Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D575 Rubber Compression Test Method

ASTM D575 Rubber Compression Test Method

Share:

ASTM D575 Rubber Compression Property Tester | UnitedTest

UnitedTest manufactures ASTM D575 compression testing machines for solid rubber compression-deflection characterization. ASTM D575 includes Method A (fixed deflection, measure force) and Method B (fixed force, measure deflection), suitable for quality control and material stiffness comparison of solid rubber compounds, excluding hard rubber and sponge rubber.


ASTM D575 defines two laboratory test procedures to characterize the compression‑deflection behavior of solid rubber compounds. It does not apply to hard rubber or sponge rubber materials. It contains two inverse procedures: Method A fixes the deflection and measures the force; Method B fixes the force and measures the deflection. This standard is widely adopted for rubber material R&D, incoming inspection, batch quality verification, and performance benchmarking for rubber seals, vibration mounts, elastomer buffers and industrial rubber components. UnitedTest’s ASTM D575 rubber compression tester delivers stable loading control, precise displacement measurement and repeatable test results to meet your elastomer compression performance evaluation requirements.


Test Principle: 

These test methods measure the compressive stiffness of rubber materials. Deflection is defined as the change in specimen thickness when a compressive force is applied, and the test quantifies the functional relationship between applied compressive load and resulting deformation.

It is fundamentally a comparative test method: valid comparisons between materials are only possible when specimens have identical dimensions and geometry, and are tested under identical deflection percentage or applied force conditions.

ASTM D575 Rubber Compression Test Method


Specific Test Methods

The standard includes two distinct test procedures, selected based on the target measurement:

Test Method A – Compression Test of Specified Deflection: Determines the magnitude of compressive force required to produce a predefined percentage deflection (strain) in the specimen.

Test Method B – Compression Test at Specified Force: Applies a defined compressive force (or mass) to the specimen and measures the resulting deflection magnitude.


Key Parameters and Stipulations

Deflection calculation: Percent deflection is calculated based on the original specimen thickness measured before the first force application.

Loading cycles: Method A uses three loading cycles (two conditioning cycles, third cycle for data recording); Method B uses a single loading cycle for rapid testing.

Hold time (Method B): The major test force is applied for exactly 3 seconds before deflection is read.


Test Specimen Information:

Standard cylindrical specimen: 28.6 ± 0.1 mm in diameter (650 mm² / 1.000 in² cross‑sectional area) and 12.5 ± 0.5 mm in thickness. All molded surface layers must be removed prior to testing.

Standard specimens are cut from flat rubber slabs. 

Specimens are punched from ground slabs using a rotating hollow die with low cutting pressure to prevent "cupping" (concave deformation) of the cut surfaces.


ASTM D575 Rubber Compression Test Method required Testing Equipment: 

Universal Test Machine

Must conform to the force calibration requirements of ASTM E4, with a controlled crosshead travel rate of 12 ± 3 mm/min (0.5 ± 0.1 in./min). 

Alternative systems (e.g., platform scales with a yoke and hand‑operated screw) are permitted if they meet accuracy and speed requirements. 

For constant‑force testing, equipment must apply minor and major loads gently without impact.

Tools

Deflection Gage: A dial‑type indicator graduated in increments of 0.01 mm.

Micrometer: Used to measure specimen thickness, in accordance with Method A of ASTM D3767.

Specimen Cutting Tool: A rotating hollow cutting die (mounted on a drill press) used to punch standard cylindrical specimens, lubricated with soapy water to produce smooth, square‑edged cuts.

Interface Material: 400‑grit waterproof sandpaper, placed between the specimen and machine platens to prevent lateral slippage. It is omitted when the specimen surface is bonded to metal.


Key Test Procedures of ASTM D575 Rubber Compression Test Method:

Test Method A (Specified Deflection)

  1. Measure the initial thickness of the specimen.

  2. Center the specimen between the platens of the test machine, with sandpaper at each contact interface (omit if bonded to metal).

  3. Apply compressive force at a rate of 12 ± 3 mm/min until the specified deflection is reached, then release the force at the same rate. Repeat this cycle a second time to condition the specimen.

  4. Apply force a third time to the same specified deflection, and record the required compressive force.

  5. (Optional) Record force values at 5 % deflection intervals during the third loading cycle to construct a stress‑strain curve.

