Home >> Products >> Industrial Specialized Testing >> Various Testing >> Geotextile - Geocells testing machine
Geotextile - Geocells testing machine

Geotextile - Geocells testing machine

Model: UT1069G (geogrid tensile shear, peeling, splitting test)

Geotextile - Geocells testing machine, also name geocells (geogrid) X-type splitting tensile testing machine is mainly used for tensile, compression, bending strength and other mechanical properties testing and analysis of geosynthetics and various metals and non-metallic materials.


Geocells testing machine is used to measure the geotextiles strength of internal structural junctions; 1,tensile shear test 2, peeling test,  3, splitting test 4, Local overstressing Test, conform with standard ISO 13426. 


General introduction

Geotextile - Geocells testing machine, also name geocells (geogrid) X-type splitting tensile testing machine is mainly used for tensile, compression, bending strength and other mechanical properties testing and analysis of geosynthetics and various metals and non-metallic materials. It can automatically obtain ReH, ReL, Rp0.2, Fm, Rt0.5, Rt0.6, Rt0.65, Rt0.7, Rm, E and other test parameters, and can be tested and provided data according to international standards such as GB, ISO, DIN, ASTM, JIS and so on.

Geocells testing machine is used to measure the geotextiles strength of internal structural junctions; 1,tensile shear test 2, peeling test,  3, splitting test 4, Local overstressing Test, conform with standard ISO 13426. 

Especially the ISO 13426-1:2019 Geotextiles and geotextile-related products,  Strength of internal structural junctions — Part 1: Geocells

For Geocells strength test
1,tensile shear test

图片.png

2, peeling test, 

3, splitting test
图片.png
4, Local overstressing Test 


Performance characteristics of geocell X-type tensile testing machine: This product uses high-strength light rods to fix the upper beam and work table, so that it constitutes a high rigidity portal frame structure. It adopts servo motor drive, and the servo motor drives the moving beam up and down through the transmission mechanism to realize the test loading process. 

Key Features

  • Splitting test procedure

All test methods are performed at a constant strain rate of 20 mm/min.
At the beginning of the test, adjust the distance between the jaws to ±3mm of the required specimen length.
The specimen is mounted in the center of the jaws. Note that the length of the specimen should be parallel to the direction of the force.
Start the pull machine and continue until the sample is destroyed. Stop the device, record and report the maximum load with an accuracy of 2% of the full-scale reading. Reports the corresponding displacement in millimeters, with one decimal place reserved.

Main technical specification

Load capacity10KN/20KN/30KN/50KN
Frame proof load capacity200 ~ 150% of rate capacity
Multiple load cell in one   machine functionYES
Load AccuracyClass 1/0.5 according   ISO7500-1
Load cell overload capacity150% of rate capacity
Load measuring resolution1/500000 FS, stepless
Position / displacement   resolution0.001mm
Crosshead travel1200mm
Tensile test space700mm
Compression test space800mm
Effective testing width   (Clearance between columns)500mm
Standard tensile test   fixtureManual wedge type
Wedge tensile fixture Flat   specimen range0-20mm
Wedge tensile fixture Flat   specimen rangeΦ4-Φ20mm
Compression platen diameterΦ100mm
Testing speed range0.001 mm/min~500   mm/min, stepless, adjustable arbitrarily(Optional max. 1000mm/min)
Weight450Kg~600kg
Standard Power220/110V, 50/60HZ, 1 phase
Analysis softwareSmartTest English version
Working systemMS Win10 / Win11
Frame structureStandard: Dual test spaceOptional: Single test space

Main accessories (Standard delivery with machine)

High Stiffness Frame1   set
Servo driving system:Servo   motor:1   set
Loadcell:  1   set
Decelerator and deceleration system1   set
Leading screw:1   set
Wedge tensile test fixture1   set
Compression test fixture(Φ100mm)1   set
Professional testing software(SmartTest, English version)1   set
Computer1   set
Printer1   set
Documents (Manual, packing list, certificate)