Home >> Products >> Test Fixtures >> Tear >> Tearing Strength Test of Fabrics
 Force-extension test curve display of UnitedTest UTM running ASTM D4533 trapezoid tear strength test for nonwoven geotextile
ASTM D4533 geotextiles tearing test machine

Tearing Strength Test of Fabrics

ASTM D4533

ASTM D4533 Tearing fixture is suitable for determining the tearing strength of geosynthetic materials using the trapezoidal method, specifically the tearing force required to initiate and subsequently propagate a tear from an initial incision under specified conditions. It is applicable to various types of geotextiles and impermeable geomembranes. It complies with the standards set forth in ASTM D4533/D4533M-15(2023)(Test Method) Standard Test Method for Trapezoid Tearing Strength of Geotextiles; JTG E50-2006 "Method for Testing Geosynthetic Materials in Highway Engineering" and GB/T13763-2010 "Determination of Tearing Strength of Geosynthetic Materials Using the Trapezoidal Method." 


UnitedTest supply the testing machine with tear fixure to meet ASTM D4533 test method that determines the tear strength of geotextiles by the trapezoid procedure using a constant-rate-of-extension-type (CRE) tensile testing machine. Tear strength is the capacity of a material to withstand the tearing force required to propagate a tear after its initiation. The trapezoid tear produces tension along a reasonably defined course such that the tear propagates across the width of the specimen. The method can be used to analyze the relative tear resistance of different fabrics or different directions in the same fabric.

General introduction

ASTM D4533 Tearing fixture is suitable for determining the tearing strength of geosynthetic materials using the trapezoidal method, specifically the tearing force required to initiate and subsequently propagate a tear from an initial incision under specified conditions. It is applicable to various types of geotextiles and impermeable geomembranes. It complies with the standards set forth in ASTM D4533/D4533M-15(2023)(Test Method) Standard Test Method for Trapezoid Tearing Strength of Geotextiles; JTG E50-2006 "Method for Testing Geosynthetic Materials in Highway Engineering" and GB/T13763-2010 "Determination of Tearing Strength of Geosynthetic Materials Using the Trapezoidal Method." 


UnitedTest supply the testing machine with tear fixure to meet ASTM D4533 test method that determines the tear strength of geotextiles by the trapezoid procedure using a constant-rate-of-extension-type (CRE) tensile testing machine. Tear strength is the capacity of a material to withstand the tearing force required to propagate a tear after its initiation. The trapezoid tear produces tension along a reasonably defined course such that the tear propagates across the width of the specimen. The method can be used to analyze the relative tear resistance of different fabrics or different directions in the same fabric.

Specification

1, Clamping width: 78mm

2, Connection thread: M12

3, Dimensions: 180*150*120mm

4. Weight: 5.3kg

Standard

ASTM D4533 Trapezoid Tearing Strength Test of Geotextiles –

ASTM D4533 test used to measure the force required to continue or propagate tearing in woven or non-woven geotextiles, using the trapezoidal method for testing. The trapezoidal tearing method is a test that generates tension along a reasonably defined path, allowing the tear to propagate across the width of the specimen. The trapezoidal tear strength of woven fabrics is mainly determined by the characteristics of the yarns clamped in the fixture.

ASTM D5587 Fabric Trapezoid Tear Strength Test –

ASTM D5587 Standard Test Method for Tearing Strength of Fabrics by Trapezoid Procedure.

ASTM D5587 defines a trapezoid tear procedure for measuring fabric tearing strength. It measurement of the tearing strength of textile fabrics by the trapezoid procedure using a recording constant‑rate‑of‑extension (CRE) tensile testing machine. It applies to most fabrics — woven fabrics, air bag fabrics, blankets, napped fabrics, knitted fabrics, layered fabrics, pile, and nonwovens — whether untreated, heavily sized, coated, resin‑treated or otherwise treated, and it gives instructions for testing dry or wet specimens.

Two result calculations are offered: single‑peak force and the average of the five highest peak forces. 


ASTM D6077 Leather Trapezoid Tear Strength Test –

ASTM D6077 Standard Test Method for Trapezoid Tearing Strength of Leather

ASTM D6077 defines a trapezoid‑method test to measure the tearing load of leather materials. Wet‑blue leather is excluded from this test scope. It quantifies exactly that: the force required to propagate a tear across a trapezoid‑shaped leather specimen. 


ASTM D2261 Tongue Tear Test for Fabric Tearing Strength –

ASTM D2261 Standard Test Method for Tearing Strength of Fabrics by the Tongue (Single Rip) Procedure (Constant-Rate-of-Extension Tensile Testing Machine)

ASTM D2261 measure fabric tearing strength via the tongue (single‑rip / trouser‑shaped) specimen approach, primarily using a Constant‑Rate‑of‑Extension (CRE) tensile tester, It evaluates the force required to propagate an existing pre‑cut tear rather than the force needed to start a brand‑new tear in intact fabric. Applies to most fabrics: woven, air bag fabrics, blankets, napped, knit, layered, pile and nonwovens — untreated, heavily sized, coated, resin-treated or otherwise treated.


ISO 13937-2 Trouser Method Fabric Tear Force Testing –

ISO 13937-2 Textiles – Tear properties of fabrics – Part 2: Determination of tear force of trouser‑shaped test specimens (Single tear method).

ISO 13937-2 is method for determining the tear force required to propagate an already-started single tear, using a rectangular specimen slit into two "trouser legs". Mainly for woven fabrics; may also apply to fabrics made by other techniques (e.g. some nonwovens). Not applicable to knitted fabrics, woven elastic fabrics, highly anisotropic fabrics, or loose fabrics where the tear tends to transfer from one direction to another. Only CRE (constant-rate-of-extension) machines are permitted.


Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.