ISO 527-3 is a common international standard that is used to determine the tensile properties of plastic film or sheeting - a plastic test specimen with a thickness less than 1 mm. The tensile properties include tensile strength, yield strength, yield strain, strain at break, and in some cases Young's Modulus. Due to the flexible, delicate nature of these plastic specimens, both gripping and strain measurement can be a challenge.

Refer UnitedTest single column electronic universal testing machine
, load range 100N ~ 5Kn.   because thin test sample, recommend the pneumatic side-action grips.

    