve (e.g. %R ≥ 29.371·Jₙᵣ3.2^−0.2633 for Jₙᵣ3.2 ≤ 2.0) .

  • Refinery / terminal QC, DOT acceptance testing, mix design and forensic pavement investigation, plus research on modifiers, warm‑mix additives, rejuvenators, and GTR/rubber binders.

  • The standard itself states it may serve as a surrogate for D5801 (toughness & tenacity), D6084/D6084M (ductilometer elastic recovery) and D7175 phase angle in measuring elasticity.


Related Standard: 

AASHTO T51

Practically identical test method for asphalt ductility, adopted by North‑American highway transportation agencies.

ASTM D5Penetration test of bituminous materials (routine companion binder test).
ASTM D113Standard Test Method for Ductility of Asphalt Materials
ASTM D2872Rolling Thin‑Film Oven Test (RTFO) for short‑term thermal‑oxidative ageing of asphalt, supplies aged‑residue samples for D113 ductility measurement.
ASTM D6648Standard Test Method for Determining the Flexural Creep Stiffness of Asphalt Binder Using the Bending Beam Rheometer (BBR)
ASTM D1754Thin‑Film Oven Test (TFOT) for asphalt ageing.
ASTM D7405Standard Test Method for Multiple Stress Creep and Recovery (MSCR) of Asphalt Binder Using a Dynamic Shear Rheometer
EN 13589

Bitumen and bituminous binders. Determination of the tensile properties of modified bitumen by the force ductility method


Keywords: ASTM D7405, MSCR test, multiple stress creep and recovery, dynamic shear rheometer, DSR asphalt tester, non-recoverable creep compliance Jnr, percent recovery asphalt test, asphalt binder rutting resistance test, polymer modified bitumen rheology, Superpave asphalt performance test, SBS modified asphalt test, bitumen creep recovery tester, asphalt rheometer equipment, AASHTO TP70 MSCR, asphalt binder stress sensitivity test, UnitedTest asphalt testing machine, highway pavement material lab test, asphalt quality control rheology instrument

Related products and device

Asphalt Materials Ductility unviersal tensile testing machine

A single column tensile tester is a sophisticated material testing instrument designed for measuring mechanical properties of various materials under tension, compression, bending, shear, and other loading conditions. As the name suggests, it features a single vertical column supporting a moving crosshead that applies force to test specimens.

asphalt briquet ductility testing equipment

Tensile test fixture for plastics is based on the test standatd ASTM D638, determination of the tensile properties of unreinforced and reinforced plastics in the form of standard dumbbell-shaped test specimens when tested under defined conditions of pretreatment, temperature, speed.

elongation long travel extension extensometer

High Elongation Extensometer is mainly used together with the tensile test machine for the rubber tension testing. It can measure the elongation of the product with high precision and accurately capture the displacement data. With a deformation measurement range typically from 10mm to 800mm.

Video extensometer / Non-contact extensometer

Video extensometer, is a non-contact real-time high-precision strain measurement system, which is based on a separate camera and real-time image processing algorithm, by taking images of the experimental process, analyzing image characteristic changes, dynamically measuring the strain changes.

Related Standard

ASTM D6648 Asphalt Binder Test | Bending Beam Rheometer (BBR) –

ASTM D6648 Determining the Flexural Creep Stiffness of Asphalt Binder Using the Bending Beam Rheometer (BBR)

ASTM D6648 measuring flexural creep stiffness and m‑value of asphalt binders with a Bending Beam Rheometer (BBR). Derived from SHRP research, it is a core low‑temperature rheology test for Superpave performance‑graded (PG) asphalt binders.


ASTM D1754 Thin-Film Oven Test (TFOT) –

ASTM D1754 Standard Test Method for Effect of Heat and Air on Asphaltic Materials (Thin-Film Oven Test)

The thin-film oven test (TFOT) defined by ASTM D1754 / D1754M-20 (equivalent to AASHTO T 179 and EN 12607-2) is the reference laboratory method for simulating the short-term aging — the combined effect of heat and air — that asphalt binder undergoes during hot mixing, hauling and paving. In the test, 50 ± 0.5 g of bitumen is held as a 3.2 mm film in a 140 mm stainless-steel pan and conditioned for 5 hours at 163 °C on a shelf rotating at 5.5 r/min. The aged residue is then tested for penetration, viscosity and ductility, and the results compared with the unaged binder to show how much the material hardens in service.


