ISO 20433 Crockmeter — Leather Colour Fastness to Crocking Test

Share:

ISO 20433 Leather Colour Fastness to Crocking Tester | UnitedTest

UnitedTest supplies ISO 20433 crocking testing machines for leather. This standard evaluates colour transfer from coloured leather via dry and wet rubbing tests, suitable for finished leather before and after surface treatments and coatings.

ISO 20433 Leather — Tests for colour fastness — Colour fastness to crocking. ISO 20433 specifies a method to determine how much colour is transferred from the surface of coloured leather to other surfaces by rubbing. Two tests are always run in parallel: one dry rubbing cloth, one wet rubbing cloth. It applies to all types of coloured leather, and — importantly — may be run before and/or after after-treatments and surface finishes, since these strongly influence colour transfer.


Test Principle

A white rubbing cloth (dry or wet) is fixed over a cylindrical finger and moved back and forth in a straight line over the leather surface under controlled load, stroke length, speed and number of cycles. The colour transferred to the white cloth ("crocking") is then assessed with the grey scale for staining. General colour-fastness testing principles follow ISO 7906. Note: what is graded is the staining of the cloth, not the colour change of the leather itself.


Test Specimen Info: 

Two representative test pieces, each not less than 140 mm × 50 mm — one for dry rubbing, one for wet rubbing (a fresh piece is used for each).

ISO 20433 Crockmeter — Leather Colour Fastness to Crocking Test


Test devie and equipment use for the ISO 20433 Crockmeter — Leather Colour Fastness to Crocking Test

Crocking test apparatus

Rubbing finger = cylinder of 16 mm diameter; linear reciprocating motion along a 100 mm ± 5 mm track; downward force 9 N

 (The Chinese version of the bilingual text gives tighter tolerances: 16 ± 0.1 mm and 9 ± 0.2 N.)

White cotton rubbing clothDesized, bleached, finish‑free cotton fabric complying with ISO 105‑F09, cut into ~50 mm × 50 mm squares.
Grey scale for staining assessmentConforms to ISO 105‑A03 for visual grading of staining.
Spectrophotometer / colorimeterInstrumental assessment device complying with ISO 105‑A04, usable for uniform‑stain samples as an alternative to visual evaluation.
Environment‑conditioning facilityTo condition leather specimens and rubbing cloth under standard atmosphere described in ISO 2419.


Test Parameters

Rubbing finger diameter16 mm
Applied downward force9 N
Reciprocating stroke length100 mm ± 5 mm
Rubbing cycles10 forward strokes + 10 backward strokes (10 crank turns total)
Crank operating speed1 turn per second
Wet‑cloth water pickupApproximately 100 % mass gain after soaking in distilled water
Wet‑cloth post‑treatmentAir‑dry at room temperature after crocking test
Pre‑conditioning duration≥24 h (standard conditioning atmosphere)


ISO 20433 Crockmeter — Leather Colour Fastness to Crocking Test Procedure:

  1. Secure each leather test piece flat on the instrument baseboard, with the test surface facing upward; align the specimen long axis parallel to the rubbing travel track.

  2. Dry crocking test: Mount dry cotton rubbing cloth onto the cylindrical finger. Run 10 crank turns (10 forward, 10 backward rubs) at one crank rotation per second with 9 N load. Remove rubbing cloth upon completion.

  3. Wet crocking test: Take a fresh conditioned cotton cloth, soak fully in distilled water to achieve ~100 % water pickup. Fit this wet cloth to the rubbing finger and use a brand‑new leather test piece. Perform identical rubbing cycles as dry test. Take off the cloth and air‑dry it at ambient room temperature.

  4. Stain preparation for evaluation: Gently brush or use clean adhesive‑tape sticky side to clear loose dust and fibre debris from both tested rubbing cloths; only dye‑caused discolouration is considered for grading.

  5. Staining evaluation: Place each used rubbing cloth backed by three layers of unused white rubbing cloth. Under suitable lighting, visually assess staining grade against the ISO 105‑A03 grey scale. If stain distribution is uniform, instrumental measurement following ISO 105‑A04 is permitted as an alternative evaluation method.

  6. Test report: Document standard reference ISO 20433, leather type description, evaluation method adopted, dry‑ and wet‑crocking staining grey‑scale ratings, any deviations from procedure, abnormal observations and test date.


Test Application (Industry Field)

  • Footwear (upper, lining, sock) — dark linings/socks staining socks and feet.

  • Leather garments and apparel, gloves — dye transfer onto light-coloured clothing.

  • Leather goods — handbags, belts, wallets, watch straps, small leather goods.

  • Automotive interiors — car seats, steering-wheel covers, trim rubbing onto light clothing.

  • Furniture/upholstery and contract interiors — seating, sofa covers.

  • Tannery and finishing QC and R&D — verifying dye fixation, comparing dyes/fatliquors, and running before/after finish or after-treatment comparisons; incoming-hide screening and supplier/lot release testing.


