Information on the most widely used ASTM standards within the materials testing industry
Model: UT3500A, ISO 6964, ISO 1408
Carbon black content tester is used to measure the carbon content in PE, PP, PB etc. , sample under nitrogen condition, through high temperature pyrolysis, then measure the weight to get the carbon level. With feature of easy operation, working reliable, and result high accuracy.
General Introduction
Carbon Black Content Tester is used to determine carbon black content in geomembranes,Polyolefin(Polyethylene ,polypropylene and polybutene ) Pipes.
The test of carbon black is obtained through the analysis of the weight of the samples under the protection of nitrogen. The instrument has advantages of convenient operation, simple operation, accurate measurement, high precision and high automation.
Carbon Black Content Tester is also named Plastic Ash Content Tester;, Ash content test Polypropylene Plastic Ash Content or Carbon Black Purity Testing Machine. The Carbon black in plastic does not show significant enhancement effect, but it can improve its thermal deformation, dimensional stability, rigidity and hardness, etc.,
![]() | ![]() |
Key Features
1. The instrument has beautiful appearance and structure and simple operation;
2. Integrated design of heating furnace body and control system, convenient for user instrument management.
3. High degree of automation, only need to set the temperature value and heating time, the instrument automatically heats up to the set value;
4. High temperature control accuracy, large temperature range, high furnace temperature uniformity;
5. 7 inch LCD touch screen display, extremely friendly operation interface, can be started with one button
6. It has excellent constant temperature function, and can set the constant temperature time, and the constant temperature accuracy is high;
7. The instrument can set any group of different heating time periods, and can have different heating temperature, heating rate, and constant temperature time;
8. Can test 4 samples at a time, with the sample feeding holder.

9. The parameter display is comprehensive, showing the number of setting groups, theoretical.
ISO 1408:1995
Rubber — Determination of carbon black content — Pyrolytic and chemical degradation methods
ISO 6964: Polyolefin pipes and fittings -- Determination of carbon black content by calcination and pyrolysis -- Test method and basic specification.
IEC 60811-4-1: INSULATING AND SHEATHING MATERIALS OF ELECTRIC AND OPTICAL CABLES - COMMON TEST METHODS - PART 4-1: METHODS SPECIFIC TO POLYETHYLENEAND POLYPROPYLENE COMPOUNDS - RESISTANCE TO ENVIRONMENTAL STRESS CRACKING - MEASUREMENT OF THE MELT FLOW INDEX - CARBON BLACK AND.
ASTM D1603 Standard Test Method for Carbon Black Content in Olefin Plastics
ASTM D1619 Standard Test Methods for Carbon Black—Sulfur Content
Main Technical Specification
| Display mode | 7 inch capacitive touch screen |
| Quartz tube size | φ44×600±5mm |
| Furnace size | Φ45×300±5mm |
| Heating element | superalloy wire |
| Heating zone length | 250mm |
| Working temperature | room temperature ~ 1150°C |
| Temperature control | intelligent programmable control, can set the segmentation program |
| Air path control | two ways, program automatic switching |
| Data calculation | the software comes with calculation function, one-click calculation; It can automatically calculate the carbon black content and ash content |
| Cooling method | rapid cooling (≤20min, 900°C to room temperature) |
| Number of test samples | 4 samples at a time |
| Sample feeding holder | yes |
| Sensor sensitivity | 0.1℃ |
| Power | 220V, 50HZ |
Customized guide rail type sample holder, easy to take and place lofts; Open lid for quick cooling; With exhaust gas filter device; With exhaust gas filter device. | |
Main accessories
| Item | Quantity |
| Heating furnace | 1 set |
| Sample holder | 1 set |
| Burning boat | 5 pcs |
| Power wire | 1 pc |
| 10A Fuse | 5 pcs |
| Exhaust gas filtration | 1 set |
| Tool | 1 set |
| Documents (Manual, packing list, certificate) | |
Standard
ISO 1408: Rubber -- Determination of Carbon Black Content -- Pyrolytic and Chemical Degradation Methods
ISO 1408 specifies three methods for determining the carbon black content of rubber compounds: a pyrolytic method (A) and two chemical degradation methods (B and C). It provides precise procedures for quantifying carbon black, a critical reinforcing filler in rubber formulations.
ISO 6964 Polyolefin pipes and fittings -- Determination of carbon black content by calcination and pyrolysis -- Test method
ISO 6964 specifies three test methods for determining the carbon black content of polyolefin compositions used in pipes and fittings, and provides a basic specification for polyethylene pipes and fittings. Carbon black is a critical additive in these materials, primarily used as a UV stabilizer to prevent degradation from sunlight exposure. Accurate determination of its content is essential for quality control, product performance, and compliance with material specifications.
IEC 60811-4-1:2004 specifying five specialized test methods for polyethylene (PE) and polypropylene (PP) compounds used as insulating and sheathing materials in electric and optical fiber cables for power distribution, telecommunications, shipboard, and offshore applications.
Test Methods specific to polyethylene and polypropylene compounds – Resistance to environmental stress cracking – Measurement of the melt flow index – Carbon black and/or mineral filler content measurement in polyethylene by direct combustion - Measurement of carbon black content by thermogravimetric analysis (TGA) – Assessment of carbon black dispersion in polyethylene using a microscope.
ASTM D1603 Standard Test Method for Carbon Black Content in Olefin Plastics
ASTM D1603 measuring carbon‑black content in olefin‑based plastics (polyethylene, polypropylene, polybutylene), It adopts inert‑atmosphere pyrolysis‑gravimetric measurement to quantify carbon‑black mass percentage. It is not suitable for materials containing extra non‑volatile inorganic fillers, brominated flame‑retardant additives, or acrylic/polar‑monomer‑modified polymers which would interfere accuracy.
IEC 60811‑605 Electric and optical fibre cables‑Test methods for non‑metallic materials‑Part 605: Physical tests‑Measurement of carbon black and/or mineral filler in polyethylene compounds
IEC 60811‑605 describes the test methods for measuring the content of carbon black added for UV stabilization of polyethylene and polyolefin compounds. These methods are not suitable for halogenated compounds. Method A is suitable only for polyethylene and polypropylene compounds. Method B is suitable for polyolefine compounds. Target measurand the carbon black content (%) and/or mineral filler content (%).
Carbon Black Content Tester Operation Video