Home >> Application >> By Standard >> Others >> EN 12201-2 Guide for PE Pipe Testing Methods and Testing Equipment

EN 12201-2 Guide for PE Pipe Testing Methods and Testing Equipment

Share:

EN 12201-2 Plastics piping systems for water supply, and for drains and sewers under pressure - Polyethylene (PE) - Part 2: Pipes

EN 12201‑2 specifies the characteristics of polyethylene (PE) pipes and the test parameters that shall be used when applying the referenced EN ISO / ISO test methods. The detailed "how to test" procedures are in the referenced method standards. 

It's requirements for buried/above‑ground PE pipes (PE40, PE80, PE100, PE100‑RC), for potable water supply, raw water, pressure drains‑sewers, vacuum sewer systems (excluding industrial piping; industrial piping follows EN ISO 15494). It covers pipe geometry, material, appearance, mechanical‑physical‑chemical performance, marking, plus corresponding test parameters and specimen rules for verifying pipe compliance. The test mainly stipulated in the standard is Hydrostatic strength, Tensile elongation, Slow crack growth, Ring stiffness test, Longitudinal and circumferential reversion, OIT test etc., 


Test methods list: 

FamilyMain methods / standardsEquipment UnitedTest should considerKey parameters from the supplied copy
Dimensional & visualEN ISO 3126; ISO 11922-1:2018; appearance, colour, marking clausesOD/ID gauges, π tapes, wall-thickness gauges, ovality fixtures, large-pipe supports, inspection lightingRound to 0.1 mm; dispute measurement ≥24 h after manufacture and after ≥4 h at 23 ± 2 °C; minimum e_min 2.0/2.3/3.0 mm; coil ID ≥18 dn
Hydrostatic strengthEN ISO 1167-1:2006 + EN ISO 1167-2; Table 3 and Table 4Multi-station pressure rig, Type A end caps, 20 °C and 80 °C baths, pumps/intensifiers, transducers, data logging, safety enclosure20 °C/100 h: 7.0/10.0/12.0 MPa for PE 40/80/100-RC; 80 °C/165 h: 2.5/4.5/5.4 MPa; 80 °C/1000 h: 2.0/4.0/5.0 MPa; 3 specimens; water-in-water; pressure from measured dimensions
Tensile elongationEN ISO 6259-1 + EN ISO 6259-3Universal testing machine, Type 1/2/3 cutters, grips, extensometer, 10–100 mm/min speed control≥350 %; Type 2 at 100 mm/min for e ≤5 mm; Type 1 at 50 mm/min for 5<e≤12 mm; Type 1 at 25 mm/min or Type 3 at 10 mm/min for e>12 mm
Slow crack growth / PE 100-RCISO 13479:2022 NPT & ANPT; ISO 18488 SHT; ISO 18489:2015 CRBNotching cell, 80 °C pressure baths, chemical-rated ANPT bath, compression moulding press, 80 °C tensile chamber, 10 Hz fatigue rigNPT: e>5 mm, 80 °C, SDR 11, 8.0 bar PE 80 / 9.2 bar PE 100, ≥500 h. ANPT: dn 110 SDR 11, 9.2 bar, ≥300 h, water-in-2 % surfactant. SHT: <Gp> ≥50 MPa, 300 µm sheet, 80 °C. CRB: ≥1.5×10⁶ cycles, Δσ 12.5 MPa normalised to 14 mm / 1.40 mm crack, 10 Hz sinusoid, 23 °C
Ring behaviourClause 8.3 + Annex D; EN ISO 9969; EN ISO 13968Compression frame with parallel platens, load cell, displacement measurement, wide platensInitial ring stiffness S_calc ≥4 kN/m² for vacuum sewer pipes
Physical characteristicsEN ISO 11357-6 OIT; EN ISO 1133-1 MFR; EN ISO 2505 longitudinal reversionDSC with oxygen gas train; melt-flow indexer; 100/110 °C baths or ovensOIT ≥10 min at 210 °C, oxygen, 15±2 mg, 4 pieces; MFR 190 °C/10 min at 2.16 kg for PE 40 or 5.0 kg for PE 80/100/RC, ±20 % deviation; longitudinal reversion ≤3.0 %, 200 mm specimen
Application / system checksClause 9.3 circumferential reversion; ISO 4433-1/-2; EN 12201-5; UK foreword RCP/squeeze-off/WIS 4-32-0880 °C conditioning tank, large-diameter metrology, chemical immersion cells, joint-test bench, high-rate RCP enclosureCircumferential reversion for dn≥250 mm, 3dn specimen, dem at 0.1dn and 1.0dn; joints to EN 12201-5; RCP critical pressure ≥PFA, e.g. 8.0 MPa SDR 11 PE 80 and 10.0 MPa SDR 11 PE 100


Industry application fields

  • PE pipes for buried and above-ground applications.

