Information on the most widely used ASTM standards within the materials testing industry
ISO 7622-1 Steel Cord Elongation Tester | UnitedTest Conveyor Belt Longitudinal Traction Test Machine
UnitedTest manufactures ISO 7622-1 longitudinal traction test machine for measuring elongation of steel cords in steel cord conveyor belts at 10% and 60% rated tensile strength, destructive elongation testing for steel carcass conveyor belts.
ISO 7622-1 is the international reference method for measuring how much a steel cord stretches under load. UnitedTest supplies complete test systems for ISO 7622-1:2013 — Steel cord conveyor belts, longitudinal traction test, Part 1: Measurement of elongation, configured to the parameters the standard actually demands: a constant jaw separation rate of 25 mm/min ± 5 mm/min, ≥ 250 mm jaw separation, an extensometer accurate to 0.01 % over a 100–300 mm gauge length, and non-slip cord holding devices that protect the specimen during gripping.
Whether you are a conveyor belt manufacturer running verification tests, an independent laboratory working to accreditation, or a mining or bulk-handling operator resolving a supplier dispute, a UnitedTest system gives you repeatable elongation values at 10 % and 60 % of specified minimum tensile strength — the two numbers that decide take-up travel, splice design and load sharing across the carcass.
Core Test purpose / principle
A single steel cord is extracted from the belt carcass and subjected to a longitudinal traction (tensile) test. The elongation is measured with an extensometer while the cord is loaded in a dynamometric tensile testing machine whose jaw separation rate is fixed and held constant. Elongation readings are taken at 10 % and 60 % of the specified minimum tensile strength. Measurement deliberately stops at 60 %: steel cord elongation is very small, so highly sensitive extensometers must be used, and they would be damaged if the specimen were pulled to break.
Test Equipment required of ISO 7622-1 Steel Cord Conveyor Belt Elongation Testing
| Universal Tensile testing machine | Force range shall match specimen strength; constant jaw separation rate adjustable and maintainable at 25 mm/min ±5 mm/min. Minimum jaw opening distance ≥250 mm; Device to record the traction force vs. elongation curve. |
| Test substrates | Two fixed grooved pulleys. Pulley diameter shall be at least 50 mm or 10 times the steel‑cord diameter d, to prevent specimen slippage during traction |
| Non‑slip cord‑holding fixtures | Minimum accuracy of 0.01 %. It should accommodate slight rotation of twisted steel cords during stretching. Measurement shall not exceed 60 % specified tensile strength to protect the sensitive instrument from break‑age impact.
|
| Extensometer | Polyethylene (PE) film for casting specimens. |
Test Specimen Information:
Quantity: four steel‑cord specimens total, two S‑twist cords and two Z‑twist cords, extracted from one belt sample.
Sampling: Cut a belt piece with minimum length of 400 mm. Remove surrounding rubber compound carefully without applying tensile stress to target cords. Strip rubber coating fully along cords or at minimum strip rubber on end sections that fit into holding fixtures.
Test Parameters & Stipulations
| Initial pre-load (zero point) | Initial tractive force = 50 × the linear density (mass per metre) of the cord — applied to define the zero point of the registration curve clearly |
| Extensometer gauge length | 100 mm – 300 mm between extensometer jaws |
| Crosshead / jaw separation rate | 25 mm/min ± 5 mm/min, constant |
| Measurement points | Elongation at 10 % and 60 % of the specified minimum tensile strength |
| Elongation expression | As a percentage of the initial length |
| Result | Arithmetic mean of the four measurements, at 10 % and at 60 % separately, reported to the nearest 0.1 % |
Test Procedures for ISO 7622-1 Steel Cord Conveyor Belt Elongation Testing
Obtain four valid cord specimens (two S‑twist, two Z‑twist) following specimen‑preparation requirements.
Store and condition specimens according to ISO 18573; test at least five days after belt production, under standard temperature‑humidity atmosphere unless agreed otherwise.
Mount one cord end onto upper holding fixture; fasten the other cord end to lower fixture. Apply defined initial pre‑traction force to establish measurement zero‑point.
Install extensometer onto the cord, set gauge‑length between 100 mm‑300 mm.
Start tensile machine, keep jaw‑separation speed constant at 25 mm/min ±5 mm/min.
Record elongation readings when load reaches 10 % and 60 % of specified minimum tensile strength.
Repeat the full test for all four cord specimens.
Compute average elongation results and compile formal test report.
Industry Application Fields
Mining and quarrying (open-pit and underground), bulk material handling, ports and terminals, cement/steel/power plants — anywhere long, high-tension steel cord belts are used.
