Information on the most widely used ASTM standards within the materials testing industry
ASTM D7264 Flexural Tester for Polymer Matrix Composite Materials | UnitedTest
UnitedTest manufactures ASTM D7264 composite flexural testing machines to measure flexural strength, modulus, strain and load-deflection behaviour of polymer matrix composites using method A and method B quasi-static beam bending tests.
ASTM D7264 is the standard test method for determining flexural properties of polymer matrix composite materials. It captures key performance indicators including flexural strength, flexural modulus, flexural strain and full load‑deflection response under quasi‑static beam bending. Two separate loading procedures, Method A and Method B, are defined to suit different specimen setups and test requirements. UnitedTest provides precision ASTM D7264 flexural test systems for composite material R&D, incoming inspection and quality control in aerospace, automotive and industrial composite labs.
Test Principle
A rectangular cross‑section bar resting on two supports is deflected at a constant crosshead rate while force and mid‑span deflection are recorded continuously until failure occurs on an outer surface (or a predefined deformation is reached).
Properties are extracted with classical (homogeneous) beam theory:
Procedure A flexural stress: σ = 3PL / (2·b·h²)
Procedure B flexural stress: σ = 3PL / (4·b·h²)
Procedure A max strain: ε = 6·δ·h / L²
Procedure B max strain: ε = 4.36·δ·h / L²
Flexural chord modulus (default): E = Δσ / Δε over the strain window 0.001 → 0.003
Secant modulus (optional): E = L³m / (4·b·h³) for A, and ≈ 0.17·L³m / (b·h³) for B, where m is the slope of the secant on the force–deflection curve
Where P = force, L = support span, b = width, h = thickness, δ = mid‑span deflection.
Specific Test Methods
Procedure A (Three‑point bending)
A rectangular beam specimen rests on two simple supports. A single central loading nose applies downward force at the mid‑point of the support span. Maximum bending stress occurs directly underneath the central loading nose. Vertical shear force exists across most of the beam length.
Procedure B (Four‑point bending)
The specimen sits on two outer supports, loaded by two symmetric loading noses. The distance between the two loading noses (load span) equals one‑half of the support span. Between the two inner loading points, bending moment stays constant and shear force becomes zero, so maximum flexural stress is uniformly distributed over the load‑span region.
Test Equipment required for ASTM D7264 Flexural test for Polymer Matrix Composites
Recommend UnitedTest Universal Testing Machine and Bending fixtures.
| Universal testing machine | Constant cross‑head displacement control; force measurement error ≤ ±1 % full‑scale, inertia lag ≤ 1 % measured force. Calibration follows ASTM E4 practice. |
Loading noses & supports (3 and 4 point bending fixture) | Cylindrical, hardness ≥ 55 HRC, finely ground, no burrs, sharp edges relieved; radius 5.0 ± 0.1 mm (both nose and supports) unless otherwise agreed; may be fixed, rotatable or rolling (fixed/rotatable typical for composites).
|
| Deflection‑measuring hardware | Accuracy ±1 % of expected max displacement, contacting the specimen at the centre of the support span, stationary relative to the supports, auto‑recording |
| Micrometers / calipers | 4–8 mm ball anvil on irregular (bag‑side) surfaces, flat anvil on machined edges; flat anvils for length; accuracy ±0.02 mm for width/thickness, ±0.1 mm for length (i.e. read to within 1 % of dimension) |
Test Specimen Information
Standard geometry: thickness 4 mm, width 13 mm, span‑to‑thickness ratio 32:1 (→ standard span 128 mm), length ≈ 20 % longer than the span (~154 mm). Drawings are given in both SI and inch‑pound versions.
Fabric‑reinforced textile composites: width must be at least two unit cells (per D6856).
If 4 mm cannot be produced, use another thickness but keep 32:1 and keep width 13 mm. Optional ratios 16:1, 20:1, 40:1, 60:1 are allowed only if noted in the report — and data from different span‑to‑thickness ratios must not be compared.
