Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D2241 PVC SDR Pressure Rated Pipe Testing Methods

ASTM D2241 PVC SDR Pressure Rated Pipe Testing Methods

Share:

ASTM D2241 PVC SDR Pressure Pipe Testing Machine | UnitedTest

UnitedTest supplies ASTM D2241 compliant testing equipment for Poly(Vinyl Chloride) SDR series pressure-rated pipe. Perform sustained pressure, burst pressure, flattening, impact and extrusion quality tests for pressurized water and compatible liquid PVC piping systems.


ASTM D2241 governs SDR‑series PVC pressure pipes for pressurized water and chemically‑compatible pressurized liquids. The mechanical performance tests include sustained pressure, burst pressure, flattening, extrusion quality and impact, plus marking rules. UnitedTest manufactures reliable ASTM D2241 PVC pipe test machines to verify long-term pressure integrity, structural stability and production quality for PVC pressure pipe manufacturers and third-party laboratories.

Industry application fields

  • Municipal & rural potable water: distribution mains, service lines, transmission lines (NSF/ANSI 61 + NSF 14 evaluation, "NSF-pw" mark).

  • Irrigation: agricultural drip/sprinkler mains, turf and golf-course systems, greenhouse water lines.

  • Industrial fluid handling: process water, brine, chemicals compatible with PVC-U, cooling water, slurry/dredge lines at low pressure.

  • Water reuse / reclaimed water (purple-pipe marking rules), dewatering, well and pump columns, temporary bypass lines.

  • Plumbing/fluid-handling OEMs and distributors who need a psi rating traceable to a recognized ASTM specification for permitting, tendering and insurance.

  • Competitor/adjacent specs a lab will meet alongside it: AWWA C900/C905 (DR classes), ISO 1452 / EN 1452 (PN classes, MRS-based), ASTM D1785 (Schedule 40/80/120 PVC), D2720/D2665 (sewer/DWV).

ASTM D2241 PVC SDR Pressure Rated Pipe Testing Methods

Test — what D2241 actually requires

#Requirement MethodSpecimensPass criterion
1Dimensions & tolerancesD2122 (OD, out-of-roundness, wall thickness)Any length; Within Table 1 OD/ovality and Table 2 min wall + tolerance
2Sustained pressureD1598 (1000 h, constant internal pressure, water, 73 °F)6 specimens0 failures of 6 pass; 1 failure → retest 6 more; any failure in retest = reject
2aOptional substitute: Accelerated regression testD1598 + D2837 statistics≥6 (3 at ≤0.10 h, 3 at ≈200 h)100 000-h projection ≥ HDB category of the material (e.g. PVC 1120 → 4000 psi HDB, 3830 psi 85 % LCL)
3Burst pressure (quick burst)D1599≥5 specimensMin burst pressures in Table 4; test time ≥60 s per specimen
4FlatteningD22413 specimens, 2 in. (50 mm) longNo splitting, cracking or breaking after compression
5Extrusion quality (fusion)D2152 acetone immersionAs cut, ≥13 mm; wall thinned if >3.2 mmNo flaking/disintegration ("attack")
6Impact resistanceD2444 (Tup B, flat-plate holder, 20 lb tup)10 specimens (¼–12 in.)≥9 pass = lot passes; ≥2 fail = lot fails


Major Mechanical & Pressure‑related Tests Specified in ASTM D2241

1, Sustained Internal Hydrostatic Pressure TestEvaluate long‑term static pressure resistance under constant internal water pressure; simulates long‑term underground water‑distribution working condition.
Test standardASTM D1598
Test Equipment

Hydrostatic pressure test bench (constant‑pressure water system, end closure fixtures, pressure monitoring within ±10 psi / 670 kPa, temperature control system).

Test Stipulation

Test pressure values from D2241 Table 3 (73 °F / 23 °C water). Hold pressure for 1000 hours. Failure includes burst, ballooning, weeping, cracking.

Pass‑fail rule: 2 out of 6 specimens fail → test failure; 1 out of 6 fails → retest additional six specimens; one failure in retest → overall failure

Test Specimen info

6 pipe specimens. Specimen length: ≥10 × nominal diameter, minimum 10 in (250 mm), maximum 3 ft (1000 mm) between end closures.

