what's tear strength test by trapezoidal method for Geosynthetics, Tearing Strength of Geotextiles
Date:2025-06-12 Source:United Test Views:100

what's tear strength test by trapezoidal method for Geosynthetics, Tearing Strength of Geotextiles, ASTM D4533. 


An outline of an isosceles trapezoid is marked on a rectangular specimen and cut. A small tear is introduced on one side of the specimen. The nonparallel sides of the trapezoid marked on the specimen are clamped in parallel jaws of a tensile testing machine. The separation of the jaws is initiated and increased so the tear propagates across the specimen. The force is measured throughout the test. 

1749699511921.png

Number of Test Specimens: 10 machine direction 10 cross machine direction

Test Specimen Size: 3" x 8"

Keywords: Tearing, trapezoidal tear


For more information or details, please contact us:

Email: export@unitedtest.com 

whatsapp: +8613911165373


Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X