Quantity: at least 5 specimens per condition (fewer only in designed experiments); consult E122 for statistically significant sampling.

Key Test Parameters:
Standard cross‑head rate: 1.0 mm/min (0.05 in/min) for standard‑dimension specimens. Adjust rate for non‑standard thickness to keep similar outer‑fiber strain rate, and document any modified test speed.
Support span L: Measured physically (not set‑value). Resolution: 0.1 mm for spans <63 mm; 0.3 mm for spans ≥63 mm. The measured span value is used in all formula calculations.
Data sampling: Minimum of 50 data points on each force‑deflection curve; higher sampling rate for capturing non‑linearity and progressive failure damage.
Span‑to‑thickness ratio: 32:1 baseline to suppress interlaminar‑shear‑dominated short‑beam failure. If >50 % specimens fail by shear, increase span‑thickness ratio for retesting.
Details Test Procedures of ASTM D7264 Flexural test for Polymer Matrix Composites
Condition and store specimens in the conditioned environment until test time.
Measure and record width b, thickness h at mid‑section and the length, to the specified accuracy.
Measure the span L to ±0.1 mm for L < 63 mm, ±0.3 mm for L ≥ 63 mm — and use the measured span in all calculations.
Set speed: 1.0 mm/min crosshead for standard specimens (alternative rates must be requested and reported; scale per D790 for A or D6272 for B).
Align noses and supports so cylindrical axes are parallel; for A the nose is midway between supports, for B the load span is ½ of the support span and symmetric. Specimen long axis perpendicular to noses/supports.
Apply force, recording ≥ 50 data points on the force–deflection curve (more if non‑linearity or progressive failure is expected).
Record failure mode, area and location using the standard three‑part failure identification code (multi‑mode failures list all applicable codes).
Test Application (Industry & Material Scope)
Aerospace — material qualification, design allowables, batch/lot acceptance for carbon/epoxy and glass/epoxy laminates.
Wind energy, marine, automotive, rail — spar caps, hull panels, body/structural panels.
Sporting goods, pressure vessels/pipes, construction & infrastructure (FRP rebar, bridge deck panels, strengthening laminates).
Any composite manufacturer/lab — quality control and specification compliance, process stability checks (cure, fibre volume, voids), ranking material systems, screening environmental effects (temperature, moisture, fluids) to identify design drivers, and generating flexural data for full structures.
Related Standard:
| ASTM D790 | Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials |
| ISO 14125 | Fibre-reinforced plastic composites -- Determination of flexural properties |
| ASTM D6272 | Standard Test Method for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials by Four-Point Bending |
| ASTM D7264 | Standard Test Method for Flexural Properties of Polymer Matrix Composite Materials |
| ISO 178 | Plastics — Determination of flexural properties |
| GB/T 9341 | Equivalent to using ISO 178 |
| JIS K 7171 | Japan standard Basically consistent with the technical content of ISO 178. (プラスチック-曲げ特性の求め方) |
| ISO 1209-1 | Rigid cellular plastics - Determination of flexural properties - Part 1: Basic bending test |
| ISO 1209‑2 | Companion part of the same series; determines flexural strength and apparent flexural modulus of elasticity for rigid cellular plastics (calculates formal flexural mechanical properties) |
| ASTM D2344 | Short‑beam strength — when a short span makes a composite delaminate, you are measuring interlaminar shear, not flexural strength. |
| EN 12089 | Thermal insulating products for building applications — Determination of bending behaviour. Three-point loading, Method A on full-size products and Method B on specimens (thickness ≤ 100 mm, length 5×thickness + 50 mm, width 150 mm); support diameters 80 ± 3 mm or 30 ± 3 mm; span 300–1200 mm (A) / 200–500 mm (B); ≥ 3 specimens; conditioning ≥ 6 h at (23 ± 5) °C; repeatability ≈ 5 %, reproducibility ≈ 15 %. It is the European product-level counterpart (harmonised under the Construction Products Regulation), whereas ISO 1209-2 is a material-level method. |
| DIN 53423 | Germany corresponding bending test for rigid foams. |
