Information on the most widely used ASTM standards within the materials testing industry
ASTM F3437 Small Bone Plate Tester | Metallic Orthopaedic Fracture Fixation Testing Machine | UnitedTest
UnitedTest manufactures ASTM F3437 static mechanical testing machine for miniature metallic orthopaedic bone plates for small bone fracture fixation. It delivers consistent in-vitro test data for design comparison of low-load finger, toe, cranial and upper facial bone implant plates for orthopaedic R&D and quality validation.
ASTM F3437 outlines static in-vitro mechanical test protocols for miniature metallic orthopaedic bone plates designed for small bone fracture fixation on low-load anatomical sites such as fingers, toes, cranium and upper facial bones. It establishes a repeatable baseline to compare mechanical performance across different small-bone plate designs. This standard does not cover screw-plate assembled constructs, auxiliary implant components including screws and wires, and in-vitro test results cannot be directly used to predict real in-vivo clinical performance of orthopaedic implants.
Four Stipulated Test Methods
| Test | Load mode | Direction per standard | Fixture concept | Key setup rule |
|---|---|---|---|---|
| Static torsion | Torque | Torque about the X-axis | Pinned-slot apparatus holding plate superiorly & inferiorly; only the strut unconstrained; fixed to frame with two off-axis screws; washers prevent looseness. Grips are an alternative. | 15 mm active length recommended if worst-case strut geometry fits; axial load ≈ 0 N during torsion |
| Static cantilever beam bending | Compression | Negative Z | Plate lies flat, eyelets up, one eyelet resting on steel block; strut + adjacent eyelet unsupported; bone screw passes through supported eyelet and drilled hole into polymeric insert | Fixture edge radius ≈ 0.25 mm; screw-hole taper transition at fixture edge; moment arm = force → fixture edge; screw must not loosen (post-test visual check) |
| Static lateral bending | Compression | Negative Y | Clamshell fixture block with side slot; plate inserted sideways; ≥1 eyelet (better: >1) inside to stop rotation; bushing over plate to avoid geometry interference; sliding X–Y table to avoid off-axis loading. Alternative: bone screws to fixture side (needs >1 attachment point) | Moment arm = force → point of contact/fixation with fixture |
| Static three-point bending | Compression | Negative Z | Two lower rollers + one centered upper roller, all same diameter; lower rollers sit over two adjacent screw holes, upper roller centered on the strut | Roller diameter ≤ 1/4 of the adjacent-roller spacing (H/2); cylindrical rollers if centre flatness deviation ≤ W/6, otherwise profiled rollers matching the plate cross-section |
Test Princile
All tests are destructive static in‑vitro mechanical tests under displacement‑control loading. Load‑displacement or torque‑angular‑displacement curves are recorded. Key mechanical parameters are derived from these curves:
Stiffness: maximum slope of linear elastic segment of curve.
Offset yield point: defined by permanent deformation: 0.002 × active length for bending, 2° angular offset for torsion. Yield load / yield torque is determined by offset‑yield method (offset displacement method, see Figure 1 in standard).
Ultimate load / ultimate torque: peak value on load‑displacement curve.
Corresponding displacement values at yield and ultimate points are extracted from curve data.
Test Equipment required for ASTM F3437 Test of Small Bone Plate Fracture Fixation
Universal test machine / Torsion testing machine | Must comply with ASTM E4 (force calibration), E2309/E2309M (displacement verification), E2624 (torque calibration) for force, displacement and torque calibration |
| Fixture blocks | Main body typically stainless‑steel; inserts preferably UHMWPE (ultra‑high‑molecular‑weight polyethylene), other polymers allowed with technical justification. Polymer inserts shall resist screw pull‑out under load. |
| Dedicated fixtures for each test |
|
Test parameters & stipulations
| Control mode | Displacement control for all tests |
| Rate | Recommended 5 mm/min or 25°/min; not to exceed 25 mm/min or 60°/min |
| Termination | Until failure, or until test-machine limits are reached |
| Active length / moment arm | 15 mm recommended where it captures worst-case strut geometry; may be shortened for short plates or lengthened to cover full worst-case geometry — but all plates being compared must use the same value if possible, with deviations justified |
| Yield definition | Permanent deformation = 0.002 × active length or moment arm (bending) or 2° (torsion) |
| Axial load in torsion | ≈ 0 N |
| Sample size | Minimum 5 specimens per static test |
| Outputs required | Offset yield displacement (mm or °), stiffness (N/mm or Nmm/°), offset yield load or torque (N or Nmm), displacement at ultimate load (mm or °), ultimate load or torque (N or Nmm) |
| Extra for bending | Bending yield moment (moment arm × load at yield) — lateral bending and cantilever only |
| Precision | Repeatability/reproducibility not yet established — pending interlaboratory study |
| Bias | No bias statement possible — destructive test, no acceptable reference values |
Test Specimen Information
Specimens must represent real implant production: same metallic implant‑grade material, cross‑section geometry, surface finish, marking and manufacturing process; any deviations need documentation in report.
