Home >> Application >> By Standard >> ISO >> ISO 20000 + >> ISO 29022 Dental adhesive shear bond strength test

ISO 29022 Dental adhesive shear bond strength test

Share:

ISO 29022 Dental Adhesion Tester | Notched-Edge Shear Bond Strength Test Machine | UnitedTest

UnitedTest manufactures ISO 29022 notched-edge shear bond strength testing machine for dental adhesion evaluation. It measures shear bond strength between direct dental restorative materials and enamel or dentine, suitable for dental adhesives, glass-ionomer cements and dental material laboratory R&D and quality validation.

ISO 29022 specifies a standardized notched-edge shear test method to quantify shear bond strength between direct dental restorative materials and hard tooth tissues, including enamel and dentine. This test is primarily developed for dental adhesive systems and can be adapted for other restorative materials such as glass-ionomer cements. It is widely used in dental material laboratories for adhesive formulation screening, bond performance comparison, pre-clinical material assessment, and batch quality control of dental bonding agents.


Test Principle

A cylindrical composite "button" of known bonded area is built on a flat, freshly prepared tooth surface using the adhesive under test. After water storage, the specimen is clamped and a notched-edge crosshead — a blade with a thin, curved lip — is brought down flush against the tooth surface and centred over the button, so the load is applied almost exactly at the adhesive/tooth interface.

Two design features define the principle:

  1. Load application at the interface, not at a distance. The thin curved lip contacts the button right at its base. Because the load is introduced close to the bond line, bending moments and tensile/peel components are minimised, so the measured value approximates true interfacial adhesive shear strength rather than peel strength. Using a crosshead without this lip edge is explicitly stated to increase result variability.

  2. Controlled, constant bonded area. The plastics button mould gives a circular bond of diameter 2,38 mm, so the bonded area is fixed at π × 1,19² = 4,45 mm².

Bond strength is simply:

σ = F / A_b  (σ in MPa; F = maximum force in N before failure; A_b = bonded area in mm²)


Test Equipment required for ISO 29022 Dental adhesive shear bond strength test

Tensile testing machine    

equipped with displacement‑controlled crosshead for applying shear load.

Notched‑edge shear test fixture assembly

including notched‑edge shear blade/crosshead with thin curved lip, metal test‑base specimen clamp (holder).

ISO 29022 Dental adhesive shear bond strength test

Auxiliary Tools

Bonding clamp + plastic button mould: mould inner hole diameter (2.38 ± 0.03) mm for forming standardized composite cylinders; spacers for adjusting specimen height.

Grinding apparatus: automatic grinding machine / drill‑press fixture, silicon‑carbide abrasive papers P120 (125 μm) and P400 (35 μm) complying with ISO 6344‑1, running water cooling system.

Potting mould: cylindrical ring mould (~25 mm inner diameter); slow‑setting self‑curing resin or dental die‑stone for embedding teeth.

Environment control: laboratory condition control for temperature and relative humidity; thermostatted water bath for specimen storage; ISO 3696 grade‑3 laboratory water; calliper for measuring composite‑button diameter; filter paper; compressed‑air supply free of oil and water.


Test Specimen Information:

Substrate (tooth specimens)

Bovine incisors (use the labial surface) or human erupted permanent third molars (buccal, mesial, distal or lingual). Occlusal surfaces must not be used. The substrate type must be recorded.

Use superficial dentine, as close to enamel as possible, and plane it parallel to the dentine–enamel junction to obtain a uniform dentine structure and reduce variation.

Final bonded test specimens

Sample size: minimum 15 bonded specimens per test group.

Tooth is potted (embedded) in resin/die‑stone, ground wet to produce a flat, planar bonding surface perpendicular to the potting cylinder axis. Grinding must be finished within 4 h before adhesive application; ground teeth are stored in room‑temperature water and used within 4 h after grinding.

A high‑modulus composite (flexural modulus > 9 GPa) forms a cylindrical button on the tooth surface via the plastic mould.

Post‑bonding storage condition: specimens are immersed in water at (37 ± 2) °C for (24 ± 2) h before mechanical testing.


Test Parameters & Stipulations

Crosshead loading speed(1.0 ± 0.1) mm/min (shear test)
Composite button nominal diameter2.38 mm; theoretical bond area 4.45 mm²
Tooth storage temperature(4 ± 4) °C
Post‑bonding water‑aging(24 ± 2) h at (37 ± 2) °C
Maximum permitted interval after grinding tooth surface before bonding4 hours
Valid usage window for extracted teeth≤ 6 months after extraction
Abrasive paper sequence for surface grindingP120 then P400 under running water


Test Procedures for ISO 29022 Dental adhesive shear bond strength test

  1. Tooth pre‑treatment & storage: collect caries‑free teeth; clean; remove pulp for bovine teeth; store in permitted medium within the 6‑month usable period.

