ASTM D3418 — Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization. ASTM D3418 uses Differential Scanning Calorimetry (DSC) to determine polymer transition temperatures and enthalpies of fusion and crystallization. It characterizes first‑order transitions (melting, crystallization) and second‑order glass‑transition behaviour for polymeric materials, supporting material identification, quality inspection, formulation development and thermal property evaluation in polymer laboratories.


Test principles: 

The specimen and an inert reference material are subjected to identical controlled heating‑cooling programmes under constant‑flow purge gas. The instrument continuously monitors the difference in heat input required to keep sample and reference at the same temperature.

  • Endothermic peaks correspond to melting (fusion, heat absorbed by sample).

  • Exothermic peaks correspond to crystallization (heat released by sample).

  • Glass transition shows a step‑like baseline shift instead of a peak, caused by changes in specific heat capacity. Peak areas are integrated to calculate transition enthalpy; characteristic temperatures are extracted from the DSC thermogram curves.

ASTM D3418 Polymers DSC Measuring Test


Test Specimen Information

FormsPowdered/granular, molded/pelleted, film/sheet
Cut sizeMicrotome, razor blade, hypodermic punch, paper punch, cork borer (No. 2 or 3), etc. — sized to fit the pan and hit target mass
Films> 40 µm → treat as molded specimens; ≤ 40 µm → cut slivers or punch disks
Referee testsMust be performed on films (§8.4)
Mass≈5 mg typical for first‑order transitions; ≈10 mg for glass transition; weighed to ±10 µg; avoid overloading
PanningCrimp a metal cover over the specimen to ensure intimate thermal contact; keep pan bottoms flat


Test Equipment for ASTM D3418 Polymers DSC Measuring Test:

Differential Scanning Calorimeter (DSC) 

  • Furnace system: controlled heating/cooling covering cryogenic temperature up to 600 °C.

  • Temperature sensor with accuracy of ±0.01 °C.

  • Differential heat‑flow sensor with minimum detection of 1 mW.

  • Purge‑gas supply system: gas flow 10‑50 ±5 mL/min (nitrogen, argon or helium are typical inert purge gases).

  • Temperature controller: ramp rate range 0.5‑20 °C/min, stability ±0.1 °C/min for dynamic runs; ±0.1 °C for isothermal holds.

  • Data‑recording device and integration software for peak‑area calculation.

  • Inert sample pans/crucibles to hold specimens.

  • Cooling accessory to achieve controlled cooling rates and sub‑ambient testing.

Analytical balancereadability ±0.0001 g for temperature testing; ±0.00001 g for enthalpy measurement.


Test parameters (key stipulations)

ParameterStipulation
Heating / cooling rate0.5–20 °C/min; preferred 10 or 20 °C/min; other rates allowed only if equivalency is demonstrated (Note 5)
Referee / dispute rateT_m and T_c at 10 °C/min; T_g at 20 °C/min
Purge gas flow10–50 ± 5 mL/min, same as used in calibration
Temperature program (melting)From ≥50 °C below to 30 °C above the melting temperature
Isothermal holds5 min after the preliminary heating, after cooling, etc.
Crystallization coolingCool to ≥50 °C below the peak crystallization temperature at the same rate as heating
Glass transitionQuench‑cool to ≥50 °C below the transition of interest; reheat at 20 °C/min (T_g is more pronounced at faster rates)
Enthalpy calculationFrom the second heating curve (10.1.8)
CalibrationTemperature per E967, heat flow per E968, at the same heating rate and with purge gas flowing


Test Application and limitations: 

  • Specification acceptance, process control and research on plastics

  • Resin producers and compounders: grade identification, lot release, crystallinity control

  • Packaging & film, automotive, aerospace (PEEK, PA), electrical/electronics, medical devices, fibers/textiles, additive manufacturing filaments, wire & cable, recycling and regrind verification

  • Polymer identification / fingerprinting of polymer alloys and additives; study of oxidation, curing of thermosets and thermal decomposition

  • Supported by DoD acceptance, so it is widely written into military/aerospace material specifications


General Test Procedures of ASTM D3418 Polymers DSC Measuring Test: 

A. First‑order transition (melting & crystallization)

  1. Purge gas on, flow identical to calibration.

  2. Load appropriate mass (≈5 mg), weighed to ±10 µg; crimp pan, flat bottom.

  3. Preliminary thermal cycle at the test rate: from ≥50 °C below to 30 °C above melting — erases prior thermal history (omitted only if it demonstrably destroys the transition of interest).

