Metal Bending & Rebending Testing Machine

Metal Bending & Rebending Testing Machine

Model: UT1017A, ISO 7438, ASTM E290

UT1017 Metal Bending & Rebending Testing Machine is used for bending tests of metal materials such as rods, sheets and rebar for construction, and is loaded with two-way hydraulic cylinders, adjusting the roll spacing by hand wheels and being able to lock itself.
It is driven by a hydraulic power source, which consists of a test host, an oil source (hydraulic power source), a standard bending head and a control system, with a maximum test force of 400kN.

ISO 7438: Metallic materials — Bend test
ASTM E290: Standard Test Methods for Bend Testing of Material for Ductility
GB/T 232 etc.

General Introduction

UT1017 Metal Bending & Rebending Testing Machine is used for bending tests of metal materials such as rods, sheets and rebar for construction, and is loaded with two-way hydraulic cylinders, adjusting the roll spacing by hand wheels and being able to lock itself.
It is driven by a hydraulic power source, which consists of a test host, an oil source (hydraulic power source), a standard bending head and a control system, with a maximum test force of 400kN.


ISO 7438: Metallic materials — Bend test
ASTM E290: Standard Test Methods for Bend Testing of Material for Ductility
GB/T 232 etc.

Key Features

  • Features

1, The test machine is a four-pillar frame structure, the main cylinder is placed on, the main structure is composed of oil source, chassis, cylinder, piston, roller assembly, light bar, upper beam and other components.
2, The test machine uses highly sealed two-way cylinders, which are highly efficient and durable.

3, Test machine design in the aesthetic, convenient, safety aspects have been fully considered, for example: the main structure parts using ball-ink cast iron precision processing, the machine rigidity and good stability;
4, The branch roller spacing is adjusted by shaking the hand-lifting screw, and the spacing adjusts the rear roller self-locking without tightening, which is convenient to operate, which greatly reduces the labor intensity.
5, Bending head is the national standard GB/T232-2010 "metal material bending test method" designed for supporting products. This product is a special tool necessary for rebar bending test, and the replacement method is convenient for plug-in operation.
6, The one-in-one design of the forward and reverse bending device does not require repeated loading and unloading of the reverse bending device, which reduces the labor intensity and improves the efficiency, and the device conforms to the requirements of the reverse bending test in the standard GB1499.2-2018 Steel for Reinforced Concrete Part 2: Hot-rolled Rib Rebar.
7, Touch screen bending test control system, simple operation, small footprint, according to the test requirements to set the bending angle and automatically calculate the desired bending head diameter and roller spacing, manual and automatic dual mode selection, automatic mode can achieve the test process one-click operation (here is the control system legend).

Main Technical Specification

ModelUT1017A
Max. Load400KN
Working stroke350mm
Max. working pressure25Mpa
Bending angle range0-180 degrees   (angle can be set)
Suitable metal sample range6-32mm,  HRB400/HRBF400/HRB400E/HRBF400E   steel rebar
Bending round sample diameter6-50mm
Can be installed Bending head diameter6- 450mm
Bending roller max. distance620 mm
Cylinder loading speedMax. 90mm/min
Motor power1.1 Kw
Dimension1450×640×2000mm
Weight1200Kg


Main Accessories

ItemQuantity
Frame (double direction cylinder, pull wire sensor)1   set
Bending head (22 pcs)  6-192mm1   set
Diameter (mm): 24/ 30 /32   /40 /48 /50 /56 /60 /64 /70/72 /80/88/90/100/110/125/140/160/168/192
Bending head base4   pcs
Touching screen controller1   set
Safety cover1   set
Documents (Manual, packing list, certificate)


Standard

ISO 7438 Metallic materials Bending test details –

ISO 7438 is a standard that specifies a method for determining the ability of metallic materials to undergo plastic deformation in bending. It is used to evaluate the flexural strength and stiffness of a material , The bend test shall be carried out in testing machines equipped with a bending device with two supports and a former; bending device with a V-block and a former; bending device with a clamp. 

ASTM E290 Metal Bend testing of materials ductility –

ASTM E290 Standard Test Methods for Bend Testing of Material for Ductility


ASTM E290 is a destructive mechanical test standard that evaluates the ductility and structural soundness of metallic materials (and welds) by subjecting specimens to controlled bending deformationASTM International. It is a widely used quality control and qualification method for metals, alloys, and welded joints across industries.

ASTM A1064 Tension, Bend, Shear test for Steel Wire and Welded Wire Reinforcement, Plain and Deformed –

ASTM A1064 test standard covers steel wire and welded wire reinforcement produced from hot-rolled rod to be used for the reinforcement of concrete. The steel wire is cold-worked, drawn or rolled, plain (non-deformed, as-drawn or galvanized), or deformed. Welded wire reinforcement is made from plain or deformed wire, or a combination of plain and deformed wire.  It specifies four mandatory tests for plain/deformed carbon-steel wire and welded wire reinforcement (WWR) for concrete: Tension Test, Bend Test, Reduction of Area Test, and Weld Shear Strength Test. 