Electronic Charpy Impact Testing Equipment ASTM D6110 , Charpy Impact is a single point test that measures a materials resistance to impact from a swinging pendulum. Charpy impact is defined as the kinetic energy needed to initiate fracture and continue the fracture until the specimen is broken. The values obtained can be used for quality control or to differentiate general toughness.
United Test product both the IZOD and Charpy impact tester, in dial display, LCD screen display and computer control used determine the impact ductility of nonmetallic materials, such as Rigid thermoplastic and thermosetting plastic, thermosetting plastic and thermoplastic after fiber-reinforced. It is widely used in the industries of plastic products, plastic manufacture, petro chemical etc, University, scientific research institute and commodity inspection department.
Charpy Test: The specimen is mounted horizontally and supported unclamped at both ends. The hammer is released and allowed to strike through the specimen. If breakage does not occur, a heavier hammer is used until failure occurs. 
 
IZOD Test: The specimen is clamped into the pendulum impact test fixture with the notched side facing the striking edge of the pendulum. The pendulum is released and allowed to strike through the specimen. If breakage does not occur, a heavier hammer is used until failure occurs. Since many materials (especially thermoplastics) exhibit lower impact strength at reduced temperatures, it is sometimes appropriate to test materials at temperatures that simulate the intended end use environment. 
Feature of XJJD series LCD Display Charpy pendulum impact testing machine: 
1, LCD display, Charpy Test model;
2, Adopts rotate encoder grating side angle technology, high accuracy, high reliability, and big measuring range;
3, Support vice, pendulum is nickel coating, good appearance and anti-corrosion.
4, Standard ISO 179, ASTM D6110, ISO 9854.
5, Indicate impact energy, impact strength, initial angle, rising angle, energy loss etc.,
6, Automatic correcting the energy loss; Auto-print and save the records. 
   
 Plastic V notch impact sample 80*10*4mm             Organic glass V notch impact sample 80*10*4mm
The Charpy impact test, also known as the Charpy V-notch test, is a standardized high strain-rate test which determines the amount of energy absorbed by a material during fracture. This absorbed energy is a measure of a given material's notch toughness and acts as a tool to study temperature-dependent ductile-brittle transition.
| Model | XJJD-5 | XJJD-50 | 
| Impact energy | 1J, 2J, 4J, 5J | 7.5J, 15J, 25J, 50J | 
| Impact speed | 2.9m/s | 3.8m/s | 
| Pendulum initial angle | 160° | 160° | 
| Pendulum center to specimen center distance | 221mm | 380mm | 
| Specimen span | 40,60,70,95(mm) | |
| Supporting blade angle radius | R=1mm | |
| Supporting blade included angle | 30° | |
| Impact blade angle radius | R=2mm | |
| Power | 220V, 50HZ | |
| Display type | LCD display | |
| Specimen clamping type | Charpy | |
| Standard Accessories | Loadframe, pendulum(1J, 2J, 4J, 5J), supporting vice jaws, specimen centering plate, spanner, power cord, manual etc. | Loadframe, pendulum(7.5J, 15J, 25J, 50J), moving supporting base, specimen centering plate, spanner, power cord, manual etc. | 
Loadframe,
pendulum,
supporting vice jaws,
specimen centering plate,
spanner,
power cord,
manual etc.
ISO 179: “Plastics -- Determination of Charpy impact properties”
ASTM D6110: “Standard Test Method for Determining the Charpy Impact Resistance of Notched Specimens of Plastics”
ISO 180: “Plastics -- Determination of Izod impact strength”
ASTM D256: “Standard Test Methods for Determining the Izod Pendulum Impact Resistance of Plastics”
ISO 9854: “Thermoplastics pipes for the transport of fluids -- Determination of pendulum impact strength by the Charpy method”
ISO 8256: "Plastic Stretch Impact Intensity Determination" (method A)
ASTM D1822: "Plastic And Electric insulation Material Stretch Impact Performance test Method".



 
            