  4. Hold 5 min.

  5. Cool at the same rate to ≥50 °C below the peak crystallization temperature; record the cooling curve.

  6. Hold 5 min.

  7. Reheat at 10 or 20 °C/min; record the heating curve — this curve is used for enthalpy.

  8. Measure T_im, T_pm, T_em, T_ic, T_pc, T_ec; report two peak temperatures if present.

  9. In case of dispute, determine T_m and T_c at 10 °C/min.

B. Glass transition

  1. Purge gas on, same flow as calibration.

  2. ≈10 mg specimen, weighed to ±10 µg.

  3. Preliminary thermal cycle at 20 °C/min, from ≥50 °C below to 30 °C above melting.

  4. Hold 5 min (Note: shorter annealing times permitted if high‑temperature annealing degrades the polymer — must be reported).

  5. Quench cool to ≥50 °C below the transition of interest; hold 5 min.

  6. Reheat at 20 °C/min until all desired transitions are complete; if first‑ and second‑order transitions are measured in the same run, use the same rate as §10.1.8 and take results from the second heating.

  7. Measure T_ig, T_mg, T_eg; report the heating rate; in dispute, T_g at 20 °C/min.


Related Standards:

ASTM D3418

Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry

ISO 11357-1Plastics — Differential scanning calorimetry (DSC) — Part 1: General principles
ISO 11357-3Plastics — Differential scanning calorimetry (DSC) — Part 3: Determination of temperature and enthalpy of melting and crystallization
ISO 11357-6Plastics - Differential scanning calorimetry (DSC) - Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT)
ASTM E793Enthalpies of fusion and crystallization by DSC (-120 to 600); the enthalpy portion of ISO 11357-3 is stated to be equivalent to it
ASTM E794melting and crystallization temperatures by thermal analysis (DSC or DTA), calibrated per E967
ASTM E1356 assignment of the glass transition temperature by DSC/DTA; its recommended reporting value is also the midpoint temperature


Keywords: ASTM D3418 DSC tester, differential scanning calorimeter, polymer thermal analysis, glass transition temperature test, melting enthalpy test, crystallization enthalpy measurement, plastic thermal property tester, resin DSC analysis, polymer transition temperature test, UnitedTest thermal testing instrument, glass transition temperature test, melting temperature test polymer, heat of fusion test, crystallization temperature test, DSC testing machine, differential scanning calorimeter, plastic testing equipment, polymer QC testing, pipe material testing,OIT test DSC, polyolefin pipe testing, R&D thermal analysis lab equipment,DSC polymer testing, crystallinity measurement DSC, Tg test method plastics

Related products and device

ASTM D3418 differential scanning calorimeter

Oxidative Induction Time testing machine is kind of differential scanning calorimeter,, check the relation of temperature with the rate differential input in test sample and reference articles. used to do Oxidative Induction Time test, heat stability, glass transition temperature, melting point.

ISO 1408 Rubber Carbon content tester

Carbon black content tester is used to measure the carbon content in PE, PP, PB etc. , sample under nitrogen condition, through high temperature pyrolysis, then measure the weight to get the carbon level.

ISO 1408 Muffle Furnace

Ash Content Test Furnace (Muffle Furnace) analysis and determination and general small steel quenching, annealing, tempering and other heat treatment heating, high temperature furnace can also be used for metal, ceramic sintering, dissolution, analysis and other high temperature heating.

Related Standard

ASTM D2663 Carbon black dispersion test in Rubber –
ASTM D2663: Standard Test Methods for Carbon Black—Dispersion in Rubber
ASTM D2663 defines four independent test methods to quantify and qualify carbon black dispersion within vulcanized/unvulcanized rubber compounds. It describes four distinct test methods (A, B, C, D) with differing precision, equipment needs, and applicability.
Target materials: All carbon black-filled rubber elastomers (NR, IR, SBR, BR, IIR, EPDM, CR, silicone rubber), including vulcanized finished rubber products and unvulcanized mixing batches/masterbatches.
ASTM D412 Tensile Strength of Rubber and Elastomers –

ASTM D412 test methods cover procedures used to evaluate the tensile (tension) properties of vulcanized thermoset rubbers and thermoplastic elastomers. These methods are not applicable to ebonite and similar hard, low elongation materials. 