| ASTM C203 | Standard Test Methods for Breaking Load and Flexural Properties of Block-Type Thermal Insulation, commonly used in North America as the functional counterpart for insulation boards. |
Keywords: ASTM D7264 flexural tester, polymer matrix composite bending test machine, composite flexural strength tester, composite flexural modulus test equipment, quasi-static beam bending tester, ASTM D7264 method A and B test, fibre reinforced composite flexural test instrument, composite material mechanical testing machine, load deflection composite tester, UnitedTest composite flexural test system, FRP bending test rig, ASTM D7264 test machine · ASTM D7264 flexural testing machine · composite flexural testing machine · three-point / four-point bending test machine for composites · universal testing machine for ASTM D7264 · polymer matrix composite flexural test equipment
Related products and device
Related Standard
ISO 178 Plastics - Determination of flexural properties
ISO 178 specifies a method for determining the flexural properties of rigid and semi-rigid plastics under defined conditions. A standard test specimen is defined, but parameters are included for alternative specimen sizes for use where appropriate. A range of test speeds is included.
ISO 178 test method is used to investigate the flexural behaviour of the test specimens and to determine the flexural strength, flexural modulus and other aspects of the flexural stress/strain relationship under the conditions defined. It applies to a freely supported beam, loaded at midspan (three-point loading test).
ISO 1209-2 Rigid cellular plastics - Determination of flexural properties - Part 2: Determination of flexural strength and apparent flexural modulus of elasticity
ISO 1209-2 specifies a three-point bending test method to determine, on rigid cellular plastics: Flexural strength (R) — the maximum fibre stress the foam develops in bending; Apparent flexural modulus of elasticity (E) — the stiffness in bending.
The word "apparent" is deliberate: cellular plastics are not homogeneous continua — the measured stiffness includes shear deflection and local cell-wall crushing/indentation under the loading and support edges, so E is an engineering, configuration-dependent value, not a true material constant valid for all geometries.
ISO 1209‑1 Rigid cellular plastics — Determination of flexural properties — Part 1: Basic bending test
ISO 1209‑1 is an simple three‑point‑bending test to evaluate bending performance of rigid cellular plastic bars. This test measures load at specified deflection or breaking load, but it cannot calculate flexural strength or apparent flexural modulus because small specimens do not establish pure‑bending stress state; those mechanical parameters are covered in ISO 1209‑2. It applies only to foams ≥20 mm thickness and is invalid for materials showing obvious crushing during testing.
ISO 14125 Fibre-reinforced plastic composites -- Determination of flexural properties
ISO 14125 specifying test methods to measure flexural properties of fibre‑reinforced plastic composites, covering both thermoplastic and thermoset composite materials (glass, carbon, aramid‑fibre reinforced laminates, SMC, BMC, GMT etc.). It defines two loading configurations: Method A (three‑point flexure) and Method B (four‑point flexure). It is intended for material screening and quality‑control rather than direct structural design input.
ASTM C203 — Standard Test Methods for Breaking Load and Flexural Properties of Block-Type Thermal Insulation
ASTM C203 evaluates breaking load and flexural properties (flexural strength / modulus of rupture) of pre‑formed block‑type thermal insulation and cellular plastics by simple‑beam bending tests.
ASTM D790: Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials
ASTM D790 determines flexural (bending) properties for unreinforced plastics, reinforced plastics, high‑modulus composites and electrical insulating materials via three‑point bending on simply‑supported rectangular beam specimens. It applies to rigid and semi‑rigid materials. Flexural strength cannot be calculated if the specimen neither yields nor fractures on its outer surface before reaching 5 % maximum outer‑fiber strain.
FAQs for ASTM D7264 (Flexural Test for Polymer‑Matrix Composites)
Q1. What is ASTM D7264?
