UnitedTest manufactures ISO 4545-1 compliant Knoop hardness testing machines. ISO 4545-1 defines the Knoop hardness test method for metallic materials, metallic coatings and inorganic coatings, covering test procedures, specimen preparation, calculation, reporting and periodic tester verification.
ISO 4545-1 specifies the Knoop hardness test method for metallic materials, metallic coatings and inorganic coatings. This standard covers complete test procedures, equipment specifications, specimen preparation guidelines, hardness calculation rules, reporting requirements and periodic verification for Knoop hardness testers. Widely applied in metal research, surface coating inspection, incoming material quality control and material certification. UnitedTest supplies high-precision ISO 4545-1 Knoop hardness test equipment for industrial laboratories, metal component factories and third-party testing institutions.
Core Test Principle
A rhombic‑pyramid diamond indenter with vertex angles α = 172.5°, β = 130° is pressed perpendicularly into the flat specimen surface with defined test force F. After removing force F, the long diagonal d of the residual rhombic indentation is optically measured. Knoop hardness (HK) is proportional to the ratio of applied test force divided by the projected indentation area of the rhombic‑pyramid impression.
Note: The indentation depth is approximately 1/30 of the long diagonal length.

Test Specimen Specifications
Test surface: Must be polished, smooth, oxide‑free, clean of lubricants and contaminants, to enable clear indent diagonal measurement.
Surface preparation: Must avoid surface work‑hardening or thermal damage. Electropolishing is recommended for metallic materials.
Thickness rule: Specimen thickness shall be at least 1/3 of the indent long diagonal length. No deformation shall appear on the specimen back‑side after indentation.
Coating special limits:
Normal surface testing: coating thickness ≥ 0.007 mm;
Cross‑section coating testing: coating thickness ≥ 0.020 mm.
Unstable / small specimens: Shall be rigidly mounted or supported metallographically to prevent movement during force application.
Test Equipment of ISO 4545-1 Metallic materials Knoop hardness test
| Hardness testing machine | must apply a predetermined force (or forces) over the required range, in accordance with ISO 4545-2. In practice: a microhardness tester using dead weights or a closed-loop force-controlled loading system, with a force range covering ≈ 1 gf to 2 kgf. |
| Diamond Knoop indenter | Rhombic‑based pyramid diamond tip, geometric tolerances defined in ISO 4545‑2.
|
| Diagonal measuring system | Optical magnification: indent long diagonal occupies 25 %‑75 % of the optical field of view; camera‑based systems can use full field if optical distortion is compensated. Measurement resolution must match indent size (e.g. 0.0004 mm for indent long diagonal 0.020 mm ≤ d < 0.080 mm). Resolution accounts for microscope optics, digital scale readout and stage step size. |
Test Parameters
Test force: Range from 0.009807 N up to 19.613 N. Select force so that indent long diagonal d ≥ 0.020 mm. Smaller indentations fall outside this standard and require ISO 14577‑1 instrumented indentation testANSI Webst....
Force application: Time from initial contact to full test force: 7 ± 5 s (acceptable range: 2 s ~ 8 s). Indenter approach velocity ≤ 0.070 mm/s.
Dwell time under full test force: 14 ± 4 s. For time‑dependent materials, modified dwell time shall be marked in hardness designation.
Indent spacing rules (critical stipulations):
Centre‑to‑edge: indent centre to specimen edge parallel to short diagonal ≥ 3.5 × short diagonal; indent centre to edge parallel to long diagonal ≥ 1 × long diagonal.
Adjacent indents: side‑by‑side indent centres ≥ 3.5 × short diagonal; end‑to‑end indent centres ≥ 2 × long diagonal. When indent sizes differ, spacing is based on the larger indent dimensionsPMC.
Indent quality check: If two segments of long diagonal (split at short‑diagonal intersection) differ by > 5 % of total long‑diagonal length, discard that measurement and check machine alignment.
Test Procedures of ISO 4545-1 Metallic materials Knoop hardness test:
Perform periodic verification of tester, measuring system and indenter (Annex A), ideally before daily testing or when force / indenter is changed, using calibrated Knoop reference blocks conforming to ISO 4545‑3.
Secure clean specimen on rigid support, ensure no movement during loading.
Focus optical measuring system on target test area.
Lower diamond indenter, apply test force vertically without shock or vibration, meet specified loading time and dwell‑time requirements. The whole test environment must isolate from mechanical shock and vibration.
Remove test force, measure the long diagonal length of residual indent. Select proper magnification for measurement.
Calculate Knoop hardness value HK from measured long diagonal; ISO 4545‑4 provides lookup tables for hardness calculation.
Evaluate measurement uncertainty following JCGM 100:2008 guidance (Annex B gives practical uncertainty estimation methods).