  • Intended service:

    • water for human consumption;

    • raw water prior to treatment;

    • drains and sewers under pressure;

    • vacuum sewer systems;

    • water for other purposes.

  • Excludes industrial applications (covered by EN ISO 15494).

  • Also covers sea outfalls, pipes laid in water and pipes suspended below bridges.

  • Allowable operating pressure PFA up to 25 bar (1 bar = 0.1 MPa) at a reference temperature of 20 °C.

  • Applicable pipe constructions:

    1. monolayer PE pipes, including identification stripes;

    2. co-extruded-layer pipes, inside and/or outside, where all PE layers have the same MRS rating (Annex B);

    3. PE pipes with an outside peelable/contiguous thermoplastics layer ("coated pipe") (Annex C).

  • Material classes include PE 40, PE 80, PE 100 and PE 100-RC.


Major Mechanical & Pressure‑related Tests Specified in EN 12201-2

1, Ring Stiffness Test for Installed LinerVerify ring stiffness performance for PE pipes used in vacuum sewer systems; minimum initial ring stiffness Scalc ≥4 kN/m².
Test standardISO 9969
Test Equipment

Ring stiffness compression testing machine (universal compression tester equipped with parallel flat loading plates, displacement & force data acquisition). 

UnitedTest ring‑stiffness testing system can meet ISO 9969 execution requirements.

Test Stipulation

PE installed liner: declared ring stiffness value ≥ 1.0 kPa.

PVC‑U installed liner: ring stiffness is derived from declared tensile E‑modulus and SDR dimension ratio.

Test Specimen infoShort ring‑shaped pipe cut‑outs.
Test Procedure

Compress pipe ring specimen per ISO 9969 procedure, calculate ring‑stiffness value.

2, Oxidation Induction Time 

(OIT, thermal‑stability test)

Purpose: Evaluate thermal‑oxidation stability / anti‑oxidant performance of PE pipe compound and identification‑strip compound.

Equipment: DSC differential scanning calorimeter.

Parameters: Isothermal OIT test temperature 210 °C; minimum requirement ≥10 min for both pipe compound and colour‑strip compound.

Referenced standard: EN ISO 11357‑6.

Specimen: Small material chips sampled from pipe inner and outer surfaces, two samples each location.

Procedure: Run isothermal DSC scan under oxygen atmosphere, record oxidation induction time.

3, Tensile TestsMeasure elongation‑at‑break and tensile performance of pipe wall material.
Test standardISO 6259‑1,  ISO 6259‑3.
Test EquipmentUniversal material tensile testing machine with extensometer / displacement sensor.
Test Stipulation

Test speed options: 50 mm/min or 100 mm/min; requirement: elongation at break ≥350 %.

Test Specimen infoType‑2 test specimens machined from pipe wall. Machine‑die‑cut Type‑2 pieces are acceptable for pipe wall thickness ≤25 mm.
Procedure

Condition specimens at (23±2) °C; mount specimen grips; apply tensile force at specified rate until break; record elongation‑at‑break.

4, Melt‑flow rate (MFR / MVR) test

Purpose: Check melt‑flow property consistency before‑and‑after pipe extrusion processing; maximum allowed deviation ±20 % vs base compound value.

Equipment: Melt‑flow indexer / plastometer.

Parameters: 190 °C test temperature, 5.0 kg loading mass.

Referenced standard: ISO 1133‑1.

Specimen: Granules sampled from finished pipe.

Procedure: Follow standard melt‑flow measurement protocol for polyolefin. Compare post‑extrusion MFR against original raw‑material MFR.

5. Longitudinal reversion test

Purpose: Assess pipe residual internal stress from extrusion manufacturing.

Equipment: Oven / liquid temperature bath for heating pipe samples, dimensional measuring tools.

Parameters: Requirement: longitudinal reversion ≤3.0 %; conditioning temperature 110 °C.

Referenced standard: ISO 2505.

Specimen: Cut pipe segments.

Procedure: Measure original marked length; expose specimen to 110 °C controlled environment; measure length change after heating and cooling; compute percentage reversion.