EN 13589 Force Ductility Test for Bituminous Materials –

EN 13589 Bitumen and bituminous binders‑Determination of the tensile properties of modified bitumen by the force ductility method

EN 13589 evaluates tensile and cohesive performance of bituminous binders (especially polymer‑modified bitumen, PmB) by measuring force‑elongation response during stretching, and calculates cohesion energy as a key quality indicator. 

ASTM D5801 Toughness and Tenacity Test of Asphalt Materials –

ASTM D5801 Standard Test Method for Toughness and Tenacity of Asphalt Materials

ASTM D5801 specifies a uniaxial tensile test procedure to quantify two core mechanical indicators—toughness and tenacity—of asphalt binders, with primary application for elastomer/polymer-modified asphalt, while also applicable to unmodified neat asphalt. This test provides critical insights into how well an asphalt can resist cracking and deformation under stress, making it a key tool in assessing durability and performance in pavement applications. While many asphalt tests focus on stiffness or viscosity, D5801 uniquely measures energy absorption during deformation—directly related to crack resistance and long-term pavement integrity.  

ASTM D412 Tensile Strength of Rubber and Elastomers –

ASTM D412 test methods cover procedures used to evaluate the tensile (tension) properties of vulcanized thermoset rubbers and thermoplastic elastomers. These methods are not applicable to ebonite and similar hard, low elongation materials. 

ASTM D412 is the primary standard for evaluating the tensile properties of vulcanized thermoset rubbers and thermoplastic elastomers (TPEs). It provides precise procedures for determining critical mechanical characteristics that define material performance under stretching forces. 

The methods appear as follows:

Test Method A—Dumbbell and Straight Section Specimens

Test Method B—Cut Ring Specimens

ISO 527-1, ISO 527-2 Tensile Test of Plastics Composites & plastics –

ISO 527-1 covers the test procedures for determining tensile properties of plastics and plastic composites. Tensile properties of plastics that are determined through the practices of ISO 527-1 include tensile strength, tensile modulus and other properties related to stress strain characteristics of plastic materials. 

ISO 527-2 specifies the test conditions for determining the tensile properties of moulding and extrusion plastics, based upon the general principles given in ISO 527-1. The methods described in ISO 527-2 are selectively suitable for use with the following range of materials: rigid and semi-rigid thermoplastics moulding, extrusion and cast materials, including compounds filled and reinforced by, for example, short fibres, small rods, plates or granules but excluding textile fibres (see ISO 527-4 and ISO 527-5).

ISO 527-3 Tensile Test on Plastic Film –

ISO 527-3 Plastics - TENSILE PROPERTIES - PART 3: FOR FILMS AND SHEETS

ISO 527-3 specifies the test conditions for determining the tensile properties of plastic films and sheets with a thickness less than 1 mm, based on the general principles of ISO 527-1. Provides standardized procedures to measure critical mechanical parameters including tensile strength, yield strength, elongation at break, and Young's modulus for thin plastic materials. It is critically important because thin films behave very differently under stress compared to rigid plastics; they are more prone to tearing, slipping, and deformation. By standardizing the test conditions, this document ensures that material specifications, quality control, and research data are globally comparable and reliable.  Specimen created following ISO 527-3 can be used to determine the tensile properties of thin plastic sheets and films including the tensile modulus of elasticity and the tensile energy to break (TEB).

Frequently Asked Questions -- ASTM D7405 MSCR Test by Dynamic Shear Rheometer

Q1. What is ASTM D7405?

ASTM D7405 is the ASTM standard test method for Multiple Stress Creep and Recovery (MSCR) of asphalt binder, run on a Dynamic Shear Rheometer (DSR). It determines two things: percent recovery (%R) and non-recoverable creep compliance (Jₙᵣ) at a specified temperature. It was originally approved in 2008, revised in 2010, 2015, 2020 and 2024 (current active version: D7405-24). It sits under ASTM Committee D04 (Road and Paving Materials), Subcommittee D04.44 (Rheological Tests), and is based on work product of the U.S. Federal Highway Administration.


Q2. What does "MSCR" actually mean, and what does the test do?

