UT2089B Elmendorf Tearing Tester is designed for the tearing test of films, sheets, flexible PVC, PVDC, waterproof films, woven materials, polypropylene, polyester, paper, cardboard, textiles and nonwovens.
Standard: ISO 6383-2-1983, ISO 1974, GB/T16578.2-2009, GB/T 455, ASTM D1922, ASTM D1424, ASTM D689, TAPPI T414
What is Elmendorf Tear testing?
Elmendorf Tear testing determines the force required to continue the tearing of an initial cut in sheet materials such as paper, plastic film, textile and non-woven.
Principle: Lift the pendulum up to a certain height to give it an initial potential energy. The pendulum tears the specimen while swinging down. Computer calculates the decreased energy caused by tearing to obtain the required force for tearing
Features:
Full touch screen control, automated and electronic measurement, easy to operate quickly
Pneumatic clamping of the sample, automatic cutting of the sample, automatic release of the pendulum, and automatic reset of the pendulum after testing greatly improve efficiency and effectively avoid system errors caused by human factors
The computer level adjustment auxiliary system can ensure that the instrument is always in the best testing state
Can be equipped with multiple sets of swing body capacities to meet different testing needs
Professional software supports data output from multiple testing units
Standard RS232 interface, convenient for external system access and data transmission.

Specimen installation.
Measuring range | 0~6400g (800g, 1600g, 3200g, 6400g) |
Tearing force arm | 104±1mm |
Tear initial angle | 0° |
Tearing distance | 43±0.25mm |
Cut length | 20mm |
Longitudinal displacement of incision | 8mm |
Paper clip size | 25*15mm |
Maximum clamping area | 6.48cm2 |
Clamping torque ratio | 2.2:0.7 |
Free swinging quantity | min≥20,mid≥25,stand≥35. |
specimen size | (63±0.5 )mm x( 50±2)mm |
Blade force arm ratio | 14:5.5 |
Tear offset | Less than 10mm of the blade extension line |
Distance between paper grippers | 2.8±0.2mm |
Clamping method | Dual cylinder pneumatic clamping, automatic paper cutting, automatic release of pendulum during testing, automatic pendulum reset after testing, automatic data capture, etc |
air pressure | 0.4~0.6mpa |
HMI | 7-inch touch screen display operation, modular integrated thermal sensing function |
Size | 460mmx400mmx560mm |
Weight | About 40kg |
Item | Quantity |
Tester Frame | 1 set |
Basic pendulum testing weights | 1 set |
calibration weights | 1 set |
Power cord | 1 pc |
Documents (Manual, packing list, certificate) | |
ASTM D295, ASTM D689, ASTM D751, ASTM D752, ASTM D4247, ASTM D1424, ASTM D1922, ASTM D5734
TAPPI T414, TAPPI T496
BS 2782, BS 4253, BS 4468
CPPA D.9
DIN 53862, DIN 53128
ISO 1974, ISO 6383-2, ISO 9290, ISO 13937-1
EN21974
SCAN P11