6. Circumferential reversion test

Check circumferential dimensional relaxation / residual stress for large‑diameter pipe (dn ≥250 mm).

80 °C water bath, outside‑diameter measuring instrument complying with EN ISO 3126.

7. Ring‑flexibility test

Purpose: Evaluate pipe ring flexibility performance.

Equipment: Ring‑flexibility compression test rig.

Parameters: Comply with requirements defined in standard table.

Referenced standard: EN ISO 13968.

8, Hydrostatic resistance to internal pressure test 

(long‑term hydrostatic strength)

Verify PE pipe long‑term burst / creep resistance under constant internal water pressure; detect ductile or brittle pipe failure. Used for batch release & product verification.
Test Equipment

Hydrostatic pressure testing machine (water‑filled pressure vessel, end caps for pipe specimen, pressure control system, temperature‑controlled water bath). 

Two working modes: water‑in‑water, water‑in‑air (water‑in‑air permitted for DN>630 mm).

Test StandardISO 1167, ISO 8772
Test Specimen info

Full PE pipe segment; Type‑B end caps allowed for nominal diameter >500 mm. 

Use measured pipe dimension for dispute judgment; nominal dimension allowed for factory batch release.

Other Test

Dimensional measurement (outer diameter, ovality, wall‑thickness)

Chemical resistance immersion test (optional, when chemical‑exposure service required).


Keywords: EN 12201-2:2024 testing machine · BS EN 12201-2:2024 test equipment · PE pipe hydrostatic pressure testing machine · EN ISO 1167 hydrostatic test rig · PE100-RC testing machine · notched pipe test equipment · cracked round bar test machine · strain hardening test equipment · ring stiffness testing machine PE pipe · UnitedTest PE pipe testing equipment

Related products and device

EN 12201-2 pipe ring stiffness test machine

pipe ring stiffness test machine is used to determine the ring stiffness of circular cross-section thermoplastic pipes, according customer’s request, it can also execute compression, ring stiffness, ring softness and creep ratio test.

EN 12201-2 Pipe Hydrostatic Pressure Tester

Elevate your pipeline testing with our advanced hydrostatic pressure testing machine, designed per ISO 1167, ASTM D1598, and ASTM D1599 standards. Perfect for evaluating the durability of plastic and compound pipelines like PP-R, PVC, and PE, it applies precise constant or rapid hydraulic pressure, ensuring reliable performance.

EN 12201-2 Electronic Universal Testing Machine

WDW Series Computer Control Electronic Universal Testing Machine made by UNITEDTEST range from 100N to 600KN load capacity with various models like single columns, table type, door frame type etc., is used to perform tension, compression, flexure/bending, shearing, peeling etc., test for metal and nonmetal specimens.

EN 12201-2 pipe Melt flow index tester

Extrusion Plastometer is for melt mass-flow rate (MFR) and the melt volume-flow rate (MVR),to measure the melt mass flow rate of thermoplastic plastics under specific temperatures and pressures, reflecting the flow performance of materials through standardized testing.

EN 12201-2 Oxidative Induction Time testing machine

Oxidative Induction Time testing machine is kind of differential scanning calorimeter,, check the relation of temperature with the rate differential input in test sample and reference articles. used to do Oxidative Induction Time test, heat stability, glass transition temperature, melting point.

EN 12201-2 Charpy & Izod Integrated Impact Tester

Charpy & Izod Integrated Impact Tester combine the Charpy and IZOD two impact method in one machine, include the full IZOD and Charpy test energy, simply change pendulum and vice, in one machine meet user multiple test requirement, enhance the working efficiency.

Heat Distortion Temperature Tester/VST softening temperature apparatus

Heat Distortion Temperature Tester for accurate measurement of plastic materials’ heat deflection under load, ensuring reliable thermal performance evaluation, quality control, and compliance with international standards.

Pipe Size Change Measuring Tester (Longitudinal reversion test)

Pipe Size Change Measuring Tester/ Longitudinal Reversion Tester suitable to measure various kinds of plastic pipe or plastic materials size change after heating, or used to heat the test sample. It can be used as a heating oven as well.

Dichloromethane soak testing machine

Methylene chloride tester/Dichloromethane soak testing machine is used to determine the resistance of unplasticised polyvinyl chloride (PVC-U) pipes to dichloromethane (methylene chloride) at a specified temperature (DCMT).

