ISO 6259-3 Thermoplastics pipes -- Determination of tensile properties -- Part 3: Polyolefin pipes
Date:2018-08-29 Source:United Test Views:100

ISO 6259-3 Thermoplastics pipes -- Determination of tensile properties -- Part 3: Polyolefin pipes

ISO 6259-3:2015 specifies a method of determining the tensile properties of polyolefin (polyethylene, cross-linked polyethylene, polypropylene, and polybutene) pipes, and the following properties: the stress at yield and the elongation at break.

Sample size:
Type 1 Dog bone : 150mm length, 20mm width
Type 2 Dumbell :  115mm length, 20mm width
Type 3:  250mm length

Pipe thickness less 5mm, use type 2 sample.
5-12mm thickness, use type 1 sample.
12-25mm thickness, use type 1 sample or type 3 sample.
large than 25mm thickness, use type 3 sample.




Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X