Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D2872 Rolling Thin Film Oven RTFO Test

ASTM D2872 Rolling Thin Film Oven RTFO Test

Share:

ASTM D2872 Rolling Thin-Film Oven Test | RTFO Asphalt Aging Tester | UnitedTest

UnitedTest manufactures ASTM D2872 rolling thin-film oven (RTFO) test equipment to evaluate short-term thermal oxidative aging of asphalt binder. This standard quantifies property changes and mass loss of semi-solid asphaltic materials exposed to heat and circulating air, widely used for Superpave asphalt quality control and road pavement material qualification.


ASTM D2872, also known as the Rolling Thin‑Film Oven Test (RTFO), evaluates the combined effect of heat and circulating air on a continuously moving thin film of semi-solid asphalt binder. This lab test simulates short-term aging that asphalt undergoes during hot mixing, transportation and paving operations. Testing records key binder properties before and after oven conditioning, and supports optional mass change measurement to assess volatile loss and ageing degradation for highway bitumen and modified asphalt formulations. UnitedTest supplies precision RTFO testing machines fully compliant with ASTM D2872 for asphalt laboratories and road construction material testing.


Test Principle

A thin film of semi‑solid asphalt binder is continuously renewed by rolling 35 g of binder inside a horizontal glass bottle while heated at 325 °F (163 °C) for 85 min in a convection oven, with a jet of heated, dried, dust‑free air blown into each bottle at the lowest point of its travel.

The physical principle is accelerated short‑term oxidative ageing + volatilisation:

  • The rolling action continuously exposes a fresh binder surface, so no surface skin forms (a skin would inhibit oxidation), the film stays thin and uniform, and modifiers stay dispersed .

  • Heat drives off light volatile fractions (mass loss); oxygen reacts with the binder to form polar, higher‑molecular‑weight species (mass gain). The net result determines whether the binder shows a mass gain or loss.

  • The outcome is a RTFO residue whose properties approximate the condition of the binder as it exists in the finished pavement, i.e. after plant mixing, hauling, laying and compaction at about 302 °F (150 °C) .

Ageing effect is quantified by measuring selected properties before and after the oven treatment (viscosity, ductility, and optionally mass change), or by feeding the residue into further tests (DSR, and after PAV, BBR/DTT).


Test Specimen Requirements

  • Material: Semi‑solid asphalt binders (neat or modified asphalt cement). The incoming sample must be free of water.

  • Specimen mass per bottle: 35 ±0.5 g asphalt binder poured into each standard glass bottle.

  • Number of containers: Up to eight bottles can be mounted on the carriage. Two separate bottles shall be used when mass‑change testing is performed.

  • Sample preparation: Heat asphalt ≤150 °C to make it fully fluid; stir gently without entrapping air bubbles. After pouring, rotate the horizontal bottle to pre‑coat the cylindrical inner wall. Cool filled bottles on the draft‑free cooling rack for 60–180 min before oven loading.


ASTM D2872 Rolling Thin Film Oven RTFO Test Required Test Equipment

Recomend UnitedTest Hot blast Oven with filme size change measuring tools:  

Double‑walled electrically‑heated convection RTFO oven

- Internal dimensions: 15 in (381 mm) height, 19 in (483 mm) width, 17±0.5 in (445±13 mm) depth.

- Symmetrical top‑bottom vents; built‑in squirrel‑cage fan running at 1725 rpm; air plenum on side walls and ceiling.

- Proportional thermostat maintaining test temperature at 325 °F (163 °C) ±1.0 °F (±0.5 °C). Must restore full‑load test temperature within 10 min after sample loading.

ASTM D2872 Rolling Thin Film Oven RTFO Test

Flow meter: measures airflow at target 4000 mL/min, calibrated periodically.

Temperature‑measuring devices. 

Standard glass sample bottles: heat‑resistant clear glass with defined dimensional specifications.

Cooling rack: stainless‑steel / aluminum wire rack allowing free air circulation for horizontal bottle cooling.

Rotating circular metal carriage

12‑in diameter, rotates at 15 ±0.2 r/min, holds up to eight glass sample bottles in horizontal orientation.

Air‑jet supply system0.040‑in (1.016 mm) orifice for each bottle; 7.6 m refrigeration‑grade copper coil at oven bottom; source of fresh, dried, dust‑free regulated air.
Analytical balance

resolution ≥0.001 g (required for mass‑change determination).