  6. Calculate and report the median force value from three specimens.


Test Method B (Specified Force)

  1. Apply a specified minor force/mass to the specimen to establish the zero baseline on the deflection gage.

  2. Apply the major test force gently (without impact) and hold it for exactly 3 seconds.

  3. Read and record the deflection at the end of the 3‑second hold period. This reading excludes any deflection caused by the minor baseline force.

  4. Calculate percent deflection relative to the original specimen thickness.

  5. Report the median deflection value from three specimens.


Industries application:

This test method is widely used across sectors where rubber components carry compressive loads:

  • Rubber material R&D: Used by rubber technologists to develop and compare compound formulations for compressive service applications.

  • Automotive industry: Qualification of engine mounts, suspension bushings, gaskets, seals, and vibration dampers.

  • Aerospace & defense: Approved for U.S. DoD use, for qualifying rubber components in military vehicles, aircraft, and equipment.

  • Industrial engineering: Performance verification of rubber pads, buffers, shock isolators, and sealing elements.

  • Quality control: Batch‑to‑batch consistency verification and incoming material inspection for rubber goods manufacturers.



Related Test Standard

ASTM D695Standard Test Method for Compressive Properties of Rigid Plastics
ISO/TR 9272 / ISO 19983     Rubber test method precision evaluation frameworks (used for the precision data in Annex D).
ASTM D3410Shear‑loading compression test for polymer‑matrix composites with unsupported gauge section, suited for high‑strength continuous‑fiber composite laminates (not pure end‑loading as D695).
ASTM D575

Standard Test Methods for Rubber Properties in Compression.

ASTM D395Measures compression set (permanent residual deformation after prolonged compression), a complementary property to the transient deflection measured by D575.
ISO 7616Cellular plastics, rigid-Determination of compressive creep under specified load and temperature conditions
ISO 844Rigid cellular plastics — Determination of compression properties
ISO 4666-3

Rubber, vulcanized — Determination of temperature rise and resistance to fatigue in flexometer testing — Part 3: Compression flexometer (constant-strain type)

ISO 3384

Compression stress relaxation; a time-dependent property, distinct from ISO 7743

ISO 604Plastics -- Determination of compressive properties 
ISO 7743Rubber, vulcanized or thermoplastic; determination of compression stress-strain properties
GB/T 7757Chinese standard Rubber, vulcanized or thermoplastic — Determination of compression stress-strain properties.
JIS K 6254Japanese standard for compression and tensile stress–strain properties. It is MOD relative to ISO 7743
ISO 815-1Compression set at ambient or elevated temperatures . It measures permanent deformation after prolonged compression, not short-term stress–strain behaviour.
ISO 5893Specification for tensile, flexural and compression test equipment of constant rate of traverse
TCVN 11993Plastics. Determination of compressive properties


Why This Test Matters for a Material

  1. Guides material formulation: It provides quantitative compressive stiffness data, allowing formulators to tailor rubber compounds to meet load‑bearing requirements for specific end uses.

  2. Enables standardized comparison: The method delivers repeatable, reproducible results that allow objective comparison between different materials, suppliers, or production batches.

  3. Supports component design: Compression‑deflection data predicts how a rubber part will deform under service loads, which is critical for designing functional components such as vibration isolators, seals, and load‑bearing pads.

  4. Supports quality assurance and qualification: It is a recognized industry and regulatory test method (including DoD approval) for material acceptance and product qualification.

  5. Characterizes functional performance: Compressive stiffness directly impacts key functional properties such as vibration damping, sealing effectiveness, and impact absorption.


Keywords: ASTM D575 tester,ASTM D575 rubber compression test,rubber compression deflection tester,elastomer compression stiffness test,solid rubber compression testing machine,rubber compression property test,rubber material quality control,rubber vibration mount test,rubber seal compression test,compression deflection test equipment,rubber mechanical property tester,UnitedTest rubber tester,elastomer compression test machine,rubber compound compression test,static compression test for rubber

Related products and device

ASTM D575 Rubber Compression Universal Testing Machine

WDW Series Computer Control Electronic Universal Testing Machine made by UNITEDTEST range from 100N to 600KN load capacity with various models like single columns, table type, door frame type etc., is used to perform tension, compression, flexure/bending, shearing, peeling etc., test for metal and nonmetal specimens.

ASTM D575 compression test platen

Compression test fixture is used to investigate the compressive behaviour of the test specimens and for determining the compressive strength, compressive modulus and other aspects of the compressive stress/strain relationship under the conditions defined.