Industrial Application Fields
Thin coatings and surface layers — electrodeposited (hard chrome, Ni), autocatalytic/electroless nickel, thermal-sprayed coatings, anodic coatings on aluminium, PVD/CVD hard coatings (TiN on cutting tools).
Case-depth / hardness-gradient profiling — carburising, nitriding, induction hardening: the elongated indent allows closely spaced traverses with fine spatial resolution.
Brittle or fragile materials — ceramics, glass, hardened/white cast iron layers, where a Vickers indent would crack.
Small, thin or localised features — foils, fine wire, small precision parts, individual microconstituents or grains, weld HAZ traverses.
Near-edge and surface-condition checks — grinding burn, decarburisation, edge hardness.
Anisotropy studies — directional hardness differences in single crystals, rolled or textured materials.
Industries: aerospace, automotive and powertrain heat treatment, electronics and connectors, electroplating/surface-engineering shops, tooling and wear parts, plus calibration and accreditation laboratories, inspection houses, and university metallurgy labs.
Related Standard:
| ISO 4545-1 | Metallic materials — Knoop hardness test — Part 1: Test method |
| ISO 4545-2 | Part 2 — verification and calibration of Knoop testing machines (direct + indirect verification). |
| ISO 6507-1 | Vickers hardness test — the closest sibling; issued in the same revision round, with an equivalent new Annex H for coatings. Same force regime, square 136° pyramid, both diagonals measured, deeper indent. |
| ISO 14577-1/-2/-3 | Instrumented indentation (Martens hardness, nano/micro range) — the route for indentations smaller than 0,020 mm or coatings below the 0,007/0,020 mm limits. |
| ISO 6506 | Paper. Determination of tearing resistance (Elmendorf method) |
| ASTM E384 | Standard Test Method for Microindentation Hardness of Materials |
Importance of ISO 4545-1 Metallic materials Knoop hardness test
Knoop test uses elongated rhombic indent, ideal for measuring thin surface layers, coatings, heat‑affected zones and small microstructural regions, which conventional macro‑hardness tests cannot achieve without substrate interference.
Hardness reflects material resistance to plastic deformation; it correlates with wear resistance, strength and brittleness, supporting material selection, heat‑treatment validation, coating quality acceptance and failure analysis.
ISO 4545‑1 standardises test conditions, specimen preparation, machine checks and reporting, ensuring reproducible and comparable hardness data across different laboratories, manufacturers and countries.
It defines metrological traceability routes (Annex C) for hardness measurement, supporting industrial quality assurance, product acceptance and material‑research data credibility.
The standard explicitly addresses measurement uncertainty, helping users understand measurement limits and avoid wrong conclusions from excessive‑size or poor‑quality indentations.
Note: Knoop hardness is an ordinal test‑dependent quantity rather than fundamental material constant; reliable cross‑scale hardness conversion is not generally feasible without direct comparison tests.
Keywords: ISO 4545-1,Knoop hardness tester,metallic materials knoop hardness test,metallic coating microhardness test,inorganic coating hardness tester,knoop indentation hardness test,metal surface hardness measurement,knoop hardness test procedure,material hardness lab equipment,UnitedTest hardness testing machine,microhardness tester for thin coatings,metal material qualification test,knoop hardness calculation,hardness tester periodic verification,metallurgical hardness testing instrument
Related products and device
ISO 4545-1 Metallic materials Knoop hardness test
1. What is the ISO 4545-1 test?
It is the standardized Knoop hardness test method for metallic materials. A diamond indenter shaped as a rhombic-based pyramid is pressed into a polished surface with a defined low force; after unloading, the long diagonal of the residual indentation is measured with a microscope and the Knoop hardness number (HK) is calculated from force ÷ projected indentation area.
2. Which test forces does ISO 4545-1 allow?
0,009807 N to 19,613 N — i.e. HK 0,001 up to HK 2. Typical scales are HK 0,001 / 0,005 / 0,01 / 0,02 / 0,025 / 0,05 / 0,1 / 0,2 / 0,3 / 0,5 / 1 and 2 (0,009807 / 0,04903 / 0,09807 / 0,1961 / 0,2452 / 0,4903 / 0,9807 / 1,961 / 2,942 / 4,903 / 9,807 / 19,613 N). Other forces are permitted, but the resulting long diagonal must be ≥ 0,020 mm.
3. How far apart must indentations be?
To the specimen edge: ≥ 3,5 × short diagonal when the long diagonal is parallel to the edge; ≥ 1 × long diagonal when perpendicular.
Between adjacent indentations: ≥ 3,5 × short diagonal side-by-side; ≥ 2 × long diagonal end-to-end.
If indentations differ in size, base spacing on the larger indentation.