ASTM D412 is the primary standard for evaluating the tensile properties of vulcanized thermoset rubbers and thermoplastic elastomers (TPEs). It provides precise procedures for determining critical mechanical characteristics that define material performance under stretching forces. 

The methods appear as follows:

Test Method A—Dumbbell and Straight Section Specimens

Test Method B—Cut Ring Specimens

ISO 37 Tensile Test on Rubber, vulcanized or thermoplastic –

ISO 37 and ASTM D412 are both widely recognized tensile test methods designed to evaluate the stress-strain characteristics of various rubber materials, including natural rubber, synthetic rubber, silicone rubber, and thermoplastic elastomers (TPEs). While both standards aim to determine the tensile properties of rubber and elastomers, they differ in their specific methodologies and applications.

ISO 812 Low-temperature brittleness Impac Test of Rubber, vulcanized or thermoplastic –

ISO 812:2017 specifies a method for determining the lowest temperature at which rubber materials do not exhibit brittle failure or the temperature at which half of the test pieces used in a test fail when impacted under specified conditions.

The temperatures thus determined do not necessarily relate to the lowest temperature at which the material can be used since the brittleness will be affected by the conditions of test and especially by the rate of impact. Data obtained by this method are, therefore, intended to be used to predict the behaviour of rubbers at low temperatures only in applications in which the conditions of deformation are similar to those specified in the test.


ASTM D2137 Rubber Brittleness Point Test of Flexible Polymers and Coated Fabrics –

ASTM D2137: Standard Test Methods for Rubber Property--Brittleness Point of Flexible Polymers and Coated Fabrics


ASTM D2137 test method is used to evaluate the brittleness of rubber materials, or rubber coated fabrics, when exposed to low-temperature flex with an impact under specified conditions of striker speed. ASTM D2137 tests performed will be used to determine the lowest temperature at which rubber compounds will not show fractures or coating cracks when exposed to specified impact conditions.

Frequently Asked Questions (Q&A for ASTM D3418 DSC Test)

Q1. What is ASTM D3418?

A. ASTM D3418‑21 is the ASTM International test method for determining transition temperatures and enthalpies of fusion and crystallization of polymers by Differential Scanning Calorimetry (DSC). The current edition was approved 1 September 2021 (originally issued 1975; previous edition D3418‑15). It is under the jurisdiction of ASTM Committee D20 on Plastics, Subcommittee D20.30 on Thermal Properties, and is approved for use by U.S. Department of Defense agencies.


Q2. What exactly does ASTM D3418 measure?

A. Three families of results:

First‑order transition temperatures (melting and crystallization): T_im (melting extrapolated onset), T_pm (melting peak), T_em (melting extrapolated end), T_ic, T_pc, T_ec (crystallization equivalents).

Glass transition temperature: T_ig (extrapolated onset), T_mg (midpoint), T_eg (extrapolated end) — the midpoint T_mg is normally reported as T_g.

Enthalpies: heat of fusion and heat of crystallization, mass‑normalized and reported in J/g.


Q3. What is the temperature range covered by the method?

A. The normal operating range is from the cryogenic region up to 600 °C. Some equipment can extend beyond this. Above 400 °C, uncertain radiation losses may degrade accuracy.


Q4. Which materials can be tested?

A. Polymers in granular form or any fabricated shape from which a suitable specimen can be cut — pellets, molded parts, films and sheets. It is used for thermoplastics, and also detects chemical events such as oxidation, curing of thermosetting resins, and thermal decomposition. Important caveat: §6.8 states the method does not apply to all polymers as written — e.g. polyarylamides crystallize only from solution, and crystallizable polystyrene can only be annealed above its T_g.


Q5. Which purge gas is used, and why?

