Home >> Products >> Test Fixtures >> Tensile >> Geotextile wide-width strip tensile test grip
Geotextile wide-width strip tensile test grip

Geotextile wide-width strip tensile test grip

ASTM D4595, ISO 10319

General introduction

Geotextile wide-width strip tensile test grip used to determine the geosynthetics material mechanical strength, matched with an universal testing machine. 

Geosynthetics are synthetic products used to stabilize terrain. They are generally polymeric products used to solve civil engineering problems. This includes eight main product categories: geotextiles, geogrids, geonets, geomembranes, geosynthetic clay liners, geofoam, geocells and geocomposites. The polymeric nature of the products makes them suitable for use in the ground where high levels of durability are required. They can also be used in exposed applications. Geosynthetics are available in a wide range of forms and materials. These products have a wide range of applications and are currently used in many civil, geotechnical, transportation, geoenvironmental, hydraulic, and private development applications including roads, airfields, railroads, embankments, retaining structures, reservoirs, canals, dams, erosion control, sediment control, landfill liners, landfill covers, mining, aquaculture and agriculture.


Geotextiles are typically used to reinforce embankments to prevent catastrophic occurances such as mudslides during rainstorms. During an event such as a storm, soils will expand once they absorb water. These soils will begin to break apart at only 1-2% strain, therefore most geotextiles are designed to expand slightly without compromising the integrity of the entire woven fabric.

Geotextile wide-width strip tensile test gripGeotextile wide-width strip tensile test grip


Description of Test
An 8" wide specimen is gripped across its entire width in the clamps of a constant rate of extension (CRE) type tensile testing machine operated at a prescribed rate of extension applying a longitudinal force to the specimen until the specimen ruptures. Tensile strength, elongation, initial and secant modulus, and breaking toughness of the test specimen can be calculated from machine scales, dials, recording charts, or an interfaced computer.

Preferred Test Sample Size
3' x roll width
Number of Test Specimens
6 machine direction 6 cross machine direction
Test Specimen Size
12" x 8"
Keywords
wide-width, tensile, elongation, modulus

Specification

Load: 10Kn, 50Kn, 100Kn.

Specimen width: 50mm, 100mm, 200mm

Standard

ISO 6237 Tensile Shear Test for Wood-to-Wood Adhesive Bonds –

ISO 6237 Adhesives – Wood-to-wood adhesive bonds – Determination of shear strength by tensile loading.

ISO 6237 specifies a laboratory method for determining the shear strength of wood-to-wood adhesive bonds using a standard specimen loaded in tension under strictly defined conditions of preparation, conditioning, and testing. It is intended only for adhesives used in bonding wood to wood in either parallel-laminated or cross-laminated construction, and is not intended for testing manufactured/finished products.

ASTM D906 Tensile Shear Test for Plywood Adhesive Bonds –

ASTM D906 Standard Test Method for Strength Properties of Adhesives in Plywood Type Construction in Shear by Tension Loading

ASTM D906 specifies a tensile-loading method for determining the comparative shear strength of wood-to-wood adhesives in plywood-type (three-ply cross-laminated) construction. It measures comparative shear strength of wood-to-wood adhesives exclusively for cross-laminated plywood-style three-ply veneer assemblies. Not designed for finished consumer wood products or parallel single-grain laminated joints.

ISO 10591 Adhesion properties of sealants after immersion in water –

ISO 10591 Building and civil engineering sealants‑Determination of adhesion/cohesion properties of sealants after immersion in water

ISO 10591 evaluating how water exposure affects the bond and internal strength of mainly plastic‑behaviour sealants used in building and civil‑engineering joints. The standard is intended for sealants with predominantly plastic behaviour (e.g. many gunnable mastics/non‑elastomeric joint fillers), not primarily for highly elastic structural sealants, although similar joint‑durability concepts apply.

ASTM D624 Rubber & Elastomer Tear Strength Test –

ASTM D624 Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers

ASTM D624‑00(R2020) defines laboratory procedures to measure tear strength, the resistance of vulcanized rubber and thermoplastic elastomers (TPE) against crack initiation and crack propagation under tensile loading. Tear failure originates at stress‑concentrated sites such as cuts, notches or material defects. Five different specimen geometries (Type A, B, C, T, CP) are provided, which produce non‑interchangeable test results, as each geometry creates different stress states.