Pipe Hoop tensile testing machine

UnitedTest Pipe Apparent Hoop Tensile Testing Machine complies with ASTM D2290, specialized in testing apparent hoop tensile strength of plastic and reinforced plastic pipes. It uses a self-aligning split disk fixture to apply tensile stress to pipe ring samples along their contour.

hoop tensile strength of plastic pipes

Hoop tensile strength of plastic pipes is designed based on the ASTM D2290, to determine the breaking strength for the pipe hoop tensile test. ASTM D2290 is a test method used to study the apparent tensile strength of plastic pipes using a specialized test fixture to pull apart a ring of pipe.

Related Standard

ISO 7685 Glass-Reinforced Thermosetting Plastics GRP Pipe Initial Ring Stiffness Test –

ISO 7685 Glass-reinforced thermosetting plastics (GRP) pipes — Determination of initial ring stiffness.

ISO 7685 defines two standardized compression test methods to measure initial ring stiffness (S₀) for circular glass-reinforced thermosetting plastic (GRP/FRP) pipes, evaluating radial deformation resistance under short-term vertical external loads.

ISO 10468 GRP Pipe Ring Creep Test –

ISO 10468 Glass-reinforced thermosetting plastics (GRP) pipes — Determination of the ring creep properties under wet or dry conditions.

ISO 10468 specify two core time-dependent mechanical properties of GRP pipes: long-term ring creep stiffness and creep factor. Two test environments are defined: dry ambient condition and fully water-immersed wet condition.

Dry creep test: For raw material batch consistency inspection and internal quality control.

Wet creep test: Simulates underground water service environments to predict long-term in-ground structural performance of buried GRP pipes.  

ISO 8513 Longitudinal tensile test for Glass-reinforced thermosetting plastic pipe –

ISO 8513 Plastics piping systems — Glass-reinforced thermosetting plastics (GRP) pipes — Test methods for the determination of the initial longitudinal tensile strength

ISO 8513 measure two core longitudinal tensile properties of glass-reinforced thermosetting plastic (GRP, also known as fiberglass-reinforced plastic FRP) pipes: Initial longitudinal tensile strength, Percentage ultimate elongation. IT only addresses tensile strength and break elongation; it explicitly excludes longitudinal tensile modulus testing, as multi-layer GRP pipe wall structures make precise strain measurement impractical.

ISO 15306 Cyclic internal pressure test of GRP pipes –

ISO 15306 Glass‑reinforced thermosetting plastics (GRP) pipes ‑ Determination of the resistance to cyclic internal pressure

ISO 15306 specifies a laboratory test method for evaluating cyclic‑pressure fatigue performance of GRP (fiberglass‑reinforced thermoset) pipes. The method can also apply to GRP fittings, not only straight pipes, which clarifies the applicable diameter range to nominal diameters up to and including DN 600.

ISO 8521 GRP Pipe Longitudinal Tensile Strength Testing –

ISO 8521 Glass-reinforced thermosetting plastic (GRP) pipes — Test methods for the determination of the initial circumferential tensile wall strength

ISO 8521 specifies six test methods (A, B, C, D, E, F) to determine the initial circumferential tensile wall strength per unit length of GRP pipes — a property also commonly called "hoop tensile strength." Both terms are interchangeable per the standard . The result is expressed in newtons per millimetre (N/mm) of circumference. "Initial" means the strength at the startof loading (short-term / instantaneous), as opposed to long-term hydrostatic strength covered by other standards. 

ASTM D2290 Apparent Hoop Tensile Strength Testing –

ASTM D2290: Standard Test Method for Apparent Hoop Tensile Strength of Plastic or Reinforced Plastic Pipe

This test method covers the determination of the comparative apparent tensile strength of most plastic products utilizing a split disk or ring segment test fixture, when tested under defined conditions of pretreatment, temperature, humidity, and test machine speed. This test method is applicable to reinforced-thermosetting resin pipe regardless of fabrication method. This test method also is applicable to extruded and molded thermoplastic pipe.


ASTM D1598, D1599 Plastic Pipe Constant or short time pressure testing methods –

ASTM D1598: Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure.

ASTM D1598 test method covers the determination of the time-to-failure of both thermoplastic and reinforced thermosetting/resin pipe under constant internal pressure.This test method provides a method of characterizing plastics in the form of pipe under the conditions prescribed.


ASTM D1599: Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings.

