Slow strain rate (SSRT) stress corrosion (SCC) tensile testing machine ASTM G47, ASTM G129.
Slow strain rate (SSRT) stress corrosion (SCC) testing machine is used to conduct corrosion tensile tests on materials in corrosive environments, mainly to study the stress corrosion sensitivity of metal materials in corrosive solutions.
The frame structure is in the form of a frame, and the loading unit is flexibly installed at the upper or lower end according to the test requirements to adapt to the test requirements of different media environments. The environmental medium is a solution medium under low temperature and normal pressure. The experimental kettle is generally made of high borosilicate glass, which not only reduces the equipment cost, but also ensures the corrosion resistance to general media.
Test function:
Ordinary tensile test
Constant load creep/stress corrosion test
Slow strain rate tensile test
Low-cycle fatigue/corrosion fatigue test
Specimen crack germination and crack propagation rate measurement test
Constant K control, rising K control, lower K control test
Features:
1) High rigidity heavy duty frame;
2) The equipment structure is simple, convenient for experimental expansion, tension and bending shear, can be used
3) The use of sensor force measurement, large speed ratio deceleration system as an afterburner mechanism, electric adjustment space, ease of operation due to the lever type host
4) High-performance all-digital servo loading control system, high speed control accuracy;
5) Double deformation sensor can be used, and the specimen deformation measurement accuracy is high;
6) Pressure balancing device;
7) Integrated STC800 measurement and control system, easy to expand and use;
Test Standard
1) ASTM G47-98 Standard Test Method for Determining Susceptibility to Stress-Corrosion Cracking of 2XXX and 7XXX Aluminum Alloy Products.
2) ISO 7539-7-2005 Corrosion of metals and alloys – Stress corrosion testing Part7: Method for slow strain rate testing
3) ASTM E606 Standard Test Method for Strain-Controlled Fatigue Testing, ASTM International, West Conshohocken
4) ASTM E647 Standard Test Method for Measurement of Fatigue Crack Growth Rates
5) ASTM E399 Standard Test Method for Linear-Elastic Plane-Strain Fracture Toughness K1c of Metallic Materials
6) ASTM G111 Guide for Corrosion Tests in High Temperature or High Pressure Environment, or Both
7) ASTM G47-98 Standard Test Method for Determining Susceptibility to Stress-Corrosion Cracking of 2XXX and 7XXX Aluminum Alloy Products
8), ASTM G129 - 00(2006) Standard Practice for Slow Strain Rate Testing to Evaluate the Susceptibility of Metallic Materials to Environmentally Assisted Cracking
Maximum test force | 50kN |
Test force range | 1% to 100% F.S |
Relative error of test force indication | ±0.5% |
Maximum moving range of loading head | 80mm |
Loading head movement speed | 1mm/s~1x10-7mm/s |
Load head displacement measurement accuracy | ±0.5% |
Loading head displacement resolution | 0.05μm |
Deformation measurement range | 0~20mm |
Deformation measurement resolution | 1 μm |
Deformation measurement accuracy | ±0.5% |
Experimental kettle operating temperature | room temperature ~ 65 °C (optional) |
Maximum operating pressure of the experimental kettle | 0.1MPa (optional) |
Experimental kettle volume | not less than 3L |
Item | Quantity |
Frame | 1 set |
Load cell (USA Celtron) | 1 set |
Servo motor (FUJI/Panasonic) | 1 set |
Test fixture | 1 set |
Raster displacement sensors | 1 pc |
Software and control card system | 1 set |
Computer | 1 set |
Documents (Manual, packing list, certificate) | |
1) ASTM G129 - 00(2006) Standard Practice for Slow Strain Rate Testing to Evaluate the
Susceptibility of Metallic Materials to Environmentally Assisted Cracking
2) ASTM E647 Standard Test Method for Measurement of Fatigue Crack Growth Rates
3) ASTM E399 Standard Test Method for Linear-Elastic Plane-Strain Fracture Toughness K1c of Metallic Materials
4) ASTM G111 Guide for Corrosion Tests in High Temperature or High Pressure Environment, or Both
5) ASTM G47-98 Standard Test Method for Determining Susceptibility to Stress-Corrosion Cracking of 2XXX and 7XXX Aluminum Alloy Products
6) ISO 7539-7-2005 Corrosion of metals and alloys – Stress corrosion testing Part7: Method for slow strain rate testing