Key test parameter: 

Oven test temperature325 °F (163 °C), tolerance ±1.0 °F (±0.5 °C)
Carriage rotational speed15 ±0.2 rpm
Air‑flow rate4000 ±300 mL/min dry clean air
Standard conditioning time (sea‑level / low elevation)85 min; adjusted upward at higher laboratory elevation (atmospheric‑pressure correction)
Air‑jet orifice position1/4 in ±1/8 in (6 mm ±3 mm) from bottle opening, horizontal jet direction
Pre‑heat requirementEither experimentally determined equilibrium time plus extra 30 min, or minimum fixed pre‑heat of 4 h
Post‑test residue testing windowResidue properties shall be measured within 72 h after finishing RTFO conditioning


Complete Test Procedures of ASTM D2872 Rolling Thin Film Oven RTFO Test

  1. Oven pre‑heat determination: Either perform thermal‑equilibration test plus extra 30 min, or use minimum 4‑h pre‑heat.

  2. Oven setup: Adjust air‑jet position, install calibrated thermometer, level oven, start fan, pre‑heat oven to reach 163 °C set‑point.

  3. Sample preparation: Heat raw asphalt to fluid state without water; pour 35±0.5 g into each glass bottle; rotate bottles horizontally to pre‑coat inner wall; cool 60‑180 min on cooling rack. Weigh bottles if mass‑change test is needed.

  4. Loading and aging: Mount bottles on rotating carriage; fill empty slots with dummy bottles; close door, start carriage rotation and regulated air flow. Maintain conditioning for elevation‑adjusted time. Confirm oven recovers test temperature within 10 min.

  5. Post‑aging sample retrieval: After conditioning time expires, take out mass‑change bottles first and place horizontally on cooling rack. Take remaining bottles one‑by‑one; pour and scrape asphalt residue into collection vessel. Keep oven door closed as much as practical, finish all removals within 5 min.

  6. Residue homogenization: Gently stir collected residue without introducing air bubbles. Perform subsequent property tests within 72 hours.

  7. Mass‑change measurement (optional): Cool dedicated bottles 60‑180 min, weigh on analytical balance, compute corrected mass‑change percentage.

  8. Report test results: Document property differences pre‑ and post‑aging, mass‑change (if measured), lab elevation and actual conditioning time.


Industrial Application Fields

  • Asphalt binder / bitumen production and refining; hot‑mix asphalt (HMA/WMA) mix design.

  • Highway and airport pavement engineering, state DOT and contractor quality control/quality assurance laboratories.

  • Binder specification compliance and certification (Superpave PG grading, AASHTO M 320 / M 332, ASTM D6373), supplier qualification, and forensic investigation of binder overheating, contamination or excessive volatiles.

  • Research on ageing kinetics, polymer‑modified and rejuvenated/reclaimed binders, warm‑mix additives, and bio‑binders.

  • Independent testing/accreditation laboratories operating under Specification D3666.


Related Standard: 

ASTM D1754

Standard Test Method for Unrestrained Linear Thermal Shrinkage of Plastic Film and Sheeting.

ASTM D2872

Rolling Thin‑Film Oven Test, RTFOT: The most comparable short‑term asphalt aging test. 

D1754 TFOT uses static thin film for 5 h at 163 °C; D2872 RTFOT uses continuously‑rolling thin‑film samples for 85 min at 163 °C with forced air flow. 

Both simulate plant short‑term aging, but are not fully interchangeable without specification adjustment.

ASTM D5

Penetration test for bituminous materials, used to test original and TFOT‑residue penetration.

ASTM D113Ductility of Asphalt Materials (residue test)
ASTM D2171Viscosity of Asphalts by Vacuum Capillary Viscometer (residue test at 60 °C)
ASTM D3666Minimum Requirements for Agencies Testing and Inspecting Road and Paving Materials
EN 12607‑1European RTFOT method for bitumen short‑term ageing
ASTM D6521Simulates long‑term in‑service asphalt aging; usually applied after TFOT / RTFOT residue to simulate pavement service‑life oxidative aging.
ASTM E145Specification for gravity‑convection and forced‑ventilation ovens, mandatory equipment reference for TFOT oven performance
OtherAASHTO T 179 / EN 12607-2 / IS 9382; RTFOT: AASHTO T 240 / EN 12607-1; 


Keywords: ASTM D2872, rolling thin film oven test, RTFO tester, asphalt binder aging test, short term asphalt aging, bitumen thermal oxidation test, Superpave asphalt test, asphalt mass loss test, modified bitumen ageing oven, highway pavement material test, asphalt rolling thin film oven, UnitedTest asphalt testing machine, AASHTO T240 RTFO equipment, bitumen binder quality control, asphalt rheology aging test

Related products and device

ASTM D2872 Rolling Thin Film Oven RTFO Tester

Suitable to measure various kinds of plastic pipe or plastic materials size change after heating, or used to heat the test sample. It can be used as a heating oven as well.

