- Introduction
- Specification
- Accessories
- Standard
- LEAFLET & VIDEO
- Contact Us
The constant temperature water tank is a crucial piece of equipment for hydrostatic pressure tests, particularly for long-term and burst tests. It is designed to maintain a constant pressure and temperature during testing, which is essential for accurately assessing the strength and durability of pipes under sustained conditions.
Feature of water tank:
1, Constant-temperature tank is composed of 304# stainless steel interior and aluminum alloy/steel plate outer plate, no corrosion,
2, Imported circulation pump, high accuracy heater and temperature holding system;
3, Rigid and thick heat insulation polyurethane foam, and temperature proof layer to ensure the temperature and energy keeping performance, avoid energy loss.
4, For big tank, the cover of tank equipped with automatic lifting device, more reliable and convenient;

Water tank suitable for 710mm large pipe in customer pipe hydrostatic pressure testing laboratory.
ISO 1167: Thermoplastics pipes, fittings and assemblies for the conveyance of fluids -- Determination of the resistance to internal pressure;
ASTM D1598: Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure;
ASTM D1599: Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings
Main Specification of constant temperature tank:
| Time count range | 1~9999h 59min 59s | |
| Time display accuracy | 1s | |
| Constant temperature media box temp. | Ambient temperature to 95℃ 15℃ to Ambient temp. with cooling unit | |
| Temp. indication accuracy | ±0.5℃ | |
| Power supply | 380V AC 50HZ, 3 phase | |
| Pipe sample diameter range | 10-2000mm (Customized) 1/2" - 24" | |
| Model | HYD-B | HYD-C |
| Display type | Digital meter & PC software both | Touching screen & PC software both |
| Working station | 1 to 20 working stations | |
| Burst test | All stations can execute the burst test | |
| Hydrostatic pressure test | All stations can execute the long-term hydrostatic pressure test | |
| Max. pressure | 0 ~ 10Mpa (100 bar) / 0 ~ 20Mpa (200 bar) | |
| Constant pressure accuracy | -1%, +2% | |
| Pressure resolution | 0.001Mpa | |
| Time count range | 1~9999h 59min 59s | |
| Time display accuracy | 1s | |
| Constant temperature media box temp. | Ambient temperature to 95℃ 15℃ to Ambient temp. with cooling unit | |
| Temp. indication accuracy | ±0.5℃ | |
| Power supply | 380V AC 50HZ, 3 phase | |
| Pipe sample diameter range | 10-2000mm (Customized) 1/2" - 24" | |
Related products:
1, Constant temperature water tank (max. 95 degree)
2, Cooling machine
3, End closure, end caps for pipe, pipe fittings (10mm to 2000mm)
| Constant temperature tank (stainless steel interior) include the heater, circulation pump, pneumatic lifting rod etc., | 1 set |
ISO 1167: Thermoplastics pipes, fittings and assemblies for the conveyance of fluids -- Determination of the resistance to internal pressure;
ASTM D1598: Standard Test Method for Time-to-Failure of Plastic Pipe Under Constant Internal Pressure;
ASTM D1599: Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings;
ASTM D2837,ISO1167, ASTM D1598, ASTM D1599, ASTMD1784,ASTM D2466,ASTM F442, ASTM D2672,ASTM D2837,ASTM D2992,ASTM D2517,ASTM D2241,ASTM D3139,ASTM D3212,ASTM D2846,ASTM D2846M