ISO 9854 Pendulum impact strength by the Charpy method
Date:2017-03-21 Source:United Test Views:100

ISO 9854: “Thermoplastics pipes for the transport of fluids -- Determination of pendulum impact strength by the Charpy method”

Specifies the general test method to be used for the determination of the impact strength of unnotched test pieces cut from thermoplastics pipes for the transport of fluids. Not intended to be a reference test method for the determination of the impact strength of pipes. May be used for scientific research, materials testing or the examination of pipes when it is not possible to take measurements in accordance with the reference method.

Charpy Test: The specimen is mounted horizontally and supported unclamped at both ends. The hammer is released and allowed to strike through the specimen. If breakage does not occur, a heavier hammer is used until failure occurs.


Charpy pendulum impact test operation video
Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X