  2. Potting (mounting): block pulp‑chamber opening; fix tooth into cylindrical mould with bonding face down; pour slow‑setting embedding medium; cool during resin polymerization to prevent thermal tooth damage; after curing, demould and store potted teeth in cold water.

  3. Wet surface grinding: under running water, sequentially grind with P120 then P400 SiC paper to expose flat superficial‑dentine or enamel bonding surface. Ensure ground plane is perpendicular to potting cylinder. Complete grinding no more than 4 h prior to bonding; rinse specimens and store in room‑temperature water.

  4. Specimen preparation (bonding assembly)

  5. Notched‑edge shear mechanical test:

    • Remove specimens from 37 °C water and test immediately; trim excess composite flash with razor blade.

    • Mount specimen in metal base clamp, align composite button with the notch of the notched‑edge crosshead blade. Ensure blade lip sits flush against tooth surface.

    • Operate universal tester at crosshead speed (1.0 ± 0.1) mm/min until bond fracture occurs; record maximum failure force (N).

  6. Data processing and report: compute shear‑bond‑strength values; document pre‑test‑failure and excluded samples; compile full test report as stipulated by the standard.


Industry Application Fields

Dental materials manufacturers — R&D screening and formulation comparison of adhesive systems; quality control during production.

Regulatory submissions and conformity assessment — the test is used to document "adheres to tooth substance" claims for notified bodies / regulators; EN ISO 29022:2013 was adopted under the EU Medical Device Directive 93/42/EEC.

Contract and academic testing laboratories — comparative adhesion studies on enamel and dentine.

Scope of use: primarily dental adhesives; with modification it can be applied to adhesive restorative materials such as glass-ionomers.

Users: dental materials researchers, testing labs, manufacturers, regulatory bodies


Related Stadard: 

ISO 4587Adhesives - Determination of tensile lap-shear strength of rigid-to-rigid bonded assemblies.
ASTM D1002Standard Test Method for Apparent Shear Strength of Single-Lap-Joint Adhesively Bonded Metal Specimens by Tension Loading (Metal-to-Metal)
ISO/TS 11405

Dentistry — Testing of adhesion to tooth structure (3rd ed. 2015, withdrawn 2019).

Gives guidance on substrate selection/storage and covers tensile bond strength, marginal gap measurement, microleakage and clinical usage tests; 

its introduction explicitly names ISO 29022 as an important publication in the field. ISO 29022 is effectively the shear counterpart to this tensile/guidance document.

EN 1465Adhesives - Determination of tensile lap-shear strength of bonded assemblies
ISO 29022Dentistry. Adhesion. Notched-edge shear bond strength test
ISO 4049 Polymer-based restorative materials (the composite/adhesive product specification family, with ISO/TS 16506 for adhesive luting materials, ISO 9917 series for glass-ionomers).
DIN 13990German shear bond strength test; in a comparative repair study it produced higher values (26,0 ± 8,9 MPa) than ISO 29022 (17,9 ± 6,3 MPa), while ISO/TS 11405 tensile gave the lowest (6,9 ± 1,8 MPa).
ASTM D5656Standard Test Method for Thick-Adherend Metal Lap-Shear Joints for Determination of the Stress-Strain Behavior of Adhesives in Shear by Tension Loading
ASTM D5868

Standard Test Method for Lap Shear Adhesion for Fiber Reinforced Plastic (FRP) Bonding


Keywords: ISO 29022, notched-edge shear bond strength test, dental adhesion tester, dental shear bond tester, enamel bond strength test, dentine bond strength test, dental restorative material test, dental adhesive bond test, glass ionomer cement bond test, composite resin shear test, dental lab testing machine, dental material universal tester, UnitedTest dental test equipment, in-vitro dental adhesion test, dental bonding agent qualification, dentistry bond strength evaluation, tooth substrate shear test, dental material mechanical test

Related products and device

ISO 29022 Notched-Edge Shear Bond Strength Tensile Testing Machine

A single column tensile tester is a sophisticated material testing instrument designed for measuring mechanical properties of various materials under tension, compression, bending, shear, and other loading conditions. As the name suggests, it features a single vertical column supporting a moving crosshead that applies force to test specimens.

Dental bonding agent qualification, dentistry bond strength evaluation

Vice Tensile test fixture for plastics is based on the test standatd ASTM D638, determination of the tensile properties of unreinforced and reinforced plastics in the form of standard dumbbell-shaped test specimens when tested under defined conditions of pretreatment, temperature, speed.

Related Standard

ASTM D1002 Lap Shear Test of Adhesively Bonded Metal Specimens –

ASTM D1002 is the most widely used standard test for measuring the apparent shear strength of metal‑to‑metal adhesive single‑lap joints under tension loading. It provides comparative data for adhesive selection, process control, and quality assurance in structural bonding applications. It is the most common test for evaluating adhesive shear performance.

