ISO 1167 Thermoplastics pipes -- resistance to internal pressure
Date:2017-02-19 Source:United Test Views:100

ISO 1167 : 2006
Thermoplastics pipes, fittings and assemblies for the conveyance of fluids -- Determination of the resistance to internal pressure.

This test method specifies a general test method for determining the resistance to internal hydrostatic pressure at a given temperature of thermoplastics pipes, fittings and piping systems for the transport of fluids. The method accommodates water-in-water, water-in-air and water-in-liquid tests.

UnitedTest supply the HYD series Pipeline hydrostatic pressure testing machine, according to ISO 1167, ASTM D1598, ASTM D1599. It’s mainly used to test the plastic pipeline, compound pipeline, such as PP-R, PP-B, PP-A, PVC, PE, PE-X etc. Under a stipulated constant hydrostatic pressure force, keeping provision time; or inside the pipe, apply a constant and rapid hydraulic pressure to make the specimen broken in a short period time, check the max. pressure force, then calculate the ring stress. This tester is necessary equipment for plastic pipe manufacturer.

\   \ 
\   \

 

Related products
contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X