At least half specimens shall retain original pipe marking in the central test zone (central zone ≥ one pipe‑diameter away from end caps)

Test Procedure

Random sampling; install end closures; fill with water; raise to specified test pressure; maintain constant pressure and 23 °C temperature for full 1000 h; continuously monitor for failure events per D1598 protocol

Accelerated regression alternative six or more specimens, three failing at ≤0.10 h and three at ≈200 h, then least-squares regression per D2837 to the 100 000-h intercept; the extrapolated HDB/LCL must meet the material's HDB category. This is the test most modern labs prefer, because it delivers a verdict in days instead of 6 weeks.
2, Burst Pressure TestMeasure short‑term hydraulic burst resistance; assess short‑term overload capacity of PVC pressure pipe.
Test standardASTM D1599
Test Equipment

Hydrostatic burst pressure test machine, pipe end‑closure fixtures, pressure recorder.

Test Stipulation

Minimum burst pressure requirements from D2241 Table 4; test medium water at 23 °C. Each specimen test duration ≥60 seconds; 

larger‑diameter pipes may need longer ramp‑up time; longer pressurizing time makes pass criteria harder to achieve

Test Specimen infoAt least five pipe specimens, same length requirements as sustained‑pressure specimens.
Test Procedure

Follow ASTM D1599 procedure; pressurize specimen until burst; record burst pressure value for each sample.

3, Flattening Test

Check ductility; detect brittleness, internal cracks or poor extrusion quality under large compressive deformation

Test EquipmentUniversal tensile testing machine with parallel flat platens.
Test Stipulation

No splitting, cracking or breaking after flattening.

Test Specimen infoThree pipe specimens, each 2 in (50 mm) long.
Test procedure

Compress specimens between parallel platens until platen distance = 40 % of pipe outer diameter. 

Complete compression within 2‑5 minutes at uniform loading speed. 

Remove load and visually inspect for crack/split/breakage. No separate referenced ASTM number;

4, Extrusion Fusion Quality TestVerify adequate fusion during extrusion; insufficient fusion will lead to premature pipe brittleness and failure in service.
Test standardAcetone Immersion Test, ASTM D2152
Test EquipmentAcetone immersion container, temperature‑controlled bath.
Test StipulationNo flaking or disintegration after acetone immersion.
Test Specimen infoExtruded pipe segments.
5, Falling‑Weight Impact Resistance TestQuality‑control check for impact toughness; note: this test is for QC only, not full service‑simulation test; it loses QC significance for pipe sizes >12 inch (305 mm).
Test StandardASTM D2444
Test EquipmentFalling‑weight impact tester (tup, drop‑height adjustment, flat‑plate support fixture).
Test StipulationImpact energy requirements from D2241. Test at 23 °C; use Tup B, flat‑plate support, 20‑lb (9 kg) tup. For 4‑12 inch nominal pipe size: ten specimens tested; ≥9 pass = lot accepted; ≥2 fail = lot rejected.
Test Specimen infoSpecimen length = nominal OD, min 6 in. (152 mm), burrs removed, random angular orientation, impact at the top of the vertical diameter, once per specimen.
Test Procedure

Follow D2444 falling‑weight impact procedure at specified drop energy; record pass / fail of each specimen.


Why this standard is critical for lining materials

  1. Unified design logic via SDR system: SDR links pipe outer diameter, wall thickness, hydrostatic design stress and pressure rating. The same SDR delivers consistent pressure rating for all nominal pipe sizes for a given PVC compound. This simplifies engineering selection, procurement and design work for civil and plumbing engineers.

  2. Dual evaluation of short‑term and long‑term material performance: PVC pressure pipe failure in service is often long‑term creep rupture under constant internal pressure. D2241 combines short‑term tests (burst, flattening, impact, acetone fusion) and long‑term sustained hydrostatic pressure test / accelerated regression test, to verify both instant overload capacity and long‑term creep‑resistance performance of PVC compounds and extruded pipesASTM Inter....