ASTM D7264/D7264M-21 is the ASTM International standard test method "Standard Test Method for Flexural Properties of Polymer Matrix Composite Materials." It is maintained by ASTM Committee D30 (Subcommittee D30.04). The current edition was approved 1 January 2021 and published February 2021 (originally approved 2006; previous edition 2015). It determines the flexural stiffness and strength of continuous-fiber-reinforced polymer matrix composites (PMCs).
Q2. What properties does the test actually produce?
Flexural strength, flexural chord modulus of elasticity (over the 0.001–0.003 strain range), flexural secant modulus (optional), maximum flexural strain, flexural stress at a given strain, and the full force–deflection (load–deflection) behaviour of the specimen.
Q3. What are Procedure A and Procedure B?
Procedure A = three-point bending: the bar rests on two supports and is loaded by a single loading nose midway between them.
Procedure B = four-point bending: two loading noses, each an equal distance from the adjacent support, with the load span fixed at one-half of the support span.
Q4. Why does D7264 only allow the half-span four-point configuration?
Unlike ASTM D6272 (which permits loading at both one-third and one-half of the support span), D7264 permits only one-half — to standardise the geometry and simplify the calculations. This is a deliberate restriction; do not mix load spans.
Q5. Which procedure should I choose, A or B?
Procedure A (3-point) is best for screening, QC pass/fail and quick comparisons. Maximum moment is concentrated at mid-span; shear is present everywhere except directly under the nose.
Procedure B (4-point) creates a constant-moment, shear-free zone between the two load points, so a much larger volume of material is stressed at the maximum level. It is preferred for modulus determination and research because shear deformation does not depress the apparent modulus in that region.
Whichever you pick: use the same procedure for every specimen in a comparison. The two procedures generally give slightly different values.
Q6. What is the standard specimen geometry?
Thickness 4 mm, width 13 mm, support span-to-thickness ratio 32:1 (→ standard span ≈ 128 mm), and overall length about 20 % longer than the span (≈ 154 mm). Separate SI and inch-pound drawings are given in the standard.
Q7. Can I use a different thickness or span ratio?
Yes, but with conditions. If 4 mm cannot be produced, use another thickness while keeping the 32:1 ratio and the 13 mm width. Optional ratios of 16:1, 20:1, 40:1 and 60:1 are permitted only if noted in the report. Critically: data from one span-to-thickness ratio must never be compared with data from another. For fabric-reinforced textile composites the width must contain at least two unit cells (per ASTM D6856).
Q8. Why 32:1 and not the 16:1 used by D790?
D7264 was developed specifically for continuous-fiber composites. The 32:1 ratio is chosen so that failure is driven by the bending moment at the outer surface, not by out-of-plane (interlaminar) shear. Short-beam shear failure is the domain of ASTM D2344/D2344M; D7264 is deliberately designed to interrogate long-beam strength and to keep shear deformation from depressing the measured modulus of highly orthotropic laminates.
Q9. How should deflection be measured — can I use crosshead travel?
No. Deflection must be measured with a calibrated device (accuracy ±1 % of expected maximum displacement) contacting the specimen at the centre of the support span, mounted stationary relative to the supports. Crosshead or loading-nose motion ignores specimen rotation about the noses and the compliance of the loading nose and crosshead, and will give wrong modulus and strain values.
Q10. What test speed is specified?
1.0 mm/min crosshead rate for standard-dimension specimens. For non-standard dimensions, scale the rate to produce a similar outer-surface strain rate using the methods in D790 (Procedure A) or D6272 (Procedure B). Alternative rates are allowed only if requested and reported.
Q11. How much force capacity does my machine need for a standard specimen?
For the standard 4 mm × 13 mm specimen at a 128 mm span, Procedure A gives P ≈ 1.08 N per MPa of flexural strength. So a 1000 MPa carbon/epoxy laminate peaks at only about 1.1 kN, and a 2000 MPa material at about 2.2 kN. A 5 kN or 10 kN frame with a suitably sized load cell is therefore the normal choice — capacity is rarely the issue; force-measurement accuracy and crosshead speed control at 1 mm/min are what matter.