Plastic Films Dimensional stability tester

Professional film heat shrink tester is precision lab equipment engineered to evaluate thermal shrinkage characteristics and thermal dimensional stability of diverse raw materials, including plastic films. compliant with international testing standards ASTM D2732 and ISO 11501.

Film Heat Shrinkage Tester

Integrated Film Thermal Shrinkage Performance Tester, simultaneously captures real-time test data including temperature, thermal shrinkage force, residual shrinkage force and shrinkage displacement, Conform with ISO 14616, DIN 53369, ASTM D2732 as a shrink force tester or comprehensive shrink tester

Related Standard

ASTM D1754 Thin-Film Oven Test (TFOT) –

ASTM D1754 Standard Test Method for Effect of Heat and Air on Asphaltic Materials (Thin-Film Oven Test)

The thin-film oven test (TFOT) defined by ASTM D1754 / D1754M-20 (equivalent to AASHTO T 179 and EN 12607-2) is the reference laboratory method for simulating the short-term aging — the combined effect of heat and air — that asphalt binder undergoes during hot mixing, hauling and paving. In the test, 50 ± 0.5 g of bitumen is held as a 3.2 mm film in a 140 mm stainless-steel pan and conditioned for 5 hours at 163 °C on a shelf rotating at 5.5 r/min. The aged residue is then tested for penetration, viscosity and ductility, and the results compared with the unaged binder to show how much the material hardens in service.


ISO 11501 Heat dimensional change of plastic films sheeting –

ISO 11501 Plastics — Film and sheeting — Determination of dimensional change on heating

ISO 11501 specifies a uniform laboratory test method to quantify thermal dimensional variation of plastic films and thin sheets (max thickness 1 mm), covering both machine (longitudinal) and transverse directions, for all plastics whether heat-shrinkable or non-shrink grade. 

ISO 17555 BOPP films biaxial stretch testing methods –

ISO 17555 applies to packaging-grade BOPP films containing ≥95% polypropylene resin; usable as single-layer film or laminates paired with other plastic substrates. The test stipulated in ISO 17555 mainly include, tensile strength & strain at break, Dimensional change on heating (thermal shrinkage), Coefficient of water vapour transmission, Haze, Wetting tension etc., 

FAQ (Question & Answer) -- ASTM D2872 Rolling Thin Film Oven RTFO Test

Q1. What is ASTM D2872?

ASTM D2872 is the ASTM standard test method for the Rolling Thin-Film Oven Test (RTFOT / RTFO). It measures the effect of heat and air on a moving film of semi-solid asphaltic material. The effect is quantified by measuring selected properties of the binder before and after the oven treatment, plus an optional determination of mass change.


Q2. Why is it called "rolling thin-film"?

Because the binder is placed in a horizontal glass bottle mounted on a vertical circular carriage that rotates at 15 ± 0.2 r/min. As the bottle turns, the binder continuously flows over the inner wall, so a thin film is constantly renewed. Fresh binder is always exposed to heat and to the air jet, no surface skin forms, and modifiers stay dispersed.


Q3. What does the test actually simulate?

Short-term (construction-phase) ageing of asphalt binder: what happens in the pug mill / drum mixer, during hauling, laying and compaction at about 302 °F (150 °C). The RTFO residue is intended to approximate the condition of the binder as it exists in the finished pavement.


Q4. How long does the test take?

The oven conditioning itself is 85 min at sea level (adjusted for laboratory elevation per Table 1: 85 min at 0–999 ft up to 92 min at 7000–7999 ft). Including sample fluidising, pouring, 60–180 min cooling, residue scraping and weighing, allow roughly 3 hours per run, plus oven pre-heat (thermal equilibrium + 30 min, or a minimum of 4 h).


Q5. What is the difference between RTFO and RTFOT?