Multiple Stress Creep and Recovery. The binder is loaded at a constant shear stress for 1 second and then allowed to recover at zero stress for 9 seconds. This cycle is repeated at two stress levels — 0.100 kPa and 3.200 kPa. Because the binder is pushed well beyond the tiny strains used in oscillatory testing, the test captures the non-linear, delayed-elastic and permanent-deformation behaviour that a truck wheel actually produces in a pavement.


Q3. What two numbers come out of the test?

  1. Jₙᵣ (non-recoverable creep compliance, kPa⁻¹) — the strain left behind after recovery divided by the applied stress. It is a direct measure of the binder's contribution to permanent deformation (rutting). Lower = better.

  2. %R (percent recovery) — how much of the creep strain the binder gives back during the 9 s rest. It is the practical measure of elastic response, and it is what distinguishes a genuinely elastomer-modified binder from one that is merely hard.

Two derived stress-sensitivity parameters are also reported: R_diff and Jₙᵣdiff, both expressed as a percentage change between the 0.1 kPa and 3.2 kPa stages.


Q4. Why was MSCR developed when G*/sin δ already existed?

The traditional Superpave rutting parameter G*/sin δ (AASHTO T 315 / ASTM D7175) is measured at very small strain, inside the linear viscoelastic region, at a single frequency. A hard unmodified binder and a properly polymer-modified binder can return the same G*/sin δ and then behave completely differently in service. MSCR was developed to close that gap: research (Bahia et al. 2001; D'Angelo et al. 2007) showed Jₙᵣ correlates far better with measured rutting on accelerated loading facility sections than G*/sin δ does. It is now the high-temperature grading test in AASHTO M 332 and ASTM D8239.


Q5. Is MSCR only for polymer-modified binders?

No. The standard applies to both polymer-modified and unmodified binders (Scope 1.3). But the elastic-response information it delivers is especially valuable for modified binders, because that is the property G*/sin δ cannot see.


Q6. Can I reuse a specimen that was already tested in oscillatory shear?

Yes. Note 3 permits testing a specimen previously run in dynamic shear per D7175, but the specimen must be left unloaded for at least 1 minute before the creep and recovery sequence starts.


Q7. What data acquisition rates does the standard require?

Stress and strain recorded at least every 0.10 s during the creep phase and at least every 0.45 s during the recovery phase, on a running accumulated time, with explicit points at 1.00 s and 10.00 s of each cycle's local time. If the DSR does not capture those exact instants, its software must extrapolate from a measured point no more than 0.10 s earlier (creep) / 0.50 s earlier (recovery). Note 4: if the curves are to be used for modelling, more frequent points may be needed.


Q8. How repeatable is the MSCR test?

Per Table 1 of D7405-20 (8 laboratories, 8 binders, five PG grades): single-operator coefficient of variation is about 2.4 % for R₀.₁, 3.0 % for R₃.₂, and 4.6–13.7 % for Jₙᵣ depending on magnitude; multilaboratory values are roughly 5.4 %, 6.5 % and 8–17 %. The acceptable range of two results (d2s %) reaches 26.6 % single-operator and 42.6 % multilaboratory for Jₙᵣ3.2 in the 0.10–0.25 kPa⁻¹ band. Below 0.1 kPa⁻¹ the standard gives no precision estimate because variability is too high.


Q9. Is ASTM D7405 the same as AASHTO T 350?

They are technically equivalent MSCR test methods. D7405-20 explicitly states its precision criteria are based on this standard and the procedure given in AASHTO T 350. T 350 began life as the provisional AASHTO TP 70; ASTM's first version appeared in 2008. In practice: ASTM D7405 = the test method; AASHTO M 332 / ASTM D8239 = the specification that uses its results.


Q10. How does it differ from the European EN 16659 MSCR method?

The cycle definition (1 s creep / 9 s recovery, 0.1 and 3.2 kPa) is the same. The main difference is conditioning: ASTM D7405 (2015 onward) and AASHTO T 350-19 require 20 cycles at 0.1 kPa, with the first 10 discarded as pre-conditioning; EN 16659:2015 requires no preloading — only 10 cycles at 0.1 kPa. Laboratories also differ on where stress and strain are recorded (e.g. at 2/3 of plate radius vs. the extremity), which affects results.


Q11. Which standards are referenced by D7405?

ASTM D7175 (DSR apparatus/specimen prep — the parent method), D2872 (RTFOT), D6521 (PAV), D6373 (PG specification), D8 (terminology), C670 (precision & bias practice), D3666 (laboratory competence). The standard also says MSCR can serve as a surrogate for D5801 (toughness & tenacity), D6084/D6084M (ductilometer elastic recovery) and D7175 phase angle when measuring elasticity. AASHTO references: T 350 and M 332.