  3. Material quality gate‑keeper: It defines minimum compound requirements (D1784 grades), limits rework‑material usage, checks extrusion fusion quality. Poor fusion or wrong PVC formulation will lead to underground premature pipe cracking, leakage or burst accidents. D2241 prevents defective material entering water‑supply infrastructure projects.

  4. Traceability & marking rules: Mandatory marking (size, material code, SDR/PR, ASTM D2241 logo, manufacturer trace code, drinking‑water certification logo) enables field identification, quality traceability and regulatory acceptance for construction projects.

  5. Safety for public water‑supply infrastructure: Compliance with D2241 together with NSF‑61 certification ensures mechanical safety and drinking‑water health safety for municipal water distribution systems, reducing water‑leakage risks and public‑health hazards.

  6. Common acceptance baseline for manufacturers, buyers and third‑party labs: Manufacturers (like customers served by UnitedTest), third‑party testing laboratories and project owners all follow identical test conditions and pass‑fail thresholds, removing ambiguity in product acceptance and quality disputes.


Keywords: PVC pressure pipe tester, SDR PVC pipe test machine, ASTM D2241 testing equipment, PVC burst pressure tester, sustained hydrostatic pressure test rig, pipe flattening test machine, thermoplastic pipe impact tester, PVC pipe extrusion quality test, plastic pipe hydrostatic tester, water supply PVC pipe testing, PVC pressure piping lab equipment, IPS PVC pipe test fixture, PVC pipe mechanical testing system, plastic pipe pressure rating verification. 

Related products and device

ASTM D2241 PVC Pipe Hydrostatic Pressure Tester

Elevate your pipeline testing with our advanced hydrostatic pressure testing machine, designed per ISO 1167, ASTM D1598, and ASTM D1599 standards. Perfect for evaluating the durability of plastic and compound pipelines like PP-R, PVC, and PE, it applies precise constant or rapid hydraulic pressure, ensuring reliable performance.

ASTM D2241 PVC Pipe ring stiffness test machine

pipe ring stiffness test machine is used to determine the ring stiffness of circular cross-section thermoplastic pipes, according customer’s request, it can also execute compression, ring stiffness, ring softness and creep ratio test.

ASTM D2241 PVC Pipe Electronic Universal Testing Machine

WDW Series Computer Control Electronic Universal Testing Machine made by UNITEDTEST range from 100N to 600KN load capacity with various models like single columns, table type, door frame type etc., is used to perform tension, compression, flexure/bending, shearing, peeling etc., test for metal and nonmetal specimens.

ASTM D2241 PVC Pipe Melt flow index tester

Extrusion Plastometer is for melt mass-flow rate (MFR) and the melt volume-flow rate (MVR),to measure the melt mass flow rate of thermoplastic plastics under specific temperatures and pressures, reflecting the flow performance of materials through standardized testing.

ASTM D2241 PVC Pressure-Rated Pipe Falling Hammer Impact Tester/ Drop weight impact test

Pipe Falling Hammer Impact Testing Machine for assessing the impact resistance and toughness of plastic and metal pipes, offering controlled hammer energy, accurate impact measurement, and reliable quality evaluation for industrial and laboratory testing.

ASTM D2241 PVC Charpy & Izod Integrated Impact Tester

Charpy & Izod Integrated Impact Tester combine the Charpy and IZOD two impact method in one machine, include the full IZOD and Charpy test energy, simply change pendulum and vice, in one machine meet user multiple test requirement, enhance the working efficiency.

ASTM D2241 Dichloromethane soak testing machine

Methylene chloride tester/Dichloromethane soak testing machine is used to determine the resistance of unplasticised polyvinyl chloride (PVC-U) pipes to dichloromethane (methylene chloride) at a specified temperature (DCMT).

ASTM D2241 Oxidative Induction Time testing machine

Oxidative Induction Time testing machine is kind of differential scanning calorimeter,, check the relation of temperature with the rate differential input in test sample and reference articles. used to do Oxidative Induction Time test, heat stability, glass transition temperature, melting point.