Belt and steel cord manufacturers — quality control, product development, verification of incoming cord.
Independent/third-party testing laboratories — certification, comparative testing, accreditation.
Procurement, specifiers and end users — acceptance testing and supplier verification.
Forensic / dispute resolution — contract claims, failure investigation, arbitration where the cord manufacturer's certificate is missing or contested.
Related Standard:
| ISO 7622-2 | ISO 7622-2 Steel cord conveyor belts — Longitudinal traction test — Part 2: Measurement of tensile strength |
| ISO 7622-1 | Steel cord conveyor belts - Longitudinal traction test - Part 1: Measurement of elongation |
| ISO 7623 | cord-to-coating bond test (initial and after thermal treatment); uses a tensile machine to ISO 7622-2, 100 ± 10 mm/min, 250 ± 10 mm jaw spacing. |
| ISO 8094 | adhesion strength of cover to core layer. |
| ISO 15236-1 | Steel cord conveyor belts - Part 1: Design, dimensions and mechanical requirements for conveyor belts for general use |
| ISO 9856 | Test method for building sealants—Part 17:Determination of elastic recovery |
| ISO 283 | textile conveyor belts, full-thickness tensile strength and elongation (the textile-belt counterpart to 7622). |
| DIN 22110 | German splice test methods; Part 3 determines the dynamic (fatigue) efficiency of splices by running endless belts to 10 000 load cycles — relevant because splice design depends directly on cord elongation behaviour. |
| GB/T 5754.1 | Steel cord conveyor belts—Longitudinal traction test—Part 1: Measurement of elongation |
| GB/T 5754.2 | Steel cord conveyor belts—Longitudinal traction test—Part 2: Measurement of tensile strength |
Why this test matters for the material
Elongation governs conveyor design and take-up travel. Steel cord belts run for kilometres under high tension. The cord's elongation at working load (10 %) and at a higher proof load (60 %) determines how much the belt will stretch in service, which directly sets the required take-up (tensioning) stroke, start-up behaviour, belt tracking and sag between idlers. Too much elongation and the take-up runs out of travel; too little, and the belt transmits shock loads harshly.
The cords carry 100 % of the load. In a steel cord carcass the rubber carries essentially no tension — it only positions the cords and transfers load, especially at the splice. So the cord's stress–strain response is the belt's longitudinal stiffness. ISO 7622-1 quantifies that response at two defined fractions of rated strength, giving a two-point stiffness/modulus picture.
Splice integrity depends on cord elongation. Splice design (cord layout, overlap length, load transfer into the rubber) is built around the cord's elongation characteristics; mismatch between cord elongation and splice geometry is a classic cause of splice creep and pull-through failure.
Uniformity between cords matters. Testing two S-twist and two Z-twist cords and averaging them detects non-uniform elongation across the carcass. Unequal elongation between cords causes uneven load sharing, belt camber/"banana" tracking problems, and premature failure of the most-loaded cords.
It is the referee method. Because it is destructive, ISO 7622-1 is explicitly reserved for litigation or when the cord manufacturer's certificate is unavailable. It provides an independent, reproducible, arbitration-grade number (mean of four, to 0.1 %) that can settle a commercial dispute — and the standard itself is honest about the caveat that rubber-coated cord values may differ from raw-cord certificate values.
Repeatability through strict control. The tight stipulations — 5-day post-manufacture wait, ISO 18573 Atmosphere B, defined pre-load (50 × linear density), 100–300 mm gauge length, constant 25 ± 5 mm/min, and a 0.01 %-accuracy extensometer — exist precisely because steel cord elongations are so small that conditioning, gripping and zero-point errors would otherwise swamp the measured value
Keywords: ISO 7622-1 tester, steel cord conveyor belt tester, steel cord elongation tester, longitudinal traction test machine, conveyor belt steel cord test, steel cord carcass elongation test, conveyor belt tensile tester, steel cord tensile elongation test, industrial conveyor belt testing equipment, steel cord destructive test, conveyor belt quality inspection machine, steel cord traction test fixture, mining conveyor belt test, steel cord elongation measurement, UnitedTest conveyor belt tester
Related products and device
Related Standard
ISO 21182 specifies test procedures to measure static coefficient of friction (μs) and dynamic coefficient of friction (μD) for light conveyor belts. Quantify how "grippy" or "slippery" a belt cover surface is when sliding against a standardized steel panel under a defined normal load.