No technical difference — both refer to the Rolling Thin-Film Oven Test. ASTM D2872 and AASHTO T 240 are the two specification numbers for essentially the same procedure.


Q6. Why is ASTM D2872 important for asphalt binder?

Asphalt binder ages fastest and hardest while it is hot — during plant mixing, transport, paving and compaction. This ageing raises viscosity and stiffness and makes the mix more brittle and crack-prone. RTFO reproduces that ageing in a standardised 85-minute laboratory window, so the binder a lab tests is the binder the pavement actually receives, not the fresh binder from the refinery.


Q7. Why is it a mandatory step in Superpave / PG grading?

In the Superpave performance-graded system, short-term-aged binder (RTFO residue) is tested for high-temperature rutting resistance, and long-term aged binder (RTFO then PAV residue) is tested for fatigue and low-temperature cracking. Without the RTFO conditioning step, DSR, BBR and DTT results are not comparable between laboratories or between binders.


Q8. What does the mass change result tell you?

Mass change is a direct measure of volatility. During the test two opposing things happen: volatile fractions evaporate (mass loss) and oxygen reacts with the binder (mass gain). Binders with few volatiles usually show a small net gain; volatile-rich binders show a net loss. Excess loss flags overheating, contamination with light ends / cut-back material, or an out-of-spec product — which is why specifications limit it.


Q9. Can an ordinary laboratory oven be used?

No. The geometry, vent areas, plenum, fan speed and direction, air-jet orifice, carriage speed and temperature recovery rate are all specified. A general-purpose oven will not produce a standard-conforming result.


Q10. How much sample is needed?

35 ± 0.5 g per bottle. Prepare enough bottles to supply every test planned on the residue. If mass change is measured, two additional dedicated bottles are used.


Q11. How should the sample be prepared?

It must be free of water. Heat it in its container with a loose cover at not more than 150 °C, only for the minimum time needed to make it fluid, then stir manually while avoiding air bubbles.


Q12. Why do I have to rotate the bottle after pouring?

To pre-coat the cylindrical inner surface so the binder forms a continuous film during the test (a full pre-coat is not always achievable for some binders). The open end need not be coated. Bottles then cool horizontally for 60–180 min in a draft-free, room-temperature spot away from heat sources.


Q13. What are the most common causes of a failed run?

Temperature not reaching 163 °C within 10 min; oven not level; wrong jet position or distance; uncalibrated airflow; bottles out of dimensional tolerance (bottles with a small annular ring are prone to leakage); static electricity on the glass disturbing weighing; samples left in the oven too long during removal (all bottles must come out within 5 min of the first); air bubbles entrained during stirring.


Q14. Are RTFO and TFOT interchangeable?

No. Research consistently finds they are not interchangeable, and RTFO is generally more severe on most binders. The two must not be substituted for one another in a specification unless the specification explicitly allows it.


Q15. What are the known limitations of RTFO?

Highly viscous binders and some polymer-modified binders (e.g. PG 70-XX and above) may not flow properly inside the bottle, so the film is not renewed correctly; there is also a risk of leakage from the bottle and of modifier segregation. Bottle dimensional compliance should be checked if flow-out is observed.


Q16. Why choose ASTM D2872 Rolling Thin Film Oven RTFO Tester from UnitedTest? 

UnitedTest is a professional manufacturer of ASTM D2872 Rolling Thin Film Oven (RTFO) test equipment for asphalt and bitumen laboratories worldwide. Our RTFO oven fully complies with ASTM D2872-22 and AASHTO T240 specifications, designed to simulate short-term thermal oxidative aging that asphalt binder undergoes during hot mixing, transportation and paving construction. The machine controls stable test temperature, constant carriage rotation speed and continuous clean air injection, to condition moving thin-film asphalt samples for 85 minutes. After RTFO conditioning, technicians test residual asphalt for mass change, viscosity, G* / sinδ and other rheological indexes. This ASTM D2872 test is a mandatory Superpave binder test, widely used in highway engineering, road construction material labs, asphalt refineries, third-party testing institutes and quality control departments. UnitedTest supplies calibrated, durable RTFO ovens with easy operation, data traceability and after-sales technical support for pavement material testing projects.

< Previous: ASTM D2863 Oxygen Index Test — LOI Testing for Plastics, Rubber, Foam & Film

> Next: ASTM D2924 External Pressure Resistance Test of Fiberglass Pipe

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.