Home >> Products >> Test Fixtures >> Tensile >> Webbing test fixture
Webbing test fixture

Webbing test fixture

ASTM D6775, ISO 283, KS K 0411

Webbing test fixture used for tensile testing of the webbing, belt test sample, determine the webbing, belt tensile strength, elongation etc., Webbing is a strong fabric woven as a flat strip or tube of varying width and fibres often used in place of rope. It is a versatile component used in climbing, slacklining, furniture manufacturing, automobile safety, auto racing, towing, parachuting, military apparel, load securing, and many other fields.


Tensile testing of webbing / belt / tapes materials involves the testing of flat strips of high-strength woven material used in various applications ranging from sporting goods to military apparel and seat belts. or high performance aramids (Kevlar) and ultra-high molecular weight polyethylene (Dyneema). The woven design without cut fiber at the edges results in a lightweight and strong product. When used in critical applications, such as safety seat belts, it is essential that tensile properties of webbing materials are understood. For example, the material should not have excessive elongation and should have consistent tensile strength properties. Therefore, conducting a tensile test on webbing materials is an important part of product design and manufacture.

General introduction

Webbing test fixture used for tensile testing of the webbing, belt test sample, determine the webbing, belt tensile strength, elongation etc., Webbing is a strong fabric woven as a flat strip or tube of varying width and fibres often used in place of rope. It is a versatile component used in climbing, slacklining, furniture manufacturing, automobile safety, auto racing, towing, parachuting, military apparel, load securing, and many other fields.


Tensile testing of webbing / belt / tapes materials involves the testing of flat strips of high-strength woven material used in various applications ranging from sporting goods to military apparel and seat belts. or high performance aramids (Kevlar) and ultra-high molecular weight polyethylene (Dyneema). The woven design without cut fiber at the edges results in a lightweight and strong product. When used in critical applications, such as safety seat belts, it is essential that tensile properties of webbing materials are understood. For example, the material should not have excessive elongation and should have consistent tensile strength properties. Therefore, conducting a tensile test on webbing materials is an important part of product design and manufacture.

Webbing capstan grips incorporate an ingenious double capstan design which provides fast, easy loading with a gripping action that results in proper breaks in the full gauge length of the specimen.


The key to the ease of loading is the use of an inner and outer capstan.
The specimen is loaded simply by inserting one end into the groove of the inner capstan and cranking it through 360 degrees.

Specification

Load capacity: 20KN, 50KN, 100Kn, 200KN.
Gripping width: 50mm/ 100mm

Roll diameter: 30 ~ 50mm

Max. sample thickness: 5mm

Weight: 14Kg


Standard

ASTM D6775 Tensile Test Textile Webbing, Tape, Belt –

ASTM D6775 specifies how to determine breaking strength and optionally elongation at a specified force (EASF) of textile webbing, tape, and braided materials, using a split-drum type clamping assembly in a tensile testing machine.

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.