Your current locationHome>Application>Standard>Other
Application
Other
ISO 8256 Plastics — Determination of tensile-impact strength test machine
Date:2019-12-25 Source:United Test Views:100

ISO 8256 Plastics — Determination of tensile-impact strength test machine, plastic tensile impact tester


ISO 8256:2004 specifies two methods (method A and method B) for the determination of the tensile-impact strength of plastics under defined conditions. The tests can be described as tensile tests at relatively high strain rates. These methods can be used for rigid materials (as defined in ISO 472), but are especially useful for materials too flexible or too thin to be tested with impact tests conforming to ISO 179 or ISO 180.


tensile impact.png

These methods are used for investigating the behaviour of specified specimens under specified impact velocities, and for estimating the brittleness or the toughness of specimens within the limitations inherent in the test conditions.


These methods are applicable both to specimens prepared from moulding materials and to specimens taken from finished or semi-finished products (for example mouldings, films, laminates, or extruded or cast sheets).


Results obtained by testing moulded specimens of different dimensions may not necessarily be the same. Equally, specimens cut from moulded products may not give the same results as specimens of the same dimensions moulded directly from the material. Test results obtained from specimens prepared from moulding compounds cannot be applied directly to mouldings of any given shape, because values may depend on the design of the moulding and the moulding conditions. Results obtained by method A and method B may or may not be comparable.

tensile impact test operation video
Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X