All test plates shall be brand‑new, never previously mechanically tested.
Plates with identical cross‑section, material, hole pattern and manufacturing but different nominal lengths can be accepted as test samples.
Minimum sample size: At least five specimens for each static test condition.
Stainless‑steel fixture blocks can be reused; polymer inserts are recommended for single‑use only.
Test procedure of ASTM F3437 Test of Small Bone Plate Fracture Fixation
Select proper fixture according to target test mode, mount fixture onto test machine.
Secure bone‑plate specimen onto fixture following fixture‑specific mounting rules, ensure no slipping during loading.
Set displacement‑controlled loading rate within allowable range.
Apply load / torque in specified axis‑direction until specimen failure or machine travel limit is reached. Keep near‑zero axial force for torsion test.
Continuously record load‑displacement or torque‑angular‑displacement curves.
Derive all required mechanical metrics (stiffness, offset‑yield values, ultimate values, displacement data) from recorded curves.
Observe and document failure location and failure mode for every broken specimen.
Related Referenced Standards
| ISO 9585 | Implants for Surgery — Determination of Bending Strength and Stiffness of Bone Plates. |
| ISO 14602 | Non‑active Surgical Implants — Implants for Osteosynthesis, Particular Requirements, referenced for implant marking requirements. |
| ASTM F382 | Standard Specification and Test Method for Metallic Bone Plates |
| YY/T 1503 | Test method for fatigue performance of metal bone plates for surgical implants |
| ASTM F3437 | Standard Test Methods for Metallic Bone Plates Used in Small Bone Fracture Fixation |
| YY/T 0119.4 | Spinal implants.Components used in the surgical fixation of the spinal skeletal system.Part 4:Metallic spinal rods |
Industry Application Field
Orthopedic, craniomaxillofacial (CMF) and neurosurgical implant manufacturers — design verification and design iteration comparison for hand, foot, cranial and mid/upper-face plating systems.
Regulatory submissions — predicate/subject device mechanical comparison for small-bone plate 510(k)-type filings and technical documentation (the standard is explicitly framed as "a basis for the mechanical comparison of small bone plates").
Worst-case justification — the functional-unit/worst-case-strut framework is what regulators expect when a plate family is represented by tested extremes.
Competitive benchmarking and supplier/process-change comparison (material, manufacturing process, hole geometry changes).
Not for: mandible/wrist/ankle plates, screw or construct evaluation, fatigue life, or clinical performance claims.
Plate types per anatomical area: maxillofacial non-mandible → flat, orbital floor, orthognathic step; hand → flat, condylar; foot → flat, step, wedge, pre-contoured, complex; neurosurgical/cranial → flat, mesh-based, burr hole, orbital roof. Data borrowed from one plate type to justify another must be justified in the report.
Keywords: ASTM F3437, small bone plate tester, miniature orthopaedic bone plate test, fracture fixation plate mechanical test, static in-vitro bone plate testing, finger bone implant plate test, toe bone fixation plate tester, cranial bone plate test, maxillofacial implant mechanical test, orthopaedic implant lab tester, metallic osteosynthesis plate test, small fragment bone plate test, UnitedTest orthopaedic testing machine, medical implant mechanical tester, orthopaedic device quality control, bone plate bending test, implant design comparison test, low load orthopaedic implant test
Related products and device
Related Standard
ASTM F382 Standard Specification and Test Method for Metallic Bone Plates
ASTM F382 unified terminology, geometric classification, material requirements, marking & packaging rules, and mechanical test protocols for metallic bone plates used in surgical skeletal internal‑fixation. It define two mandatory test methods: Single‑Cycle Bend Test and Bending Fatigue Test. Both adopt four‑point bending configuration. It is of great significance for ensuring the safety and reliability of metallic bone plates, which are widely used to align and fix bone segments in orthopedic reconstructive surgeries.