Related Standard

ASTM D695 Plastic & composites Compressive Testing –

ASTM D695: Standard Test Method for Compressive Properties of Rigid Plastics

ASTM D695 test covers the determination of the mechanical properties of unreinforced and reinforced rigid plastics, including high-modulus composites, when loaded in compression at relatively low uniform rates of straining or loading. Test specimens of standard shape are employed. This procedure is applicable for a composite modulus up to and including 41,370 MPa (6,000,000 psi). It is technically equivalent to ISO 604 Plastics‑Determination of Compressive Properties. This test applies end‑loading compression on standard‑geometry specimens under controlled environmental and displacement‑rate conditions, delivering compressive strength, yield strength, offset yield strength, compressive elastic modulus, and compressive deformation data.


ASTM D2412 Plastic Pipe Deflection Testing by Compression Loading Test –

ASTM D2412: Standard Test Method for Determination of External Loading Characteristics of Plastic Pipe by Parallel-Plate Loading

ASTM D2412 test method covers the determination of load-deflection characteristics of plastic pipe under parallel-plate loading. It covers thermoplastic resin pipe, reinforced thermosetting resin pipe (RTRP), and reinforced polymer mortar pipe (RPMP). Pipes tested under ASTM D2412 must be smaller than the envelope of the two compression platens by at least a half an inch. Square or circular platens can be used, with most customers choosing a square platen. Care must be taken to account for the mid-section of the pipe which will expand slightly as the pipe is compressed.

The characteristics determined by ASTM D2412 test method are pipe stiffness, stiffness factor, and load at specific deflections.

ASTM D3410 Shear Loading compression Test for Polymer Matrix Composite Materials with Unsupported Gage Section –

ASTM D3410 Shear Loading compression Test Method for Compressive Properties of Polymer Matrix Composite Materials with Unsupported Gage Section. 

ASTM D3410 measuring in‑plane compressive properties for high‑modulus‑fiber‑reinforced polymer‑matrix composites using pure shear‑loading via wedge grips, with an unsupported gage section on the test coupon. Test method determines the in-plane compressive properties of polymer matrix composite materials reinforced by high-modulus fibers. It is applicable to composites made from unidirectional tape, wet-tow placement, textile (for example, fabric), short fibers, or similar product forms. Some product forms may require deviations from the test method.

ISO 14126 In-Plane Compressive Test of Fiber-Reinforced Material –

ISO 14126 Compression test Fibre-reinforced plastic composites — Determination of compressive properties in the in-plane direction

ISO 14126 specifies how to determine in‑plane compressive properties (i.e. load applied parallel to the plane of lamination, in directions "1" and "2") of fibre‑reinforced plastic composites with thermosetting or thermoplastic matrices. Specimens are machined from a flat test plate or from finished/semi‑finished products.

ISO 604 Compressive Strength Testing of Plastics –

ISO 604 specifies a method for determining the compressive properties of plastics under defined conditions. It is used to investigate the compressive behavior of test specimens and to determine key mechanical properties such as compressive strength, compressive modulus, and other aspects of the compressive stress/strain relationship. Specimen length is adjusted to avoid buckling that would distort results. 

ISO 7743 rubber compression test for stress and strain with parallel platens –

ISO 7743 Rubber, vulcanized or thermoplastic — Determination of compression stress-strain properties

ISO 7743 defines standardized methods for measuring the compression stress-strain properties of vulcanized or thermoplastic rubber, applicable to standard laboratory test pieces, finished products, or product segments.


ASTM D575 Rubber Compression Test Method

1. What is ASTM D575?

ASTM D575-91(2024), Standard Test Methods for Rubber Properties in Compression, is an ASTM Committee D11 method for determining the compression-deflection characteristics of solid rubber compounds, excluding hard rubber and sponge rubber. It contains two procedures: Method A (force at a specified deflection) and Method B (deflection at a specified force). SI units are normative; inch-pound values are for information only.


2. Why is the ASTM D575 test important?

Because it turns a rubber compound into a repeatable stiffness number under compression. That number drives seal contact pressure, assembly/insertion force, engine-mount and bushing stiffness, bridge-pad load capacity and cushioning feel. It also gives compounders, OEMs and test labs a common QC language. Shore hardness alone cannot predict it: a durometer measures local indentation, while D575 loads the whole specimen and captures bulging, interfacial friction, strain rate and loading history.