Q12. Which industries use this test?

Asphalt refineries and terminals (product certification), state/provincial DOTs and highway agencies (acceptance testing and PG verification), independent and commercial asphalt laboratories, paving contractors and mix-design consultants, polymer/modifier producers (SBS, rubber/GTR, warm-mix additives, rejuvenators), and university / pavement research institutes.


Q13. What are the practical cautions when running MSCR?

Results depend on operator competence and on DSR capability, calibration and maintenance — compliance with D3666 alone does not guarantee reliable results. Watch specifically: true stress-control mode, torque rise time ≤ 0.003 s, correct 25 mm / 1 mm geometry and radius parameter, genuine thermal equilibrium, correct 1.00 s / 10.00 s data capture, and the negative-recovery and low-Jₙᵣ pitfalls described above.


Q14. Why choose UnitedTest Dynamic Shear Rheometer, ASTM D7405‑20 MSCR Multiple Stress Creep and Recovery Test Equipment? 

UnitedTest manufactures high‑performance Dynamic Shear Rheometer (DSR) fully compliant with ASTM D7405‑20 & AASHTO T350 for asphalt binder MSCR Multiple Stress Creep and Recovery test. Measure Jnr non‑recoverable creep compliance & percent recovery to evaluate asphalt rutting resistance for road‑pavement laboratories.


UnitedTest is a professional manufacturer of asphalt rheology laboratory testing instruments. Our Dynamic Shear Rheometer (DSR) fully complies with ASTM D7405, AASHTO T350, ASTM D7175 and related global asphalt binder standards, delivering reliable Multiple‑Stress Creep and Recovery (MSCR) test results for road‑pavement material labs, highway research institutes, asphalt plants and third‑party testing organizations worldwide.

The ASTM D7405 MSCR test has become the critical modern test method to assess high‑temperature rutting resistance and nonlinear elastic performance for both neat asphalt and polymer‑modified asphalt binders. Unlike conventional oscillatory DSR measurements, MSCR applies cyclic creep‑recovery loading at 0.1 kPa and 3.2 kPa stress levels, generating key parameters including percent recovery (R0.1, R3.2) and non‑recoverable creep compliance, which directly correlate with real‑world pavement permanent deformation under repeated vehicle traffic load.

UnitedTest DSR system adopts precise stress‑control mode, with certified fast torque response meeting ASTM D7405‑20 requirements. Supporting standard 25 mm parallel‑plate geometry with 1 mm gap setting, the built‑in dedicated MSCR test software automatically runs full test sequences: sample conditioning cycles, data acquisition cycles, strain extrapolation, per‑cycle calculation and final standard‑format report generation according to ASTM D7405 reporting rules. It supports testing unaged, RTFOT‑aged and PAV‑aged asphalt binder residues for complete performance‑grade (PG) asphalt binder evaluation following AASHTO M332 specifications.

Whether you perform asphalt QC production testing, highway material research, third‑party lab accreditation tests or modified asphalt material development projects, UnitedTest ASTM D7405‑compliant DSR offers stable repeatability, user‑friendly workflow and comprehensive data output for MSCR Multiple Stress Creep and Recovery characterization of asphalt binders.


Key Search‑friendly bullet points for page content:

  • ✅ Fully meets ASTM D7405‑20 MSCR Multiple Stress Creep and Recovery standard

  • ✅ Compliant with AASHTO T350 MSCR test for asphalt binders

  • ✅ Stress‑control DSR for measuring Jnr non‑recoverable creep compliance & percent recovery

  • ✅ 25 mm parallel‑plate geometry, 1 mm test gap for asphalt binder MSCR test

  • ✅ Auto‑calculate R0.1, R3.2, Jnr0.1, Jnr3.2, stress‑difference indexes

  • ✅ Supports unaged / RTFOT / PAV aged asphalt binder samples

  • ✅ Complete solution for PG performance‑graded asphalt binder high‑temperature rutting‑resistance testing

< Previous: ASTM D7078 V-Notched Rail Shear Test for Composite Materials

> Next: ASTM D7615 Open-Hole Fatigue Testing for Polymer Matrix Composite Laminates

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.