ASTM D897 Tensile Test of Adhesive Bonds –

ASTM D897 prescribed a method for determining the comparative tensile properties of adhesive bonds in a standard specimen when tested under specific conditions. Its primary purpose was to measure the tensile strength of an adhesive bond between two rigid substrates (metal to metal). 

ASTM D412 Tensile Strength of Rubber and Elastomers –

ASTM D412 test methods cover procedures used to evaluate the tensile (tension) properties of vulcanized thermoset rubbers and thermoplastic elastomers. These methods are not applicable to ebonite and similar hard, low elongation materials. 

ASTM D412 is the primary standard for evaluating the tensile properties of vulcanized thermoset rubbers and thermoplastic elastomers (TPEs). It provides precise procedures for determining critical mechanical characteristics that define material performance under stretching forces. 

The methods appear as follows:

Test Method A—Dumbbell and Straight Section Specimens

Test Method B—Cut Ring Specimens

ISO 812 Low-temperature brittleness Impac Test of Rubber, vulcanized or thermoplastic –

ISO 812:2017 specifies a method for determining the lowest temperature at which rubber materials do not exhibit brittle failure or the temperature at which half of the test pieces used in a test fail when impacted under specified conditions.

The temperatures thus determined do not necessarily relate to the lowest temperature at which the material can be used since the brittleness will be affected by the conditions of test and especially by the rate of impact. Data obtained by this method are, therefore, intended to be used to predict the behaviour of rubbers at low temperatures only in applications in which the conditions of deformation are similar to those specified in the test.


ISO 37 Tensile Test on Rubber, vulcanized or thermoplastic –

ISO 37 and ASTM D412 are both widely recognized tensile test methods designed to evaluate the stress-strain characteristics of various rubber materials, including natural rubber, synthetic rubber, silicone rubber, and thermoplastic elastomers (TPEs). While both standards aim to determine the tensile properties of rubber and elastomers, they differ in their specific methodologies and applications.

ASTM D2137 Rubber Brittleness Point Test of Flexible Polymers and Coated Fabrics –

ASTM D2137: Standard Test Methods for Rubber Property--Brittleness Point of Flexible Polymers and Coated Fabrics


ASTM D2137 test method is used to evaluate the brittleness of rubber materials, or rubber coated fabrics, when exposed to low-temperature flex with an impact under specified conditions of striker speed. ASTM D2137 tests performed will be used to determine the lowest temperature at which rubber compounds will not show fractures or coating cracks when exposed to specified impact conditions.

ISO 4587 Adhesives Tensile Shear Test of rigid bond material –

ISO 4587 Adhesives — Determination of tensile lap-shear strength of rigid-to-rigid bonded assemblies

ISO 4587 determining tensile lap-shear strength of adhesive single-lap joints between two rigid substrates, for comparative evaluation rather than structural engineering design data. UnitedTest manufactures high-precision ISO 4587 compliant lap-shear test machines, designed to evaluate the tensile shear performance of rigid-to-rigid adhesive bonded assemblies for industrial quality control and adhesive material comparison. 

ISO 29022 — Notched-Edge Shear Bond Strength Test: FAQs

Q1. What is ISO 29022?

ISO 29022:2013 is an International Standard published by ISO/TC 106/SC 1 (Dentistry — Filling and restorative materials). It specifies a shear test method for determining the adhesive bond strength between direct dental restorative materials and tooth structure (dentine or enamel). It is written principally for dental adhesives and covers substrate selection, tooth storage and handling, specimen production, and the complete test procedure. 


Q2. Why is this test important for dental materials?

Because adhesion is the functional weak link of a restoration. If the adhesive interface fails, the restoration loses retention, the margin opens, and the clinical consequences are microleakage, marginal staining, post-operative sensitivity, secondary caries and premature replacement. Bond strength to dentine/enamel is therefore one of the very few quantitative performance attributes an adhesive can be judged on — it drives formulation R&D, batch quality control, marketing claims and regulatory documentation.


Q3. Why is a standardised method needed, rather than any shear test?

Without a standard, bond strength numbers are simply not comparable. Substrate species, tooth age, storage medium, abrasive grit sequence, smear layer, bonded area, composite elastic modulus and load-application geometry all shift the result. Finite-element analyses have shown interfacial stresses can differ dramatically purely because of the composite's modulus and where the load is applied. ISO 29022 fixes every one of these variables, which is why it is the design used for regulatory approval of dental materials.


Q4. Why "notched-edge"? What does the notch actually do?

Two things:

  1. It puts the load at the interface. Because the thin curved lip contacts the button at its base, bending moments and peel/tensile components are minimised, so the result approximates true interfacial adhesive shear strength rather than peel strength.