4. Why is only the long diagonal measured?
The Knoop indentation is about 7 times longer than it is wide, so the long diagonal is far easier to resolve optically. Measuring one long line instead of two short ones makes the result less sensitive to the ±0,001 mm reading error that plagues low-force Vickers measurements — one of the main reasons Knoop is preferred at very low loads.
5. What is the 5 % asymmetry rule?
If the indentation looks asymmetric, split the long diagonal at its intersection with the short diagonal and measure both halves. A difference of more than 5 % of d means you must check the parallelism of the support and measuring planes and the alignment of the indenter — and discard results with deviations above 5 %.
6. How shallow is a Knoop indentation, and why does it matter?
Depth is approximately 1/30 of the long diagonal (0,033 d) — about half the depth of a Vickers indentation at the same force. That shallow, slender impression is exactly what lets you test thin coatings, thin case-hardened layers, foils and brittle surfaces without the substrate influencing the result or the material cracking.
7. Can ISO 4545-1 be used on coatings?
Yes — this is the headline change of the 2023 edition. It applies to metallic and other inorganic coatings (electrodeposited, autocatalytic, sprayed, anodic on aluminium), both normal to the surface and on cross-sections, provided coating smoothness and thickness allow an accurate diagonal reading. Requirements: coating ≥ 0,007 mm for surface testing and ≥ 0,020 mm for cross-section testing; surface roughness typically Ra < 0,3 µm and < 5 % of maximum indentation depth; at least 5 valid indentations with the coefficient of variation reported (commonly < 5 %); position and orientation recorded for anisotropic coatings; reduce speed or force if a brittle coating cracks. Full rules are in Annex F (normative). The scope absorbed the content of the withdrawn ISO 4516:2002.
8. When should I choose Knoop instead of Vickers?
Choose Knoop when the feature is thin or fragile: thin coatings and plated layers, case-depth profiling of carburised/nitrided parts, brittle materials (ceramics, glass, white cast iron) that crack under a Vickers indent, measurements close to an edge, small parts, foils and fine wire, individual microconstituents or grains, weld HAZ traverses, and studies of hardness anisotropy. For general-purpose microhardness, Vickers remains the common default.
9. Which standards are related to ISO 4545-1?
ISO 4545-2 — verification and calibration of Knoop testing machines (normative reference).
ISO 4545-3 — calibration of Knoop reference blocks.
ISO 4545-4 — tables of Knoop hardness values.
ISO 6507-1:2023 — Vickers test method (its sibling; adds Annex H for coatings).
ISO 4516:2002 — withdrawn; its coating content moved into ISO 4545-1 Annex F and ISO 6507-1 Annex H.
ISO 14577-1/-2/-3 — instrumented indentation, for indentations below 0,020 mm.
ASTM E384 — the US microindentation standard covering both Knoop and Vickers.
ISO 18265 — hardness conversion tables (use with caution).
10. Why choose ISO 4545‑1 Knoop Hardness Tester from UnitedTest?
UnitedTest manufactures ISO 4545‑1:2023 compliant Knoop hardness testers for metallic materials, thin‑film coatings and cross‑section metallographic samples. Our Knoop microhardness test machines meet ISO 4545‑2 calibration requirements, support full ISO 4545‑1 test workflow, periodic machine verification and automated indent diagonal measurement for industrial quality control & material laboratory research.
UnitedTest is a professional manufacturer of Knoop micro‑hardness testing machines fully compliant with ISO 4545‑1:2023 Metallic materials‑Knoop hardness test‑Part 1: Test method.
Our Knoop hardness testers cover test force range from 0.009807 N to 19.613 N, suitable for metal substrates, electrodeposited coatings, autocatalytic coatings, thermal‑sprayed layers and aluminium anodic coatings. The system integrates high‑resolution diagonal measuring microscope, precise diamond Knoop indenter, rigid specimen support, and shock‑damping frame, fully satisfying ISO 4545‑1 requirements on indent magnification, loading speed, dwell‑time control and indent spacing inspection.
UnitedTest Knoop hardness tester supports user‑level periodic verification defined in ISO 4545‑1 Annex A, working with ISO 4545‑3 calibrated reference blocks for routine performance check. Operators can follow the full ISO 4545‑1 test workflow: specimen mounting, force application, indent measurement, HK hardness calculation and standardized test‑report export.
Ideal application fields: surface‑coating quality inspection, heat‑treated case‑depth evaluation, weld‑zone micro‑hardness mapping, brittle metallic material testing, metallographic cross‑section analysis, R&D laboratory and industrial incoming‑goods QC.
UnitedTest Knoop hardness test equipment complies with supporting standards ISO 4545‑2 for machine verification and calibration. We provide complete technical documentation, on‑site commissioning and training services to help laboratories achieve ISO 4545‑1‑compliant hardness measurement and reliable metrological traceability.