ASTM D2241 GRP Hoop tensile testing machine

UnitedTest Pipe Apparent Hoop Tensile Testing Machine complies with ASTM D2290, specialized in testing apparent hoop tensile strength of plastic and reinforced plastic pipes. It uses a self-aligning split disk fixture to apply tensile stress to pipe ring samples along their contour.

hoop tensile strength of plastic pipes

Hoop tensile strength of plastic pipes is designed based on the ASTM D2290, to determine the breaking strength for the pipe hoop tensile test. ASTM D2290 is a test method used to study the apparent tensile strength of plastic pipes using a specialized test fixture to pull apart a ring of pipe.

Related Standard

ISO 1167 Thermoplastics pipes resistance to internal pressure test –

ISO 1167: 2006 Thermoplastics pipes, fittings and assemblies for the conveyance of fluids -- Determination of the resistance to internal pressure.

ISO 1167 test method specifies a general test method for determining the resistance to internal hydrostatic pressure at a given temperature of thermoplastics pipes, fittings and piping systems for the transport of fluids. The method accommodates water-in-water, water-in-air and water-in-liquid tests. It defines uniform hydrostatic pressure testing to evaluate short-term and long-term pressure-bearing durability of thermoplastic fluid-transport piping systems.


Hydrostatic pressure testing is a valuable method for assessing the strength and integrity of pressurized systems, ensuring that they can meet operational demands without failure. Hydrostatic pressure testing can evaluate these items by filling pipelines, tanks, or containers with water before pressure is applied to detect any potential leaks or issues. 

Hydrostatic pressure tester is critical across multiple industries, from pipeline engineering to industrial piping. It helps prevent costly failures or leaks by verifying whether the system can safely reach the specified pressure levels.

ASTM D1598, D1599 Plastic Pipe Constant or short time pressure testing methods –

ASTM D1598: Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure.

ASTM D1598 test method covers the determination of the time-to-failure of both thermoplastic and reinforced thermosetting/resin pipe under constant internal pressure.This test method provides a method of characterizing plastics in the form of pipe under the conditions prescribed.


ASTM D1599: Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings.

ASTM D1599 test method establishes the short-time hydraulic failure pressure of thermoplastic or reinforced thermosetting resin pipe, tubing, or fittings. Data obtained by this test method are of use only in predicting the behavior of pipe, tubing, and fittings under conditions of temperature, time, method of loading, and hoop stress similar to those used in the actual test. They are generally not indicative of the long-term strength of thermoplastic or reinforced thermosetting resin pipe, tubing, and fittings


ASTM D1599 Pipe short-time hydraulic burst pressure test –

ASTM D1599 is titled "Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings." It is a fundamental short-term, destructive pressure test used to determine the ultimate failure pressure (often called the "burst pressure") of thermoplastic pipe, tubing, or fittings under rapidly applied internal pressure at a specified temperature. Typically completed within 60–70 seconds, mainly for quality control and short-term design validation. 

ASTM D2290 Apparent Hoop Tensile Strength Testing –

ASTM D2290: Standard Test Method for Apparent Hoop Tensile Strength of Plastic or Reinforced Plastic Pipe

This test method covers the determination of the comparative apparent tensile strength of most plastic products utilizing a split disk or ring segment test fixture, when tested under defined conditions of pretreatment, temperature, humidity, and test machine speed. This test method is applicable to reinforced-thermosetting resin pipe regardless of fabrication method. This test method also is applicable to extruded and molded thermoplastic pipe.


ISO 7685 Glass-Reinforced Thermosetting Plastics GRP Pipe Initial Ring Stiffness Test –

ISO 7685 Glass-reinforced thermosetting plastics (GRP) pipes — Determination of initial ring stiffness.

ISO 7685 defines two standardized compression test methods to measure initial ring stiffness (S₀) for circular glass-reinforced thermosetting plastic (GRP/FRP) pipes, evaluating radial deformation resistance under short-term vertical external loads.

ASTM D2444 Pipe falling weight impact test standard –

ASTM D2444 test method covers the determination of the impact resistance of thermoplastic pipe and fittings under specified conditions of impact by means of a tup (falling weight). This method is applicable to isolated batches of pipe tested at 0 °C (information is also given for sampling from the continuous production of pipe).