ISO 25539-3 defines mechanical performance tests as core bench evaluations for filter systems (filter + delivery/retrieval/conversion systems), plus supplementary tests for materials, imaging, biocompatibility, clinical validation, sterilization and packaging. Include the Filter Tensile Strength, Torsional Bond Strength,Tensile Bond Strength, Radial Force, Force to Deploy test etc.,
Based on the ISO/TS 17137 standard the evaluation of mechanical properties is a critical part of the design and safety validation process. Mechanical Evaluation like tension, radial force, Cyclic Fatigue Durability like constant pulsing. Because absorbable implants lose their structural integrity over time through degradation, their mechanical performance must be assessed not just at the time of implantation, but throughout their intended functional lifetime.
ISO 7198 specifies test and performance requirements for tubular vascular grafts and vascular patches (surgical vascular prostheses). It defines mechanical tests (with full method/equipment/sample details) and other physicochemical, biological, dimensional, preclinical/clinical tests.
ASTM F2942 specifies in vitro test methodologies to evaluate the cyclic durability of vascular stents under non-radial mechanical deformations (axial, bending, and torsion) that occur in vivo due to musculoskeletal motion, breathing, or cardiac activity.
ASTM F1798 Standard Test Method for Evaluating the Static and Fatigue Properties of Interconnection Mechanisms and Subassemblies Used in Spinal Arthrodesis Implants.
ASTM F1798 provides standardized methods for mechanically testing the interconnections within spinal implant systems. It is for evaluating the uniaxial static/fatigue strength and loosening resistance of interconnection mechanisms in spinal arthrodesis implant subassemblies, providing a standardized way to characterize mechanical performance of connections like rod-clamp, screw-rod, and hook-rod assemblies. It is critical for design validation, regulatory compliance, and clinical safety in the spinal implant industry.
ASTM F2502 Standard Specification and Test Methods for Absorbable Plates and Screws for Internal Fixation Implants
ASTM F2502 defines the requirements and mechanical test methods specifically for bioabsorbable (or biodegradable) orthopedic implants used to stabilize bone fractures. Unlike permanent metal implants, these devices are designed to provide temporary support and then gradually dissolve in the body. This standard ensures they possess sufficient initial mechanical strength and that their degradation properties are characterized in a standardized way.
ASTM F2706 is a critical biomechanical evaluation tool in the medical device industry, specifically for spinal implants. ASTM F2706 establishes standardized mechanical test methods to evaluate the static (strength) and fatigue (long-term durability) performance of spinal implant assemblies intended for use in the occipito-cervical (OC) and cervico-thoracic (CT) regions (from the skull to the upper back). It simulates a worst-case scenario: a complete vertebrectomy (removal of a vertebra), creating a highly unstable spine segment that the implant must stabilize.
ASTM F2706 establishes standardized mechanical test methods to evaluate the static (strength) and fatigue (long-term durability) performance test, defines in‑vitro mechanical test protocols for posterior occipital‑cervical (OC) and occipital‑cervical‑thoracic (OCT) spinal fixation assemblies under a vertebrectomy worst‑case model, aiming for relative mechanical comparison of implant designs, rather than defining pass‑fail performance thresholds.
ASTM F1717 Standard Test Methods for Spinal Implant Constructs in a Vertebrectomy Modelis a fundamental standard for evaluating the static and fatigue mechanical performance of spinal implant assemblies. Unlike ISO 12189, which focuses on a single device(an interbody cage), ASTM F1717 tests the entire posterior spinal construct—typically rods, screws, and cross-connectors—stabilizing a segment where a vertebral body has been removed (a "vertebrectomy" or "corpectomy" model). It simulates worst-case spinal instability to assess the implant's ability to maintain alignment and support loads.
ASTM F2068: Standard Specification for Femoral Prostheses – Metallic Implants
ASTM F2068 covers metallic stemmed femoral prostheses used to replace the natural hip joint by means of hemi-arthroplasty or total hip surgical procedures. Prostheses for hemi-arthroplasty are intended to articulate with the natural acetabulum of the patient. Prostheses for total hip replacement are intended to articulate with prosthetic acetabular cups. Prostheses may have integral femoral heads or cones designed to accept modular heads.