  2. It controls the bonded area. The plastics button mould (Ø 2,38 mm) fixes the bond area at π × 1,19² = 4,45 mm².

The standard explicitly warns: using a crosshead without the thin curved lip edge increases variability of results.


Q5. Can a standard universal testing machine be used?

Yes — the notched-edge shear fixture is mounted to a universal testing machine. The practical requirements are a stable, low-speed crosshead (1,0 ± 0,1 mm/min), a load cell appropriately sized for the few-tens-of-newtons range typical of a 4,45 mm² bond, and a rigid base to hold the test base clamp.


Q6. Which teeth can be used?

Bovine incisors (labial surface) or human erupted permanent third molars (buccal, mesial, distal or lingual). The occlusal surface must not be used (difficult to find a suitable bonding area). The substrate type must be recorded in the report.


Q7. Any restrictions on tooth condition and age?

Teeth must be caries-free; human teeth that are restored or root-filled (endodontically treated) must not be used. Teeth must be used within 6 months of extraction — older teeth may undergo degenerative changes in dentinal proteins.


Q8. Why must the tooth surface stay wet?

Exposure of a tooth surface to air for even a few minutes can cause irreversible changes in bonding character; dentine is especially sensitive to dehydration. The standard requires surfaces be kept wet at all times — brief air drying is only permitted to visualise the exposed dentine area.


Q9. Why must a high-modulus composite be used?

A high-modulus composite (flexural modulus > 9 GPa) minimises deformation of the composite button during shear, so the measured load reflects the interface rather than the button's compliance. The standard also requires that the same composite be used when comparing adhesives.


Q10. How is the specimen aligned, and why is it fiddly?

The specimen sits in the test base clamp with the bonding surface flush with the clamp front and the button on the vertical central axis. The notch must be centred over the button and flush against the tooth. A recommended trick from the standard: lower the crosshead slightly too low for the button to fit, then raise it slowly while gently pressing the specimen against the back of the crosshead until the button just slides into the notch.


Q11. How are pre-test failures handled?

A pre-test failure is recorded as 0 MPa — except where the operator inadvertently caused or contributed to the failure (e.g. the button was dislodged during de-moulding or while removing flash with a razor blade), in which case the specimen is excluded. This prevents labs from quietly discarding genuine early failures and inflating the mean.


Q12. What are the most common sources of error?

  • Allowing the dentine surface to dehydrate

  • Grinding too deeply into dentine (bond strength drops) or perforating the pulp chamber

  • Arching of the plastics mould (lifts it off the tooth and lets composite spread beyond the mould) — tighten only until half the wave spring is compressed

  • Over-filling the mould, or using a non-high-modulus / inconsistent composite

  • Applying shear, bending or rotational force when de-moulding

  • Using a crosshead without the thin curved lip edge


Q13. Why is ISO 29022 often preferred over tensile or other shear designs?

Because it produces the highest proportion of genuine adhesive failures — 41 % in that comparative study, versus 18 % for DIN 13990 and 4 % for the tensile test. An adhesive failure means you measured the interface; a cohesive failure in dentine means you measured the tooth. The authors concluded ISO 29022 is the method of choice for evaluating bond strength for that reason.


Q14. How does ISO 29022 relate to ISO/TS 11405?

ISO/TS 11405, Dentistry — Testing of adhesion to tooth structure (3rd ed. 2015, withdrawn 2019), is a guidance document covering substrate selection/storage plus tensile bond strength, marginal gap measurement, microleakage and clinical usage tests; its introduction explicitly names ISO 29022 as an important publication in the field. ISO 29022 is effectively the shear counterpart — a full normative test method rather than guidance.


Q15. What about microtensile testing?

The microtensile test (Sano et al.) was introduced to avoid cohesive failure of dentine and to obtain multiple specimens from one tooth. Because the tested area is much smaller (~1 mm²), microtensile values are typically higher than macro shear values, though the methods correlate and tend to rank materials in the same order. Both share the criticism that data scatter is high and many "interfacial" failures are not truly interfacial.


Q16. Can the method be used for materials other than adhesives?

Yes — with modification, it may be applied to adhesive restorative materials such as glass-ionomers, but users must evaluate its suitability for their particular application.


Q17. Who uses ISO 29022?

Dental materials manufacturers (R&D screening, formulation comparison, batch QC), contract and academic testing laboratories, and regulatory bodies / notified bodies — EN ISO 29022:2013 was adopted under the EU Medical Device Directive 93/42/EEC for documenting "adheres to tooth substance" claims.

< Previous: ISO 28580 Wheel Radial Load Fatigue Testing for Methods of measuring rolling resistance Single point test Passenger car truck, bus and motorcycle

> Next: ISO/TR 29381 Instrumented indentation test of Evaluation tensile properties

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you