ISO 10468 GRP Pipe Ring Creep Test –

ISO 10468 Glass-reinforced thermosetting plastics (GRP) pipes — Determination of the ring creep properties under wet or dry conditions.

ISO 10468 specify two core time-dependent mechanical properties of GRP pipes: long-term ring creep stiffness and creep factor. Two test environments are defined: dry ambient condition and fully water-immersed wet condition.

Dry creep test: For raw material batch consistency inspection and internal quality control.

Wet creep test: Simulates underground water service environments to predict long-term in-ground structural performance of buried GRP pipes.  

ISO 8513 Longitudinal tensile test for Glass-reinforced thermosetting plastic pipe –

ISO 8513 Plastics piping systems — Glass-reinforced thermosetting plastics (GRP) pipes — Test methods for the determination of the initial longitudinal tensile strength

ISO 8513 measure two core longitudinal tensile properties of glass-reinforced thermosetting plastic (GRP, also known as fiberglass-reinforced plastic FRP) pipes: Initial longitudinal tensile strength, Percentage ultimate elongation. IT only addresses tensile strength and break elongation; it explicitly excludes longitudinal tensile modulus testing, as multi-layer GRP pipe wall structures make precise strain measurement impractical.

ISO 15306 Cyclic internal pressure test of GRP pipes –

ISO 15306 Glass‑reinforced thermosetting plastics (GRP) pipes ‑ Determination of the resistance to cyclic internal pressure

ISO 15306 specifies a laboratory test method for evaluating cyclic‑pressure fatigue performance of GRP (fiberglass‑reinforced thermoset) pipes. The method can also apply to GRP fittings, not only straight pipes, which clarifies the applicable diameter range to nominal diameters up to and including DN 600.

ISO 8521 GRP Pipe Longitudinal Tensile Strength Testing –

ISO 8521 Glass-reinforced thermosetting plastic (GRP) pipes — Test methods for the determination of the initial circumferential tensile wall strength

ISO 8521 specifies six test methods (A, B, C, D, E, F) to determine the initial circumferential tensile wall strength per unit length of GRP pipes — a property also commonly called "hoop tensile strength." Both terms are interchangeable per the standard . The result is expressed in newtons per millimetre (N/mm) of circumference. "Initial" means the strength at the startof loading (short-term / instantaneous), as opposed to long-term hydrostatic strength covered by other standards. 

ASTM D2241 PVC Pressure-Rated Pipe (SDR Series): Test Requirements, Test Methods & FAQ

What is ASTM D2241?

ASTM D2241 is the ASTM specification for PVC pressure-rated pipe in the SDR series. It covers material classification, the PVC pipe material designation code, dimension tables, and the required tests — sustained pressure, burst pressure, flattening, extrusion quality and impact resistance — plus marking and quality assurance requirements.

Which tests are required by ASTM D2241?

Six checks: dimensions per ASTM D2122; sustained pressure per ASTM D1598 (1000 h); quick burst per ASTM D1599; flattening per ASTM D2241 §8.6; extrusion quality per ASTM D2152; and impact resistance per ASTM D2444 (Tup B, flat plate, 20 lb tup). All specimens are conditioned at 23 ± 2 °C and 50 ± 5 % RH for at least 40 h per ASTM D618.

How long is the ASTM D2241 sustained pressure test?

1000 hours (about 42 days) on six specimens, held within ±10 psi in water at 73.4 ± 3.6 °F. Specimen length is at least 10 × nominal diameter, minimum 10 in., maximum 3 ft between end closures. Zero failures of six passes; one failure requires a retest of six more; any failure in the retest rejects the lot.

Can the 1000-hour hydrostatic test be replaced?

Yes, at the manufacturer's option, by the accelerated regression test: at least six specimens per ASTM D1598 (three failing at ≤0.10 h, three at ≈200 h), extrapolated by least-squares regression per ASTM D2837 to the 100 000 h intercept, which must meet the material's Hydrostatic Design Basis category — for PVC 1120, a 100 000 h projection of 3830 psi at the 85 % LCL.

What is the difference between ASTM D1598 and ASTM D1599?