ASTM D1599 test method establishes the short-time hydraulic failure pressure of thermoplastic or reinforced thermosetting resin pipe, tubing, or fittings. Data obtained by this test method are of use only in predicting the behavior of pipe, tubing, and fittings under conditions of temperature, time, method of loading, and hoop stress similar to those used in the actual test. They are generally not indicative of the long-term strength of thermoplastic or reinforced thermosetting resin pipe, tubing, and fittings


ASTM D1599 Pipe short-time hydraulic burst pressure test –

ASTM D1599 is titled "Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings." It is a fundamental short-term, destructive pressure test used to determine the ultimate failure pressure (often called the "burst pressure") of thermoplastic pipe, tubing, or fittings under rapidly applied internal pressure at a specified temperature. Typically completed within 60–70 seconds, mainly for quality control and short-term design validation. 

ISO 1167 Thermoplastics pipes resistance to internal pressure test –

ISO 1167: 2006 Thermoplastics pipes, fittings and assemblies for the conveyance of fluids -- Determination of the resistance to internal pressure.

ISO 1167 test method specifies a general test method for determining the resistance to internal hydrostatic pressure at a given temperature of thermoplastics pipes, fittings and piping systems for the transport of fluids. The method accommodates water-in-water, water-in-air and water-in-liquid tests. It defines uniform hydrostatic pressure testing to evaluate short-term and long-term pressure-bearing durability of thermoplastic fluid-transport piping systems.


Hydrostatic pressure testing is a valuable method for assessing the strength and integrity of pressurized systems, ensuring that they can meet operational demands without failure. Hydrostatic pressure testing can evaluate these items by filling pipelines, tanks, or containers with water before pressure is applied to detect any potential leaks or issues. 

Hydrostatic pressure tester is critical across multiple industries, from pipeline engineering to industrial piping. It helps prevent costly failures or leaks by verifying whether the system can safely reach the specified pressure levels.

FAQ of EN 12201-2 for PE Pipe Testing Methods and Testing Equipment

What is EN 12201-2, and is it a test method or a product standard?

EN 12201-2:2024 is the European product standard for polyethylene (PE) pressure pipes used in water supply, pressure drains and sewers, vacuum sewer systems and other water applications. It is not a standalone test method: it specifies pipe characteristics, acceptance requirements and test parameters, then references EN ISO and ISO methods such as EN ISO 1167-1, ISO 13479:2022 and ISO 18489:2015 for the detailed procedures. For a testing-machine buyer, this means one standard maps to a complete laboratory platform rather than a single tester.


Which PE pipe types and sizes fall under EN 12201-2?

The standard covers monolayer PE pipes with identification stripes, co-extruded-layer pipes where all PE layers have the same MRS rating, and PE pipes with an outside peelable thermoplastics layer. Material classes include PE 40, PE 80, PE 100 and PE100-RC. The 2024 revision extended the size range to dn 3000 mm, so large-diameter handling, wide compression platens and large pressure end caps are part of the equipment envelope.


Can one testing machine cover all EN 12201-2 requirements?

No. EN 12201-2:2024 calls for dimensional metrology, long-duration hydrostatic pressure testing, tensile elongation, notched pipe and PE100-RC crack-growth tests, ring stiffness/flexibility, DSC, melt-flow, reversion and chemical or joint tests. UnitedTest should offer a modular PE pipe testing laboratory: independent pressure stations, a universal tensile/compression frame, thermal and rheology instruments, notching and specimen-preparation tools, and dedicated PE100-RC fatigue or strain-hardening systems.


Which testing machine is required for EN 12201-2:2024 hydrostatic strength tests?

A modular hydrostatic pressure testing machine to EN ISO 1167-1:2006 and EN ISO 1167-2 is required, with Type A end caps, 20 °C and 80 °C temperature-controlled water baths, pressure generation and control, calibrated transducers, supports, safety containment and long-duration data logging. Type B end caps are permitted only for batch-release tests at diameters of 500 mm and above.


What are the EN 12201-2:2024 hydrostatic hoop stresses at 20 °C and 80 °C?

Table 3 specifies: at 20 °C for 100 h, PE 40 7.0 MPa, PE 80 10.0 MPa, PE 100 and PE100-RC 12.0 MPa; at 80 °C for 165 h, 2.5, 4.5 and 5.4 MPa respectively; at 80 °C for 1 000 h, 2.0, 4.0 and 5.0 MPa respectively. Test pressure is calculated from measured pipe dimensions, and three test pieces are used for each condition.


What does water-in-water mean, and when can water-in-air be used?