Related standard: 

AATCC TM8Colorfastness to Crocking (Wet & Dry)
AATCC 165Colorfastness to Crocking: Textile Floor Coverings-Crockmeter
ISO 105-X12Textiles - Tests for colour fastness - Part X12: Colour fastness to rubbing
ISO 105-X01Colour Fastness to Flat Abrasion, Related test for flat surface abrasion resistance
GB/T 3920Textiles - Tests for colour fastness - Colour fastness to rubbing
ISO 11640Leather colour fastness for repeated cyclic to‑and‑fro rubbing
ISO 7906Leather — Tests for colour fastness — General principles of testing
ISO 105-D02Textiles – Tests for colour fastness Part D02 : Colour fastness to rubbing : Organic solvents
ISO 20433Leather — Tests for colour fastness — Colour fastness to crocking
ISO 15701Leather colour fastness to migration into polymeric/plastic material (storage-contact bleeding, a different failure mode from rubbing).
ISO 11641Leather colour fastness to perspiration.
ISO 17700 (Method A)Footwear-specific rubbing/colour-transfer test for uppers, linings and insocks, often used by shoe brands.


Keywords: ISO 20433 crocking tester, leather crock fastness test, leather colour transfer test, dry wet rubbing colour fastness tester, finished leather crocking test, leather surface finish colour fastness, leather colour crocking test machine, UnitedTest leather colour fastness equipment, pigmented leather crock test, leather coating rubbing test

Related products and device

ISO 20433 Leather Colour Fastness to Crocking Tester

​Dual-station electric friction color fastness tester is suitable for testing the degree of color fading of fabrics and leather after rubbing. The test method involves using dry or wet white cotton cloth wrapped around a friction cone.

ISO 20433 dry wet rubbing colour fastness tester, finished leather crocking test

Colour fastness friction tester is suitable for textiles, knitwear, leather, electrochemical metal plate, printing and other industries. Conforms to ISO105x12 and GB3920-2008 standards, and is tested for color fastness friction performance.

Related Standard

ISO 105-X12 Textiles Tests for colour fastness to rubbing –

ISO 105-X12: Textiles -- Tests for colour fastness to rubbing

ISO 105-X12 specifies a method for determining the resistance of the colour of textiles of all kinds, including textile floor coverings and other pile fabrics, to rubbing off and staining other materials.

It evaluates a fabric's resistance to "crocking"—the transfer of color from a textile to another surface through rubbing. Whether it's a vibrant printed t-shirt, a woven carpet, or yarn-dyed upholstery, this test ensures that the color remains fast and does not stain other materials during everyday use. The standard accommodates both dry rubbing and wet rubbing tests, providing a complete picture of a textile's durability and color stability.  crockmeter, textile colour fastness to rubbing tester

ISO 105-D02 Textiles Colorfastness Test - Organic solvents –

ISO 105-D02 defines a uniform lab testing method to quantify textile colour resistance against combined mechanical rubbing plus organic solvent spot cleaning (hand-applied local stain removal with dry-cleaning solvents), excluding loose staple fibre as test object.


FAQs for ISO 20433 Leather Colour Fastness to Crocking Test

Q1: What is ISO 20433:2024?

ISO 20433:2024 (IULTCS/IUF 452:2024) is the latest international standard for leather colour fastness to crocking (rubbing‑off colour test). It replaces the old ISO 20433:2012. It measures how much dye transfers from coloured leather onto white cotton cloth under controlled dry and wet rubbing conditions.


Q2. What does "crocking" mean?

"Crocking" is the industry term for colour transfer by rubbing — dye, pigment, finish or buffing dust rubbing off a coloured surface onto a contacting material (clothing, socks, lining fabric, light-coloured leather or skin). ISO 20433 quantifies it by rubbing a standard white cotton cloth over the leather and grading how much the cloth is stained.


Q3. How big is the specimen and how is it prepared?

Two representative test pieces, each ≥ 140 mm × 50 mm (one for dry, one for wet). If starting from a whole hide/skin, sample first per ISO 2418. Both pieces and the dry rubbing cloth are conditioned ≥ 24 h under standard conditions per ISO 2419 (commonly 23 ± 2 °C, 50 ± 5 % RH).


Q4. Which products and industries require this test?

Footwear (uppers, linings, insocks), leather garments and gloves, leather goods (bags, belts, wallets, watch straps), automotive interiors (seats, steering wheel covers, trim), furniture/upholstery, and tannery/finishing QC and R&D.


Q5. Does it apply to all leather types?

Yes — the method applies to all types of coloured leather. Critically, it may be run before and/or after after-treatments and surface finishes, because finishes, fatliquors and topcoats strongly change the degree of colour transfer. This makes it a direct tool for comparing dye systems and finishing processes.


Q6. Can it be used on coated/synthetic leather or textiles?

The scope is leather. In practice the same crockmeter hardware also serves the textile methods ISO 105-X12 and AATCC TM8; results are simply reported against the standard that applies to the substrate. Footwear-specific variants use ISO 17700 Method A.


Q7. How many rubs?

10 turns of the crank = 10 forward + 10 backward strokes (20 traverses) over the 100 mm track at 9 N, at 1 turn/second. The same cycle count applies to both dry and wet rubbing.


