Information on the most widely used ASTM standards within the materials testing industry
Model: QK-20, Manual
QK-20 notch sample reparation machine is used to process the non-metal material impact test specimen notch, such as the plastics, organic glass etc., it’s an ideal notching machine for plastic impact test. Surface with nickle coating, more reliable.
General introduction
QK-20 notch sample reparation machine is used to process the non-metal material impact test specimen notch, such as the plastics, organic glass etc., it’s an ideal notching machine for plastic impact test. Surface with nickle coating, more reliable.
ISO 179: “Plastics -- Determination of Charpy impact properties”
ASTM D6110: “Standard Test Method for Determining the Charpy Impact Resistance of Notched Specimens of Plastics”

Key Features
Manual cutting; Easy operation.
Notch Machining Function: Can machine V-shaped (angle 45°, notch depth 2mm, etc.) and U-shaped (radius 0.25mm, 0.5mm, etc.) notches according to standard requirements (such as ISO, ASTM, GB/T, etc.).
Precision Positioning Function: Equipped with sample positioning devices and size adjustment mechanisms to ensure accurate control of the notch position, depth, and angle.
ISO 179: “Plastics -- Determination of Charpy impact properties”
ASTM D6110: “Standard Test Method for Determining the Charpy Impact Resistance of Notched Specimens of Plastics”
ISO 180: “Plastics -- Determination of Izod impact strength”
ASTM D256: “Standard Test Methods for Determining the Izod Pendulum Impact Resistance of Plastics”
Plastic Manufacturing Companies: Used for incoming raw material inspection, production process quality monitoring, and finished product testing to ensure that the product meets impact performance standards.
Research Institutions: In the development of plastic material formulations and modification studies, used to prepare standard samples and evaluate the optimization effects on material impact performance.
Testing Agencies: Used by third-party testing laboratories for sample preparation when undertaking plastic product quality testing services, ensuring the fairness and accuracy of test reports.
University Laboratories: Used in teaching experiments and research projects in materials science, polymer materials, and related fields, providing equipment support for student practice and academic research.
Main technical specification
| Cutting stroke | 20mm |
| Notch blade | A: 45°±1° R=0.25±0.05mm B: 45°±1° R=1.0±0.05mm C: 45°±1° R=0.1±0.02mm |
| Dimension | 460*250*240mm |
| Weight | N.W.: 28kg, G.W.: 35kg |