The mechanical strength (fatigue test ISO 7206-4, ISO 7206-6, shear strength test ASTM F1044, tensile test ASTM F1147, abrasion resistance test ASTM F1978), corrosion resistance, and biocompatibility of the head portions of one-piece integral implants are covered by this specification.
ASTM F3495 Standard Test Methods for Determining the Static Failure Load of Ceramic Knee Femoral Components
ASTM F3495 defines two destructive test procedures to measure the static ultimate failure load of ceramic femoral components used in total knee replacement (TKR), specifically for cruciate retaining (CR) designs that cover the medial/lateral condyles and patellar surface. Both procedures simulate physiological in vivo loading conditions; one additionally replicates intraoperative impaction loading. Modifications may be required to accommodate alternative femoral component geometries.
ASTM F3437 Test of Small Bone Plate Fracture Fixation: Frequently Asked Questions
Q1. What is ASTM F3437?
ASTM F3437-23 is the Standard Test Methods for Metallic Bone Plates Used in Small Bone Fracture Fixation. Current edition approved 1 April 2023 (DOI 10.1520/F3437-23), under ASTM Committee F04 / Subcommittee F04.21 on Osteosynthesis. It provides static test methods — torsion and three bending configurations — for metallic plates used in minimally load-bearing anatomy.
Q2. Which implants are in scope, and which are excluded?
In scope: plates for fingers, toes, cranium and upper face (midface). Explicitly excluded: lower face/mandible, wrist and ankle plates — those are larger and substantially loaded, so they must be evaluated by other methods (typically ASTM F382).
Q3. Is it only for metals?
Yes — the standard covers metallic bone plates (implant-grade stainless steel, titanium and titanium alloys, cobalt-chrome, etc.). Materials must be biocompatible and intended for surgical implant use; ASTM Subcommittee F04.12 maintains the relevant material specifications.
Q4. Does F3437 include a fatigue test?
No. F3437-23 is static testing only (torque or load applied monotonically to failure). Cyclic/durability evaluation of bone plates is covered by ASTM F382 Annex A2 and other fatigue standards.
Q5. Does it evaluate screws, wires or the whole construct?
No. the standard does not address the mechanical performance of the plating construct or accessory components such as screws and wires. Screw testing belongs to ASTM F543; construct testing is a separate biomechanical study.
Q6. What is a "functional unit"?
A simplified worst-case configuration: a single-line fracture spanned by a plate with one screw hole on each side of the fracture. It makes worst-case strut geometry easy to define. If a plate's shape or hole pattern does not allow this, tests may be modified or dropped — with rationale documented.
Q7. How do I choose the worst case?
Always evaluate the weakest strut and/or screw-hole geometry, and consider worst-case loading orientation. Plates for comparison must be tested in the same orientation unless a deviation is justified. For plates with a "bone interface" side, orientation must be a deliberate choice.
Q8. What testing machine do I need?
A machine conforming to ASTM E4 (force calibration/verification), E2309/E2309M (displacement measurement verification) and E2624 (torque calibration). Practically:
A low-capacity electromechanical UTM (typically ≤1–2 kN) with fine displacement control for the three bending tests.
A torsion channel or dedicated torsion tester (low N·m range, angular resolution ≤0.1°) for static torsion.
An axial-torsion (biaxial) system is the most efficient single-frame solution because it covers all four methods.
Q9. Why UHMWPE inserts?
The insert receives the bone screw in the cantilever fixture. It must be rigid enough that the screw cannot pull out axially during the test. Other polymers are allowed if justified. Steel blocks may be reused if undamaged; polymeric inserts are recommended for single use.
Q10. What is the recommended active length / moment arm?
15 mm, provided it captures the worst-case strut geometry. It may be shortened for very short plates or lengthened to include the full worst-case geometry — but all plates being compared must use the same value whenever possible, and any deviation must be justified in the report.
Q11. At what speed is the test run?
Displacement control, recommended 5 mm/min or 25°/min, and never faster than 25 mm/min or 60°/min. Continue until failure or until the test machine limits are reached.
Q12. What axial load applies during torsion?
Approximately zero newtons — the plate must be twisted without an axial preload.
Q13. How is yield defined?
Bending: permanent deformation equal to 0.002 × active length (or moment arm) — the classic 0.2 % offset.