ISO 9856 specifies a laboratory method for determining the elastic elongation, permanent (non-recoverable) elongation, and elastic modulus of a conveyor belt's tensile member (fabric carcass or steel cord reinforcement) under cyclic loading.
ISO 8094 specifies a test method for determining the adhesion strength between the cover rubber and the core layer of a steel cord conveyor belt, it applies exclusively to steel cord conveyor belts (not fabric/textile ply belts).
ISO 505 specifying a universal tensile test method to quantify the tear propagation resistance of textile carcass conveyor belts, tested either at full belt thickness or stripped carcass-only condition, targeting belts prone to dangerous longitudinal splitting in service.
ISO 252 specifies two test methods (A and B) for measuring adhesion strength between the constituent layers of conveyor belts: between top/bottom covers and carcass, and between individual plies.
ISO 283 is the core tensile test standard for textile-reinforced conveyor belts. It specifies how to cut a full-thickness test piece from the belt and pull it in uniaxial tension until rupture, to determine the Full-thickness tensile strength, Elongation at break, Elongation at the reference force (load).
FAQ: ISO 7622-1 Steel Cord Conveyor Belt Elongation Testing
Q1. What is ISO 7622-1?
ISO 7622-1:2013 is an International Standard titled Steel cord conveyor belts — Longitudinal traction test — Part 1: Measurement of elongation. It specifies a laboratory method for measuring how much an individual steel cord taken from the carcass of a conveyor belt elongates when loaded to forces equal to 10 % and 60 % of the specified tensile strength. It applies only to conveyor belts with a steel (steel cord) carcass.
Q2. Is ISO 7622-1 the same as ISO 7622-2?
No — they are two halves of one series and are usually cited together:
ISO 7622-1 = elongation (how much the cord stretches at 10 % / 60 % load). Slow speed, extensometer-based, test stops at 60 % of rated strength.
ISO 7622-2 = tensile strength (how much force the cord takes before it breaks). Pulled to break at 100 mm/min ± 10 mm/min.
If you only test to Part 2, you know the strength but not the stiffness. If you only test to Part 1, you know the stiffness but not the strength.
Q3. Is the test destructive?
Yes. The cord must be cut out of the belt and the rubber stripped from it. Because of this, the standard's own Introduction states the method is intended for use in the event of litigation, or where the cord manufacturer has issued no certificate of compliance. It is a referee/verification method, not a routine in-process check.
Q4. How is the cord gripped?
With a holding device that makes slipping impossible. The standard's example is two fixed grooved pulleys (upper and lower) of diameter at least 50 mm, or at least 10 × the cord diameter d. Because the rubber is stripped, grip slip and grip damage are the classic failure modes of this test.
Q5. Why is cord elongation so important for a conveyor belt?
The steel cords carry essentially all of the longitudinal load in a steel cord belt — the rubber positions the cords and transfers load, but carries almost no tension. So the cord's stress–strain behaviour is the belt's longitudinal stiffness. It directly determines:
Take-up / tensioning stroke required (how much the belt will stretch in service);
Start-up and braking behaviour and shock-load transmission;
Belt sag between idlers and tracking;
Splice design — overlap length and load transfer into the rubber are built around the cord's elongation;
Load sharing between cords — if cords elongate differently, some carry more load and fail first.
Q6. Why measure at exactly 10 % and 60 %?
Two points give a practical two-point stiffness picture. 10 % approximates the low-load/working region where take-up behaviour matters most; 60 % is a higher proof load that reveals whether the cord's response stays proportional. The standard deliberately caps the measurement at 60 % because steel cord elongation is very small, so a highly sensitive (and fragile) extensometer must be used — and it would be destroyed if the cord were pulled to break.
Q7. Why does the standard require both S-twist and Z-twist cords?
Steel cords are stranded, and lay direction influences elongation behaviour. Belt carcasses are normally built with alternating S and Z lay cords to keep the belt running straight. Testing two of each and averaging catches non-uniformity between cords — a common hidden cause of belt camber, uneven load sharing and premature failure.
Q8. Can the result differ from the cord manufacturer's certificate?
Yes, and the standard says so explicitly. Differences in elongation can occur between raw steel cords and rubber-coated (belt-extracted) cords. Values obtained by this method may therefore differ from the values stated in a cord manufacturer's certificate. This is one reason the method is framed as a dispute-resolution tool.
Q9. How many specimens, and how are they prepared?
Four cords — two S-twist and two Z-twist. From a belt sample at least 400 mm long, cut the compound between the cord layer and the rest of the belt, isolate four cords from the central part, and strip the rubber from the whole length or at least from the ends that go into the grips.