Water-in-water means water is inside the test piece and the test piece is immersed in water outside, giving stable temperature control during hydrostatic testing. EN 12201-2:2024 allows water-in-air for pipes larger than 630 mm. A water-in-liquid configuration is used for the PE100-RC accelerated notched pipe test, where the external medium is a detergent solution rather than plain water.


Why must hydrostatic test pressure be calculated from measured pipe dimensions?

EN 12201-2:2024 requires test pressure to be calculated from measured dimensions; nominal dimensions may be used only for batch-release testing, and measured dimensions are mandatory in case of dispute. This makes EN ISO 3126 dimensional measurement, wall-thickness gauges and traceable data transfer to the pressure controller part of the compliance chain, not just incoming inspection.


How long do EN 12201-2:2024 pressure tests take, and how many stations do I need?

Hydrostatic tests run for 100 h, 165 h and 1 000 h; NPT for at least 500 h; ANPT for at least 300 h; and the alternative long-term PE100-RC NPT for 8 760 h. A single 1 000 h test occupies one station for more than 41 days, so UnitedTest recommends independent modular pressure cells with per-station control, alarms, power-failure recovery and tamper-evident logging.


Which machine measures elongation at break to EN ISO 6259-3, and what test speed applies?

A universal testing machine with Type 1, Type 2 or Type 3 specimen cutters, suitable grips and extensometry is used. EN 12201-2:2024 requires at least 350 % elongation: Type 2 at 100 mm/min for wall thickness up to 5 mm, Type 1 at 50 mm/min for 5 mm to 12 mm, and Type 1 at 25 mm/min or Type 3 at 10 mm/min above 12 mm. The controller should cover 10–100 mm/min and map wall thickness to the correct recipe.


What is a strain hardening test machine for PE100-RC per ISO 18488?

A strain hardening test (SHT) system combines a compression-moulding press, regrind preparation, a 300 µm sheet cutter, thickness metrology, a tensile machine with an 80 °C chamber and software for the strain-hardening modulus. EN 12201-2:2024 requires <Gp> of at least 50.0 MPa. SHT is intended for size group 1 PE100-RC and is a material-characterization platform, not a conventional pipe pressure tester.


What is a cracked round bar fatigue tester per ISO 18489:2015?

A CRB tester applies a 10 Hz sinusoidal cyclic load to a 14 mm round bar machined axially from a PE pipe with wall thickness over 16 mm. EN 12201-2:2024 requires at least 1.5 million cycles at an interpolated stress range of 12.5 MPa, normalised to a 14 mm diameter and 1.40 mm initial crack, in air at 23 °C. At least four specimens are evenly distributed around the pipe circumference; precision notching, crack measurement and cycle logging are essential.


What ring stiffness testing machine is needed for EN 12201-2:2024 vacuum sewer pipes?

Clause 8.3 requires an initial ring stiffness S_calc of at least 4 kN/m² for vacuum sewer pipes and refers to Annex D. EN ISO 9969 and EN ISO 13968 are the referenced ring stiffness and ring flexibility methods. A compression frame with parallel platens, calibrated load and displacement measurement, wide platens and large vertical clearance is the core machine. The complete Annex D procedure should be confirmed against the full standard before validating acceptance recipes.


What is the difference between longitudinal and circumferential reversion testing?

Longitudinal reversion to EN ISO 2505 uses a 200 mm pipe specimen with wall thickness up to 16 mm, heated at 100 °C for PE 40 or 110 °C for PE 80, PE 100 and PE100-RC; change must be no more than 3.0 % and the original appearance retained. Circumferential reversion applies to dn 250 mm and above: a 3dn specimen is conditioned in 80 °C water and mean outside diameter is measured at 0.1dn and 1.0dn from the end. They need different baths, fixtures and dimensional stations.


What should I check before buying an EN 12201-2 PE pipe testing machine?

Check the exact standard edition, material classes, dn range up to 3000 mm and wall thickness, number of independent pressure stations, 20 °C / 80 °C temperature stability, Type A end-cap inventory, measured-dimension pressure calculation, calibration coverage, data integrity and safety containment. Verify that your copy includes Table 1 and Annexes B, C and D; incomplete copies omit dimensional tolerances, co-extruded-layer, peelable-layer and vacuum-sewer details.

< Previous: IEC 60068-2-75 Hammer Test for Enclosure Impact Verification

> Next: EN 16094 Micro-Scratch & Polishing Resistance Test for Laminate Floor Coverings

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.