3. What is the difference between Method A and Method B?

Method A is deflection-controlled: drive to a specified percentage deflection at 12 ± 3 mm/min, condition with two load/unload cycles, and read the force on the third application. Method B is force-controlled: apply a minor force to seat and zero the deflection gage, then apply the major force for 3 s and read the deflection. Method A suits R&D and stress–strain curves; Method B suits rapid QC and parts with a known design load.


4. Which ASTM D575 method should I choose?

Use the method named in your material specification, part drawing or customer requirement. If the specification defines "stress at X% deflection", use Method A. If it defines "deflection under Y kN / Y kPa", use Method B. Do not convert one result into the other without the full force–deflection curve.


5. Does ASTM D575 require 25% deflection or a fixed force?

No. D575 says "specified deflection" and "specified force"; the value comes from the governing material/part specification or a buyer–supplier agreement. 25% is a common industry convention for Method A, but it is not a D575 default. Always report the value used — results at different deflections or forces cannot be compared.


6. Why does Method A use three loading cycles?

The first two cycles mechanically condition the specimen; the force is read on the third. Filled rubber softens over the first few compressions (the Mullins effect) and then stabilises. Comparing a first-cycle result with a conditioned third-cycle result can look like a batch difference when it is actually a loading-history difference.


7. What machine capacity and load cell should I choose for ASTM D575?

D575 does not specify a force — capacity must follow the expected peak force of your compound and target deflection. As a scale reference, the standard 650 mm² disc at the 1989 pooled Method A mean of 1636 kPa carries only about 1.06 kN, and the highest tabulated material level of 2591 kPa is about 1.68 kN. A low-force load cell (commonly in the 1–5 kN range) on a stiff, well-aligned frame is therefore usually more appropriate than a 100 kN frame with an oversized cell. Select in this order: expected specimen force → load cell range → frame capacity → platen size and alignment → software.


8. How is ASTM D575 different from ASTM D395 / ISO 815?

D575 measures short-term stiffness while loading — force versus deflection in minutes. ASTM D395 and ISO 815 measure compression set — the permanent deformation remaining after a specimen is held compressed (often 25% for 22–168 h at elevated or low temperature) and then allowed to recover. Both may use a ~29 × 12.5 mm disc, but they answer different engineering questions; a compound can be excellent at one and poor at the other.


9. How is ASTM D575 related to ISO 7743, GB/T 7757 and JIS K 6254?

ISO 7743:2017 is the closest international counterpart for compression stress–strain properties of vulcanized or thermoplastic rubber, with four methods: lubricated standard test piece A, bonded test piece A, standard test piece B, and a product/part with lubricated plates. GB/T 7757 is the Chinese adoption of ISO 7743 and JIS K 6254 is a modified Japanese adoption. They are not identical to D575: ISO 7743 typically uses ~29 mm discs, 10 ± 2 mm/min, lubricated or bonded interfaces, four conditioning cycles and reports a compression modulus. Do not treat D575 and ISO 7743 results as interchangeable.


10. Is ASTM D575 suitable for sponge rubber, foam or hard rubber?

No. The scope explicitly excludes rubber compounds usually classified as hard rubber and sponge rubber. Sponge/expanded rubber, flexible polyurethane foam and microcellular urethane are covered by other ASTM methods such as D1056, D3574 and D3489, and normally need much lower-capacity load cells.


11. Why choose UnitedTest Leading Manufacturer of ASTM D575 Rubber Compression Testing Machines? 

UnitedTest designs and manufactures high-precision ASTM D575 compression testing machines engineered to meet the exact requirements of ASTM D575-91 (Reapproved 2024) for determining compression-deflection characteristics of rubber compounds. Our universal compression testers deliver controlled crosshead speeds of 12 ± 3 mm/min, fully compliant with ASTM E4 force calibration standards, and support both Test Method A (specified deflection) and Test Method B (specified force) on a single platform.


Ideal for rubber compound development, quality control labs, automotive component manufacturers, and aerospace material qualification, UnitedTest's rubber compression test equipment comes standard with high-resolution deflection measurement, intuitive test software, and optional environmental chambers for temperature-controlled testing. Whether you need to measure compression stiffness, generate stress-strain curves, or perform routine production QC, our ASTM D575 test systems deliver accurate, repeatable results trusted by rubber technologists and testing laboratories worldwide.

< Previous: ASTM D570 Moisture test Method for Water Absorption of Plastics

> Next: ASTM D624 Rubber & Elastomer Tear Strength Test

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.