Information on the most widely used ASTM standards within the materials testing industry
Model: XJB-30E, ASTM D1709, ISO 7765-1. ISO 6603-1
XJB-30E Heavy duty frame falling dart impact testing machine mainly used to test plastic, film, or sheet thickness below 1mm, impact by falling dart, check the energy when 50% of test specimen broken.
Conform with standard: ISO 7765-1, ASTM D1709, GB 9639. ASTM D5628, ISO 6603-1.
Scope:
Falling dart impact is a traditional method for evaluating the impact strength or toughness of a plastic film. This test uses a single dart configuration and a single drop height, while varying the weight of the dart. Test results can be used either as a quality control evaluation or for end use comparisons.
General Introduction
XJB-30E Heavy duty frame falling dart impact testing machine mainly used to test plastic, film, or sheet thickness below 1mm, impact by falling dart, check the energy when 50% of test specimen broken.
Conform with standard: ISO 7765-1, ASTM D1709, GB 9639. ASTM D5628, ISO 6603-1.
Scope:
Falling dart impact is a traditional method for evaluating the impact strength or toughness of a plastic film. This test uses a single dart configuration and a single drop height, while varying the weight of the dart. Test results can be used either as a quality control evaluation or for end use comparisons.
Specimen size:
Film samples that can be cut to 230 mm x 230 mm (9" x 9") specimens
A minimum of 30 specimens are required for the test

Falling dart impact tester, drop dart impact testing equipment.
Features
ISO 7765-1: Plastics film and sheeting -- Determination of impact resistance by the free-falling dart method -- Part 1: Staircase methods
ASTM D1709: Standard Test Methods for Impact Resistance of Plastic Film by the Free-Falling Dart Method.
JIS K 7124-1 - Plastics film and sheeting.
ASTM D5628 Standard Test Method for Impact Resistance of Flat, Rigid Plastic Specimens by Means of a Falling Dart (Tup or Falling Mass)
ISO 6603-1 Plastics - Determination of puncture impact behaviour of rigid plastics - Part 1: Non-instrumented impact testing.
Main parameters
| Model | XJB-30E |
| Dart weight | A method: R19±1mm (2 pcs) B method: 25±1mm (1 pc) |
| Weight | 50--2000g (5g increment) 5g (5 pcs), 15g (15 pcs), 30g (10 pcs), 45g (10 pcs), 60g (10 pcs), 90g (15 pcs) |
| Specimen clamper | OD 150mm, ID 125mm |
| Max. energy | 30J |
| Impact height | 1500mm |
| Power | 220V, 50HZ |
| Dimensions | 650mm×650mm×2600mm |
| Weight | 150Kg |
| Standard Accessories | Loadframe, Dart head, weight unit, tools, power cord, manual etc. |
Main accessories
Loadframe,
Dart head,
weight unit,
tools,
power cord,
manual etc.
Standard
ISO 6603-1 specifies falling-dart methods to measure the puncture‑impact performance of rigid plastics using only the 50% impact‑failure energy (E₅₀) threshold, without recording force–time or force–deflection curves.
ASTMD5628 specifies a falling‑dart/tup method to measure the threshold impact‑failure energy for flat rigid plastics. It uses the Bruceton Staircase (Up‑and‑Down) Method to determine the energy causing 50% of specimens to fail (mean‑failure energy, MFE).
ASTM D1709: Standard Test Methods for Impact Resistance of Plastic Film by the Free-Falling Dart Method
ASTM D1709 test methods cover the determination of the energy that causes plastic film to fail under specified conditions of impact of a free-falling dart. This energy is expressed in terms of the weight (mass) of the missile falling from a specified height which would result in 50 % failure of specimens tested.
ISO 7765-1:1988 Plastics film and sheeting — Determination of impact resistance by the free-falling dart method
Part 1: Staircase methods
ISO 7765-1 and ASTM D1709 specifies methods for the determination of the energy, that causes plastics films and sheet less than 1 mm in thickness to fail under specified conditions of impact of a free falling dart from a specified height, that would result in failure of 50 % of the specimens tested. Two methods are described. Method A employs a dart with 38 mm diameter hemispherical head, dropped from a height of 0,66 m, and method B employs a dart with a 50 mm diameter hemispherical head dropped from a height of 1,50 m. The measurement technique is the staircase method.
Drop Dart Impact Resistance of Plastic Film ASTM D1709, ISO 7765
ASTMD5420 measures the relative ranking of materials based on the energy required to crack or break a plastic sheet when struck by a falling weight (the "Gardner Impact" method).
ASTMD3029 is designed to determine the relative ranking of rigid plastic materials based on the energy required to crack or break them under specified impact conditions.
ASTM D4226 Standard Test Methods for Impact Resistance of Rigid Poly(Vinyl Chloride) (PVC) Building Products
ASTM D4226 covers determination of the energy required to crack or break rigid poly(vinyl chloride) (PVC) plastic sheeting, profile flat sections used in building products, and extruded/molded test samples, under a free-falling standard weight striking an impactor in contact with the specimen.
Also known as the Gardner falling-weight impact test for rigid flat plastic panels. It quantifies the impact energy required to crack, puncture, shatter, or tear rigid PVC sheets, extruded profiles, and molded flat coupons via a free-falling standardized weight striking a defined impactor tip. It uniquely distinguishes ductile failure (plastic tearing, stretching) and brittle failure (sharp cracking, shattering) to characterize the ductile-to-brittle transition of PVC building plastics.
JIS Z1707 General rules of plastic films for food packaging
JIS Z1707 unifies universal technical requirements for single-layer and multi-layer plastic films (<250 μm thickness) directly contacting food for food packaging. Not include laminated films containing paper or metal foil as structural layers.The test stilupated in this standard is mainly include: Tensile test, Heat-seal strength, Puncture strength, Static / kinetic friction, Impact strength, Water vapor transmission rate, Oxygen transmission rate, Heat resistance, Wetting tension, Haze, Surface roughness, Anti-fog properties, Shrinkage etc.,
ASTM E2486 Standard Test Method for Impact Resistance of Class PB and PI Exterior Insulation and Finish Systems (EIFS)
ASTM E2486 evaluates how an EIFS laminate responds to rapid, localized deformation caused by a falling weight, and then assigns the system to a standardized impact-resistance class. It uses a drop‑weight impact setup to produce rapid deformation on EIFS specimens and judges performance based on visible breakage of reinforcing mesh under normal lighting.
ASTM C1629 Standard Classification for Abuse‑Resistant Nondecorated Interior Gypsum Panel Products and Fiber‑Reinforced Cement Panels
ASTM C1629 defines three performance grades: Level I (lowest), Level II, Level III (highest) for interior non‑decorated wall panels, purely based on laboratory mechanical abuse‑resistance test results of panel products (not full wall assembly systems). All tests inside C1629 focus on abrasion, indentation, hard‑body impact, soft‑body impact mechanical performance.
EN 477 Plastics‑Poly(vinyl chloride) (PVC)‑based profiles‑Determination of the resistance to impact of profiles by falling mass
EN 477 specifies a drop‑weight impact test for rigid unplasticized PVC‑U profiles, primarily performed at −10 °C, and can also apply for other defined test temperatures for PVC‑based profiles.
Frequently Asked Questions