Q8. How is the wet cloth prepared?

Weigh a conditioned cloth, wet it out thoroughly in distilled water until water pick-up ≈ 100 %, rub on a fresh test piece, then remove the cloth and dry it at room temperature before grading.


Q9. How is the result graded?

Grade the staining of the white rubbing cloth against the ISO 105-A03 grey scale: 5 = no staining, 1 = severe staining (half grades customary). Before grading, remove dust/fibres by light brushing or clear adhesive tape, back the cloth with three layers of unused white cloth, and view under suitable illumination. If staining is even, ISO 105-A04 allows instrumental grading.


Q10. What is a "pass" value?

ISO 20433 only tells you how to test — it sets no limits. Pass/fail comes from the buyer's spec, brand quality manual or product standard. Typical commercial expectations are dry ≈ 4 to 4–5 and wet ≈ 3 to 3–4, with lower targets accepted for suede, nubuck and deep aniline shades (e.g. suede dry 2.5–3, wet 2–2.5). Never accept "good fastness" wording — always require a numeric grey-scale grade.


Q11. Why is wet rubbing nearly always worse than dry?

Water swells the fibre/finish and mobilises unfixed dye and surface pigment, so more colour moves onto the cloth. That is why the wet rating is the number that shows up in real complaints — rain, humidity, sweat and cleaning are the realistic worst case.


Q12. ISO 20433 vs. ISO 11640 (VESLIC) — what's the difference?


ISO 20433 (crocking)ISO 11640 / IUF 450 (VESLIC)
Rubbing mediumwhite cotton clothundyed wool felt
Motionlinear, 100 mm trackshorter stroke (≈35–40 mm)
Load9 N500 g or 1000 g (5 N / 10 N)
Cyclesfixed: 10 back-and-forthset by product spec (e.g. dry 50, wet 20)
Wet mediawater (~100 % pick-up)water or artificial perspiration pH 8
Gradingcloth staining onlyfelt staining + leather colour change


Q13. Why is this test important for leather as a material?

  1. It predicts the #1 consumer complaint — dark leather staining light clothing, socks, linings, car seats or skin, which drives returns, claims and brand damage.

  2. It measures dye fixation and finish quality, not just shade — fatliquor, oil, pigment and topcoat levels all move the number.

  3. It lets tanneries run before/after finish comparisons, so finishing chemistry can be optimised objectively.

  4. It flags high-risk materials — aniline, semi-aniline, suede, nubuck and deep shades are the classic offenders.

  5. It produces a numeric, auditable, cross-border metric for supplier scorecards, incoming-hide screening and third-party lab release.


Q14. My crock images look like poor circles — what's wrong?

Per Annex A.3, abnormal circular crock images indicate a maintenance/alignment problem in the crocking apparatus (worn finger face, incorrect pressure, loose cloth, contaminated or non-flat specimen backing, worn abrasive base pad). Causes and corrective actions are detailed in AATCC TM8:2016. Check finger diameter, verify the 9 N load with a calibrated gauge, replace the base abrasive, and refit the cloth flat and taut.


Q15. Can one instrument cover ISO 20433, ISO 105-X12 and AATCC TM8?

Yes — all three use a 16 mm finger and 9 N load with a 100 mm-class stroke, so a compliant crockmeter with interchangeable finger/load kits typically covers them. ISO 11640 (VESLIC) requires a separate felt-based machine with 500 g/1000 g loading and a shorter stroke, so it is normally a second instrument.


Q16. ISO 20433 Crockmeter Leather Colour Fastness to Crocking Tester from UnitedTest? 

UnitedTest is professional manufacturer of ISO 20433:2024 crockmeter / leather colour fastness to crocking tester. Fully compliant with IULTCS IUF 452 standard for dry & wet rubbing‑off colour test for all coloured leather. Lab‑grade leather rubbing fastness testing equipment.


UnitedTest is a reliable manufacturer specialised in leather physical and colour‑fastness testing instruments. Our ISO 20433 crockmeter (colour fastness to crocking tester) is fully built to meet ISO 20433:2024 and IULTCS/IUF 452 requirements for leather dry and wet crocking test.

This lab‑testing machine simulates real‑world friction contact to measure colour transfer from dyed leather onto white cotton rubbing cloth. It strictly maintains standard parameters: 16 mm cylindrical rubbing finger, 9 N downward test force, 100 mm reciprocating stroke length and defined rubbing cycles.

Our leather crock fastness tester is widely used in tanneries, footwear factories, leather‑bag manufacturers, furniture‑leather producers, third‑party test laboratories and quality‑control departments. It helps you perform accurate dry‑crock and wet‑crock colour‑fastness evaluation for all coloured leather, verifying dyeing quality and surface‑finish performance to meet global buyer specifications.


UnitedTest testing instruments support visual grading with grey scale and connectable spectrophotometer for instrumental assessment as defined in ISO 20433. We provide complete solutions including machine installation, operation training, calibration guidance and after‑sales support for leather‑testing laboratories worldwide.

< Previous: None

> Next: ISO 21138-1 Plastics piping systems

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you