Q10. What is the single biggest specimen-preparation mistake?
Subjecting the cord to tensile stress during extraction. The standard explicitly warns against it: a pre-stretched cord has already taken up elongation, so the measured value will be too low. Handle, cut and strip without pulling.
Q11. What extensometer accuracy is required?
At least 0.01 %. Steel cord elongations are tiny, so a coarse extensometer simply cannot resolve them. The standard also recommends an extensometer that can accommodate the cord rotation produced by the cord's twisted nature.
Q12. What gauge length and pre-load are used?
Extensometer jaws set 100 mm – 300 mm apart.
An initial tractive force equal to 50 × the linear density (mass per metre) of the cord is applied first, purely to define a clear zero point on the registration curve.
Q13. Who actually uses this test?
Steel cord and conveyor belt manufacturers (QC and development), independent third-party testing laboratories, mining/quarrying/bulk-handling and port operators, procurement and specification teams, certification bodies, and forensic or legal experts resolving performance disputes.
Q14. Why choose ISO 7622‑1 Steel Cord Conveyor Belt Elongation Testing Machine from UnitedTest Manufacturer?
UnitedTest manufactures ISO 7622‑1 compliant longitudinal traction testing machines for steel‑cord conveyor belts, measuring steel‑cord elongation at 10 % & 60 % specified tensile strength. Complete fixtures, high‑precision extensometer, meet ISO 7622‑1 and ISO 7622‑2 standards for mining & port conveyor‑belt labs.
UnitedTest is a professional manufacturer supplying complete testing systems complying with ISO 7622‑1:2013 Steel cord conveyor belts‑Longitudinal traction test‑Part 1: Measurement of elongation, also compatible with ISO 7622‑2 for steel‑cord breaking‑strength testingUnitedTest.
Our ISO 7622‑1 test system is purpose‑built for laboratories, conveyor‑belt factories, third‑party inspection institutes, mining technical centers and port bulk‑material handling quality departments. It performs accurate elongation measurement on rubber‑coated steel cords dissected from finished steel‑cord conveyor‑belt carcass, capturing strain values at 10 % and 60 % of specified minimum tensile strength as defined by international standard requirements.
Precision load frame & drive system: Supports adjustable constant jaw separation speed set to 25 mm/min ±5 mm/min; jaw opening ≥ 250 mm, matches ISO 7622‑1 apparatus specification. Both electronic servo and hydraulic horizontal tensile machine configurations are available for different steel‑cord force rangesUnitedTest.
Special anti‑slip steel‑cord holding fixtures: Supplied with grooved pulley assemblies complying with standard dimension rule: pulley diameter ≥ 50 mm or ≥ 10 × cord diameter d, eliminating specimen slippage during traction test.
High‑accuracy extensometer: 0.01 % strain‑accuracy extensometer, supports twisted‑cord rotation compensation, dedicated for low‑strain steel‑cord elongation measurement. System stops automatically at 60 % tensile‑strength threshold to protect delicate extensometer from cord‑break damage.
Software for ISO 7622‑1 workflow: Built‑in test procedure, records elongation data at 10 % and 60 % load, auto‑calculates arithmetic mean of four specimens (2×S‑twist, 2×Z‑twist), outputs percentage‑elongation results rounded to 0.1 %, and generates full test reports referencing ISO 7622‑1:2013.
Environment‑compatible: Works together with temperature‑humidity chambers to satisfy ISO 18573 standard atmosphere‑B (23 °C ±2 °C, 50 % ±5 % RH) conditioning requirements.
Dual‑standard capability: Same test bench can execute ISO 7622‑2 steel‑cord ultimate tensile‑strength tests with simple fixture change‑over.
Quality control for steel‑cord conveyor‑belt manufacturers
Third‑party inspection & material‑acceptance testing
Technical dispute / litigation verification for mining, coal mine, harbour bulk‑conveyor projects
R&D for new‑formula steel‑cord reinforced conveyor‑belts
Conveyor‑belt incoming‑material laboratory audit
UnitedTest delivers complete turn‑key solutions including main tensile machine, ISO‑standard fixtures, precision extensometer, dedicated test software, installation, training and after‑sales support. Our test systems are widely deployed in rubber‑conveyor‑belt labs worldwide. Whether you need bench‑type or heavy‑duty horizontal tensile machines for high‑strength steel‑cord specimens, UnitedTest can customize force capacity, travel length and accessories to match your ISO 7622‑1 / ISO 7622‑2 test requirements.
Require More Customized Solutions?