Home >> Products >> Impact Testing Machine >> Sample Preparation Machine >> Test specimen Injection molding machine
Test specimen Injection molding machine

Test specimen Injection molding machine

Model: UT2075E, for tensile, impact test specimen

Electrical Test Sample Injection Moulding machine is small version of production machine. Used to produce the plastic test sample for tensile, impact etc., It is small, Easy to move, suitable for laboratory, classroom teaching and small sample making.

The product includes mold clamping parts, sol injection parts, the host body, heating system, control system and motor driving leading screw to loading. Prepare the tensile, dumbbell shape, impact, bending, HDT/VICAT etc., test specimen sample. 

It has the advantages of simple structure, easy handling, electricity and raw material saving, non-noise and non-pollution, can be used at any places with 220V power supply.

General introduction

This Electrical Test Sample Injection Moulding machine is small version of production machine. It is small, Easy to move, suitable for classroom teaching and small sample making.

The product includes mold clamping parts, sol injection parts, the host body, heating system, control system and motor driving leading screw to loading. Prepare the tensile, dumbbell shape, impact, bending, HDT/VICAT etc., test specimen sample. 
Test specimen Injection molding machine

It has the advantages of simple structure, easy handling, electricity and raw material saving, non-noise and non-pollution, can be used at any places with 220V power supply.


Key Features

  • Key Features

Compact design and space saving

Rugged stainless steel body and hard anodized aluminum frame structure;

All electric water free cooling system;

Fully automatic precision sensor;

Injection speed control ensures the filling rate of the mold cavity;

Electronic temperature control system is adopted for temperature control and adjustment;

Touch screen for easy operation and control, automatic cycle counting;

Each injection cycle does not exceed 30 seconds (the mold opens and ejects parts every 30 seconds);

Simple operation, less mold opening cost and low operation cost.

Main technical specification

ModelUT2075E
Screw dia.(mm)20mm
Heating zone3
Injection volume (g)10-80g
Max. mold size(mm)120x120x100
Mold opening stroke (mm)100
Diameter of clamping screw rod (mm)20mm
Motor86 steps
Clamping force (T)3T
Machine size (mm)850x350x380
Machine weight80kg
Machine power supply(V)AC220V
Main componentsElectrical and control system: OmronPLC and touchable screen: Rexay brandMachine frame: Aluminum alloy profile