Q12. Why is my measured flexural modulus lower than the tensile modulus?
Most common causes: (a) shear deformation in highly orthotropic laminates tested at low span-to-thickness ratios; (b) the result is an apparent modulus derived from homogeneous beam theory while the specimen behaves as a plate — deviations grow with width and with a high proportion of ±45° plies; (c) stacking sequence effects — flexural modulus and strength of multidirectional laminates are stacking-sequence dependent and need not correlate with extensional modulus, which is not. Use a high span-to-thickness ratio, and in extreme cases run separate specimen sets for modulus and for strength.
Q13. Can I compare my results with data from D790, ISO 14125 or GB/T 1449?
Not directly. Different span-to-thickness ratios, nose/support radii and test speeds produce systematically different numbers (for example, GB/T 1449's 16:1 ratio and 10 mm/min tend to introduce interlaminar shear and yield somewhat lower strength values than D7264's 32:1 and 1 mm/min). Treat each standard's data as a self-consistent set.
Q14. Why is flexural testing so widely used for composites?
Four practical reasons: (1) No grips, tabs or load-introduction hardware are needed, avoiding the gripping and alignment problems of tensile and compression tests; (2) bending loads one face in tension and the other in compression simultaneously, which is how real structures are loaded, and the failure mode tells you which side governs; (3) the results are highly sensitive to matrix state, fibre–matrix interface, cure, void content, fibre volume fraction and stacking sequence, making it an excellent process-stability and QC probe; (4) combined with short-beam shear (D2344), it separates in-plane flexural capability from through-thickness shear capability.
Q15. Why choose ASTM D7264 Flexural Testing Machine & Fixtures from UnitedTest?
UnitedTest manufactures ASTM D7264/D7264M‑21 compliant flexural testing machines & 3‑point / 4‑point bending fixtures for polymer‑matrix composite laminates. Accurate flexural strength & modulus test solution for aerospace, wind‑energy & automotive composite materials.
UnitedTest supplies complete mechanical testing solutions complying with ASTM D7264/D7264M‑21 Standard Test Method for Flexural Properties of Polymer Matrix Composite Materials, for continuous‑fiber reinforced composite laminates including carbon‑fiber, glass‑fiber and textile‑fabric reinforced polymer composites.
Our universal testing machines are configured for both Procedure A (three‑point bending) and Procedure B (four‑point bending) per D7264 requirements, equipped with precision composite flexural test fixtures: 5.0 mm radius loading noses & supports (HRC≥55), alignment jigs, independent mid‑span deflection transducer mounting interface, and test software supporting toe‑compensation correction, stress‑strain calculation, failure‑mode logging and automatic statistical output (mean, standard deviation, CV value).
Our test system follows critical D7264 specifications:
Supports adjustable support‑span setting for standard 32:1 span‑to‑thickness ratio, also compatible with optional 16:1, 20:1,40:1,60:1 ratios
Avoids cross‑head‑displacement‑based deflection error; supports external deflectometer input for true specimen mid‑span deflection measurement
Pre‑programmed calculation templates for D7264 three‑point / four‑point flexural stress, outer‑fiber strain, flexural chord modulus (0.001‑0.003 strain range), secant modulus
Data sampling meets ≥50 points per force‑deflection curve requirement
UnitedTest D7264 composite flexural test systems serve quality‑control labs, composite R&D institutes, aerospace component manufacturers, wind‑turbine blade factories and automotive lightweight composite developers. Our equipment also supports related composite standards: ASTM D2344 short‑beam shear, ASTM D3039 tensile test, ASTM D5687 specimen preparation guidance.
Contact UnitedTest for custom quotes for ASTM D7264 flexural testing machine, interchangeable 3‑point / 4‑point composite bending fixture, training and test‑method setup support.
Require More Customized Solutions?