A. Typically 99+ % pure nitrogen, argon or helium, at 10–50 mL/min. A dry purge gas is recommended (and is essential for sub‑ambient operation) unless moisture effects are being studied. The gas prevents oxidative interference and must be flowing during both calibration and testing, at the same flow rate.


Q6. How is the DSC calibrated for this method?

A. Temperature signal per ASTM E967 and heat‑flow signal per ASTM E968, using the same heating rate as the test (preferably 10 or 20 °C/min) and with purge gas flowing. Some instruments allow simultaneous temperature + heat‑flow calibration — in that case follow the manufacturer's instructions and report the heating rate.


Q7. How much sample is needed?

A. About 5 mg for first‑order transitions (melting/crystallization) and about 10 mg for the glass transition, weighed to ±10 µg. Overloading must be avoided. Because only milligram quantities are used, the specimen must be homogeneous and representative.


Q8. How should specimens be prepared?

A. Powder/granules: avoid grinding unless the preliminary thermal cycle is performed — grinding introduces friction/orientation effects that alter thermal history.

Molded/pelleted: cut with a microtome, razor blade, hypodermic punch, paper punch, or No. 2/3 cork borer to fit the pan and reach the target mass.

Film/sheet: > 40 µm treated as molded specimens; ≤ 40 µm cut into slivers or punched disks.

Referee tests must be performed on films.

Specimens being compared should have approximately the same particle size.


Q9. Why is crimping the pan important?

A. intimate thermal contact between pan and specimen is essential for reproducible results. A metal cover is crimped against the pan with the sample sandwiched between, and pan bottoms must be kept flat. Poor contact produces broadened, shifted peaks and poor repeatability.


Q10. What is the standard heating/cooling rate?

A. The controller must support 0.5–20 °C/min; the standard prefers 10 °C/min or 20 °C/min. Other rates are permitted but the user must demonstrate equivalency. For referee/dispute cases: T_m and T_c at 10 °C/min; T_g at 20 °C/min.


Q11. Why is a "preliminary thermal cycle" (first heat) required?

A. Heating from at least 50 °C below to 30 °C above the melting temperature erases the specimen's previous thermal history so that all specimens start from a comparable state. It is followed by a 5 min hold. If the preliminary cycle demonstrably destroys or creates a transition of interest, it may be omitted — and this must be justified/reported.


Q12. Why are enthalpies calculated from the second heating curve?

A. The second heating (after a controlled 5 min hold, a controlled cool to ≥50 °C below the peak crystallization temperature, and another 5 min hold) represents a known, reproducible thermal history. The first heat still carries the unknown processing/annealing history of the as‑received sample, so its peak area is not a reliable basis for enthalpy.


Q13. Why is ASTM D3418 important for a material?

A. Because it fixes the numbers that determine how a polymer can be processed and used:

T_g defines the upper service temperature of amorphous polymers and the onset of rubbery behaviour — stiffness, dimensional stability and creep resistance collapse above it.

T_m sets the maximum use temperature and the minimum processing/melt‑processing temperature of semicrystalline polymers.

Heat of fusion converts into degree of crystallinity, which governs stiffness, barrier performance, chemical resistance, opacity and shrinkage.

First‑heat vs. second‑heat comparison exposes prior thermal history: annealing, quenching, orientation, residual stress and relaxation peaks.

It acts as a QC fingerprint for grade identification, blend/alloy verification, contamination and wrong‑grade detection, and flags side reactions (oxidation, crosslinking, curing, degradation).

It is rapid and cheap (a few milligrams, one scan), which is why it runs from R&D through incoming inspection to failure analysis.


Q14. What industries use ASTM D3418?

A. Plastics and polymer producers/compounders, packaging and film, automotive, aerospace (e.g. PEEK, PA), electrical and electronics, wire and cable, medical devices, fibres and textiles, construction/building products, additive‑manufacturing filament, and plastics recycling/regrind verification. The standard explicitly states it is useful for specification acceptance, process control and research, and because it is DoD‑approved it is widely written into military and aerospace material specifications.


Q15. What are the main sources of error?

A. Heating/cooling rate and final temperature (especially for enthalpy); impurities that form solid solutions or are miscible in the melt; radiation losses above 400 °C; particle‑size differences; oxidation when air‑sensitive specimens are not blanketed; non‑representative milligram sampling; and confusing degradation with a transition near the melting region. Toxic or corrosive effluents are also a safety consideration.