Torsion: a permanent angular deformation of 2°.
Q14. Which related standards are cited?
ASTM F382 and ISO 9585 (alternative bone-plate test methods), ISO 14602 (particular requirements for osteosynthesis implants), ASTM E4, E2309/E2309M, E2624 (machine calibration), ASTM F983 (permanent marking), ASTM F2503 (MR-environment labeling).
Q15. How does F3437 differ from ASTM F382?
F382 uses four-point bending (Annex A1 single-cycle, Annex A2 fatigue at R = 0.1) and suits larger plates; its fixture becomes hard to set up at small-plate scale. F3437 offers four static methods scaled to small plates, with 15 mm spans, and contains no fatigue annex.
Q16. How does it differ from ISO 9585?
ISO 9585 is a static bending method for straight plates and is not recommended for plates shorter than 50 mm or for intramedullary-associated devices — precisely the population F3437 was written for.
Q17. Why is ASTM F3437 testing important?
It converts a plate's material, cross-section and hole geometry into comparable, defensible numbers: stiffness, yield and ultimate strength, and failure location. Those numbers drive design iteration, material selection, worst-case justification and regulatory submission for hand, foot, cranial and midface plating systems.
Q18. Why is bending stiffness clinically significant?
the plate is the primary stabilizer of the fragments, and bending stiffness directly affects the rate and completeness of healing. Too stiff → stress shielding of the fracture; too compliant → excessive gap motion. That is why stiffness, not just strength, is a mandatory output.
Q19. Why choose ASTM F3437‑23 Testing Machine & Custom Fixture Solutions from UnitedTest?
UnitedTest manufactures ASTM F3437‑23 compliant test machines & custom fixtures for static torsion, cantilever, lateral & three‑point bending of small metallic bone plates for orthopedic implant R&D and regulatory verification.
UnitedTest is a professional manufacturer of mechanical testing systems and custom test fixtures for orthopedic medical‑device validation. Our complete test solutions fully comply with ASTM F3437‑23 Standard Test Methods for Metallic Bone Plates Used in Small Bone Fracture Fixation, supporting implant R&D, quality control and FDA‑aligned pre‑market bench evaluation for small bone plates used for fingers, toes, cranium and upper‑face fracture fixation.
ASTM F3437‑23 specifies four optional static loading modes: static torsion, static cantilever‑beam bending, static lateral bending and static three‑point bending. Conventional universal testers lack properly sized miniature fixtures for tiny orthopedic plates, leading to specimen slippage, mis‑alignment and non‑compliant test results. UnitedTest delivers turn‑key hardware‑software packages including servo‑controlled main test frame, torsion module, and custom‑built fixtures following F3437‑23 drawing specifications:
‑ Torsion test fixture: pinned‑slot clamping, anti‑loosening washer structure, configurable 15 mm reference active‑length
‑ Cantilever‑beam bending fixture: UHMWPE polymer insert, 0.25 mm fixture corner radius, adjustable moment‑arm
‑ Lateral‑bending clamshell fixture: anti‑rotation design, optional XY sliding stage to eliminate off‑axis loading
‑ Three‑point‑bending roller fixture: cylindrical or profiled rollers complying with F3437‑23 roller‑diameter rules for flat or crescent‑section bone plates.
Our test machines satisfy ASTM E4, E2309/E2309M and E2624 calibration requirements for force, displacement and torque measurement. The dedicated test software runs displacement‑controlled loading sequences, auto‑records load‑displacement / torque‑angle curves, and calculates key parameters: stiffness, offset yield load / torque, ultimate load / torque, yield displacement and ultimate displacement. Exportable test reports help you meet ASTM F3437‑23 reporting requirements for regulatory submissions.
Custom‑engineered miniature fixtures optimized for mini orthopedic implants; support standard 15 mm span plus user‑defined active‑length / moment‑arm.
High‑precision force‑torque sensors with traceable calibration for medical‑device lab compliance.
Pre‑configured software workflows for torsion, cantilever bending, lateral bending and three‑point bending test sequences.
Engineering support for fixture modification; we supply documentation for fixture deviations to include in your final test report.
Our platforms support extra orthopedic implant standards including ASTM F382, ASTM F543, ISO 9585 and ISO 14602.
Contact UnitedTest to request quotation for ASTM F3437‑23 testing machine and custom fixture kits.
Require More Customized Solutions?