ASTM D1598 holds constant internal pressure until failure and yields a time-to-failure for long-term hydrostatic design basis work. ASTM D1599 ramps pressure so the specimen bursts in about 60–70 seconds and yields a burst pressure in psi. D2241 uses D1598 for the 1000 h requirement and D1599 for the minimum quick burst on at least five specimens.

Why must the ASTM D1599 burst test fail in 60 to 70 seconds?

Thermoplastic burst strength is time dependent, so the standard fixes the failure window for comparability. If a specimen fails in under 60 s, the loading rate must be reduced and the test repeated. ASTM D2241 additionally requires each specimen to be tested for not less than 60 s, and notes that larger sizes may need longer, which makes passing more difficult.

What is the flattening test in ASTM D2241?

Three 2 in. long specimens are compressed between parallel plates to 40 % of the outside diameter, at a uniform rate completed in 2 to 5 minutes. After unloading there must be no splitting, cracking or breaking.

What is the acetone immersion test?

ASTM D2152 checks PVC fusion adequacy by immersing specimens in dried acetone for 20 minutes and looking for attack (material lifting or removal) on the inner, outer or mid-wall surfaces. Swelling alone is not attack. ASTM D2241 requires that the pipe shall not flake or disintegrate.

How is impact resistance tested for ASTM D2241 PVC pipe?

By ASTM D2444: a 20 lb tup with Tup B nose on a flat plate support at 73.4 ± 3.6 °F. For pipe 1/4 in. through 12 in., ten specimens are tested; 9 or more pass means the lot passes, 2 or more failures means it fails. Minimum values range from 10 ft-lbf to 160 ft-lbf depending on size.

What PVC material does ASTM D2241 require?

The compound must equal or exceed ASTM D1784 cell class PVC 12454 or PVC 14333. Only the manufacturer's own clean rework is allowed. Material designations covered are PVC 1120, 1220 and 2120 (HDS 2000 psi), PVC 2116 (1600 psi), PVC 2112 (1250 psi) and PVC 2110 (1000 psi).

What does SDR mean and how is pressure rating calculated?

SDR is the ratio of average outside diameter to minimum wall thickness. Pressure rating follows the ISO equation 2S/P = R − 1, i.e. PR = 2S / (SDR − 1). For PVC 1120 at 73 °F: SDR 13.5 = 315 psi, 17 = 250 psi, 21 = 200 psi, 26 = 160 psi, 32.5 = 125 psi, 41 = 100 psi, 64 = 63 psi.

Which industries use ASTM D2241 PVC pipe?

Potable water distribution, irrigation and agriculture, industrial process and cooling water, water reuse and reclaimed water, well and pump columns, and dewatering or temporary bypass lines. Potable water service also requires NSF/ANSI 14 and NSF/ANSI 61 evaluation.

What marking does ASTM D2241 require?

Marking at intervals of no more than 5 ft: nominal pipe size; OD system (IPS/PIP) for 14 in. and over; material code such as PVC 1120; SDR or pressure rating in psi (rating mandatory for pressure service); ASTM D2241; manufacturer's name or trademark plus a production code with year, month, day, shift, plant and extruder; and, for potable water, the certifying laboratory's mark.

What testing equipment does a laboratory need for ASTM D2241?

A constant-pressure hydrostatic pressure test machine with heated bath and end closures (D1598), a programmable PVC pipe burst tester (D1599), a drop weight impact tester with Tup A/B/C and flat/V holders (D2444), a compression or universal testing machine with parallel plates for flattening, an acetone immersion station (D2152), dimensional gauges (D2122), and a conditioning chamber (D618).

Can PVC pressure pipe be tested with compressed air instead of water?

Not for compliance. ASTM D2241 is written for pressurized liquids only and warns that compressed air or gas stores large amounts of energy and presents serious hazards on failure; some manufacturers prohibit pneumatic testing. Use de-aerated water and consult the pipe manufacturer before any pneumatic procedure.

< Previous: ASTM D2210 Mullen Test for Leather Grain Stretching Crack & Extension

> Next: ASTM D2256 Thread and Yarn Tensile Testing of Single-Strand String

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.