Q16. Which standards are referenced inside ASTM D3418?

A. E473 (Terminology: Thermal Analysis and Rheology), E1142 (Terminology: Thermophysical Properties), E967 (Temperature Calibration of DSC and DTA), E968 (Heat Flow Calibration of DSC), E691 (Interlaboratory Study / precision), E1953 (Description of Thermal Analysis and Rheology Apparatus), plus ISO 11357‑1, ‑2, ‑3.


Q17. How does ASTM D3418 relate to ISO 11357?

A. D3418 is similar but not equivalent to ISO 11357‑1 (general principles), ‑2 (glass transition temperature) and ‑3 (temperature and enthalpy of melting and crystallization). The ISO procedures provide additional information not supplied by D3418. The wider ISO 11357 family also covers specific heat capacity (‑4), reaction curve temperatures/enthalpies and conversion (‑5), oxidation induction time/temperature (‑6), crystallization kinetics (‑7) and thermal conductivity (‑8).


Q18. Why choose UnitedTest ASTM D3418‑21 Compliant Differential Scanning Calorimeter (DSC Machine)?

A. UnitedTest is professional manufacturer of ASTM D3418‑21 compliant Differential Scanning Calorimeter (DSC). Our DSC instruments accurately test polymer melting point Tm, crystallization temperature Tc, glass transition Tg, heat of fusion and crystallization enthalpy for plastic QC, R&D and incoming‑material inspection. Full support for ASTM E967, ASTM E968, ISO 11357 standards. Contact us for DSC solution.


UnitedTest is a trusted manufacturer and supplier of high‑performance differential scanning calorimeter (DSC) fully compliant with ASTM D3418‑21 Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry.

Our DSC testing equipment is purpose‑built for polymer laboratories, plastic factories, compounding plants, university research institutes and third‑party testing labs that need to run standardized ASTM D3418‑21 polymer thermal analysis.

✅ Main test capabilities following ASTM D3418‑21:

  • Measure melting extrapolated onset temperature, melting peak temperature \(T_{pm}\)

  • Measure crystallization onset & peak temperature \(T_{pc}\)

  • Detect glass‑transition temperature \(T_g\) (mid‑point, extrapolated onset & end)

  • Calculate heat of fusion (enthalpy of melting) and heat of crystallization (J/g)

  • Support full DSC test workflow: pre‑thermal cycle, controlled heating / cooling, isothermal hold, peak‑area integration.

✅ Instrument features matching ASTM D3418‑21 requirements:

  • Wide temperature range: cryogenic to 600 °C (extended temperature range optional)

  • Programmable heating / cooling rate: 0.5 °C/min ~ 20 °C/min, rate stability ±0.1 °C/min

  • High‑sensitivity differential heat‑flow sensor (1 mW resolution), high‑precision temperature sensor (±0.01 °C)

  • Controlled purge‑gas system: adjustable gas flow 10‑50 mL/min for nitrogen, argon and other inert gas

  • Supporting calibration workflow: compatible with ASTM E967 temperature calibration and ASTM E968 heat‑flow calibration

  • Powerful analysis software: auto‑integrate melting endotherm and crystallization exotherm peak areas, export full ASTM‑compliant test reports

  • High‑precision analytical balance for milligram‑level polymer specimen weighing.

✅ Typical application industries:Thermoplastic resin production, polymer compounding, plastic film & injection‑molded parts, polymer alloy / blend R&D, composite material, rubber & elastomer, new‑material laboratory, third‑party inspection laboratories.

✅ Supported related standards:ASTM D3418‑21, ASTM E473, ASTM E967, ASTM E968, ISO 11357‑1 /‑2 /‑3.

UnitedTest provides complete DSC instrument, installation, operation training and after‑sales support. If you are looking for reliable DSC machine to run ASTM D3418 polymer thermal transition test, please contact our engineering team for customized quotation and technical solution.

< Previous: ASTM D3410 Shear Loading compression Test for Polymer Matrix Composite Materials with Unsupported Gage Section

> Next: ASTM D3420 Test Method for Pendulum Impact Resistance of Plastic Film

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.